In-situ experimental treatment and consolidation of degraded timber elements from a XIX century building
2012 - IRG/WP 12-10767
This paper presents the in situ experimental conservation work performed on three timber structural elements from a XIX century building: two floor beams and one roof beam. The palace was built in 1877 in the centre of Lisbon initially with residential purposes. It has four floors, with timber structural horizontal elements, stairs and roof beams (generally of Pinus sylvestris L.). The exterior wa...
D F Henriques, J de Brito, L Nunes


Laboratory and Field evaluation on Natural Resistance and Feeding Preference of Different Wood Species to Subterranean Termites (Isoptera: Rhinotermitidae, Termitidae) in Pakistan
2012 - IRG/WP 12-10769
The resistance of twenty four different woods to attack and damage by subterranean termite species Heterotermes indicola (Wasmann) and Coptotermes heimi (Wasmann) was evaluated by choice and no choic in laboratory and field trials. Mean wood mass loss was calculated for both laboratory and field trials results using Analysis of Variance (ANOVA). Mean percentage termite mortality was calculated fo...
S A Malik; F Manzoor, B M Ahmed (Shiday)


Long term durability of the heartwood of seven common softwood species in above ground conditions
2012 - IRG/WP 12-10771
The natural durability for wood in above ground use has been evaluated based on results after 11 years of exposure in a test site situated at the Danish Technological Institute in Taastrup, Denmark. Selected results for seven common softwood species exposed horizontally are reported. The test results cover samples with direct rain exposure (use class 3 of the European standard EN335-1:2006) and sa...
E Tang Engelund, M Klamer, T Mark Venås, B Lindegaard


The Technical Criteria on Biological Evaluation of Wood Preservatives for Use Category C4.1 in Southern China
2012 - IRG/WP 12-20481
According to the Regulations on Pesticide management of the People's Republic of China, wood preservatives belong to agrochemicals. The establishment of registration system on wood preservatives would be benefit to management of preservatives, including the market entrance and safety insurance to the human beings, livestock and the environment associated by the application of these preservati...
Xingxia Ma, Mingliang Jiang


Novel microscopic approaches to visualise chitosan within impregnated wood
2012 - IRG/WP 12-20485
Chitosan, a deacetylated product of an abundant naturally occurring biopolymer chitin, has been used in a range of applications, particularly in food and health areas, as an antimicrobial agent. In the work reported here Pinus radiata wood was impregnated with chitosan as an environmentally compatible organic biocide. It is important to understand micro-distribution of bioprotectants in impregnate...
A Singh, T Singh


Use of the durable species Coast Redwood as a reference system for field testing of Wood Protection systems
2012 - IRG/WP 12-20486
Data is provided and discussed for a number of field exposure tests where the naturally durable wood species Coast redwood, Sequoia sempervirens, was included along with untreated pine and standard preservative treatments. In general, there is potential for higher variability of results with this naturally durable species, but it does suggest that redwood can be a useful reference material for te...
A Zahora, A Preston, L Jin


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


In-ground variability of decay intensity within a test field
2012 - IRG/WP 12-20496
Timber exposed in the ground faces most severe conditions in terms of exposure to wetting and fungal decay in the terrestrial environment, therefore wood durability tests are often conducted in test fields preferably ensuring the occurrence of all relevant decay organisms. One can also expect differences in decay within an individual field-test site due to localized distribution of certain organis...
C Brischke, S Olberding, L Meyer, T Bornemann, C R Welzbacher


Performance of Wood Protection Systems at Multiple Field Test Sites Using the Ground Proximity Test Method
2012 - IRG/WP 12-20499
A series of preservative systems were used to treat southern pine ground proximity test samples which were then exposed at a range of test sites located throughout the world. The sites were chosen on the basis of having vastly different Scheffer Climate decay indices. After almost 14 years exposure, distinct differences are apparent in how different preservative systems perform at the different ...
A Zahora, A Preston, L Jin


Mould resistance of bamboo timber treated with tebuconazole-loaded micells
2012 - IRG/WP 12-30586
In this paper both anti-mould test through inhibition zone and mould resistance test on bamboo samples were carried out evaluate mould resistant effect of tebuconazole (TBA) loaded micells. Results showed that TBA loaded micells prepared with a ratio of TBA to PEG113-b-PCL28 50:25 had the best mould resistance, followed by micells prepared with a ratio of TBA to PEG113-b-PCL28 50:50. PEG113-b-PCL2...
Sun Fangli, Chen Anliang, Bao Binfu, Zhou Yueying, Zhang Shaoyong, Zhang Xu


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Effects Of Wood Preservative On Mechanical Properties Of Glulam Manufactured From Lower Density Malaysian Tropical Timber
2012 - IRG/WP 12-40590
This study is to investigate the effect of wood preservative on the mechanical properties of glulam timbers made from low density Malaysian hardwood timbers. Utilization of lower density Malaysian tropical timber for structural applications have not exploited extensively due to their inferior strength. By converting into treated glued laminated (glulam) timbers it could offer the possibility of th...
L Francis, Z Ahmad


Durability of Furfurylated Wood – Results from Laboratory and Field Tests in the Ecobinders project
2012 - IRG/WP 12-40602
Within the EU project Ecobinders, laboratory tests were performed with furfurylated wood produced in semi-industrial scale in the factory of Kebony ASA. Field trials in Horizontal double layer decks and in-ground of transmission poles were also started. Four wood species, Southern yellow pine (SYP), maple, beech and aspen were treated to two treatment levels by using two impregnating liquids with ...
M Westin


