Natural durability of wood tested in different environments in Northern Europe
2011 - IRG/WP 11-10747
Moisture is often recognised as a key factor regarding the long time performance of wooden products, and one of the main challenges for timber products is to predict accurate service life in use class 3 (not covered above ground) and use class 4 (in soil or fresh water contact). A range of durability classification studies have been performed both in field and laboratory. But for several wood spec...
P O Flæte, G Alfredsen, F G Evans


Service life prediction of wooden components - Part 3: Approaching a comprehensive test methodology
2011 - IRG/WP 11-20464
This paper is the third in a series on 'service life prediction' of wooden components and should be considered as a discussion paper. The authors tried to analyze the topic with a look from a distance and comment sometimes with a smile on the current controversial discussion about SLP issues. Nevertheless, the viewpoints of different groups, such as natural scientists, engineers, approva...
C Brischke, C R Welzbacher, L Meyer, T Bornemann, P Larsson Brelid, A Pilgård, E Frühwald-Hansson, M Westin, A O Rapp, S Thelandersson, J Jermer


Quantitative design guideline for wood outdoors above ground applications
2011 - IRG/WP 11-20465
This paper describes the background and principles behind an engineering design guideline for wood in outdoor above ground applications, i.e. use class 3 according to EN 335. The guideline has been developed in the European research project WoodExter and can be seen as a first prototype for a quantitative design tool in the area of wood durability. It is based on a defined limit state for onset of...
S Thelandersson, T Isaksson, E Suttie, E Frühwald, T Toratti, G Grüll, H Viitanen, J Jermer


Performances of Douglas fir in real outdoor use conditions
2011 - IRG/WP 11-20472
The European standard EN 350-2 classifies Douglas fir as moderately resistant to fungal decay on the basis of standardized laboratory and field tests. However, the lifespan expectancy of outdoor structures such as cladding, decking and elements of wood construction carpentry may also vary according to environmental conditions (climate, exposure to weathering), maintenance and design. An investigat...
M Kutnik, S Lepetit, S Le Nevé


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Fixed Borates Anyone?
2011 - IRG/WP 11-30563
The quest for a borate based preservative system that resists leaching or is “fixed” has long been a research goal. Boron fixation has been attempted with numerous strategies but there have been problems associated with past methods. This paper discusses new fixation systems based on bio-materials and presents up to five year outdoor exposure testing on full-size decks. Generally, the new f...
C R McIntyre, M A Lake


Standardized Field Trials with Micronized Copper
2011 - IRG/WP 11-30564
In 2008, an extensive review of all available data from standardized tests of micronized copper systems was published and there has been considerable work since then. This paper discusses over 20 field stake trials underway in well-known sites such as Gainesville, FL, Hilo, HI and the Dorman and Saucier sites in MS as well as tests from Australia and New Zealand. In addition, 4 ground proximity ...
C R McIntyre, M H Freeman


Comparison of rates of wood decay from four different field test protocols following 4-5 years exposure at a site in New Zealand
2011 - IRG/WP 11-30565
The rate of decay of Pinus radiata was evaluated using four different field test protocols at a site near New Plymouth, New Zealand. The average Scheffer index was 86 over the five year period of testing. The field tests were an in-ground stake test (AWPA Std E7-01) and three above ground tests – lap-joint (AWPA Std E16-98), decking (AWPC protocol) and ground proximity tests (AWPA Std E18-06) T...
P Lobb, K Day, A Siraa


Evaluation of an optimized industrial process aiming to improve the natural durability and mechanical behavior of bamboo for outdoor use
2011 - IRG/WP 11-40554
Mao Bamboo (Phyllostachys pubescens) is characterized by high contents of sugar and starch and by high hygroscopicity, which makes it susceptible to biodegradation, and specifically to fungal decay. Still, many bamboo based products regularly enter the European wood construction market, competing with traditional solid wood products used for outdoor decking and cladding. The performance of a heat ...
F Simon, M Kutnik, I Le Bayon, G Moisset, V Gatimel


Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller


Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria). The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, S Bollmus


Characterizing long term leaching behaviour of copper from preservative treated wood in a practical exposure scenario
2011 - IRG/WP 11-50278
To investigate the prediction of the long term emission of copper from preservative treated wood in a Use Class Class 3 scenario, treated boards were exposed vertically above ground to natural weather conditions. The study included two products; an amine copper ACQ-type formulation, air-dried after treatment to a 22 kg/m3 retention, and the same formulation which was hot oil vacuum dried after tre...
T Mark Venås, M Klamer


Extractives in Norwegian-Grown and North American-Grown Western Redcedar and Their Relation to Durability
2012 - IRG/WP 12-10762
The extractives responsible for the natural durability of western redcedar (WRC) are not well understood. Recent work by the Norwegian Institute of Wood Technology and the Norwegian Forest and Landscape Institute has evaluated the natural durability of Norwegian wood species and reference species, including Norwegian-grown WRC and North American-grown WRC, in a series of decay tests. The availabil...
R Stirling, P O Flæte, G Alfredsen, P I Morris


Laboratory and Field evaluation on Natural Resistance and Feeding Preference of Different Wood Species to Subterranean Termites (Isoptera: Rhinotermitidae, Termitidae) in Pakistan
2012 - IRG/WP 12-10769
The resistance of twenty four different woods to attack and damage by subterranean termite species Heterotermes indicola (Wasmann) and Coptotermes heimi (Wasmann) was evaluated by choice and no choic in laboratory and field trials. Mean wood mass loss was calculated for both laboratory and field trials results using Analysis of Variance (ANOVA). Mean percentage termite mortality was calculated fo...
S A Malik; F Manzoor, B M Ahmed (Shiday)


