Extraction and analysis of DNA from green and seasoned timber as basic methods for determination of wood species and origin
2013 - IRG/WP 13-20523
Against the background of the European timber trade regulation EUTR, commenced to law by March 2013, the determination of wood species and tracing of its origin is getting a great importance. A promising approach for establishing fast and reliable tracking systems for wood products is DNA analysis. A critical point is the extraction of analysable DNA from the wood and its lignified cell walls. Thu...
K Jacobs, H Mende, W Scheiding


Virulence of two Laboratory Test Strains and one Natural Isolate of Rhodonia (Oligoporus) placenta against Thermally Modified Pine and Beech Wood
2013 - IRG/WP 13-20524
Rhodonia (Oligoporus) placenta is known as a relative aggressive basidiomycete fungus against thermally modified timber. In durability lab tests, this often results in a lower durability class, compared to other test fungi. In the reported work, the virulence of three different strains of Rhodonia placenta for untreated and thermally modified timber was determined and compared. Therefore, two lab ...
K Plaschkies, W Scheiding, K Jacobs, N Rangno


Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2013 - IRG/WP 13-20535
A round robin involving 15 European participants was set up in 2006. The round robin consists of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. When comparing EN 84 preconditioning (two weeks water leaching) with natural preconditioning (1 year in field, above ground) according to CEN/TS 15397, no significant difference...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, B Mazela, E Melcher, R Möller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Performance testing of DMDHEU-modified wood in Australia
2013 - IRG/WP 13-30613
Chemical wood modification with dimethyloldihydroxy-ethyleneurea (DMDHEU) or its derivatives has been researched for many years and shown to be applicable to improve certain wood properties to both solid lumber and wood-based composites. Earlier research proved a high biological resistance of DMDHEU-modified wood against biological degradation in laboratory and field tests in Europe. Due to the ve...
H Militz, J Norton


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell


Application of a model for the prediction of fungal degradation of thermally modified beech timber by Trametes versicolor
2013 - IRG/WP 13-40622
Colour measurement technology is found to be feasible for characterization of the property changes of thermally modified timber (TMT). In opposite to time-consuming and expensive laboratory tests a non-destructive test represents an improvement for the manufacturer of TMT. Therefore the aim of this study was to develop a method which allows sorting the different treatment intensities after the man...
Clauder, L., Richter S., Unger, W., Pfriem, A


Field performance of wood impregnated with siloxanes using supercritical carbon dioxide
2013 - IRG/WP 13-40632
This paper presents preliminary results from a 13-month field test containing pine sapwood samples (Pinus sylvestris) impregnated with a mixture of siloxane and organic biocides using supercritical carbon dioxide as carrier. Samples were exposed above ground at a Danish field test site using matched non-treated sapwood controls for every treated sample. All samples were painted before exposure. Pi...
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Quantification of copper and chromium in field stakes after different exposure times: Remaining metal content and distribution
2013 - IRG/WP 13-50291
In order to determine the distribution of copper and chromium as well as their remaining concentration EN 252 specimens and thicker pine sapwood stakes (non standard format) were treated with a commercial CC salt in a vacuum pressure process. The stakes were installed in the test field of the Institute of Wood Research, Hamburg, in August 2010. In all cases three stakes were removed after 4, 8, 12...
T Liese, M Bahmani, E Melcher


Modelling the risk for mould growth on timber stored outdoors protected from rain
2013 - IRG/WP 13-20529
A mould resistance design (MRD) model was used to calculate the maximum duration of storage of timber outdoors under cover (protected from rain) before the onset of mould growth on the surface of wood. The prediction model is based on laboratory tests performed in constant and cyclic climates and were also confirmed against exposure tests in attics and crawl spaces. The prediction model presented ...
E Frühwald Hansson, S Bardage, S Thelandersson


Durability of alternatives to CCA-treated wood - Results from field tests after 11 years exposure
2013 - IRG/WP 13-30633
The present study was initiated as a consequence of restrictions against the use of CCA-type wood preservatives in Sweden in the 1990s. New copper-based formulations were introduced on the market and to some extent, also alternatives to preservative-treated wood, such as thermally and chemically modified and linseed oil treated wood as well as heartwood of non-tropical naturally durable wood s...
P Larsson Brelid, M-L Edlund


Estimation of service life of treated wood in ground contact based on early indicators
2013 - IRG/WP 13-20536
A well-known problem with field testing is that it takes a long time before meaningful and reliable results are achieved. Only when a trial has come to an end the so called average life for the samples in a group can be calculated and compared with other samples. The aim of the present study was to investigate if it is possible to get a reasonable and good estimation of the average life long befor...
M Hansson, J Jermer, P Larsson Brelid, N Terziev


Microbial Community Analysis of Naturally Durable Wood in an Above Ground Field Test
2014 - IRG/WP 14-10826
This paper presents preliminary results of an above ground field test wherein eight naturally durable wood species were exposed concurrently at two sites in North America. Surface samples were taken at regular intervals from non-durable controls and compared to their more durable counterparts. Terminal Restriction Fragment Length Polymorphism was performed to characterize the microbial (bacteria, ...
G T Kirker, S V Diehl, P K Lebow


