Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can


Field trials of wood preservatives in UC3 retention. Part 1. Durability results after 13 years in and above ground
2010 - IRG/WP 10-30548
In 1996 an extensive field trial program was set up in order to obtain more data on wood treated with chromium and arsenic free preservatives in Use Class 3 retention. Apart from durability in and above ground, other features were also assessed, e.g. discoloration by staining fungi, depletion of active ingredients, weathering and corrosion of fasteners in con¬tact with the treated wood. Wood spec...
M Westin, J Jermer, M-L Edlund, P Larsson Brelid, I Johansson


The Effects of Natural Weathering on the Properties of Heat Treated Alder Wood
2010 - IRG/WP 10-40484
Heat treatment is an effective method to improve the dimensional stability and biological durability of wood. The heat treatment technology and the heat treated wood products were recently introduced to Turkey. However, only a few studies have been reported on the effect of natural weathering on the properties of heat treated wood in both Turkey and the world. In this study, heat treated alder (Al...
S Yildiz, Ü C Yildiz, E D Tomak


Hydrothermal modification for upgrading the durability properties of soft deciduous wood
2010 - IRG/WP 10-40494
To extend the application potentialities of soft deciduous wood, upgrading the durability properties, hydrothermal modification (HTM) of aspen alder and birch wood was investigated. The treatment was conducted in a multifunctional laboratory device WTT. In the previous cases it has been found that the treatment at 160oC improves the durability insufficiently. The modification at 180oC ensured a hi...
B Andersons, I Andersone, V Biziks, I Irbe, J Chirkova, E Sansonetti, J Grinins, H Militz


Ecological methods and products for wood protection used for restoration and conservation of built heritage cultural assets to increase natural durability and duration of exposure in open air museums
2010 - IRG/WP 10-40506
Wood is a perishable material, hygroscopic and fuel, which cause attention to selecting the wood species that is going to be exhibited in relation to humidity and soil. With variable depending on its humidity and moisture from the atmosphere or soil, wood is a good living environment for fungi and insects, but suffer biodegradation processes and dimensional changes. Observations over time on wood ...
M Pruna, D Purice, D Dumitru Copacean


Direct estimation of the durability of high-pressure steam modified wood by ESR-spectroscopy
2010 - IRG/WP 10-40508
Heat generated persistent free radicals have been detected by electron spin resonance measurement of thermally modified wood, prepared by high pressure superheated steam treatment. The specific density of these radicals have been correlated with the durability against basidiomycetes, as measured by the European standard EN113 test. In the lower range of specific radical densities, the found correl...
W Willems, A Tausch, H Militz


Durability of heat treated Malaysian bamboo Gigantochloa scortechinii strips
2010 - IRG/WP 10-40514
Bamboo is one of the fastest growing plants and can be used for various products. In tropical countries such as Malaysia bamboo is abundantly available at reasonable prices, therefore it is used for numerous purposes. However, bamboo (as a lignocellulosic material) is susceptible to fungal and insect attack and it is difficult to protect by preservative treatment. Heat treatment is an option to im...
N Kamarudin, K Sugiyanto


Moisture dynamics of WPC as basis for biological durability
2010 - IRG/WP 10-40520
The largest market for wood-polymer composites (WPCs) is currently decking. Although many products are commercially available, a proper standard for the assessment of the biological durability of WPC does not exist. Recommended standards for testing resistance against basidiomycetes should be completed with a method to bring the specimens in a worst case situation, obtaining a moisture level high ...
N Defoirdt, J Van Acker, J Van den Bulcke


Biological degradation of acetylated wood after 18 years in ground contact and 10 years in marine water
2010 - IRG/WP 10-40522
This paper addresses the resistance to biological degradation of acetylated wood. Firstly, it presents results from an EN 252 test after 18 years’ exposure. The test is still running in Nordic NWPC test fields, Simlångsdalen in Sweden and Viikki in Finland. Results from this test were presented after 5 years’ exposure ( IRG/WP 97-30139), and showed that the resistance of acetylated wood wit...
P Larsson Brelid, M Westin


Testing of decay resistance of sapwood and heartwood of thermally modified Scots pine and Norway spruce
2010 - IRG/WP 10-40523
Thermal modification at elevated temperatures changes the chemical, biological and physical properties of wood. One of the main targets of thermal modification is to increase the biological durability and decay resistance of wood. Although the effects of thermal modification on wood have been widely studied, the significance of sapwood and heartwood on the resistance of thermally modified wood has...
H Viitanen, S Metsä-Kortelainen


Effect of Nano-Silver Treatment on Densified Wood Properties. Part One: Swelling, Recovery Set, Bending Strength
2010 - IRG/WP 10-40533
In this research the effect of Nano-Silver treatment on compressed wood properties, was studied. Wood specimens were cut from Popolus alba (poplar) and impregnated with Nano-Silver and water. Then the saturated samples were compressed through radial direction in a hot press under pressure of 6 MPa, for 1 and 4 hours. The temperatures of press were 150°C and 175°C. Swelling (24h), recovery set ...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khaje


