Recycling of pressure impregnated timber and preservatives - incineration techniques
2001 - IRG/WP 01-50166-19
The object of the recycling research projects is to determine the technical and economical requirements of the recycling of CCA-impregnated wood. In the first recycling of impregnated timber project the amount and location of recyclable treated wood in Finland was determined and the costs of recycling were calculated. An incineration test was also made (1998). The conclusion of the first project i...
T Syrjänen, E Kangas


Test procedure to determine the effect of timber substrate on the effectiveness of different preservatives in sea-wate
1975 - IRG/WP 414
R A Eaton


Eco-tax - A new threat for wood preservation? The Belgian experience
1993 - IRG/WP 93-50001-32
At the end of January 1993, a bill was put for Belgian Parliament related to the introduction called "Eco-taxes" on a series of products, such as packaging for drinks (especially on PVC-bottles), non-returnable articles (shavers, small cameras), batteries, pesticides for non-agricultural use and paper....
G Van Steertegem, F De Jaeger


Light organic solvent preservative treatment of glue-laminated radiata pine
1986 - IRG/WP 3380
The high permeability of radiata pine (Pinus radiata D. Don) is associated with ray-tissue and in particular the cross-field pits linking ray-tissue to tracheids. This pathway is absent in the tangential grain direction, leading to poor preservative penetration when treatment is restricted to the radial face - for example, timber fabricated into glue-laminated beams....
P Vinden


Blue stain in timber in service. Results of co-operative tests to compare different artificial weathering systems 1981-82
1983 - IRG/WP 2193
The paper describes results of the third phase of co-operative laboratory experiments comparing the effects of different artificial weathering systems on chemicals to control blue-stain in service. Atlas, Xenotest and Marr equipments are shown to give essentially the same results for 5 of the 6 chemicals tested....
A F Bravery, D J Dickinson


Efficacy of anhydrides as wood protection chemicals - II. Performance against soft rot fungi
1998 - IRG/WP 98-30174
Pine sapwood modified with various anhydrides and with butyl isocyanate was tested for its resistance to soft rot decay. Small stakes were exposed for 20 months in unsterile soil in a fungal cellar test. Wood modified with butyl isocyanate performed better than any of the anhydrides tested, with a threshold level of protection (less than 3% weight loss) at 12% weight percent gain (WPG). Stakes ac...
S C Forster, M D C Hale, G R Williams


The identification and preservative tolerance of species aggregates of Trichoderma isolated from freshly felled timber
1992 - IRG/WP 92-1553
The surface disfigurement of antisapstain treated timber by preservative-tolerant fungi remains a major problem in stored timber. Identification of a range of isolates of Trichoderma based on microscopic morphological characteristics was found to be imprecise due to the variable nature of this organism. In addition, studies to compare visual (morphological) characteristics of these isolates with t...
R J Wallace, R A Eaton, M A Carter, G R Williams


A survey to assess the current and future usage of timber in British port structures
1998 - IRG/WP 98-10247
Port engineers responsible for 30 British ports were surveyed by questionnaire or interview to establish current and prospective usage of timber in those ports. The ports surveyed account for about 25% of total cargo handled annually in Britain and being located all around the British mainland, were considered to form a representative sample. The survey identified the hardwoods and softwoods in us...
G S Sawyer, S E M Plaster


Procedure for a collaborative study of leaching from CCA-treated timber in the sea
1988 - IRG/WP 4143
As a follow-up to the collaborative IRG/COIPM marine trial of CCA and CCB preservatives, a further trial is proposed with the objective of measuring the degree of leaching of CCA components from three timber species at marine sites in Malaysia and the U.K.. Details of the planned procedure are given....
S M Cragg, J E Barnacle, J D Bultman, R A Eaton, B R Johnson, L E Leightley, K D Singh


Regulations of pesticides (including wood preservatives) in the United States
1977 - IRG/WP 397
G B Fahlstrom


Wood-attacking organisms in Brazil
1982 - IRG/WP 1168
Lists of the main wood-attacking beetles, termites, fungi and marine borers in Brazil are presented with the respective wood species from which they were collected....
M S Cavalcante


A standardised procedure for the treatment of timber with test chemicals
1986 - IRG/WP 2257
A procedure is described which allows the standardisation of sample handling and data manipulation during trials invastigating the treatability of timber with test chemicals. The use of computer software allows the data to be handled efficiently....
J Norton, A Zosars, L E Leightley