The Significance of Natural Durability of Croatian Mediterranean Wood Species for their Traditional and Present Protection Methods and Use
2012 - IRG/WP 12-10770
The aim of this article is to contribute to the better cognition of the protection and use of some most important Croatian autochthonous Mediterranean wood species. Their traditional use and protection are observed by two aspects. The first one is the presence of these species in the Croatian Mediterranean regions for many centuries, and the long tradition of their use, regardless of their natural...
R Despot, M Hasan


Long term durability of the heartwood of seven common softwood species in above ground conditions
2012 - IRG/WP 12-10771
The natural durability for wood in above ground use has been evaluated based on results after 11 years of exposure in a test site situated at the Danish Technological Institute in Taastrup, Denmark. Selected results for seven common softwood species exposed horizontally are reported. The test results cover samples with direct rain exposure (use class 3 of the European standard EN335-1:2006) and sa...
E Tang Engelund, M Klamer, T Mark Venås, B Lindegaard


Laboratory evaluation of the natural durability and treatability of Cryptomeria japonica grown in La Reunion Island
2012 - IRG/WP 12-10772
The Japanese cedar Cryptomeria japonica is the main resource for timber construction in La Reunion Island, an overseas territory belonging to France. The natural durability of C. japonica originating from East-Asia has been considered so far as quite poor and the European standard EN 350-2 classifies this species ‘not durable’ with regard to its resistance to termites, xylophageous beetles and...
M Kutnik, J Vuillemin, I Paulmier, I Le Bayon, S Legay, E Raphalen, M Jequel, N Farnier, T Glandut


Evaluation of fungal infestation and decay in a simulated use class 3 situation (block test) after some years of exposure
2012 - IRG/WP 12-20487
The so named “block test” was designed as part of the assessment methodology for testing the behaviour of natural and modified wood used under use class 3 (EN 335-2) conditions. The test was developed to expose the wood close to the ground to an environment with high humidity and high biological activity, but not in soil contact. The present study describes the evaluation of fungal infestatio...
A Gellerich, K Röhl, S Adamopoulos, H Militz


Corrosion of fasteners in heat-treated wood – progress report after nine years’ exposure outdoors
2012 - IRG/WP 12-40601
The corrosion of common fastener materials now in use - mild steel, zinc-coated steel, aluminium and Sanbond Z-coated steel – has been evaluated after nine years’ exposure outdoors in untreated and heat-treated (thermally modified) spruce (Picea abies). Spruce from south-western Sweden was used. The heat-treatment was carried out in Finland by Stora-Enso Oy according to the ThermoWood process ...
J Jermer, B-L Andersson


Tar-oil uptake vs time in immersion treatment of short pine posts: A simple technique applicable to rural communities of Papua New Guinea
2012 - IRG/WP 12-40608
Pinus caribaea and Araucaria cunninghamii logs ca. 100 mm in diameter were shortened to lengths 25-30 cm, conditioned to at/below fibre saturation point (FSP) for immersion/dip treatment using a hot- and- cold bath open- tank process. Before oven-drying and subsequent treatment, individual test specimens were numbered, their green weights and volumes, and dry weights recorded for basic density, vo...
B K Gusamo, R Tulo


Classifying white rot decay resistance of some hardwoods from Sarawak and Peninsular Malaysia and correlations with their tropical in-ground durability
2012 - IRG/WP 12-10788
White rot wood decay under Malaysian (humid tropical) terrestrial conditions pose more serious threats to the in-ground service life of hardwoods than other common fungal decay types. A study is made on decay resistance variation for a total combined list of 30 Peninsular Malaysian and Sarawak timber species (plus 6 exotic reference temperate commercial woods for comparison) using the laboratory s...
A H H Wong, J M E Jem, Lai Jiew Kok


Effect of growth rate and radial position on the natural durability of Douglas-fir
2012 - IRG/WP 12-10791
In terms of natural durability, Douglas-fir (Pseudotsuga menziesii (Mirb.) Franco) fame owns to the favourable characteristics of centuries-old trees harvested in old-growth North American forests. The properties of wood coming from plantations harvested between 50 and 100 years-old are likely to be different. In such stands, plantation density and thinning intensity may have a large impact on the...
C Pollet, J-M Henin, B Jourez, J Hébert


Sustainable Mycological Alternatives in Natural forest and Conifer plantations in México
2012 - IRG/WP 12-10792
Concepts of mycoforests, mycosylviculture and their relationship to education, production and sustainable management of fungi in forests in México are analyzed. These concepts may be applied in Mexican protected areas, parks and forestry rural communities and improve socio-economic conditions. Two decades ago commerce of wild edible mushroom in the world was relatively small; mushroom industries ...
F Garza Ocañas, A Carrillo Parra


The effect on moisture content of water trapped in wood joints
2012 - IRG/WP 12-40613
To predict the service life of a structure, a model where the exposure of a structure is compared to its resistance can be used. Which exposure and resistance parameters that are relevant depend on which materials the structure consist of. This approach, with an exposure and a resistance parameter, is similar to the one used in structural engineering where a load (exposure) is compared to the bear...
M Fredriksson, L Wadsö, P Johansson


Transferable Durability: Enhancing decay resistance of non-durable species with extractives from durable wood species
2013 - IRG/WP 13-10808
Extractive content and composition is a vital component of naturally durable woods; however, variability in extractives can limit their usefulness in the field. Two extractive-free, non-durable wood species were pressure treated with ethanol-toluene extractives from 8 durable wood species. Extracted Southern pine, Paulownia and unextracted Southern pine blocks were treated and challenged in soil b...
G T Kirker, A B Blodgett, S Lebow, C A Clausen