Deterioration of wooden heritage in outdoor exposure in Romania
2010 - IRG/WP 10-40535
The paper contains a study of the deterioration of wooden heritage in Romania, in outdoor exposure. Romania belongs to the few countries having a rich heritage of this kind. A quantitative image of this heritage reveals the 1,350 objectives transferred and reconstructed in 16 open-air museums, over 1,500 wooden churches, more than 4,000 buildings and technical facilities, historical monuments ...
L Bucşa, C Bucşa


Comparative Study of Heat Treatment of Beech Wood in Hot Water and Steam Medium
2010 - IRG/WP 10-40536
Heat treatment of wood is an effective method to improve the dimensional stability and durability against biodegradation. Heat treatments of beech wood in 2 different mediums (hot water and steam) in 180ºC were compared in physical, mechanical and anatomical properties. Mass loss in hydrothermally treated wood was higher than hygrothermally treated samples. Mechanical properties (MOR, MOE and CS)...
A Talaei, K Yaghoobi, A N Karimi


Natural durability of wood tested in different environments in Northern Europe
2011 - IRG/WP 11-10747
Moisture is often recognised as a key factor regarding the long time performance of wooden products, and one of the main challenges for timber products is to predict accurate service life in use class 3 (not covered above ground) and use class 4 (in soil or fresh water contact). A range of durability classification studies have been performed both in field and laboratory. But for several wood spec...
P O Flæte, G Alfredsen, F G Evans


Methods of field data evaluation - time versus reliability
2011 - IRG/WP 11-20466
Field testing of wood and wood-based products is so far the most reliable way to get information on performance with respect to durability and expected service life. However, field trials are extremely time and cost consuming. The main objective of the present study was to investigate possible correlations between early stages of decay, preferably during the first 5 years, and the actual service l...
P Larsson Brelid, C Brischke, A O Rapp, M Hansson, M Westin, J Jermer, A Pilgård


Improving our understanding of moisture and other durability-related properties of wood in building envelope performance prediction
2011 - IRG/WP 11-20468
Building science has become an increasingly important field in recent years with rapid changes in construction methods, building materials and consumer expectations. The field has also been brought to prominence by a few large-scale premature building envelope failures in a few regions across the world. Considerable effort has been put into developing hygrothermal models to simulate heat, air, vap...
Jieying Wang, P Morris


A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


ISPM No. 15 and the Incidence of Wood Pests: Recent Findings, Policy Changes, and Current Knowledge Gaps
2011 - IRG/WP 11-30568
Largely as a result of international trade, hundreds of species of bark- and wood-infesting insects have become established in countries outside their native range. Many of these exotic insects have caused severe economic and environmental impact to urban and forest trees in the receiving countries. Most bark- and wood-infesting insects have been transported to new countries by means of the wood...
R A Haack, E G Brockerhoff


The potential of propolis and other naturally occurring products for preventing biological decay
2011 - IRG/WP 11-30575
The potential of using a range of naturally occurring plant extracts and propolis from bee hives for enhancing the durability of timber in service as well as helping with the conservation of archaeological timbers is considered in this paper. Results reported demonstrate that there is some degree of protective effect noted, suggesting a viable treatment option might be developed based on a deeper ...
D Jones, N Howard, E Suttie


The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon


The resistance to Basidiomycetes fungi of chipboard 35 years after their industrial preservation with wood preservative on fluoroborate basis
2011 - IRG/WP 11-40546
The research on wood-based panels’ (WBP) behaviour towards fungi impact demonstrated rather low resistance of wood-based materials to wood rotting fungi. However, these materials are used in construction under conditions favourable to fungi growth. In such conditions WBP treated with wood preservatives should be used. Preservation durability is of great importance in such cases. The resistance o...
A Fojutowski, A Kropacz


Study of the durability of the Maderon® against wood decay fungi and insects
2011 - IRG/WP 11-40548
Many industries produce residues that are not easily degradable. One of these is nut husks which, due to their high level of resistance to biological and environmental degradation, have become an ecological problem. Maderón® is a material invented and patented in Spain employed as an ecological substitute and a modern alternative to certain uses of wood. At present, Maderón® is commercialized ...
M T Troya, F Llinares, P Jiménez, J I Fernández-Golfín, M Conde, R Díaz


Effects of Heat-Treatment in Hot Water and Steam Mediums on Gas Permeability of Beech Wood
2011 - IRG/WP 11-40557
Heat-treatment, as a major method of wood modification, improving dimensional stability, and natural durability, has been studied greatly from different aspects. The effect of heat-treatment on gas permeability, as an important physical property of wood, in two different mediums of hot water and steam, as well as in two buffers of 7 and 8, is the main topic of the present study. Hydrothermal treat...
H Reza Taghiyari, A Talaei, A Karimi


Utilization of thermodesorption coupled to GC-MS to study kinetics of thermodegradation of different wood species
2011 - IRG/WP 11-40559
Thermdesorption coupled to Gas Chromatography coupled to Mass Spectroscopy (TD-GC-MS) has been investigated to identify volatile degradation products generated during wood heat treatment by mild pyrolysis. For this purpose, wood samples of different softwood and hardwood species have been heat treated under nitrogen for different temperatures comprised between 180 and 230°C during 15 min. in the ...
K Candelier, M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin