Resistance to decay of particle boards: Presentation of a test method
1986 - IRG/WP 2260
The experimentations were undertaken on particle boards 35 and 50 mm thick. The rot resistance tests were carried out on specimens whose dimensions were 600 x 75 x 35 mm³ for particle boards 35 mm thick and 800 x 75 x 50 mm³ for particle boards 50 mm thick according to a method derived from the one described in the documents IRG/WP/2214 and IRG/WP/2243. Two exposure periods were used: 12 and 16 ...
G R Y Déon, N Trong


Evaluation of outdoor weathering performance of modified wood
2004 - IRG/WP 04-20296
Interlace treated, oil treated, silicon treated as well as untreated Scots pine samples have been exposed outdoors. For evaluating the samples on their long term performance an internal standard had been developed. Parameters to be determined were the uptake of liquid water (submersion test), weight variation during exposure, crack performance, surface roughness and colour change. This paper disc...
Y Schulte, S Donath, A Krause, H Militz


Performance of preservative-treated wood not in ground contact
1975 - IRG/WP 254
Experimental sash units of Pinus strobus L. and Pinus resinosa Ait. wood were removed from a test fence at Ottawa, Canada after outdoor exposure of over 20 years. The units were superficially treated, prior to painting, with preservatives containing either copper naphthenate, pentachlorophenol or a combination of zinc naphthenate and pentachlorophenol. Results indicated that all treatments were ef...
J K Shields, J Krzyzewski


Soil termiticides: A review of efficacy data from field tests
1987 - IRG/WP 1323
This paper reports efficacy data from the field evaluation of various soil termiticides by the U.S. Department of Agriculture, Forest Service, Gulfport, Mississippi. These chemicals, which include a number of chlorinated hydrocarbon, organophosphate, pyrethroid, and carbamate insecticides in a range of concentrations, have been in long-term tests at seven field sites. Data are reported for the gro...
J K Mauldin, S C Jones, R H Beal


Facility for Conducting Field Tests on Coptotermes formosanus at LSU Agricultural Center
2003 - IRG/WP 03-20274
Efforts by Louisiana State University Agricultural Center (LSU AgCenter) and Mississippi State University (MSU) research scientists, to conduct cooperative research on C. formosanus and other wood-related topics, have led to establishing an FST field test site at the LSU Agricultural Center Citrus Research Experiment Station, Port Sulfur, Louisiana. A minimum of 32 termite colonies will be establi...
W R Smith, T L Amburgey, G Henderson, D R Ring


Premature failure of CCA treated vineyard posts from brown rot
1993 - IRG/WP 93-10016
A survey of CCA (AWPA Type C) treated posts used as grape vine trellis supports, to determine the extent and type of decay was carried out at a terraced vineyard in the Hawkes Bay region of the North Island of New Zealand. Of 357 posts examined out of a total of 970 in the vineyard, 47% had moderate to severe decay or had failed, 20% had established decay, 10% had a trace of decay and 23% had no s...
R N Wakeling, A P Singh


Biological control of decay
1975 - IRG/WP 135
One approach to the biological control of decay in standing poles, live trees or seedlings is with microbial immunising commensals or IC.·These are microorganisms able to grow in the wood without damaging it and as a result of such growth to protect against certain types of decay. Scytalidium and Trichoderma spp have been tested in the field. The latter species have shown an establishment rate in...
J Ricard


Relationship between degradation of wood, cellulose or lignin-related compounds and production of hydroxyl radical or accumulation of oxalic acid in cultures of brown-rot fungi
1994 - IRG/WP 94-10062
The degradation activities of brown rot fungi against wood, cellulose, and lignin-related compounds were measured in cultures containing glucose or wood as a carbon source. Also the activities of one-electron oxidation and hydroxyl radical production and the amount of oxalic acid present in the cultures were measured. The degradation activities of the fungi against wood, crystalline cellulose and ...
S Itakura, T Hirano, H Tanaka, A Enoki


