Blue Staining of Coated Modified and Unmodified Wood
2006 - IRG/WP 06-10589
We investigated resistance of unmodified, DMDHEU modified and oil heat treated uncoated and coated Scots pine wood against blue stain fungi. Both EN 152-1 and the reverse exposure tests showed excellent resistance of DMDHEU and especially of oil heat treated wood against blue staining. It is not needed to add any additional protective coating layers to prevent modified wood from staining. However,...
M Petric, M Pavlic, M Humar, M Tomažic


Quantification of methylene bis thiocyanate in wood and its effect on a sapstain fungus Ophiostoma floccosum
2006 - IRG/WP 06-10591
The mobility and concentrations of MBT at different depths of wood billets (200 mm long, 40 mm in diameter) were determined using NMR spectroscopy and ICP-ASE, and then correlated the effect of wood MBT concentrations on growth of O. floccosum in a bioassay using stereomicroscopy and confocal laser scanning microscopy (CLSM). The 13C NMR spectra showed the presence or absence of MBT in wood but w...
T Singh


Direct analysis from wood of the blue stain fungi Aureobasidium pullulans and Hormonema dematioides by denaturing gradient gel electrophoresis
2006 - IRG/WP 06-10595
Aureobasidium pullulans and Hormonema dematioides are the two organisms used in the EN 152 laboratory method for determining the effectiveness of preservatives against blue stain in service. The literature concerning the disfigurement of surface coatings and exposed timber in-service states that A. pullulans is the dominant blue stain fungus, due to its frequent isolation from stained material. In...
M J Ray, D J Dickinson


Study of new wood preservatives from biological origin and low toxicity against wood decay organisms (fungi and termites)
2006 - IRG/WP 06-10600
Wood as an organic material is likely to be attacked by living organisms if no protecting treatment is applied to improve its durability. The biological agents, which in Spain, due to its specific climatologic, cause major damage to wood, are the stain fungi, the rot fungi and the subterranean termites. The commercialisation of the products actually used to treat wood against fungi and to treat t...
M T Troya, M J Prieto, F Rubio, D Lorenzo, J J Teixidó


Efficacies of an insecticide and a fungicide for preventing blue-stain of Japanese red pine logs
2006 - IRG/WP 06-20329
We examined blue-stain fungi on Japanese red pine at 3 forests and 2 saw mills in Iwate Prefecture, Japan. The isolated ophiostomatoid fungi were Leptographium sp and Ophiostoma sp. There were 3 routes of the blue-stain; fungal growth from the spore or hypha stuck on the cross cut surfaces, fungal spread through the inner bark by bark beetles and fungal invasion around whorled knot. The larger ext...
H Taniuchi, T Koiwa, H Masuya, S Doi


EN 152: Is this Standard Relevant for today’s Wood Preservatives? A Critical Review.
2006 - IRG/WP 06-20331
The paper critically reviews the Blue stain test method described in EN 152 including possible test variables. Whereas EN 152 has been successfully used for solvent borne wood preservatives, it appears that the methodology is not suited for modern water borne products, where the majority fail. The paper will show that there exist different quality claims not concordant with EN 599-1 within diff...
B Jensen, F Imsgard, J Larsen


Beetle-Fungus Associations in Woody Substrates in the Context of International Trade
2007 - IRG/WP 07-10610
Interest in the role of insects in transmitting various fungi and in the potential for outbreaks of insects vectoring plant disease organisms has resulted in a large volume of literature on insect-fungi relationships. Mites are mentioned as an important third partner in these associations. This paper summarizes information and provides an update on major aspects of these intricate associations in ...
A Uzunovic


Efficacies of physical barriers for preventing blue-stain of Japanese red pine logs
2007 - IRG/WP 07-20359
This paper deals with field trials on physical barriers to prevent blue stain on Japanese red pine logs using a fly screen, bark and leaves of Japanese cedar as covering materials. These barriers arrested blue stain and bark beetle attacks to low levels than control for 1 month except covering with a small amount of bark. Covering with the fly screen and a large amount of bark permissibly suppress...
H Taniuchi, T Koiwa, H Masuya, S Doi


