IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1244 documents. Displaying 25 entries per page.


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


Performance trials of treated hardwood fences
2002 - IRG/WP 02-30281
This paper examines the performance of the traditional hardwood paling fence used in Australia, after preservative treatment. Unseasoned rails, palings and plinths of the low natural durability species Eucalyptus regnans (mountain ash) and E. obliqua (messmate) were treated with PEC (pigment emulsified creosote) or PROCCA (an oil emulsion of CCA). Treated posts of these species were also compared ...
L J Cookson D Scown, B Iskra


Performance of borate-treated sill plates (dodai) in a protected, above-ground field test in Japan
2002 - IRG/WP 02-30278
This document is supplemental to the previous IRG document (IRG/WP 2000-30239). An experiment to simulate the dodai (sill plate) of the Japanese houses was conducted at the termite field test site of the Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. DOT...
K Tsunoda, A Adachi, A Byrne, P I Morris, J K Grace


New conception for shortering the duration of fungitoxic test of wood preservatives. Part 2: Computer-assisted miniaturisation of wood specimens
1994 - IRG/WP 94-20052
The mass loss of wood used as a criterion in the standarised agar-block method of evaluation of toxic value of preservatives depends upon the relationship between volume of specimens, their outspread planes and ratio of areas of particular anatomic sections. Upon the computer-assisted mathematical basis the dimensions of miniaturized specimens which make 1/2, 1/4, and 1/8 part of standarized ones ...
J Wazny, K J Krajewski


Evaluating the potential of amine chemicals for use as wood protecting agents. Part 1: Investigation of cation components of quaternary ammonium compounds
1994 - IRG/WP 94-30049
Quaternary ammonium compounds (quats) have shown a great potential as more environmentally acceptable wood preservatives. In order to identify chemicals possessing the wood protecting potential, an evaluation was carried out of a range of commercially available 'quats', using a modified soil block test. Ponderosa pine sapwood blocks were treated with selected 'quat&a...
Hang Tang, J N R Ruddick


Decay resistance of densified ammonia-plasticized stems of oil palm (Elaeis guineensis)
1991 - IRG/WP 3673
When wafers of oil palm stems (Elaeis guineensis) were plasticized with 28% aqueous ammonia and immediately compressed mechanically, the treated material, gained 73% in basic density (average basic density, 0.695 g/cm³), and was highly resistant to decay by wood rot basidiomycetes. Compared with the control specimens (density, 0.403 g/cm³), resistance to decay of the densified specimens by Corio...
A H H Wong, M P Koh


Bacteria are important degraders of cooling tower timbers: New Zealand experience
1995 - IRG/WP 95-10128
Microscopic examinations of CCA-treated Pinus radiata timbers in industrial cooling towers in New Zealand showed bacteria and soft rot fungi to be primarily responsible for the decay of these timbers. Of these micro-organisms, erosion bacteria appeared to be most widespread, attacking wood cell walls independently as well as together with tunnelling bacteria and soft rot fungi. Tunnelling bacteria...
A P Singh, R N Wakeling


The dry rot fungus (Serpula lacrymans) in nature and its history of introduction into buildings
1999 - IRG/WP 99-10300
For many years the True dry rot fungus (Serpula lacrymans (Wulf.: Fr.)Schroet.) has exclusively been found in buildings. That is why it is called the True dry rot fungus. The origin of the fungus has always been a mystery, but a wild ancestor must have occured. In the literature there is some information about finds of Serpula lacrymans in nature, however it is difficult to distinguish it from the...
J Bech-Andersen, S A Elborne


Dimensional lumber model demonstrates the sensitivity of the particle capture immunoassay in early detection of brown-rot fungi
1995 - IRG/WP 95-20058
A dimensional lumber model was designed to test the sensitivity of the particle capture immunoassay (PCI) compared to traditional methods of culturing and microscopic examination for detection of brown-rot fungi. Southern yellow pine 2 x 4's (5.1x10.2 cm²), and 86.4 cm in length, were inoculated on one end with the brown-rot fungus, Postia placenta, and tested over the full length of the...
C A Clausen, L Ferge


