Limited variability in biological durability of thermally modified timber using vacuum based technology
2011 - IRG/WP 11-40567
The SmartHeat® thermal timber treatment is a new technology based on the process parameters being steered very precisely mainly due to the vacuum applied and heating system involved. Timber treated with this technology shows a potential for less variability of biological durability in one batch. Several batch treatments were sampled and assessed on statistical variability of decay resistance agai...
J Van Acker, S Michon, J Van den Bulcke, I De Windt, B Van Swaay, M Stevens


Effect of Nano-silver Treatment on Densified Poplar Wood Properties. Part Two: Spring Back, Compression set, Impact Load Resistance and Hardness
2011 - IRG/WP 11-40568
This paper is the second part of the study of applying nano-silver treatment before densification of poplar wood (Popolus alba). The specimens were prepared in four groups of: 1) nano-silver impregnated 2) water impregnated 3) dried with no impregnation and 4) the control specimens. The impregnation process was done by empty cell process. Then, the groups of 1 to 3 were compressed in a hot press a...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khajeh


Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria). The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, S Bollmus


Effects of nano-silver on brittleness of heat-treated solid woods
2011 - IRG/WP 11-40572
The present study is aimed at the effect of heat-treatment of normal as well as nano-silver-impregnated Populus nigra, Populus deltoides, and Fagus orientalis on brittleness. Specimens were impregnated with 200 ppm water-based solution of nano-silver particles under 3 bars in a pressure vessel using empty-cell process. For heat treatment, both nano-silver-impregnated and normal specimens were kept...
H Reza Taghiyari, B Moradi Malek, A Karimi


Re-use of casting timber
2011 - IRG/WP 11-50283
Re-use of casting timber could be a way of saving timber resources, particularly in countries where most timber for construction purposes has to be imported. The objective of the present study was to investigate residual concrete on casting timber re-used five times. Moulds were made of sections of Norway spruce, untreated and treated with a casting oil and a wax formulation applied by a vacuum-pr...
I Johansson, S Breyne, H Egnell, J Jermer


Effect of an antioxidant on the efficacy of organic wood preservatives in an accelerated soil contact decay test
2012 - IRG/WP 12-30583
In comparison to inorganic wood preservatives, organic biocides in transient carriers are considerably less effective when the treated wood is exposed to soil contact. Various oils are used in some formulations with pentachlorophenol to improve the efficacy. However, use of these oils imparts unacceptable properties to products used in residential applications. Consequently, there is a need to de...
D D Nicholas, J Shi, T P Schultz, L Sites


Effect of Biodiesel on the Efficacy of Pentachlorophenol Treated Wood
2012 - IRG/WP 12-30584
Pentachlorophenol (PCP) is widely used as a wood preservative for utility poles and other wood products. Recently, it has been proposed that a modified PCP carrier system based on a diesel/biodiesel mixture should be used in place of the conventional diesel/KB3 carrier, but there is some question as to whether or not this modified carrier system can provide the same service life for wood products ...
S Keshani Langroodi, H Borazjani, D Nicholas, L Prewitt, S V Diehl


Supercritical impregnation of wood with siloxane
2012 - IRG/WP 12-30595
This paper describes the effect of supercritical impregnation with siloxane on the water repellency of Scots pine (Pinus sylvestris) sapwood samples. Samples were impregnated with a low amount of siloxane dissolved in supercritical carbon dioxide using isopropanol as a co-solvent. Siloxane retention (i.e. weight percent gain (WPG)) of the treated samples was 1.3 % (w/w) as found by mass balance. T...
A Kjellow, F Imsgard, J Fernandes, O Henriksen, E Klaassen, R Wagner, J Delis


Effect of preservative treatment on dimensional stability of plywood made of treated simul (Bombax ceiba) veneer
2012 - IRG/WP 12-40575
The dimensional stability such as thickness swelling and water absorption of plywood made of treated simul (Bombax ceiba) veneers were investigated after 2 hours and 24 hours soaking under water. The veneers were treated with hot water and cold water solution of borax-boric acid (1:1), neem leaves and mahogany seeds of different concentration (1:10, 1:20, and 1:40) at different treatment duration....
K Akhter, M Mahabubur Rahaman, A Ara


The effect of press time on springback and water absorption of acetylated particleboard
2012 - IRG/WP 12-40579
In this study the effect of press time on springback, thickness swelling and water absorption was investigated. After 24 hours soaking in acetic anhydride, in order to achieving WPG 17%, acetylated particles were heated in an oven at 120 0C for 360 minutes. Acetylated and nonacetylated (control) particleboards were produced with 10% melamine urea formaldehyde (based on the oven-dry weight of part...
F Bavaneghi, M Ghorbani, A Kargarfard


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


The resistance of thermo and thermo-oil modified black poplar wood (Populus nigra L.) to Basidiomycetes fungi
2012 - IRG/WP 12-40585
The share of area taken by poplar tree species in Poland account for 2.0% of the area of state forests, 4.8% of national parks and for 2.3% in the privately-owned forests. It is shown and expected an increase in the share of poplar stands connected with plantation of fast growing trees. The poplar wood is not resistant to Basidiomycetes fungi, easy attacked by insects and in consequence is regarde...
A Fojutowski, A Kropacz, A Noskowiak


