IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3503 documents. Displaying 25 entries per page.


Wood preservation in the Australian beekeeping industry
1988 - IRG/WP 3473
This paper reports the results of a survey of Australian commercial beekeepers working 200 or more hives in June/July 1985. Nine hundred and forty seven apiarists were asked to participate and to provide information on their wood preservation methods, painting procedures and maintenance of bee boxes. Three hundred and eighty-four apiarists returned completed questionnaires (41%). The main wood pre...
P J Robinson, J R J French


Effect of sterilization method on germination of spores of wood decay fungi observed by contact agar block method
1978 - IRG/WP 2117
Previous studies of germination of spores of wood decay fungi on wood have generally concluded that method of wood sterilization has little significant effect on germination response. This study expands the numbers of test fungi as well as number of sterilization methods employed to determine the influence of sterilization method on spore germination response of decay fungi. Germination was assess...
E L Schmidt, D W French


Non-enzymatic Gloeophyllum trabeum decay mechanisms: Further study
2001 - IRG/WP 01-10395
Information will be presented on the mechanisms involved in, and potential application of, non-enzymatic wood decay by brown rot decay fungi. Specifically, the hypothesized role of low molecular weight phenolate derivatives will be discussed in relation to non-enzymatic degradation of wood. The mechanism of binding of iron by cellulose, and binding and reduction of iron by fungal derivatives and m...
B Goodell, J Jellison


Combined effects of the treatment of wood with formaldehyde
1978 - IRG/WP 3117
Treatment of fibrous materials with reagents in a vapor phase is neither new nor unique. Numerous examples exist in literature of vapor phase experiments on cellulose fibers and fabrics, and on wood. For many years the textile research and industry have used vapor phase processes for the treatment of textiles. The chemical modification of cellulose is based on different types of reactions e.g. est...
M Stevens, J Schalck


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Final draft of a monographic card for Pole Fungus A, L Harmsen, Rigidoporus vitreus (Fr.) Donk according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 178
L Harmsen


Effects of the anaerobic wood decay bacterium Clostridium xylanolyticum on unbleached Pinus and Eucalyptus pulp
1991 - IRG/WP 1506
Clostridium xylanolyticum has been shown to produce extracellular enzymes capable of degrading wood. The present work was conducted to quantify growth on various lignocellulosic substrates and degradation of pulped wood fibre. In the latter tests Clostridium xylanolyticum was incubated at 35°C under anaerobic conditions in a medium containing 0.2% (w/v) peptone and 4% (w/v) unbleached Pinus and E...
G D Shelver, U Matai, W Van Wyk, A A W Baecker


Decay resistance of resin treated wood
1999 - IRG/WP 99-30206
Selected natural resin systems were evaluated for their potential as wood protecting agents according to standard test procedures. As indicated by the European standard EN 599 both a Basidiomycete test according to EN 113 and a ENV 807 soil bed test were carried out. Six resin treatments were tested using 3 concentration or treatment levels. Using the biocidal activity criteria as usually applied ...
J Van Acker, A J Nurmi, S M Gray, H Militz, C Hill, H Kokko, A O Rapp


Wood decay in Danish buildings
1985 - IRG/WP 1261
At Technological Institute identification of fungi and advisory activity concerning repair of damages has taken place since 1935. Statistical analyses based on material from 1982 and 1983 are compared to earlier investigations worked out by L. Harmsen. The material shows that building traditions influence the diversity and frequency of fungal species. Many fungal damages in the last decade have sh...
A P Koch


The influence of building design on wood decay
2000 - IRG/WP 00-10339
The cheapest and most effective way to prevent wood decay is to KEEP THE WOOD DRY! You and I know that, but we often forget and attempt a preservative solution to a problem better solved with good design and construction. It's also the answer to a frequently missed exam question in my Architecture class. Just as caulking is a poor substitute for proper design, so preservative treatment sh...
W W Wilcox


A short note on the subject of pretreatment decay in wood
1984 - IRG/WP 1245
The paper reviews five national standards for wood utility poles and some literature that concerns the problems of pretreatment decay. Finally it is proposed to form a new sub-group to study that problem....
J A Taylor


Monographic information on Serpula (Merulius) lacrymans (Schum. ex Fr.) S. F. Gray, according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 170
J Segmüller, O Wälchli


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Effects of some essential oils on wood destroying organisms
1993 - IRG/WP 93-10047
Three wood destroying fungi: Botryodiplodia theobromae Pat. (stain), Gloeophyllum sepiarium (brown rot), and Pycnoporus sanguineus (white rot) were exposed to six plant essential oils: the peppermint, kaffir lime or leech lime, lavender, tarragon, holy basil, and the eucalyptus. The peppermint oil showed most effective to inhibit fungal growth, while eucalypus oil was the least effective. The othe...
K Atisongkroh, C Anantachoke, P Lekuthai, S Pensook, T Kittirattrakarn


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


Effect of asphyxiation on wood decay fungi treated with argon and nitrogen gas
2002 - IRG/WP 02-10452
The effects of low-oxygen conditions, achieved with either argon or nitrogen gas, on the viability of wood decay fungi Coniophora puteana, Antrodia vaillantii and Trametes versicolor, cultivated on PDA medium and infected wood samples, were examined. The fungal cultures were exposed to low oxygen concentration (below 10 ppm) for one to five weeks in hermetically sealed vessels. Anoxic treatment di...
C Tavzes, F Pohleven, M Janisek, R J Koestler


Use of fluorescent-coupled lectins as probes for studying fungal degradation of wood
1986 - IRG/WP 1288
The ability of the fluorescent-coupled lectins wheat germ agglutin (WGA) and Concanavalin A (Con A) to react with selected Basidiomycetes, Ascomycetes, and Fungi Imperfecti was evaluated using pure cultures of 35 fungi grown on malt extract agar. WGA, which binds specifically to the n-acetylglucosamine residues found in fungal chitin, reacted with nearly all hyaline fungal structures but did not r...
J J Morrell, R L Krahmer, L C Lin


Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer


Monographic information on Serpula (Poria) incrassata according to the "Model Questionnaire for preparation of monographic cards for wood-destroying fungi"
1980 - IRG/WP 160
J G Palmer, W E Eslyn


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


The Pilodyn instrument as a non-destructive tester of the shock resistance of wood
1978 - IRG/WP 2107
A new non-destructive shock resistance tester, the PILODYN, has been developed. The instrument measures the fracture surface area created by a constant amount of energy. It operates by shooting a blunt pin into wood by an exact amount of energy. The penetration depth is read on a scale. A wide field of application is open to a non-destructive shock resistance tester such as: 1) assessment of the r...
P Hoffmeyer


Methods of assessing decay in poles in service with the Pilodyn wood tester
1978 - IRG/WP 2107 A
H Friis-Hansen


Detection of trace organics by ion mobility spectrometry
1990 - IRG/WP 3635
Ion Mobility Spectrometry (IMS) is a time of flight analytical technique that is suited to detect chemicals in the low parts per billion range. Some of the advantages of IMS are: operation at atmospheric pressure, fast response time (0.1-10 sec), and the ability to characterize individual chemical species in complex matrices without any prior sample preparation. In this paper, the utility of IMS i...
A H Lawrence


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


Previous Page | Next Page