Detection of brown-rot antigens in southern pine
1996 - IRG/WP 96-20090
Brown rot fungal antigens were detected by particle capture immunoassay (PCI) in southern pine 2 x 4's beyond visible or culturable hyphal growth. Further analysis of test samples revealed changes along the 2 x 4's that could be grouped into zones. Zone 1, the point of inoculation through 6 cm, showed low pH, measurable oxalic acid, high moisture, and high protein. Zone 2, throug...
C A Clausen


Lignin degradation by a non-enzymatic system supposed to be active in white rot fungi
2000 - IRG/WP 00-10340
Electron microscopic investigations have shown that ligninolytic enzymes of white-rot fungi are only able to penetrate the wood cell wall in late stages of degradation. Thus, the selective degradation of lignin of certain white-rot fungi can only be explained on the basis of a low molecular weight, highly diffusible system. A system, consisting of copper, a coordination compound and either H2O2 or...
P Lamaipis, W Gindl, T Watanabe, K Messner


Durability of surface coating systems. Mycologg - an accelerated mycological test.
2004 - IRG/WP 04-20301
Field testing and natural aging/degradation of test sample, e.g. coated wooden surfaces is a slow process. Accelerated tests focus on mechanical properties, water uptake or sometimes stain fungi. Artificially weathered coated panels are not easily compared with naturally aged panels, and show the importance of involving the biological component among the degrading facors. It is a need for acce...
L Ross Gobakken, J Mattsson, B Jacobsen, F G Evans


Hemicellulosic induction of oxalic acid in Postia placenta
1994 - IRG/WP 94-10060
Most studies suggest that enzymes produced by brown-rot fungi are too large to penetrate sound wood structures, even after decay begins. Thus, nonenzymatic agents have been proposed to initiate brown-rot decay. We have reported that the brown-rot fungus Postia placenta MAD-698 initiates a 2-fold decrease in wood pH within 7 days of colonization which is mediated by production of oxalic acid. Strai...
F Green III, M Larsen, T L Highley


Biological resistance of wood treated with waterbased resins and drying oils in a mini-block test
1998 - IRG/WP 98-40107
In recent years it was found that the resistance of wood against fungal degradation could be increased by impregnation with an etherificated melamine formaldehyde resin. Using this resin as a reference, a waterbased fatty acid modificated alkyd-resin and two drying-oils were assessed for their biological performance in a mini-block laboratory test. Although drying-oils, like linseed-oil, are often...
M Sailer, A O Rapp, R-D Peek


Comparison of methods for monitoring CCA fixation
1994 - IRG/WP 94-40023
The CCA fixation status in the outer 12.5 mm of pole sections of southern pine (Pinus sp.), red pine (Pinus resinosa) and lodgepole pine (Pinus contorta var. latifolia) were followed during fixation at 21°C under non-drying conditions by the following procedures: - Qualitative CrVI indication by the chromotropic acid spot test. - Quantitative CrVI in the expressate by the diphenylcarbazide method...
P A Cooper, Y T Ung, G Zanjani


A bibliography of the dry rot fungus, Serpula lacrymans
1988 - IRG/WP 1337
For many decades the occurrence of dry rot in buildings has been the cause of serious concern in temperate regions of the world. Consequently, much effort has concentrated on determining the morphology of dry rot and on finding means of prevention and control. During early studies, observers tried to understand the phenomenon of dry rot as a whole, and in the course of the 19th century aspects cha...
G Seehann, B M Hegarty