Microwave Modification of Bamboo Culm to Improve Permeability
2012 - IRG/WP 12-40592
Bamboo is a woody, valuable and strong material that has been used for a long time. In spite of its numerous beneficial properties, bamboo is susceptible to attack by fungus and insect therefore preservative treatment is regarded as necessary. Preservative treatment must provide sufficient uptake and even distribution in the culms for adequate protection. The treatability of dry bamboo, however, i...
K Sugiyanto, P Vinden, G Torgovnikov, S Przewloka


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


The Effects of Industrial-Scale Heat Treatment and Impregnation with Boron Compounds on Water Uptake and Tangential Swelling of Some Wood Species
2012 - IRG/WP 12-40599
This study evaluated the effects of boron impregnation and heat treatment on water uptake and tangential swelling of spruce (Picea orientalis), pine (Pinus nigra), beech (Fagus orientalis) and poplar (Populus deltoides) wood species. The samples (10 x 5 x 40 - tangential x radial x longitudinal cm) were impregnated with 4 % boric acid and 4 % borax according to the ASTM D-1413 standard method. Aft...
A Can, S Yildiz, Ü C Yildiz


The effect of nanozycosil on the water absorption and dimensional stability of Beech wood
2012 - IRG/WP 12-40606
Zycosil is a clear penetrating water repellent. This product works by penetrating into the substrate and modifying the surface tension to inhibit water intrusion. Beech wood (Fagus orientalis) was modified by treatment with nanozycosil. Then water absorption and dimensional stability in terms of volumetric swelling percent and anti-swelling efficiency were determined and found to be improved on t...
M Ghorbani, F Bavaneghi


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and imported Russian spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Effect of growth rate and radial position on the natural durability of Douglas-fir
2012 - IRG/WP 12-10791
In terms of natural durability, Douglas-fir (Pseudotsuga menziesii (Mirb.) Franco) fame owns to the favourable characteristics of centuries-old trees harvested in old-growth North American forests. The properties of wood coming from plantations harvested between 50 and 100 years-old are likely to be different. In such stands, plantation density and thinning intensity may have a large impact on the...
C Pollet, J-M Henin, B Jourez, J Hébert


The effect on moisture content of water trapped in wood joints
2012 - IRG/WP 12-40613
To predict the service life of a structure, a model where the exposure of a structure is compared to its resistance can be used. Which exposure and resistance parameters that are relevant depend on which materials the structure consist of. This approach, with an exposure and a resistance parameter, is similar to the one used in structural engineering where a load (exposure) is compared to the bear...
M Fredriksson, L Wadsö, P Johansson


Water absorption and desorption of non treated, pressure impregnated, and pine oil treated glulam made of small diameter Scots pine and Norway spruce
2012 - IRG/WP 12-40616
A growing proportion of harvested timber originates from the first or second commercial thinning stands in Finland, which means smaller average log volumes in comparison to final felling stands. Smaller log volume means challenging wood properties such as higher proportion of juvenile wood and sapwood. Due to these facts, products made of small diameter logs are prone to twist and check, and have ...
H Heräjärvi, V Möttönen, R Stöd


Surface moulds and staining fungi on acetylated wood – effect of increasing acetyl content
2013 - IRG/WP 13-10797
Wood used in outside applications is susceptible to weathering and photo degradation, which often leads to surface discoloration, loss of brightness and surface deterioration. Research has shown that acetylated wood is more resistant against brown rot, white rot and soft rot, and more dimensionally stable than untreated wood. However, acetylated wood seems still to be disfigured by surface moulds ...
L Ross Gobakken, S Bardage, C J Long II


Micronized Copper Wood Preservatives: Strong Indications of the Reservoir Effect
2013 - IRG/WP 13-30609
Micronized copper wood preservative systems were launched commercially in May 2006. Now, over 75% of the residential lumber produced in the USA is treated with micronized wood preservative formulations. Although considered controversial at first, the mode of action of micronized copper has been clearly defined by multiple authors over the years, as well as a need for a co-biocide in water-borne sy...
M H Freeman, C R McIntyre


Performance testing of DMDHEU-modified wood in Australia
2013 - IRG/WP 13-30613
Chemical wood modification with dimethyloldihydroxy-ethyleneurea (DMDHEU) or its derivatives has been researched for many years and shown to be applicable to improve certain wood properties to both solid lumber and wood-based composites. Earlier research proved a high biological resistance of DMDHEU-modified wood against biological degradation in laboratory and field tests in Europe. Due to the ve...
H Militz, J Norton


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell


Effect of soil contact on reacted copper(II) levels in micronized copper treated wood
2013 - IRG/WP 13-30616
Small 3 to 4 mm thick and approximately 80 to 100 mm long, samples were removed from wood treated with micronized copper quat (MCQ) or micronized copper azole (MCA) and buried full length in a soil bed. Samples were removed after 2, 4 and 8 weeks. The total copper was determined by x-ray fluorescence (XRF) spectroscopy and the amount of reacted micronized copper measured by electron paramagnetic r...
Wei Xue, P Kennepohl, Xingguo Jin, J N R Ruddick