Protection of wood for above ground application through modification with a fatty acid modified N-methylol/paraffin formulation
2007 - IRG/WP 07-40378
Hydrophobic chemical modification can be regarded as an alternative approach to conventional wood preservation using biocides in order to protect wood in hazard class 3 according the European Standard EN 335-1. A formulation containing fatty acid modified N-methylol/paraffin and an aluminium salt catalyst was used to change the material properties of wood in order to protect wood from fungal dec...
Nguyen Hong Minh, H Militz, C Mai


End Coating Masson Pine Grown in South China to Prevent the Development of Blue Stain
2007 - IRG/WP 07-30428
One end (randomly selected) of logs of mason pine (Pinus massoniana) were coated with a wax-type end coating called ANCHORSEAL® immediately after tree cutting. The logs were then stored in summer weather in Guangxi, China. During the storage, at week 1, 2, 3, 4, 6, 8 and 12, five logs of mason pine were sawn into lumber or veneer for the visual observation and measurement of blue stain at the coa...
Zhao Youke, Qin Li, Huang Rongfeng, Lu Jianxiong


Laboratory test of blue stain control by chemicals
2007 - IRG/WP 07-30430
8 chemicals and some mixtures against Botryodiplodia theobromae Pat., Fusarium verticillioides(Sacc.)Nirenberg, Trichoderma harzianum Rifai, Trichoderma viride Pers., and Penicillium purpurogenum Stoll were conducted in laboratory by inhibition zone in the paper. The results were shown that: CBZ and benomyl as well as copper oxine alone are much high efficacy for inhibiting most of the 5 fungi tha...
Zhijuan Wang, Zehui Jiang, Mingliang Jiang, Chungen Piao


The effect of brighteners on wood surface aesthetics – exploring the use of various organo-phosphonates based precursors
2007 - IRG/WP 07-30441
Freshly cut hardwood lumber such as white oak, red oak, beech, or redwood are rich in mineral stain (mostly iron and calcium), which provides a strong discoloration of the wood surface significantly influencing the aesthetic of the wood surface and strongly affecting the cost of this lumber. The influence of mineral stain on soft wood discoloration (Southern Yellow Pine, Douglas fir, etc.) is les...
R Craciun, P Mitchell


Genome-wide survey of cellulase related genes of white rot fungus,Pleurotus ostreatus
2007 - IRG/WP 07-10627
A white rot fungus, Pleurotus ostreatus, which is a important edible mushroom, has received much attention to apply to bioremediation and bioconversion because it has both cellulase and ligninase. To confirm copy number of cellulase-related genes encoded in P. ostreatus genome, we attempted to genomic Southern hybridization of P. ostreatus. The draft genome sequence and a large quantity of EST and...
T Tamenori, S Horisawa


Effect of fiber type and content on the natural durability of wood flour/high density polyethylene composites against rainbow fungus (Coriolus versicolor)
2007 - IRG/WP 07-40387
In order to evaluate the effect of fiber type and content on the natural durability of wood flour/high density polyethylene (HDPE) composites against Coriolus versicolor, samples containing 25% and 50% by weight of various natural fibers and HDPE were selected. Natural fibers included in the study were wood flour, rice hulls, hemp fibers and newsprint. Samples containing 25% and 50% natural fiber ...
A Karimi, M Tajvidi, S Pourabbasi


Effect of Compatibilizer on the Natural Durability of Wood Flour/High Density Polyethylene Composites Against Rainbow Fungus (Coriolus versicolor)
2007 - IRG/WP 07-40388
To evaluate the effect of compatibilizer on the natural durability of wood flour/high density polyethylene composites against Coriolus versicolor, composites containing 25% and 50% by weight maple wood flour and 1% and 2% compatibilizer (Maleic anhydride polyethylene (MAPE)), respectively, were sampled. Identical specimens of the same composites without the compatibilizer were also prepared. ...
Sara Pourabbasi, A Karimi, D Parsapajouh, M Tajvidi, M Soleymani


Decay resistance of propionylated Iranian beech against the white rot fungus Tramets versicolor
2008 - IRG/WP 08-30449
In this study, the decay resistance of propionylated beech was investigated against the white rot fungus Trametes versicolor. Iranian beech (Fagus orientalis) was modified with propionic anhydride at different temperatures, concentrations and times without using any catalyst. Different weight percentage gains (WPGs) were obtained under different conditions. The decay resistance of the esterifed wo...
M R M Farahani, S M Hosseini