Occurrence of termite species on decaying heartwood specimens exposed 18 to 23 years at an Australian site
1998 - IRG/WP 98-10270
The occurrence of species of subterranean termites on hardwood and softwood specimens (including preservative-treated), exposed in-ground at a semi-arid site at Walpeup (north-western Victoria), 18 to 23 years after installation, is reported. This paper presents maps of the cumulative occurrence on specimens, after six annual inspections, of the following species: Coptotermes acinaciformis, Hetero...
J W Creffield, J-D Thornton, G C Johnson


Tolerance of Wood Decay Fungi to Commercial Copper Based Wood Preservatives
2002 - IRG/WP 02-30291
Due to the use of copper based preservatives like CCB or CCA for more than a century, copper tolerant fungi have appeared in some European countries in recent times. It is therefore important to find out whether this phenomenon is specific for only classical copper ingredients, or generally for all copper based formulation. Thus, we tested the tolerance of three commercial copper based pres...
F Pohleven, M Humar, S A Amartey, J Benedik


Decay resistance of Platanus acerifolia wood against White Rot Fungi (Coriolus versicolor)
2002 - IRG/WP 02-10431
Degradation of the lignocellulose complex in wood varies on the microorganism causing decay and chemical composition of wood. The weight loss of Platanus acerifolia wood after decay by white rot fungus (Coriolus versicolor) for period 16 weeks were evaluated according to European standard EN 113 and beech wood as a control. The samples were collected in October 2000 from Nantes, France. The aim of...
M Irmouli, O Duchelier, N Ayadi, B Charrier


Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


On the occurrence of Phialophora species in preservative treated wood in ground contact
1977 - IRG/WP 163
Phialophora is a fairly large genus comprising about thirty described species. They are widespread in very diverse environments, such as soil, sea water, wood and wood pulps. Some species are known as parasites on plants and animals, including man. Phialophora species were early known for their ability to produce blue stain in timber. Later it was discovered that several species were able to produ...
T Nilsson, B Henningsson


The long road to understanding brown-rot decay. A view from the ditch
1995 - IRG/WP 95-10101
Interest in understanding how brown-rot fungi decay wood has received increasing interest in recent years because of a need to identify novel targets that can be inhibited for the next generation of antifungal wood preservatives. Brown-rot fungi are unique in that they can degrade holocellulose (cellulose and hemicellulose) in wood without first removing the lignin. Furthermore, they degrade holoc...
F Green III, T L Highley


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 18. Report of seventh inspection (72 months) in Australia
1984 - IRG/WP 4108
This report includes the results for the 72 month inspection of the IRG/COIPM International Marine Test installed in Sydney Harbour. Although, overall, attack by teredinid and limnorid borers have been most commonly encountered in test specimens at this site, slight attack, mainly by sphaeromatids, has recently been initiated on some hitherto unattacked treated Alstonia scholaris and Pinus sylvest...
L J Cookson, J E Barnacle


A shower test protocol for measuring antisapstain wash-off from small individual log billets
1996 - IRG/WP 96-50069
According to New Zealand Timber Industry Federation statistics New Zealand exported 4,835,000 m³ of logs in 1994 and it is estimated that c. 20% were anti-sapstain treated. Loss of preservative from logs as a result of rain impact after application is of considerable concern both with respect to potential loss of efficacy and environmental contamination. Whilst Environment Canada have a proposed ...
A J Pendlebury, H Pearson


Effect of test site, preservative and wood species on decay type Glenbervie pastoral and radiata pine forest sites
2000 - IRG/WP 00-30248
Pinus radiata stakes were treated with 0.8, 1.2, 1.8, 2.7 and 4.1 kg/m3 of CCA and Fagus sylvatica with 2.7, 4.1 and 6.1 kg/m3 of CCA. Both wood species were also treated with equivalent retentions of a copper plus triazole preservative (CT) (0.89, 1.3, 2 and 3 kg/m3 of copper for pine & 2.5 and 4 for beech) and chlorothalonil plus chlorpyriphos in oil (CC) (1.4, 2.1, 3.2 and 4.8 kg/m3 of chlo...
R N Wakeling


Previous Page | Next Page