The preliminary evaluation of selected sulfonium salts for use in wood preservation
1984 - IRG/WP 3278
Five sulfonium compounds, including two sulfonium methosulfates, one sulfonium bromide and two amphoteric sulfonium propanesulfonates, were prepared in crude form and subjected to various biocidal screening tests. A rapid screening test in which treated Pinus radiata pulp pellets were exposed to one of three wood-decaying fungi growing on malt agar revealed that dodecyl dimethyl sulfonium methosul...
D V Plackett


Biological degradation resistance of pine wood treated with dimethylol compounds
1989 - IRG/WP 3528
The study reports the increase of dimensional stability and biological degradation resistance of pine wood (Pinus sylvestris L) after impregnation with dimethyloldibydroxyethyleneurea. Decay resistance was determined according to BS 838:961. Nearly complete protection against Coniophora puteana, (Schum.ex Fr. Karst) weight loss of 2-3% was shown when modification, expressed as weight gain, exceede...
C L Videlov


Characterization of glycopeptide from white-, brown- and soft rot fungi
2002 - IRG/WP 02-10424
Extracellular low-molecular-weight substances that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radicals have been isolated from wood degrading cultures of white-rot, brown-rot, and soft-rot fungi. They contained protein, neutral carbohydrate, and Fe(II). These substances were glycosylated (glycated) peptides and suggested to form Amadori product (ketoamine). The...
H Tanaka, S Itakura, A Enoki


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


Fungicidal properties of boron containing preservative Borosol 9
2004 - IRG/WP 04-30348
The fungicidal properties of new boron containing wood preservative Borosol 9 is described in this paper. These properties were of particular interest as this new boron containing preservative, exhibit very good performance against wood damaging insects. But because the tested boron formulation contain also nitrogen compounds, we wanted to verify if nitrogen as a nutrient could promote...
G Babuder, M Petric, F Cadež, M Humar, F Pohleven


Evaluation and approval of wood preservatives in Japan
1988 - IRG/WP 2303
Japanese standardized decay test methods, performance requirements and approving system are briefly described. JIS (Japanese Industrial Standard) A 9302, which is related to a testing method for evaluating effectiveness of wood preservatives when applied to pressure treatment, is fundamentally a sand-block laboratory test method. According to performance requirements in JIS A 9201, mean percentage...
K Tsunoda


Effect of felling time related to lunar calendar on the durability of wood and bamboo -Fungal degradation during above ground exposure test for 2 years- (Preliminary report)
2005 - IRG/WP 05-20311
Current study was carried out to know whether the felling time of trees and bamboos based on lunar calendar affects natural durability of felled wood-bamboo or not. Each of one sugi (Cryptomeria japonica) tree of 28 years old and one Moso bamboo (Phyllostachys heterocycla) of around 3 years old was cut 12 times between February and December in 2003. Six sets of sugi tree and bamboo were felled in ...
K Yamamoto, S Uesugi, K Kawakami


Soil chemistry and wood decay
1978 - IRG/WP 2109
Soil is a most complex biological, chemical and physical material; its study is effectively a separate branch of science but almost entirely in relation to ist ability to grow plants - this paper is intendet just to note some known facets that might have relevance to the decay of wood and the performance of wood preservatives....
E A Hilditch


Electronic noses for detection of rot in wood
1996 - IRG/WP 96-20098
In an ongoing project an electronic nose is being studied and developed for detection of volatile organic compounds (VOC) emitted from wood colonised and decayed by fungi. The electronic nose consists of an array of gas sensors with different selectivity patterns for different groups of volatile organic compounds (VOC). The use of pattern recognition routines implemented by artificial neural netwo...
K Nilsson


Effect of soft-rot decay on the static bending strength of wood
1991 - IRG/WP 2361
In this study, a modified static bending test has been developed as a method for measuring soft-rot decay in soil bed studies. A good correlation was found between the strength loss of the southern pine test specimens and extent of decay. This data suggests that it may be possible to develop a dynamic test based on stress relaxation that is more sensitive than static bending....
D D Nicholas, J A Wilson, R C Vasishth


Decay, decayed wood and the Shigometer
1980 - IRG/WP 281
A L Shigo


Antifungal properties of new quaternary ammonium and imidazolium salts against wood decay, staining and mould fungi
2004 - IRG/WP 04-30347
The biological activity of twenty-four potential wood preservatives – imidazolium and quaternary ammonium salts with a modified anion structure was determined employing screening agar-plate and agar-block methods. Experiments were carried out on Scots pine (Pinus sylvestris L.) wood. The aim of the performed studies was to investigate the effect of structure modification of IC and QAC with organ...
J Zabielska-Matejuk, W Wieczorek