Biological control of the sapstain fungus Diplodia pinea (syn. Sphaeropsis sapinea) in the field
2008 - IRG/WP 08-10663
Diplodia pinea, syn. Sphaeropsis sapinea, is well known as the worldwide ocurring causal agent of the Diplodia tip-blight disease on various pine species, leading to great losses of valuable wood in the forests. Moreover, this fungus is also responsible for the fornation of sapstain of felled logs, leading to undesired disation of surface layers in the OSB manufacturing industry. In Central Europe...
C Gradinger, T Boisselet, K Messner, K Fackler


Relationship between coating properties and their performance on treated wooden decks
2008 - IRG/WP 08-30454
Preservative treated wood benefits from the application of a surface coating to protect it from weathering (UV and rain). Different preservative formulations may affect surface properties of treated wood differently; therefore compatibility of coatings with different preservative treated wood types should be considered. This paper examines coatings characteristics and their weathering performance ...
M Ahmadinejad, P A Cooper


The efficacy of commercial silicones against blue stain and mould fungi in wood
2008 - IRG/WP 08-30471
Scots pine (Pinus sylvestris L.) wood samples were vacuum pressure impregnated with quatsilicone micro emulsion (<40 nm particle size), aminosilicone macro emulsion (110 nm) and silicone macro emulsion with alkyl modified side groups (740 nm) and the resulting material properties were studied. Quatsilicone micro emulsion resulted in maximum bulking (4.8%) and anti-swelling efficiency (21.8%) in...
S C Ghosh, C Mai, H Militz


Control biológico de la mancha azul en madera aserrada de Pinus radiata D. Don.
2008 - IRG/WP 08-10681
Radiata pine wood is highly susceptible to the attack of sapstaining fungi promoting a discoloration which results in important economical losses. The use of chemicals, a customary procedure to prevent its occurrence is becoming nowadays, due to environmental concern, a more questionable practice. The biological control of blue stain fungi with albino isolates of the Ophiostoma genera appear to ...
J Navarrete, A Segura, P Martínez, R Vera, C Segovia, P Herrera, L Reyes, D McNew, T C Harrington, R L Farrell, J M Thwaites, B Held, R A Blanchette


Mechanical and chemical properties of blue stained wood
2009 - IRG/WP 09-10686
Discoloration of wood is frequently caused by blue-staining fungi. In the previous researches there was general opinion that blue-stain fungi do not influence mechanical properties. On the other hand, there were some opposite results reported as well. In order to elucidate this issue, specimens made of Pinus sylvestris sapwood were exposed to two the most frequent and important blue stain fungi Au...
M Humar, V Vek, B Bučar


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh


Laboratory test of some formulations against stain and mould fungi isolated from bamboo wood
2009 - IRG/WP 09-30508
To screen the effective anti-mould formulations, fungicides such as carbendazim, tebuconazole, fludioxonil, difenoconazole, prochloraz, benomyl and 8-hydroxy-quinoline copper (copper oxine) were selected to conduct the laboratory test of fungicidal activity by method of inhibition zone against Botryodiplodia theobromae Pat., Fusarium sp., Alternaria tenuis Nees., Penicillium purpurogenum Stoll, Tr...
Xingxia Ma, Airui Sun, Mingliang Jiang, Daochun Qin


Use of wax emulsions for upgrading of wood properties
2009 - IRG/WP 09-40451
Waxes are used for treatment of wood surfaces for several decades, predominately as surface treatments, because they did not penetrate into the wood. In order to overcome this issue, water emulsions were applied in present experiment. Five water emulsions of various concentration was used namely; two emulsions of montan wax (LGE, MW1), emulsion of polyethylene (WE1), emulsion of ethylene copolymer...
B Lesar, F Pohleven, M Humar


Modelling hyphal growth of the bio-incising fungus Physisporinus vitreus
2010 - IRG/WP 10-10710
The white-rot fungus Physisporinus vitreus preferentially degrades the pit membranes of bordered pits in tracheids and subsequently enhances wood permeability. Thus, P. vitreus can be used to improve the uptake of wood preservatives and environmentally-benign wood modification substances. This process can be used to enhance the use and sustainability of native conifer wood species by the wood indu...