Your search resulted in 1244 documents. Displaying 25 entries per page.


The preliminary characterization of ß-1,4-xylanase of the brown-rot fungus Gloeophyllum trabeum
1990 - IRG/WP 1447
The extracellular ß-1,4-xylanase of the brown-rot fungus, Gloeophyllum trabeum, was isolated from crude extract by chromatofocusing method (PBE 94 column chromatography). The isoelectric point was estimated to 4.2-4.8 by cromatofocusing and 4.5 by isoelectric focusing (IEF). The molecular weight of the enzyme was estimated to 37,000 dalton by SDS-PAGE. The optimal temperature for the crude extrac...
A-C Ritschkoff, M Rättö, L Viikari


Computer-assisted numerical clustering analysis of various strains of Serpula lacrymans (Wulfen:Fr.) Schroeter apud Cohn
1992 - IRG/WP 92-2396
Eight strains of Serpula lacrymans were compared in relation to their previously determined factors (5 physiological and 10 toxicometrical). A numerical clustering analysis was used along with, as coefficient of similarity, "cos Q" after standardization of all results. Results with respect to the combined factors showed a mutual similarity within four groups of strains. The first of these groups c...
J Wazny, J D Thornton, P Stenzel


The variability of preservative distribution in test blocks
1973 - IRG/WP 220
The techniques for the assessment of likely effectiveness of preservative systems have long been the subject of much discussion. The whole field has recently been reviewed by Hilditch and Hamblyn (1971) who described in detail many of the laboratory test procedures used, but who also indicated the deficiencies in many of these techniques. It has long been the view of many associated with the wood ...
F W Brooks, M R Gayles, R W Watson


The effect of low molecular weight chelators on iron chelation and free radical generation as studied by ESR measurement
2000 - IRG/WP 00-10367
The focus of this work was to improve our current knowledge of the non-enzymatic mechanisms involved in brown-rot decay. Electron Spin Resonance (ESR), also known as Electron Paramagnetic Resonance (EPR), is an attractive technique for the identification and study of chemical species containing unpaired electrons (such as radicals and certain transition metal species). ESR spin-trapping techniques...
Yuhui Qian, B Goodell


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 9: Report of third inspection (2 years) in Italy
1980 - IRG/WP 461
The wood samples were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitudine 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian sea. The recorded temperature varies between 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 1 year (4/1978) and 2 years (4/1979)....
A Gambetta, E Orlandi


How to keep coated wood structures sufficiently dry to avoid damage caused by rot
1991 - IRG/WP 2376
During the last ten years, a new type of problems with wood rot has emerged in Scandinavia. Thousands of houses have been damaged by wood rot attaching to the exterior wood panel. This paper provides an overview of finished and ongoing work in order to identify the cause of these problems. In field tests, the moisture conditions were measured in panels coated with different paint systems. The infl...
S Hjort


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 7: Second report on the samples in Papua New Guinea
1980 - IRG/WP 459
This report presents the findings to date regarding specimens installed in Papua New Guinea, as part of a world-wide marine trial of certain timbers treated with CCA or CCB preservatives. The details of the trial are set out in document number IRG/WP/414. The report discusses the findings in the context of the conditions prevailing at the trial site and of the properties of the trial timbers. The ...
S M Cragg, C R Levy


Biological resistance of phenol-resin treated wood
1990 - IRG/WP 3602
Biological resistance of PF (phenol formaldehyde resin) - treated wood has been tested in relation to the resin properties, wood species and biological factors. When tested using water-soluble PF (mol. wt. 170), ca. 10% RI (resin impregnation) was enough to suppress the decay of Japanese cedar (Cryptomeria japonica) and western hemlock (Tsuga heterophylla) blocks exposed to Tyromyces palustris (br...
M Takahashi, Y Imamura


Ekki heartwood - is “Durable”
2002 - IRG/WP 02-10444
Severe decay damages of bridges made of ekki (Lophira alata Banks) wood which is classified as a durable species in the EN 350:2 as already reported at the 31 IRG annual meeting. This paper deals with results of long-term decay tests of ekki heartwood specimens using 3 isolates (Loweporus tephroporus 2 strains and a fungus of other sp. from damaged ekki bridges) and Trametes versicolor as a refere...
S Doi, R Itoh, S Horisawa


Test Methods – Performance Based Requirements
2004 - IRG/WP 04-20297
In this paper is briefly described the present approach to service life prediction as an essential part of the architectural engineering process. The system of testing the durability of wood is described more in detail including laboratory tests as well as field trials. It is concluded that the system has a lot of weaknesses which makes it less well suited for practical building applications. A le...
M-L Edlund, F Englund, J Jermer, T Nilsson, M Westin, K Ödeen


Suppression of aerial hypha formation by spent culture filtrate of a non-degradative strain of Postia placenta
1991 - IRG/WP 1498
ME20, a wild-type monokaryotic strain of the brown-rot fungus Postia placenta, does not cause significant weight losses in standard soil-wood block decay tests and fails to form aerial hyphae in liquid and agar culture. This abnormal morphological feature may be caused by the same aberrant physiology that prevents the strain from degrading wood efficiently. ME20 releases elevated levels of the aut...
J A Micales


Evaluating the natural durability of a number of lesser known species of Ghanaian hardwoods using a short term laboratory assay
2004 - IRG/WP 04-10540
Resistance of a number of Ghanaian hardwoods to attack by the crustacean Limnoria quadripunctata was assessed by measuring the production of faecal pellets under forced feeding conditions over a two week period. Small sticks of commercially available, lesser known timber species, were leached in seawater for one week then placed in a cell culture chamber with one animal and 4 ml of seawater. At in...
J R Williams, S M Cragg, L M S Borges, B Shayler


