IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1244 documents. Displaying 25 entries per page.


Durability of wood in the area of wood-inhabiting termites in Slovenia
1981 - IRG/WP 1139
This report describes a research dealing with resistance and durability of five different species of wood. The experiment was made in natural conditions in the Slovene area of wood-inhabiting termites. The results of our experimental field, which correspond to the results of the former laboratory experiments, show a very weak resistance of spruce-wood, fir-wood, and beech-wood. They also show thei...
L Kervina


Physiologic response of Phanerochaete chrysosporium to exposure to triazole fungicides
1994 - IRG/WP 94-10066
Triazoles are increasingly important fungicides which are employed for a variety of applications included wood protection. Several recent studies suggest that white rot fungi are more tolerant of triazole compounds than other wood degrading fungi. Cultural studies using a white rot fungus, Phanerochaete chrysosporium, and 0.2 or 0.8 ppm of tebuconazole or propiconazole suggested that mycelial dry ...
J J Morrell, R K Velicheti


Evaluating the potential of modified wood for use in marine environments using a short-term laboratory bioassay
2004 - IRG/WP 04-10525
Chemically modified wood may be an alternative to preservative treated timber for marine structures. In this study a screening laboratory test using the wood-boring isopod crustacean Limnoria quadripunctata was used to assess the durability of chemically modified Pinus sylvestris, Pinus radiata and Picea sp. Most of the treatments used a combination of one of two of types of the resin dimethyloldi...
L M S Borges, S M Cragg, M van der Zee


Information from the COIPM Wood Group
1986 - IRG/WP 4130
The Chairman outlined the progress of the co-operative work "testing the resistance to marine borers of heat shrinkable polyolefin sheathings and of wood treated by vacuum/pressure with polymers (polystyrene)". The first part of the work has been started: the samples of wood wrapped with shrinkable polyolefin sheathings have been prepared and sent to the stations participating. The second part of ...
A Gambetta


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests. Results after 40 months fungal cellar exposure
1983 - IRG/WP 2200
Decay rates of preservative-treated Pinus radiata stakes during 40 months exposure in the FRI fungus cellar were compared with those of similarly treated material in a field test. Decay rates in the fungus cellar were from 4 to 100 times higher than in the field, although for the majority of preservatives the rate was between 7 and 12 times higher. The lag phase before onset of decay, noticeable w...
M E Hedley


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki


An evaluation of CCA, CCB and CCP preservatives using a "sandwich test"
1991 - IRG/WP 2370
The last two years has seen some important changes in standards and preservative types used in Scandinavia, which have led to a wider choice for specifiers. In order to identify those treatments suitable for replacement or reinforcement of decayed constructional timbers, it was felt necessary to modify the standard EN 113 test. Impregnated blocks were sandwiched between two untreated blocks, previ...
A P Koch, L B Sheard


Methyl bromide eradication of the oak wilt fungus in logs. Laboratory and field fumigation
1981 - IRG/WP 3168
Concern over accidental introduction of the oak wilt fungus (Ceratocystis fagacearum) into oak-importing nations has prompted a study supported by the U.S. National Lumber Exporter's Assn. to assess the efficacy of methyl bromide fumigation to eradicate the fungus from logs and lumber. Laboratory and field fumigation trials to develop a reliable and realistic treatment were performed on r...
E L Schmidt, M M Ruetze, D W French


Work programme of CEN/TC 38 (April 1999) and European publications
1999 - IRG/WP 99-20165
Scope of the CEN/TC38: Standardization of the characteristics of natural or conferred durability of wood and its derived materials against biological agents, including the characteristics of protection products and associated processes to obtain this durability. This applies in particular to: - the identification of hazard classes-, - the test methods (wood preservatives and treated wood and wood ...
R Hüe


A Soil Bed Test of the Effect of CCA Penetration on the Performance of Hem-fir Plywood
2004 - IRG/WP 04-30332
An accelerated decay test was set up to compare the performance of CCA-treated Western hemlock/amabilis fir plywood treated to meet the preserved wood foundation (PWF) retention standard with various patterns of preservative penetration. Short lengths of treated plywood and comparable untreated material were installed in a soil bed. After eleven years of exposure, the CCA treatments were all sou...
P I Morris, J K Ingram