Guideline for Environmental Product Declaration for Thermally Modified Timber
2012 - IRG/WP 12-50287
Environmental Product Declarations (EPD) intend to enable the comparison of the environmental attributes of products that meet equivalent functional requirements. This guideline describes the proceedings of EPD for thermally modified timber (TMT). The main objective is the general survey on requirements on EPD which are based on European and international standards.Up to now only a few EPDs for na...
L Clauder


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Effectiveness of CCA-C and CCB preservatives after a 30 years stake test
2012 - IRG/WP 12-30606
The objective of this experiment was to assess the durability of four pine species treated with waterborne preservatives. In order to determinate this, a stake field test, following the IUFRO (International Union of Forestry Research Organizations) recommendations, was installed at Experimental Station of Luiz Antonio (21º 32’ S and 47º 42’ W), State of São Paulo, Brazil. Species under t...
I PJankowsky, E S Lepage, C Salvela, J M Vidal, S Takeshita


Seed oil and defatted cake proximate composition of non timber product Annona squamosa (Annonaceae) grown in Benin
2012 - IRG/WP 12-30607
Annona squamosa L. is a small tree which grows wild in many places in the tropical regions, locally called “xwingle” in Benin. Its produces edible fruits, typically globular or heart-shaped which are highly appreciated and the seeds are not used. In the course of work about identifying new oil sources from a large number of oil bearing seeds grown in Benin, we report here on the chemical compo...
T S Djenontin, J Dangou, P Lozano, D Pioch, D C K Sohounhloue


Influence of a pulsed electric field on the growth of surface fungi
2013 - IRG/WP 13-10795
The colonization of mold and staining fungi are not only an aesthetical problem. Blue stain fungi are able to penetrate paint films. Maintenance of coatings on wood are time consuming and costly. A new approach uses a pulsed electric field (PLEOT) in order to protect wood against surface fungi. This technology is evaluated in non-sterile laboratory conditions on different coated and uncoated Scots...
M Starck, A Treu


Survival of Bursaphelenchus xylophilus exposed to different active ingredients of wood protectors
2013 - IRG/WP 13-10802
The pine wilt nematode (PWN) Bursaphelenchus xylophilus (Steiner and Buhrer 1934) Nickle, 1970 is a quarantine organism with a high potential to damage Conifer forests in Europe. This has driven the European Union to protect forest stands from the propagation and dispersion of this pathogen.The nematode was first detected in Europe in Setubal (Portugal) in 1999 and eradication measures were taken....
S C Arcos, M T Troya, L Robertson, F Llinares, M Conde, A Navas


Update on "Sandwich" Type Above Ground Field Test Methods
2013 - IRG/WP 13-20506
Our research group has been investigating a number of new designs for above ground field testing to try to provide rapid methods to compare the relative performance of systems in above ground, unprotected exposures. This paper provides an update on what we have found with three variations on a "sandwich" type above ground test arrangement, with comparison to the more traditional lap-joint method ...
A Zahora, L Jin, A Preston


Characterization of test fields
2013 - IRG/WP 13-20508
Test field characteristics and impact of test fields on wood degradation is important when testing wood protection. The current EN 252 standard has no requirement for knowledge of decay hazards, but most commonly a test field is known as a “brown”,- “white”,- or “soft rot” field. To understand which decay hazard wood preservatives are tested against, each test field should be character...
U Råberg, N Terziev, G Daniel


A critical view on early indicators for above ground field performance of wood
2013 - IRG/WP 13-20509
Above ground field tests are quite often a balancing act between the provision of realistic test conditions, reliable statistics, and acceptable long test durations. Within this study we therefore reviewed 543 data sets from above ground field tests performed at 36 different test sites in 8 countries in Australia and Europe. The main objective was to investigate possible correlations between early...
C Brischke, L Meyer, G Alfredsen, P-O Flæte, L Francis, M Hansson, P Larsson Brelid, J Jermer


Quasi-in-situ durability tests on oak timber bridges
2013 - IRG/WP 13-20510
This study aims on developing a method for determination of wood durability on samples taken from real structures in service. Therefore quasi-in-situ durability tests have been conducted exemplarily on timber bridges made from English oak (Quercus robur L.). Drilling cores were found to be a feasible alternative to standard specimens for laboratory durability tests against pure cultures of Basidio...
C Brischke, C J Behnen, M-T Lenz, K Brandt, E Melcher


Statistical analysis of durability tests - Part 2: Principles of time-to-failure and application on field test data
2013 - IRG/WP 13-20512
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing is therefore essential, in combination with proper monitoring and analysis tools. A crucial concept is variability and the incorporation of variability in tests and analysis. In this paper we focus on t...
J Van den Bulcke, I De Windt, C Brischke, C R Welzbacher, A O Rapp, J Van Acker


Accelerated H3 above-ground decay testing
2013 - IRG/WP 13-20520
An above-ground H3 fungal field trial was installed at two sites in Australia and one in New Zealand, as well as in two Accelerated Field Simulators. The aim was to find a method that would shorten the time required for evaluating new preservatives and protection systems. One-quarter H3 retentions were installed, as first results suitable for registration occur when these reach 70% soundness. Twel...
L J Cookson, D Page, T Singh


Previous Page | Next Page