Observations on the failure of anti-sapstain treated timber under non-drying conditions
1990 - IRG/WP 1437
A range of bacteria and yeasts were isolated from antisapstain treated timber and fresh sawdust. Solution samples containing 100 ppm of TCMTB in a nutrient medium were inoculated with these organisms and incubated at 25°C for 5 days. The levels of TCMTB remaining in solution were determined by HPLC analysis after this time. Results indicated high losses of active ingredient for a range of organis...
G R Williams


Leaching of Active Components from Preservative Treated Timber. Stage 1: Semi-Field Testing
2004 - IRG/WP 04-20302
The project is aiming at finding realistic leaching rates from preservative-treated wood in use class 3 (above ground). The project focuses on developing a field trial method for investigating leaching. Panels are subjected to outdoor exposure under natural weather conditions at a test field at the Danish Technological Institute. The leachate is collected and monitored by chemical analysis of the...
N Morsing, B Lindegaard


Ecotoxicological risks of anti-sapstain preservatives washed off from treated timber
2000 - IRG/WP 00-50144
A field method for ecotoxicity assessment of rain water wash-off from anti-sapstain treated timber was developed. In the course of this study freshly sawn timber treated with 1.5% Busan 30 L (reference preservative) and a control stack with untreated pine were exposed to weathering. The run-off water was ecotoxicologically tested with organisms from three trophic levels (Vibrio fischeri, Kirchneri...
G Aschacher, R Gründlinger


Reliability-based service life prediction methodology for assessment of water protection efficiency for coatings on wood
2003 - IRG/WP 03-20268
Assessment of water protection efficiency according to EN 927-5 has been shown to give significant differences in water absorption values for different types of coatings on wood. It is shown that the combination of EN 927-5 and an artificial weathering procedure gives more information regarding expected durability and long-term performance than a single measurement of water absorption on fresh, un...
J Ekstedt


United States Federal Committee on Wood Protection
1971 - IRG/WP 43
A C Jewett


Proposed test procedure to determine the effect of timber substrate on the effectiveness of a copper/chrome/arsenic preservative in seawater
1975 - IRG/WP 411
R A Eaton


Marine borers and marine wood protection - Some answers and some outstanding questions - A comment
1990 - IRG/WP 4163
A brief description of the nature of hazards encountered in different parts of the marine environment is given. An attempt is then made to assess what were the essential findings of selected areas of research in the marine wood protection field and what still needs to be done. That is, if we are to more adequately understand what we are attempting to do in this field of study!...
J E Barnacle


The role of communication in the field of environment protection: A case study "Wood Protection"
1990 - IRG/WP 3574
L Wöss


An insight into brown rot decay of timber as revealed by 13C CP/MAS NMR
1985 - IRG/WP 1259
L E Leightley


The collaborative developement of soil acceptance criteria for timber treatment chemicals in New Zealand
1995 - IRG/WP 95-50040-34
In New Zealand, the issue of potential contamination on timber treatment sites arose in the late 80's due to the long history of use of PCP by the industry. One of the recommendations from the task group set up to investigate the issue was the development of a set of acceptance criteria to define trigger levels for remediation. A technical group from the government, industry and regional ...
H C Boyd


Ultrastructure of the attack of a naturally durable timber by tunnelling bacteria
1990 - IRG/WP 1462
The attack of the wood of Eusideroxylon zwageri, a naturally durable species, by tunnelling bacteria (TB) was examined by light microscopy and transmission electron microscopy. Observations were made primarily on fibres. Parenchyma were included in some cases. Both fibres and parenchyma are rich in extractives. In fibres, extractives are primarily present in the lumen. The amber colouration of fib...
A P Singh, T Nilsson, G F Daniel


Marine borers as wood degraders in Bangladesh and their protection
1996 - IRG/WP 96-10186
Field study on timber piles used in Bangladeshi brackish waters revealed that untreated and pentachlorophenol treated piles drastically degraded by the attack of molluscs and pholads (marine borers). Adequately CCA-C impregnated (30 kg/m³ or 6% W/W dry oxide retention) timber piles can protect the attack of molluscs. It is very difficult to protect pholads which can invade naturally very durable ...
A K Lahiry


Migration of active ingredients from treated timber into fresh water
1991 - IRG/WP 3669
Spruce roundwoods and segments were treated with three different wood preservatives. Two of them containing copper and chromium the other one free of chromium. After fixation (3 weeks, 20°C) the specimens were leached by using artifical rain or by shaking the segments for one hour in contact with demineralized water. The water was analysed for the relevant elements of the preservative tested. Lea...