Wood characterization of Tetraclinas articulata and evaluation of its resistance against lignilolytic fungi
2009 - IRG/WP 09-10697
Coniferous trees of the Tetraclinis articulata known under the Common name thuja from Berberie, is an endemic species from North Africa. The solid wood is much appreciated for its natural beauty and homogeneity and its quality for marquetry and furniture. The aim is to improve Tetraclinis articulate uses. At present, its wood is widely underestimated and sub-used compared to its announced qualitie...
F El Bouhtoury-Charrier, A Hakam, A Famiri, M Ziani, B Charrier


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...
E Tang Engelund, B Lindegaard, N Morsing


Evaluation of exposure conditions for wooden facades and decking
2009 - IRG/WP 09-20408
During their functional life, building components are exposed to moisture and other environment stress conditions in numerous ways. This is a fact that should be taken into account during manufacture, product development, designing and work execution of building components. For wood material, moisture stress and biological factors like mould and decay fungi are often critical in cladding and decki...
H Viitanen, T Toratti, R Peuhkuri, T Ojanen, L Makkonen


Potential synergy between natural product extracts for limiting fungal decay
2009 - IRG/WP 09-30495
Natural products often exhibit tremendous potential for inhibiting various microorganisms when they are tested in petri dish tests, but perform poorly when tested in vivo. The failures can often be attributed to a lack of broad spectrum activity against the range of organisms present in a natural environment. One method for overcoming this challenge is to use extracts from a number of sources with...
M Maoz, C Freitag, J J Morrell


Laboratory and above ground exposure efficacy of silicon-boron treatments
2009 - IRG/WP 09-30510
The study deals with silicon compounds, namely tetraethoxysilane (TEOS), phenyltriethoxysilane (PhTES) and methyltriethoxysilane (MTES) at concentrations of 23, 16 and 10% in combination with 1.2-1.5% boric acid. The aim with the study was to combine the chemical approach with the necessary biological tests of the impregnated wood. The tested silicon-boron combinations ensured mass loss less than ...
N Terziev, D Panov, A Temiz, S Palanti, E Feci, G Daniel


Component leaching from CCA, ACQ and a micronized copper quat (MCQ) system as affected by leaching protocol
2009 - IRG/WP 09-50261
Leaching results for Cu, Cr and As (CCA) and Cu (ACQ and MCQ) from southern pine are compared for laboratory tests (AWPA E11, and draft OECD methods I and II) and natural weathering of horizontally and vertically oriented lumber samples over two seasons. This paper expands on results and comparison of results presented at the IRG regional meeting in Costa Rica in Dec 2008 (Cooper and Ung 2008) a...
P A Cooper, Y T Ung


Termite Resistant Properties of Wood and Natural Fiber Plastic Composites - AWPA E1 Test Data
2009 - IRG/WP 09-40466
This paper deals with resistance properties of wood plastic composites against Formosan Subterranean Termites (FSTs) based on the AWPA E1 test standard. Sixteen laboratory WPC formulations, four WPC commercial materials, and southern pine (Pinus sp.) wood control were tested for termite mortality, sample weight loss, and sample damage rating. The results show that FSTs did attack WPC products in ...
Q Wu, T Shupe, J Curole, K Ragon, M Voitier, M Freeman, D Ring


The natural durability and preservative treatability of 11 bamboo species
2010 - IRG/WP 10-10708
Tests on the natural durability and preservative treatability of 11 common bamboo species were conducted. The results showed that there was a linear relation between bamboo density and its preservative retention by mass, and the preservative retention of bamboo reduced while its density increased. The test also showed that there were significant differences in the natural durability of bamboos, bu...
Chen Lifang, Su Haitao, Zhang Yanjun, Wang Yuxia, He Xuexiang, Ma Hongxia, Xie Guijun


Assessment of the marine borer resistance and abrasion resistance of lesser known hardwood timber species for use in marine construction
2010 - IRG/WP 10-10711
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, candidate timber species were selected for testing both in the laboratory...
J R Williams, G S Sawyer, G Malyon, S M Cragg, J D Icely, J Simm, M Meaden