Ground contact performance of wood treated by the MSU process
1990 - IRG/WP 3609
Environmental concerns have prompted a renewed interest in accelerated fixation schemes for CCA-treated wood. Results from stake tests of southern pine (Pinus sp.) treated using a conventional Bethell cycle are compared with matched stakes treated using the MSU Process. The effects of adding boric acid to the preservative formulation are also discussed. Differences among test plots are discussed....
H M Barnes, T L Amburgey, R W Landers


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson


Performance of treated and untreated sawn fence posts of Scots pine and Norway spruce
2000 - IRG/WP 00-30247
Sawn fence posts are a rather important product and the objective of this trial was to assess their durability. In 1985 a field trial with treated and untreated fence posts of Scots pine (Pinus sylvestris L.) and Norway spruce (Picea abies (L.) Karst.) was set out at the test field in Ultuna, Uppsala, Sweden. The posts had a dimension of 75 x 100 x 1400 mm3. The preservatives applied were a CCA, a...
Ö Bergman


Towards a colour assay of wood degradation
1982 - IRG/WP 2180
A colour assay for the enzyme catalase is described. Since the activity of this enzyme has previously been shown to be correlated with degree of wood degradation as determined by other methods, this assay may provide a rapid quantitative indicator of superficial and internal wood decay....
M A Line


Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel


Water sprinkled pine wood: A microscope study on boards showing streaking
1993 - IRG/WP 93-10033
Boards sawn from the outer sapwood of pine lumber previously water sprinkled for periods of 10-18 weeks and kiln dried, showed streaking after staining. Two types of enhanced stain uptake were noted: 1) a more concentrated and localized form after 10 weeks and 2) a more diffuse type which developed in later stages of water sprinkling. Areas showing enhanced stain uptake were examined using light a...
G F Daniel, T Elowson, T Nilsson, A P Singh, K Liukko


The effect of low molecular weight chelators on iron chelation and free radical generation as studied by ESR measurement
2000 - IRG/WP 00-10367
The focus of this work was to improve our current knowledge of the non-enzymatic mechanisms involved in brown-rot decay. Electron Spin Resonance (ESR), also known as Electron Paramagnetic Resonance (EPR), is an attractive technique for the identification and study of chemical species containing unpaired electrons (such as radicals and certain transition metal species). ESR spin-trapping techniques...
Yuhui Qian, B Goodell


How to keep coated wood structures sufficiently dry to avoid damage caused by rot
1991 - IRG/WP 2376
During the last ten years, a new type of problems with wood rot has emerged in Scandinavia. Thousands of houses have been damaged by wood rot attaching to the exterior wood panel. This paper provides an overview of finished and ongoing work in order to identify the cause of these problems. In field tests, the moisture conditions were measured in panels coated with different paint systems. The infl...
S Hjort


Biological resistance of phenol-resin treated wood
1990 - IRG/WP 3602
Biological resistance of PF (phenol formaldehyde resin) - treated wood has been tested in relation to the resin properties, wood species and biological factors. When tested using water-soluble PF (mol. wt. 170), ca. 10% RI (resin impregnation) was enough to suppress the decay of Japanese cedar (Cryptomeria japonica) and western hemlock (Tsuga heterophylla) blocks exposed to Tyromyces palustris (br...
M Takahashi, Y Imamura


Ultrastructural aspects of bacterial attacks on an archaeological wood
1993 - IRG/WP 93-10007
Transmission electron microscopy of wood from a Chinese ship submerged in the mud for over 900 years showed bacteria to be the main factor for its deterioration. The micromorphology of degraded wood cell walls was similar to that observed during the attacks of wood by erosion bacteria. Other bacterial forms, previously considered lo be scavenging bacteria, were also abundant in degraded areas of t...
Yoon Soo Kim, A P Singh


The resistance of wood coated with different solvent-borne paints against colonisation by decay fungi
2009 - IRG/WP 09-40468
This paper examines different solvent-borne paints characteristics and their decay resistance when applied on pine wood surface. It was determined by the standard ENV 839 procedure. The part of samples were subjected to accelerated ageing according to the EN 84 standard. The discussed commercial paint systems were typical stains or penetrating oil-based products, with or without biocides....
B Mazela, P Hochmańska


Isolation and identification of bacteria from degraded wood - A progress report
1986 - IRG/WP 192
During attempts to isolate tunnelling bacteria in pure culture, physical separation from other bacteria was successfully achieved by the use of cellophane. Cellophane was used in liquid cultures as a substrate for tunnelling bacteria that were present in a mixture with other bacteria. By tunnelling into cellophane, TB were physically removed from contaminating bacteria which could then be removed ...
J A Drysdale, P J Ruland, J A Butcher