Biological agents of timber degradation in Portugal. Marine borers
1991 - IRG/WP 4171
A brief report of the studies carried out in Portugal on marine borers is presented. The marine borers found in the portuguese coast are refered as well as the wood species where those organisms were identified. Emphasis is given to a study carried out from 1960 to 1975 at the Tagus estuary in Lisbon with the purpose, among others, of establishing the natural durability of different timbers....
J S Machado, L Nunes


Wood preservation in East European countries
1989 - IRG/WP 3527
The paper discusses the main problems of wood preservation in Bulgaria, Czechoslovakia, German DR, Hungary, Poland, Rumania and the USSR. The main types of wood preservatives produced have been presented, as well as the state of standarization to test their properties. There have been considered methods of wood treatment in use and application range of treated wood....
J Wazny


An investigation to assess the feasibility of developing an accelerated laboratory test to determine the abrasion resistance of lesser-used timber species for use in marine constructio
2005 - IRG/WP 05-20317
The paper describes the evaluation of a laboratory-accelerated test to compare the shingle abrasion resistance of current and potential timbers for use in marine construction. Useful results were achieved in 47.5 hours, but identified a number of issues to be resolved for the test to be refined and the subsequent results to be interpreted correctly....
G S Sawyer, J R Williams


An interim report on studies of the tolerance by Sphaeroma (Crustacea: Isopoda) of CCA-treated timber
1982 - IRG/WP 491
In Papua New Guinea any untreated timber exposed to seawater close to mangrove stands is liable to be attacked in the intertidal zone by the crustaceans Sphaeroma terebrans or Sphaeroma triste. Even CCA-treated timber is sometimes vulnerable. The mouth-parts of these animals are adapted for boring, but whether wood particles are ingested remains to be resolved. Some limbs of Sphaeroma terebrans ap...
S M Cragg, J D Icely


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


Effects of timber surface properties and dipping conditions on uptake of antisapstain actives from two aqueous suspensions, and ultimate effects on efficacy against mould and staining organisms
1995 - IRG/WP 95-30073
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, and the resultant surface retentions of active ingredients MTC (methylene bisthiocyanate), CTL (chlorothalonil) or TCMTB (2(thiocyanomethylthio)benzothiazole) were monitored by chemical analysis. Surface retentions increased with suspension concentration and surface rou...
M J Kennedy, T L Woods


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Observations on the penetration of preservatives into green timber
1985 - IRG/WP 3335
Differences in the rate and extent of diffusion of MBT and NaPCP-based preservatives following a short dip treatment were observed. The importance of preservative distribution as well as toxicity to the target organisms in governing the ultimate performance of any anti-sapstain compound is discussed....
G R Williams, R A Eaton, D A Lewis


Inventaire des "déchets" ou produits connexes de la filière bois
1993 - IRG/WP 93-50001-33
G Marcotte


Some biological observations on the management of preservativion experiments with submerged timber in the marine environment
1976 - IRG/WP 421 E
P Deschamps


The benefits to New Zealand of boron salt treatment of Pinus radiata
1992 - IRG/WP 92-3692
The historical reasons for New Zealand adopting boric salt diffusion of Pinus radiata are summarised, and present day processes and their associated costs are given. The biological hazards of using Pinus radiata untreated are then argued, using endemic fungal and insect species as examples, as well as a discussion of the risks from species that may yet be accidentally introduced into the country....
D J Cross


The use of C CP/MAS NMR in the chemical identification of decayed and undecayed, tropical timber species
1984 - IRG/WP 1224
13C CP/MAS NMR was found to be an extremely powerful tool for elucidating the chemical composition of Eucalyptus maculata, Pinus elliottii and Alstonia scholaris. The differences in lignin composition were different for each timber and discussed in relation to decay caused by soft-rot and white rot fungi. In particular the presence of syringyl and guaiacyl lignin types are discussed.
L E Leightley


Framework document for an international code of good practices for wood preservation and wood protection (anti-sapstain) facilities
1992 - IRG/WP 92-3683
At the Kyoto meeting, the Health & Safety committee agreed to form a task force to prepare a global plan for writing a code of good practices (Code) for wood protection and preservation facilities (Doc. No. IRG/WP/3681). The Canadian document had been presented to the IRG group earlier (Doc. No. IRG/WP/3447) and similar documents were solicited from other countries for preparing a framework do...
V N P Mathur, G Das


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


The biological natural durability of timber in ground contact
1994 - IRG/WP 94-20051
The BRE ground contact field trials for the determination of the biological natural durability of different timber species have recently been reviewed. The data obtained from these trials have been used to appraise the different ways in which natural durability may be expressed. It is concluded that the use of the mean as a method of assigning the timber to one of five durability classes may be ac...
G A Smith, R J Orsler


Weather testing of timber - discoloration
2001 - IRG/WP 01-20221
The brightness and color saturation of the timber were reduced over time. The perception of an increasingly dark color in the timber over time is due to the gradual reduction in brightness. The period from May to September was characterized by the greatest discoloration of all three periods of the year. Because this period has the largest number of sunlight hours, and the timber is subjected to a ...
T Toyoda, M Azuma, Y Hikita


Maintaining the adoption of the equilibrium moisture content in timber by bifluorides under outdoor circumstance
1989 - IRG/WP 3541
A description is given of the practical application of bifluorides, f. ex. Diffusec in maintaining the adaption of the equilibrium moisture content in timber, as a result of a many years observation of treated timber under outdoor circumstances....
H F M Nijman


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Regulatory and Consumer Challenges Facing Timber Preservation and Durability Interests in New Zealand and Australia
2003 - IRG/WP 03-20282
Timber preservation and durability interests in Australia and New Zealand are facing many challenges and threats arising from regulation and standards changes, to direct competition from competitive materials producers. Industry can address these challenges by pro-active initiation of sound, holistic, research, that addresses the performance needs of the regulators and specifiers and the expectati...
C MacKenzie


Protection of Ochroma pyramidale from fungal decay with N,N-napthaloylhyroxylamine
1998 - IRG/WP 98-30182
Fungal decay of wood in service results in billions of dollars (U.S.) in losses annually. Recent environmental restrictions, both U.S. and international, are limiting and eliminating the use of broad-spectrum, heavy metal biocides for wood preservation. Restrictions result primarily from problems with disposal. New wood preservatives need to be developed and tested which specifically target key el...
F Green III, T L Highley


Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer


Co-operative Field Experiment: Performance of preservative-treated timber: Report on condition of specimens after seven years installed in New South Wales - Australia
1986 - IRG/WP 3362
R S Johnstone


Work program of CEN/TC 38 (April 1993). Durability of wood and wood-based products
1993 - IRG/WP 93-20012
R Hüe


A risk model for termite attack in Australia
2003 - IRG/WP 03-10468
This paper describes a model to predict the risk of termite attack on a house in Australia. It is based on a survey of expert opinion and data from 5000 houses. The model gives a quantitative estimate of risk, and as such is useful for the development of risk management systems. An example of the application of such a system is given....
R H Leicester, C-H Wang, L J Cookson


Physical and mechanical properties of a suitable constructional timber of Bangladesh
1997 - IRG/WP 97-40102
The study of physical and mechanical properties of lohasirish timber (Derris robusta Roxb.) grown in Bangladesh revealed that the sapwood is whitish to yellowish white, heartwood is dark grey to blackish in colour; the texture is moderately fine, the grain in mostly straight and coarse with whitish rings of parenchyma; shrinkage is moderate; the EMC ranges from 12% to 16%; fuelwood colorific value...
A K Lahiry