IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3298 documents. Displaying 25 entries per page.


Interactions between water-borne preservatives and emulsion additives that influence the water repellency of wood
1991 - IRG/WP 2374
Incorporation of non-polar additives into water-borne treatments through of emulsion technology can greatly improve the physical characteristics of wood in service. Of specific interest with these emulsions is their effectiveness in reducing the rate of wood swelling. We have observed that the presence or absence of preservatives can often significantly influence the resultant effectiveness of the...
A R Zahora


Occurrence of wood-boring pholads in Kochi harbour waters (south-west coast of India)
1992 - IRG/WP 92-4175
The paper reports the occurrence of four species of wood-boring pholads (Pholadidae: Martesiinae), namely Martesia (Martesia) striata (Linnaeus), Martesia (Martesia) fragilis Verrill and Bush. Martesia (Particoma) nairi Turner and Santhakumaran and Lignopholas fluminalis (Blanford), in the Kochi back-waters, south-west coast of India. Of these Martesia nairi and Lignopholas fluminalis are now reco...
L N Santhakumaran, M V Rao


Influences of the hydro-thermal treatment on physical properties of beech wood (Fagus orientalis)
2005 - IRG/WP 05-40303
Influences of the hydro-thermal treatment on physical properties of beech wood were studied. Wood specimens (2×2×2cm) were treated in two steps. At first step, samples were treated at 160,180 & 200ºC for 4, 5 & 6 hours. At second step, treated samples were cured based on their first step treatment temperatures (160,180 & 200ºC) for 16 hours. The treated samples were soaked in water...
B Mohebby, I Sanaei


Movement of water through quaternary ammonium treated wood
1987 - IRG/WP 3440
Radiata pine sapwood stakes were treated with didodecyl methyl 1, 3 dichloropropenyl ammonium chloride and distearyl dimethyl ammonium chloride. Various ratios of these two chemicals were, tested to determine the extent of water movement through the treated wood. Measurements were taken of the amount of water moved through the wood, degree of wetting of various sectors of the stakes, and the distr...
P J Hayward, J Duff


Ponding of radiata pine (Pinus radiata) - 2. The effect of ponding on coating penetration into wood
1998 - IRG/WP 98-10249
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks, dried and subsequently coated with a primer and examined by light microscopy after staining sections with Sudan IV to enhance the contrast of the primer material. A correlation between the extent of ponding and the extent of coating penetration into wood was observed. The coating penetration var...
A P Singh, S S Gallagher, U Schmitt, B S Dawson, Yoon Soo Kim


The suitability of isothiazolone microemulsions as long term wood preservatives
1997 - IRG/WP 97-30150
Microemulsion formulations of 4,5 dichloro-2-n-octyl-4-isothiazolin-3-one were investigated to determine the leaching potential of these formulation types as well as their efficacy against decay fungi. These patented low leaching formulations exhibited good anti fungal efficacy in standard tests combined with minimal leaching of the active ingredient from the wood. The data suggests that the excel...
B M Hegarty, Bing Yu, L E Leightley


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Microemulsion formulations for wood protection chemicals
1993 - IRG/WP 93-30030
A microemulsion is a thermodynamically stable oil-water dispersion system. As a formulation it provides many unique features such as water compatibility for water-insoluble chemicals, formulation stability, good bioavailability and environmental acceptance. This paper discusses the major criteria for the formulations of water-insoluble wood biocides and the comparison in properties between convent...
Bing Yu, L E Leightley


Soft-rot in Tabebuia sp. wood used in water cooling tower: identification and degradation capacity of the fungi
1998 - IRG/WP 98-10253
Tabebuia sp. (ipe), a native Brazilian wood, is considered of high natural resistance to decaying fungi, and has been used in harsh environments, as cooling towers. Fifty-one fungi, belonging to mitosporic fungi group (Fungi Imperfecti), were isolated from deteriorated Tabebuia sp. wood samples, collected from the mist eliminator and packing of a cooling tower in operation for about 23 years. The ...
S Brazolin, M Tomazello, I H Schoenlein-Crusius


Screening of modified linseed oils on their applicability in wood protection
2004 - IRG/WP 04-30346
In this study modified linseed oils, rape oil and three waxes were screened on their efficacy as wood protecting agents. By testing all products when impregnated with high retentions in Scots Pine sapwood on water repellence qualities, additionally an accelerated weathering test, drying quality, accelerated brown rot and blue stain test, an indication is formed of the capability of these products ...
A Treu, J Lückers, H Militz


Preliminary evaluation of the answers to the 2nd IRG/WP-questionnaire on the state of pollution control in the field of wood preservation
1982 - IRG/WP 3209
This preliminary evaluation of the answers to the 2nd IRG/WP-Questionnaire only gives a general survey on those questionnaires which the author received until April 30th, 1982. Details, such as correlations between importance of wood preservation and pollution control, as well as a comparison of the answers with those to the first questionnaire (Doc. IRG/WP/369), could not be considered due to lac...
H Willeitner


