From fungal detoxification systems to wood durability in neotropical forests
2019 - IRG/WP 19-10946
White-rot fungi are able to mineralize all the wood components due in particular to an efficient detoxification system. We hypothesised that components of this detoxification systems, glutathione transferases, could be used as tools to explore the natural durability of neotropical wood species. Analysis of the interactions between six glutathione transferases of Trametes versicolor and extracts of...
T Perrot, G Salzet, N Amusant, J Duchene, E Gelhaye


Characterization of Pectinases from Brown-rot Fungus Fomitopsis palustris
2019 - IRG/WP 19-10951
Brown-rot fungi occur on softwood used as building materials and cause destructive breakdown of wood structure. Therefore, a more accurate understanding is important from the perspective of wood protection. Previous studies have reported that hyphae of brown-rot fungi go through bordered pits on tracheids when the fungi grow into softwood [Francis W.M.R.Schwarze (2007)], and torus existing in the ...
Y Tanaka, N Konno, T Suzuki, N Habu


Chemical composition, antitermite and antifungal activity of Dacryodes edulis oleoresin
2019 - IRG/WP 19-20653
Damages to wood structures and other cellulosic materials caused by wood destroying insects and fungi are estimated to several billions of dollars each year in the world. Among these, termites are considered as one of the most economically important pests for wooden structures. In the past, several wood protection chemicals like CCA, creosote, lindane or pentachlorophenol have been used. However, ...
W F Bedounguindzi, K Candelier, P E Engonga, Se Dumarcay, M-F Thevenon, P Gerardin


Improvement of analytical methods of wood preservatives and its validation with collaborative testing
2019 - IRG/WP 19-20655
This discussion paper presents on-going collaborative test of analytical methods of wood preservatives according to the standardization process of Japan Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries (MAFF). Food and Agricultural Materials Inspection Center (FAMIC) in close cooperated organization with the MAFF, has wide range of tasks about inspections and anal...
T Miyauchi, K Yamamoto, N Shota, Y Akabori, M Ikeda, J Eisawa, K Kambara, T Osawa, C Igarashi, Y Baba, W Ohmura, M Shimizu, M Samejima


Hydroxyl accessibility - A brief review of deuterium exchange studies on modified wood
2019 - IRG/WP 19-20656
Wood modification imparts dimensional stability and decay resistance. The mechanism(s) by which this occurs are thought to be related to the bulking of the wood cell wall and subsequent moisture exclusion. Hence, quantification of accessible hydroxyl (OH) groups is of great interest when evaluating and increasing the understanding of the performance of modified wood. The aim of this study was to b...
G Beck, C Hill, G Alfredsen


Durability classification of preservative treated and modified wood
2019 - IRG/WP 19-20659
EN 350 (2016) allows formally to determine durability classes (DC) for wood products and wood-based materials, which was previously only possible for untreated wood in the form of natural durability. In a first study, the University of Goettingen carried out the durability classification of chemically modified (modified with 1,3-dimethylol-4,5-dihydroxyethyleneurea, DMDHEU) and preservative-treate...
S Bollmus, L Bachle, C Brischke, H Militz


Development of accelerated decay test for CLT using a fungus grown on agar medium
2019 - IRG/WP 19-20664
CLT is a large-scale wooden board which consists of several layers of sawn lumber stacked in altering directions. Therefore, a lot of large cross sections appear on all narrow faces of CLT. As water penetrates easily into timber from cross section, wooden material whose cross section is exposed to water in in a usage environment is susceptible to deterioration by organisms. Wood deterioration orga...
T Miyauchi, K Kambara, W Ohmura, T Mori, H Matsunaga, N Hattori


Biocidic effect of nano metal fluorides against brown-rot fungi
2019 - IRG/WP 19-30732
Metal fluoride nanoparticles are promising because of their low water solubility, which reduces the need for fixatives required in widely used active ingredients in wood preservatives such as copper and boron. The effectiveness of nano metal fluorides was compared to sodium fluoride treated wood samples. Wood specimens treated with homo-dispersed sols of MgF2 and CaF2 were tested against brown-rot...
S M Usmani, K Klutzny, I Stephan, E Kemnitz