A comparison of the resistance of pyrethroid-treated wood to damage by Coptotermes acinaciformis in Australia and C. formosanus in China and the USA
2014 - IRG/WP 14-10830
Field trials, using a single aboveground method of exposure, were used to assess a range of retentions of two pyrethroids (bifenthrin and permethrin) in Pinus radiata D. Don sapwood against two species of Coptotermes in three countries to provide directly comparable results. Coptotermes acinaciformis (Froggatt) in Australia, C. formosanus Shiraki in China and C. formosanus in the USA consumed simi...
J Creffield, M Lenz, D Scown, T Evans, Junhong Zhong, B Kard, J Hague, K Brown, E Freytag, J Curole, R Smith, T Shupe


Moisture performance testing of wood – Practical experiences
2014 - IRG/WP 14-20546
Different methods are used to characterize the moisture performance of wood and to quantify the effect of moisture loads on the resulting service life. These methods can be divided into direct and indirect methods. Furthermore they can be distinguished by characteristics like continuous or periodical measurements and measuring local or global moisture content (MC). Furthermore each measuring metho...
L Meyer, C Brischke, M Kasselmann, C Rösmann


In-ground durability of wood-based products – Comparative assessment of graveyard field tests and terrestrial microcosms
2014 - IRG/WP 14-20538
Traditionally wood durability and the effectiveness of wood preservatives are determined in so-called graveyard tests (according to EN 252 or AWPA E7). For laboratory testing, terrestrial microcosms (TMC) can serve as an alternative. Both tests have been applied for different types of wood-based materials, preservative treated, modified and unmodified wood. However, the usability of laboratory res...
A Soetbeer, L Meyer, C Brischke, P Larsson-Brelid, J Jermer


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


On-site remediation treatments for framing timber in leaky buildings
2014 - IRG/WP 14-20549
Weathertightness failures in New Zealand buildings due to the combined effects of cladding choices, design and construction faults and the use of untreated framing timber has led to the so called ‘leaky building syndrome’. The latest estimated cost of the leaky building crisis in New Zealand is about NZ$11 billion. This research was conducted to provide a better understanding of the option...
T Singh, D Page, A Bennett


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Efficacy of commercial wood preservatives against Bursaphelenchus xylophilus, a quarantine organism in Europe
2014 - IRG/WP 14-30638
Bursaphelenchus xylophilus (Steiner and Buhrer 1934) Nickle, 1970, pine wilt nematode (PWN), is a quarantine organism with a high potential to damage Conifer forests in Europe. This has driven the European Union to protect forest stands from the propagation and dispersion of this pathogen. Since the nematode was detected in Europe, eradication measures were taken. However, these measures were unsu...
C S Arcos, A Navas, L Robertson, M T Troya, M Conde, F Llinares


Laboratory investigation of fire protection coatings for creosote-treated timber railroad bridges
2014 - IRG/WP 14-30639
As the incidence of timber railroad bridge fires increases, so has the need to develop protective measures to reduce the risk from accidental ignitions primarily caused by hot metal objects. Of the six barrier treatments evaluated in the laboratory for their ability to protect timbers from fires sourced with ignition from hot metal objects only one intumescent coating provided adequate fire prote...
C A Clausen, R H White, J P Wacker, S T Lebow, M A Dietenberger, S L Zelinka, N M Stark


Field trials results of preservative treated ground contact stake conducted in Korea
2014 - IRG/WP 14-30640
The field trials results from Korea preservative treated ground contact stake are reported. There was two site which was in southern area(Anmeon) and east area (Jungsun) of Korea. The CUAZ, CCA and CBHDO preservatives were use in this study. The sapwood of Japanese red pine stake was treated with these preservatives according to Korea standard method and then installed in 2003. Every year the insp...
Dong Won Son, Won Jung Hwang, Hyun-mi Lee, Dong-heub Lee, Sang-bum Park


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


CreoSub – New protection technology to substitute creosote in railway sleepers, timber bridges, and utility poles
2014 - IRG/WP 14-30644
Creosote oil is one of the oldest industrially used wood preservatives. Due to its toxic profile, the European Commission has restricted the use of creosote specific applications, but it is highly controversial within the European Commission. Its approval for use after 2018 is very questionable and may depend on derived research results until then, i.e., the viability of alternatives developed to ...
U Hundhausen, K-C Mahnert, A Gellerich, H Militz


Three-year field test of preservative-treated Canadian species in Korea
2014 - IRG/WP 14-30646
The purpose of this study was to generate field performance data in Korea on Canadian softwood species preservative-treated to Canadian standards. Two field tests of preservative-treated Canadian softwood species, one in ground contact and one above ground, were installed in Jinju, Korea in November 2010. Western hemlock and white spruce were incised and pressure-treated with alkaline copper quate...
Jieying Wang, Jong Bum Ra, P I Morris


Field performance of wax treated wood
2014 - IRG/WP 14-30649
The durability and outdoor performance of wax treated Scots pine sapwood was investigated in above ground field tests. Therefore wood impregnated with three different waxes was exposed in horizontal lap-joint test which is running since eight years. Durability, wetting resistance and the susceptibility to checking has been investigated. In summary, all wax treated wood performed better compared to...
C Brischke, E Melcher