A soil-less test of treated wood
1978 - IRG/WP 2105
The objective of this work is to devise an accelerated test for preservatives to be used in places away from soil contact. There may be compounds or mixtures which will protect wood or wood derived materials from decay in such articles as sash and doors, boardwalks, steps, laminated arches and the like, and possess properties that make them preferable to the heavy-duty preservatives used for poles...
E A Behr


Performance of Two Imidacloprid-Treated Malaysian Hardwoods in an Accelerated Aboveground Termite Test
2005 - IRG/WP 05-30389
The performance of the chloronicotinyl insecticide imidacloprid as a wood protecting termiticide, under a simulated Malaysian biological hazard class H2 (exposure aboveground indoors against termites and wood borers), was evaluated by a novel termite field test protocol. Replicate end-grain sealed air dried test blocks (20 x 20 x 20 mm) of two Malaysian hardwoods, Kembang Semangkok (Scaphium spp.)...
A H H Wong


Status of Work on OECD Test Guidelines for Emissions of Wood Preservatives to the Environment
2005 - IRG/WP 05-50224-3
In April, 2003, OECD published an ESD on wood preservatives that provides guidance on how to estimate emissions: 1) during the wood preservative application processes and storage of treated wood prior to shipment; and 2) from treated wood-in-service. The ad hoc Expert Group that developed the wood preservatives ESD identified the need to develop Test Guidelines to estimate the amount of biocides ...
W Jakob


Influence of acidification on decay processes of CCB treated wood
2004 - IRG/WP 04-10514
The phenomenon of copper tolerance by brown rot fungal strains has been known for a long period but the complete mechanism of copper tolerance by these fungi is not understood yet. Copper tolerance has previously been linked to oxalic acid excreted by copper tolerant brown rot fungal strains. This acid reacts with copper in the wood to form an insoluble and therefore less toxic copper oxalate. The...
M Humar, S A Amartey, M Šentjurc, F Pohleven


Soil treatment tests with the three products of boric acid for the prevention of the hyphal growth of Serpula lacrymans
1992 - IRG/WP 92-3693
Laboratory soil treatment tests were conducted for the evaluation of fungicidal or fungistatic effect of boric acid products against Serpula lacrymans. Boric acid products tested were the following three: a thickened boric acid solution in triethanolamine, boric acid-silica gel complex granules, and a nonwoven fabric laminated with a polypropylene film and coated with boric acid granules on one si...
S Doi, A Yamada, Y Mineki, M Mori


Effectiveness of some microbiocides against the development of molds and sapstain in Pinus elliottii
1981 - IRG/WP 3169
Eleven commercial biocidal formulations were tested in the field to determine their effectiveness in protecting logs and lumber of Pinus elliottii sapwood from sap stain and molds. Among these formulations 2-(thiocyanomethylthio) benzothiazole showed the best performance in controlling both types of fungi. Potassium N-hydroxymethyl-N-methyl dithiocarbamate and the mixture potassium N-methyl dithio...
S Milano


The remaining concentration of inorganic wood preservative components in EN 252 stakes after ground contact
2000 - IRG/WP 00-50159
In order to determine the biological efficiency and the remaining concentration of different inorganic and organic active ingredients during service, EN 252 specimens were impregnated with 3 copper based wood preservatives. The stakes were installed in the test field of the DESOWAG GmbH, Rheinberg, for at least 7 years. At the end of the field test some of these stakes were divided into 10 uniform...
E Melcher, H-W Wegen


The role of oxidation in wood degradation by brown-rot fung
1992 - IRG/WP 92-1562
Brown-rot fungi are suggested to degrade cellulose by oxidation with hydrogen radicalsformed eg. in the conversion of hydrogen peroxide in the Fenton type reactions. The stuctural changes in the holocellulose in wood induced by Fenton's reaction on wood components are very similar to those caused by brown-rot fungi. In this work the effect of the Fenton reaction on wood components was stu...
A-C Ritschkoff, J Pere, J Buchert, L Viikari