Relative efficacy of various oxine copper formulations against brown-rot fungi
2019 - IRG/WP 19-30741
This paper investigates the relative resistance of three different oxine copper formulations (oil-borne, water-borne, water-borne with pH-adjustment) as a preservative treatment for wood against brown-rot fungi. Impregnated southern pine sapwood cubes were exposed to R. placenta and G. trabeum cultures in a soil-block test. After eight weeks, the weight losses of the cubes were examined in relatio...
M Petruch, J Lloyd, A Taylor


Performance of field cut preservatives above-ground and in ground contact exposures
2019 - IRG/WP 19-30742
Field cut preservatives are needed to protect cut ends and drill holes that expose the untreated interior of preserved wood. A series of field cut preservatives were assessed in ground contact and above-ground exposures. After 10 years in ground contact exposure, all of the untreated controls had failed or exhibited very advanced decay. In contrast, the copper naphthenate (2% Cu in mineral spirits...
R Stirling, D Wong


Color change of timber exposed outdoors - Influence of season exposure test starts
2019 - IRG/WP 19-40865
For the client the material and color of the exterior wall are important, because they affect the impression of the building [1]. However, discoloration of the exterior wall begins as soon as the building is completed, by various factors such as rainfall. We tried to quantitatively evaluate the changes of the exterior wood, and to organize the influences of climate conditions, in order to use the ...
K Usami, H Ishiyama


Chemical Analysis of Southern Pine Pole Stubs Sixty Months Following Treatment with a Methylisothiocyanate-Based Solid Fumigant Stick
2019 - IRG/WP 19-30740
Methylisothiocyanate-based fumigants have been commercially used in the United States for over 35 years to control internal decay in utility poles and other wooden structures with little technological advancement. The most recently commercialized methylisothiocyanate-based fumigant is chemically known as dazomet. Dazomet is a free-flowing powder or granule that decomposes in the presence of mois...
D J Herdman, T Pope, R R Browning


Different levels of acetylation lead to groupwise upregulation of non-enzymatic wood degradation genes of Rhodonia placenta during initial brown-rot decay
2020 - IRG/WP 20-10958
Rhodonia placenta, often used as a model fungus to represent brown rot fungi, uses a two-stepped degradation mechanism to degrade wood. Regarding the overcoming of wood protection systems the initial degradation phase seems to be the crucial point. A new laboratory test enables the separation of the non-enzymatic oxidative and the enzymatic degradation phases, which has previously been proven chal...
M Kölle, R Ringman, A Pilgård


FTIR analysis of wood blocks decayed by brown-rot fungi
2020 - IRG/WP 20-10959
Calibration curves of the relative lignin contents in Cryptomeria japonica decayed by brown-rot fungi were developed with Infrared Spectroscopy and Klason technique. First, wood decay test was conducted using brown-rot fungi (Fomitopsis palusris, F. pinicola, Wolfiporia cocos, Gloeophyllum trabeum, and Neolentinus suffrutescens) and white-rot fungus (Trametes versicolor) was used as a comparison. ...
R Kondo, Y Horikawa, R Kose, M Yoshida


Performance of naturally durable decks after 15 years of field exposure
2020 - IRG/WP 20-10963
A decking test of Canadian species considered to be naturally durable was inspected after 15 years of exposure at test sites in Ontario and British Columbia. Based on the materials used in this experiment, Douglas-fir and yellow cypress had the greatest decay resistance, followed by eastern white cedar and western redcedar, and then by western larch and tamarack. All materials tested were more dur...
R Stirling, D Wong


Performance of bio-based building materials – durability and moisture dynamics
2020 - IRG/WP 20-20666
When exposed to conditions favourable for decay, bio-based building materials can be susceptible to degradation. Their ability to withstand deterioration over time (performance) depends on the intrinsic or enhanced durability of the material as well as its wetting and drying behaviour. The effect of fungicidal components in wood is known since long. Other material characteristics, such as the mate...
L De Ligne, J Caes, S Omar, J Van den Bulcke, J M Baetens, B De Baets, J Van Acker