Natural Durability of Fence Poles from Fourteen Semi-Arid Land Species after Six-Month Exposition
2010 - IRG/WP 10-10724
A sample of thirty fence poles from each of fourteen tree native species from Northeast Mexico were tested in ground contact in a wood-cemetery area located in Linares, Nuevo Leon, Mexico. The samples were submitted to six treatments (control, debarked, chemical treated, used cooking oil, thermal and creosote) and randomly distributed in five blocks. The effectiveness of using a bark gauge tool â€...
A Carrillo, F Garza, V Bustamante, S Sandoval, H Villalón


Non-structural carbohydrates mobilization throughout the stem of Tectona grandis: A strategy for enhancing the wood natural durability
2010 - IRG/WP 10-10729
Non-structural carbohydrates (NSC) storage is an important feature of heartwood substances formation. Radial distributions of NSC before and after chemical (acid and basic) hydrolysis, were quantified using a spectrophotometric method after enzymatic reaction and the corresponding macromolecules of conjugated NSC analyzed by HPLC, were studied in teak stem with reference to wood in environmental c...
B F Niamké, N Amusant, D Stien, A Amissa Adima, C Jay-Allemand


Early detection of colonisation by blue stain and mould on modified wood using PCR technique
2010 - IRG/WP 10-10730
The aim of this research was the early detection of fungal attack on the surfaces of modified and unmodified wood after natural weathering. The investigation was carried out by molecular techniques and the development and establishment of genus/species specific PCR for important moulds and sapstain fungi was part of this work. After adaption of the method, a monitoring of the succession of Ascomyc...
A Steitz, B Schmöllerl, N Pfabigan, S Bollmus, G Grüll


Structural changes, basidiomycete richness, enzyme activity and proteomic profiling of decay resistant and non-resistant woods over 18 months in soil contact
2010 - IRG/WP 10-10733
Wood decay fungi damage wood by production of enzymes that attack the structural components. The objective of this study was to better understand which suite of decay genes and proteins are expressed during biodeterioration of three different wood types in forest soil over time. Variation in decay genes and proteins were determined for pine (non-resistant), cedar (naturally durable), and ACQ-treat...
Youngmin Kang, S Diehl, L Prewitt, D Nicholas


Natural durability of Mulberry wood from Iran
2010 - IRG/WP 10-10737
Mulberry wood (Morus alba L.) is traditionally used in Iran to manufacture music instruments such as tar and setar. But little is know and contradictory statements are found on the natural durability of Morus alba. Moreover, in many cases, Iranian instrument makers leave freshly cut Mulberry timber into water (cold or hot) for a time period depending on the craftsman habit, without any real knowle...
A Se Golpayegani, M-F Thevenon, J Gril, K Pourtahmasi


Decay Resistance of Maple (Acer Insigne) Wood Against White Rot
2010 - IRG/WP 10-10740
In this study, the decay resistance of maple (Acer insigne) in natural state and treated with ACC (Acid copper chromate) was investigated against the white rot fungus (Coriolus versicolor). ACC is a kind of water borne preservatives that was used in this study for treating specimens under vacuum and pressure (Bethell procedure) with 3 percent concentration. In conducting mentioned evaluation, koll...
V Tazakor Rezaei


Natural durability of African Padauk and Niove. Comparison of new trials and former data from the CIRAD database
2010 - IRG/WP 10-10743
African Padauk (Pterocarpus soyauxii) and Niove (Staudia kamerunensis) were tested in laboratory against Basidiomycetes. The results were calculated according to the requirements of EN 350-1 (1994) and XP CEN/TS 15083-1 (2006). Padauk samples showed a high durability and very small variations between trees and within tree. Niove presented a high durability, but with notable differences according ...
Y N N’Kolo Meze’e, N Leménager, C Baudassé, M-F Thévenon


Stained wood: The identification of natural dyes and mordants in wooden works of art
2010 - IRG/WP 10-20434
On the basis of current knowledge only natural-colored wood species crafted to veneers were used for the decorative design of furniture and wooden interior in classical antiquity.First applications of artificially stained wood can be dated to the late Middle Ages. In the Renaissance wooden works of art were manufactured by using intarsia of natural-colored, fungus-stained and artificially stained ...
A Unger, W Unger