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Screening of lignin peroxidase from white-rot fungi
1998 - IRG/WP 98-10274
Since lignin peroxidase was first found in the ligninolytic culture of Phanerochaete chrysosporium, it has been regarded as an enzyme responsible for the lignin biodegradation and studied comprehensively. As the results of these studies its unique characteristics have been revealed. On the other hand, the features of lignin peroxidase produced by other white-rot fungi have not been studied so much...
I Momohara


Bending creep test of plywoods under long term exposure to fungal attack
1981 - IRG/WP 2163
Bending creep test and decay test were coupled in order to evaluate the durability of structural plywoods and preservative efficacy. Experimental blocks, 5.0 x 1.2 cm² section x 35.0 cm length, were impregnated with distilled water and inoculated with mycelial fragments of test fungus. Polyethylene bags stretched with metal frame were used as decay chambers. The chambers containing inoculated blo...
M Takahashi


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980's against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


Premature decay of CCA-treated pine posts in horticultural soils - An overview
1984 - IRG/WP 1241
The recent discovery in New Zealand of early decay in CCA-treated pine posts set in horticultural soils led to the establishment of a comprehensive research programme. The objectives and outline of this programme are presented together with an overview of research progress to date. Results suggest that premature decay of CCA-treated timber is restricted to material placed in highly cultivated soil...
J A Butcher


Oxalate production and calcium oxalate accumulation by Gloeophyllum trabeum in buffered cultures
1994 - IRG/WP 94-10075
Most basidiomycetous fungi produce oxalic acid as a result of their metabolic activities and nutrient procurement. There is currently a renewed interest in the role that oxalic acid may play in the decomposition of wood by basidiomycete fungi. It has been observed that although most wood degrading fungi have the capacity to produce oxalic acid, not all of these organisms express this capacity equa...
J H Connolly, J Jellison


Calculation of preformance index of Bardac 20 (an alkylammonium compound) evaluated in a field stake test
1982 - IRG/WP 3206
Bardac 20 treated stakes have been in test for three years at the Westham Island test site near Vancouver, B.C. The Performance Index for the preservative was calculated and found to be 0.009 which infers that, at the standard retention, Bardac 20 added 0.9 y to the life of the stake. It may be concluded that when tested using a standard field stake test using ponderosa pine (Pinus ponderosa Laws)...
J N R Ruddick


Correlation between different international standard assessment procedures with termites. Part 1: Field exposure
1983 - IRG/WP 1198
Ramin treated with copper-chrome-arsenic (CCA), pentachlorophenate and lindane, each at three retentions, and three other untreated timbers were assessed in the field against Coptotermes lacteus and Nasutitermes exitiosus. Replicate specimens were exposed around five mounds of each termite species over a period of five years in south-eastern Australia. The field results provided the basis for judg...
M Lenz, C D Howick, N Tamblyn, J W Creffield, M Westcott


Leaching results of shower test on L-joints with boric acid, bifluoride and TBTO rods
1995 - IRG/WP 95-50051
As part of the EC-project "Improvement of a local preservation process for wood products with reduced environmental impact", TNO has performed a leaching test on L-joints treated with pills with boric acid (Defence corner), bifluorides (Woodpil 55) and TBTO (Woodcap). The L-joints were exposed in an adapted shower test during 10 days, using 70 liters of water per day. The experiment is designed to...
P Esser, M J Boonstra, W L D Suitela, A J Pendlebury


Identification of terminal structures in cellulose degraded by the brown-rot fungus Postia placenta
1989 - IRG/WP 1389
To gain insight into the biochemical mechanism employed by brown-rot fungi to depolymerize cellulose, we identified the end-groups of chemically pure cellulose that had been depolymerized by the brown-rot fungus, Postia placenta. The depolymerized cellulose was acid hydrolyzed and the anion fractions isolated by ion chromatography. Sugar acids were identified by gas chromatographic and mass spectr...
T K Kirk, T L Highley, R E Ibach, M D Mozuch


Biosynthesis of ß-Glucan microfibrils by cellular fractions from brown-rot fungus Postia placenta (MAD-698 and ME-20) and white-rot fungus Schizophyllum commune (MAD-619)
1993 - IRG/WP 93-10025
In this study, we compared the brown rot fungus Postia placenta (MAD-698 and ME-20) with the white rot fungus Schizophyllum commune (MAD-619) to determine the location and distribution of glucan synthetase. We also measured the soluble protein content in subcellular fractions obtained by differential centrifugation MAD-698 is a degradative isolate, but ME-20 and MAD-619 do not produce significant ...
S C Croan, T L Highley


Previous Page | Next Page