Water interactions in wood polyesterified with sorbitol and citric acid
2020 - IRG/WP 20-40888
Polyesterifcation of wood with sorbitol and citric acid seems to be a promising chemical wood modification technique that is both low-cost and produced from bio-based chemicals. An interesting aspect of the modification is the interaction of water with the polyesterified wood since the relationship with moisture appears to be unique compared to other wood modification systems. This communication p...
G Beck, A Treu, E Larnøy


Long-term field exposure of wood-plastic composites processed on a commercial-size extruder
2020 - IRG/WP 20-40894
Wood-plastic composites (WPC) contain wood fiber (or flour), thermoplastics and additives and are exposed to UV light, moisture, and biological deterioration in outdoor installations. Accelerated laboratory tests can help to predict the durability of WPCs, but long term evaluations are needed to validate these results. Field exposed above-ground WPC deck boards (30.5 x 139.7 x 609.6 mm) and in-gro...
R E Ibach, C M Clemmons, N M Stark


Impact of fungal decay on the bending properties of wood
2020 - IRG/WP 20-20671
Wood used outdoors is generally prone to fungal degradation, and its impact on the structural integrity of wood is an immanent factor for service life planning with timber. Wood decayed to very small mass losses can suffer from a significant reduction in mechanical strength and elastic properties. Hence, the latter are preferred indicators to detect decay in wood durability studies. Numerous previ...
S Bollmus, P B van Niekerk, C Brischke


The iron reduction by chemical components of wood blocks decayed by wood rotting fungi
2021 - IRG/WP 21-10979
Brown-rot fungi, a group of wood rotting fungi, is well known to be one of major microorganisms that cause the deterioration of wooden buildings in Japan and have been considered to use chelator-mediated Fenton (CMF) reaction in concert with hydrolytic and redox enzymes for degradation of wood cell wall. CMF can be described as a non-enzymatic degradation system that utilizes hydroxyl radicals pro...
R R Kondo, Y Horikawa, K Ando, B Goodell, M Yoshida


Changes in topochemistry and mechanical properties of Beech (Fagus orientalis L.) by natural fungus infestation
2022 - IRG/WP 22-10986
Beech is one of the major hardwood species in Europe. It is, however, highly susceptible to fungal attack both in the fresh state and during the storage. Understanding the alteration in chemical and mechanical properties of beech wood during the initial degradation state can lead to improved raw material utilization. Therefore, UV-microspectrophotometer (UMSP) and High-Performance Liquid Chromatog...
H Sivrikaya, M Rehbein, F Divos, S Adamopoulos, R Hosseinpourpia


In Vitro Growth of the Basidiomycetes Physisporinus vitreus strains in various conditions in comparison with some white rot fungi
2022 - IRG/WP 22-10987
The paper has preliminary test results to select Pysisporinus vitreus fungal strains for further experiments in a large research project on copper tolerance of P. vitreus by chemotropic test, choice test, and agar plate toxicity tests and determination of the effect of various ions on oxalic acid secretion by these white rot fungi. In the project, it is also aimed to run fungal decay tests to dete...
E E Soytürk, S N Kartal


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang


Combining MRI and X-ray CT to monitor fungal decay of plywood and OSB in a lab test
2022 - IRG/WP 22-20683
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, T Núñez Guitar, C Vanhove, J Van Acker, J Van den Bulcke


Above-Ground Termite Resistance of Naturally Durable Species in Ontario and Mississippi
2022 - IRG/WP 22-30767
A collaborative above-ground protected termite field test was initiated by FPInnovations and the USDA Forest Service at sites in Ontario and Mississippi. The aims of the experiment were to compare the rate of attack in protected, above-ground exposures by the subterranean termite species, Reticulitermes flavipes, between northern (Ontario) and southern (Mississippi) test sites and to generate perf...