Improved analysis of field test data related to service life prediction of tropical wood species
2010 - IRG/WP 10-20458
Long field trials of wood in ground contact give valuable data on the natural durability of the material. The European Standard EN 350 gives guidance on how to perform these durability classification, but is limited to the use of averages of in-service life of a set of specimens compared to a reference set. Starting from a database of visual assessment of field stake testing, it is possible to obt...
J Van den Bulcke, A Wong, Ling Wang Choon, Yoon Soo Kim, J Van Acker


Effects of Cunninghamia Lanceolata Heartwood Extracts on the Growth of Wood Decay Fungi
2010 - IRG/WP 10-30527
China-fir (Cunninghamia lanceolata) wood is well known for its good durability. This species is native to China and has been extensive planted there. Mainly, extractives are responsible for the wood resistance to decay fungi. In this paper, the extractives of China-fir heartwood were studied for their effects on various wood decay fungi. Sequential extraction of heartwood in hexane, ethyl acet...
Shujun Li, Jing Wang, Jian Li


Evaluation of ACQ-D treated Chinese fir and Mongolian Scots pine with different post-treatments after 20 months of exposure
2010 - IRG/WP 10-30530
The performance of alkaline copper quat-type D (ACQ-D) treated Chinese fir (Cunninghamia lanceolata Hook.) and Mongolian Scots pine (Pinus sylvestris Linn. var. mongolica Litv.) stakes after 20 months exposure in Chengdu and Guangzhou of southern China were evaluated according to AWPA standard E07-07. The ACQ-D treatments used two concentration levels (0.5 and 1.0%) and four different post-treatme...
Lili Yu, Jinzhen Cao, Wei Gao, Haitao Su


Mobility of Copper from MCQ in Shell-Treated Wood Exposed Above Ground
2010 - IRG/WP 10-30534
Most Canadian treated decking in service has been given just a thin shell of preservative treatment but it has still performed very well. This is because copper migrated into checks and prevented germination of basidiospores on the freshly exposed untreated wood. Unlike soluble copper systems, MCQ has its copper primarily in the form of small basic copper carbonate particles. For MCQ to be effecti...
R Stirling, P I Morris


Natural compounds: A review of their use for wood protection
2010 - IRG/WP 10-30545
A lot of research in the field of wood protection has focused on natural compounds but very few of these have been implemented by industry. This review is an attempt to bring together information from selected area of work: - A brief review of the work done on natural products as organic biocides for wood protection. - Table containing information on natural products, their use as organic biocid...
T Singh, A P Singh


The Effects of Natural Weathering on the Properties of Heat Treated Alder Wood
2010 - IRG/WP 10-40484
Heat treatment is an effective method to improve the dimensional stability and biological durability of wood. The heat treatment technology and the heat treated wood products were recently introduced to Turkey. However, only a few studies have been reported on the effect of natural weathering on the properties of heat treated wood in both Turkey and the world. In this study, heat treated alder (Al...
S Yildiz, Ü C Yildiz, E D Tomak


Performance of selected types of coated and uncoated modified wood in artificial and natural weathering
2010 - IRG/WP 10-40510
The objective of the present work was to investigate the influence of commercial wood modification methods on weathering behaviour and coating performance. It was aimed to compare modification methods and to set up maps of weathering behaviour for these methods with and without a semi-transparent wood stain. Artificial and natural weathering trials were carried out with a selection of different ty...
G Grüll, L Podgorski, M Truskaller, I Spitaler, V Georges, S Bollmus, A Steitz


Deterioration of wooden heritage in outdoor exposure in Romania
2010 - IRG/WP 10-40535
The paper contains a study of the deterioration of wooden heritage in Romania, in outdoor exposure. Romania belongs to the few countries having a rich heritage of this kind. A quantitative image of this heritage reveals the 1,350 objectives transferred and reconstructed in 16 open-air museums, over 1,500 wooden churches, more than 4,000 buildings and technical facilities, historical monuments ...
L Bucşa, C Bucşa