Alkaline building materials and controlled moisture conditions as causes for dry rot Serpula lacrymans growing only in houses
1985 - IRG/WP 1272
Dry rot Serpula lacrymans ( Fr.) S.F. Gray is commonly found in houses, though never with certainly in nature, like other wood destroying fungi which grow both indoors and outdoors. In investigating series of dry rot instances it was shown that this fungus is always found in covered places, close to a moisture source, the distance being from 0 a maximum of 600 cm. Owing to the dry rot has been abl...
J Bech-Andersen


Comparison of the FRIM and forest research laboratory methods for screening of anti-sapstain formulations
1999 - IRG/WP 99-20170
Two laboratory methods for screening of anti-sapstain formulations were compared. The method adopted by the Forest Research Institute Malaysia (FRIM) involved 3 weeks assessment of rubberwood (Hevea brasiliensis) blocks, dipped in the candidate formulation and inoculated with mycelial/spore suspension of sapstain (Botryodiplodia theobromae) or decay (Schizophyllum commune) fungi, and incubated on ...
A H H Wong, D R Eden, C M Chittenden, M E Hedley, R N Wakeling


Susceptibility of antisapstain fungicides to rain wash-off
1994 - IRG/WP 94-30046
Results of trials using miniature timber packets and simulated rain wash-off are described. Six fungicidal actives in five commercial antisapstain formulations were involved, and a clear influence of rainfall timing after antisapstain treatment was demonstrated. Differences between actives and formulations were most marked where water-spray was applied in the first hour after treatment, though eve...
R N Wakeling, D J Cross, D R Eden, P N Maynard


Identification of brown rot fungi on wood in above ground conditions by PCR, T-RFLP and sequencing
2004 - IRG/WP 04-10512
Fungi selected in test fields in Germany and Estonia and fungi (Coniophora puteana) cultivated on medium have been identified by the molecular methods PCR (Polymerase Chain Reaction), T-RFLP (Terminal Restricted Fragment Length Polymorphism) and sequenced to species level. The samples from the German field test showed that the fruit body sample was a different fungus than from the mycelium sample....
U Råberg, N Högberg, C J Land


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Old and new facts on the dry rot fungus Serpula lacrymans
1991 - IRG/WP 1470
The article collates some of the recent literature on the biology of the dry rot fungus Serpula lacrymans. The fungus can grow at 28°C, and maximum wood moisture is above 55%. Serpula Iacrymans degrades crystalline cellulose. The intensive production of extracellular oxalic acid is neutralized by calcium and iron. There is considerable variation among the strains with regard to factors such as gr...
O Schmidt, U Moreth-Kebernik


Resistance of acetylated wood to biological degradation. Evaluation of field test
1997 - IRG/WP 97-30139
Acetylated wood samples were tested in ground contact (stake test) at two test fields, one in Simlångsdalen, Sweden, and one in Viikki, Finland, according to European standard EN 252. The test samples were inspected annually and their condition was compared with that of untreated controls and of samples treated with two reference CCA preservatives. The use of untreated controls and preservative t...
P Larsson Brelid, R Simonson, Ö Bergman


Pentachlorophenol and tributyltin oxide - the performance of treated Pinus radiata after 12 years' exposure
1986 - IRG/WP 3361
Pinus radiata samples were impregnated with a range of light organic solvent preservatives and copper/chrome/arsenic salt and exposed with no surface coating both in and above ground for 12 years. Inspection of the test samples revealed that some formulations of light organic solvent preservatives will give good fungal protection and reduce splitting in Pinus radiata exposed externally without a s...
R S Johnstone


Five years leaching of Boron
1999 - IRG/WP 99-30195
The diffusibility of Boron in wood and thus its leaching behaviour in water contact is known since long. Nevertheless quantitative data on the long-term leaching behaviour are rare. Consequently, field exposure tests were started with beam-segments treated with pure boric acid and with poles treated with CCB. Detailed data of more than five years of field exposure are now available. Pure boron tre...