Test methods used for approval of wood preservatives in Indonesia
1994 - IRG/WP 94-20045
Indonesian regulation stipulates that all pesticides, including wood preservatives, must be registered and obtain legal permit from the Minister of Agriculture, c.q. the Pesticide Committee before they are eligible for public use. For that purpose they have to meet safety and efficacy requirements approved by the Pesticide Committee. To meet the efficacy requirements, wood preservatives must be te...
A Martawijaya


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 20: Report on the inspection of specimens at Sekondi, Ghana after 48 months
1985 - IRG/WP 4116
The results of the second inspection of CCA- and CCB-treated test panels exposed at Sekondi, Ghana, in June 1980, are presented. The panels of Pinus sylvestris treated with 3% CCA are stil unattacked after 48 months. Panels treated with 10% CCA and still in test (Fagus sylvatica, Pinus sylvestris and Alstonia scholaris) are still free of attack. Locol species treated with 3% CCB have all been dest...
F F K Ampong, N Asare-Nyadu


Effect of mineral wools on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi
1991 - IRG/WP 1481
The influence of stone wool and glass wool on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi was studied. Mass losses of pine wood caused by Serpula lacrymans and Gloeophyllum trabeum were increased when stone wool was present. Glass wool had no influence on mass losses. Coniophora puteana, Serpula lacrymans and Gloeophyllum trabeum grew into stone wool and destroy...
L Paajanen, A-C Ritschkoff


Wood degradation mechanisms by the brown rot fungus Gloeophyllum trabeum
1997 - IRG/WP 97-10229
A mechanism for the degradation of wood by the brown rot fungus Gloeophyllum trabeum is outlined. The mechanism includes the function of redox-cycling, low molecular weight phenolic derivatives which sequester and reduce iron in acidic environments. The role of oxalate for the sequestration of iron (hydr)oxides and the pH dependent transfer of iron to the G. trabeum phenolic chelators, as well as ...
B Goodell, J Jellison


Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell


Natural durability of wood in ground contact - A correlation between field and laboratory tests
1985 - IRG/WP 2182
A field test is being carried out to evaluate the natural durability of 20 hardwoods. The resistance to decay and termite attack was evaluated in accelerated laboratory tests. The results of the field test after 6 years and 8 months indicate that there is not necessarily agreement between results from laboratory and field tests. It is pointed out that apart from the artificiality of the laboratory...
M S Cavalcante, G A C Lopez, R G Montagna, M E S Fosco Mucci


Co-operative field trial. Background notes and questionnaire for field sites
1992 - IRG/WP 92-3733
The first co-operative field trial was designed to study the occurrence of soft-rot in CCA treated hardwoods. Generally speaking very similar results were obtained from the different field sites. In the early part of the trial considerable variability was evident with regard to the rate and type of attack which occurred in the untreated material. With the CCA treated timber the type of decay was p...
D J Dickinson


In-ground evaluation of a copper azole wood preservative (Tanalithâ E) at a tropical Australian test site
1996 - IRG/WP 96-30100
A field trial to determine the in-ground termite and decay resistance of Pinus radiata D. Don impregnated with a copper azole formulation, TANALITHâ E, has been established at a tropical site in the Northern Territory of Australia. Four retentions of TANALITHâ E, containing 1.54, 2.08, 2.92 and 4.30 kg/m³ of Cu, are being evaluated. For comparison, Pinus radiata specimens treated to two retenti...
J W Creffield, J A Drysdale, N Chew


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 4: Report of second inspection (12 months) in Australia
1979 - IRG/WP 448
Previous reports have presented full details of the treatment and installation of the test specimens in Sydney Harbour during December, 1977, and of the results of the first (6 months) inspection made during June, 1978. At the June inspection it was apparent that the plastic tubing used to make up the frames from which to suspend the specimens was inadequate for the job and not strong enough to su...
J Beesley


Natural resistance of different species of timber to marine borer attack in the Trondheimsfjord (Western Norway)
1978 - IRG/WP 435
Natural resistance of 34 timber species to marine wood-borers has been discussed, based on data collected from panels immersed in selected localities in the Trondheimsfjord during 1977-78. The wood-borers encountered on the panels were Psiloteredo megotara, Xylophaga dorsalis, Xylophaga praestans and Limnoria lignorum. The number of borers present and their growth were taken as the criterion for a...
L N Santhakumaran, J A Sneli


Ten year field test with a copper-borate ground line treatment for poles
1993 - IRG/WP 93-30017
A wood preservative paste consisting of borax and copper naphthenate has been tested to determine its efficiency in protecting wood from decay fungi and insects. The paste was applied to polyethylene-backed wraps that were fastened to the below-ground portions of unseasoned southern pine pole stubs. After 4 years of exposure in Mississippi, the untreated control stubs were completely deteriorated....
T L Amburgey, M H Freeman


Chemical analyses of IRG/COIPM INTERNATIONAL MARINE TEST (to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water) samples
1987 - IRG/WP 4114
Chemical analysis of CCA and CCB treated timber was carried out after exposure at tropical and temperate marine sites. Results indicated that losses of all elements had occurred. In particular, losses of boron were severe. Arsenic and copper were also lost. The chromium components in both formulations was the most dominant metal remaining. The results suggest that chromium modification was importa...
L E Leightley


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...