New principles for the protection of wood: Impregnation with waterborne resins
1995 - IRG/WP 95-40047
The environmental impact of classical wood preservatives as well as the use of tropical wood species with high natural durability is regarded increasingly critically in the public. Therefore other partially new principles for the protection of wood, like chemical modification, or treatment with resins were examined especially in USA, Japan and in Europe with promising results predominantly in the ...
A O Rapp, R-D Peek


The effect of a chelator mediated fenton system on activation of TMP fibres and decolorization of synthesized dyes
2004 - IRG/WP 04-50223
The purpose of this work is to improve our current knowledge of the non-enzymatic mechanisms involved in the brown rot degradation of wood, but also to study the potential applications of a chelator-mediated Fenton system in activation of wood fibers and decolorization of synthesized dyes. In this work, Electron Spin Resonance (ESR) spin-trapping techniques were used to study the generation of hyd...
Yuhui Qian, B Goodell, J Jellison


Mobility and bioavailability of wood preservation chemicals in soil - actual field measurements
1998 - IRG/WP 98-50101-11
Wood material intended for outdoor use is often impregnated with chemicals to withstand attack from fungi and bacteria. Both inorganic and organic substances are used to protect the wood, and they are used in a toxic and bioavailable form. At wood preservation facilities severe soil contamination can be encountered due to spills and deposition of sludge, especially at old sites. Two sites, one whe...
S Andersen, G Rasmussen


Health and safety regulations on the use of wood preservatives in Switzerland
1980 - IRG/WP 3148
There is not any doubt that the chemical protection of wood (besides the architectional-constructional wood protection) is of utmost importance for the increase of the durability of technically used timber. The toxic properties of wood preservatives make certain legal regulations necessary for the protection of human beings, animals and the environment. Thereby wood preservatives fall under the po...
O Wälchli


Diffusion and interaction of components of water-borne preservatives in the wood cell wall
1988 - IRG/WP 3474
This study investigates the rates of diffusion and ultimate distributions of copper and arsenate components of wood preservatives in wood cell walls following vacuum treatment. Adsorption studies of copper on red pine (Pinus resinosa) and trembling aspen (Populus tremuloides) wood confirm the importance of cation exchange reactions on the ultimate distribution of copper in the wood substance and i...
P A Cooper


Optimisation of an analytical method for the determination of total fluoride in preservative-contaminated soils using water steam distillation and an ion-selective electrode
1999 - IRG/WP 99-20153
This paper describes a simple modified procedure for the quantitative fluoride determination of different origin in a soil matrix using a water steam distillation and an ion-selective electrode. Distillation methods generally require a preliminary preparation step like fusing. The modified method presented here is based on the direct distillation of fluoride so that no further sample preparation i...
E Melcher


Biosorption of metals for wood waste effluent clean up
1997 - IRG/WP 97-50090
The common filamentous fungi can sorb metal ions from aqueous solutions. The biosorption of metal ions like copper Cu2+, chromium Cr6+ and arsenic As5+ by dead fungal mycelia was investigated. Two industrial fermentation byproducts are tested: Mucor miehei and Aspergillus oryzae. The adsorption of metal ions depends on parameters such as chemical treatment of fungi before biosorption (acid or basi...
S Legay, G Labat


Recovery of copper, chromium, and arsenic compounds from the waste preservative-treated wood
1991 - IRG/WP 3651
In Japan, about 40 percents of waste wood is incinerated and the residue is dumped into the landfill site. The waste preservative-treated wood, which is mixed in nontreated wood, is incinerated in the same way, too. However, it will cause the serious problems that the gases contained with high concentration arsenic compounds are discharged from the smokestacks of the incineration facilities and th...
A Honda, Y Kanjo, A Kimoto, K Koshii, S Kashiwazaki


Comparison of Temporal Changes in Metal Leaching and Aquatic Toxicity from Wood Treated with CCA and Alternative Preservatives
2005 - IRG/WP 05-50236
This study compares the temporal variation of chemical leaching and aquatic toxicity of wood treated with chromated copper arsenate (CCA) and other copper-based wood preservatives (alkaline copper quaternary (ACQ), copper boron azole (CBA), copper citrate (CC) and copper dimethyldithiocarbamate (CDDC)). Treated wood blocks were leached for 21 days and the leachate collected was analyzed for prese...
B Dubey, T G Townsend, G Bitton, H M Solo-Gabriele


Electrochemical deterioration of wood in sea-water
1981 - IRG/WP 464
In the specialistic literature only few items can be found dealing with the specific kind of wood deterioration called electrochemical corrosion of wood. This deterioration occurs predominantly on marine vessels, yachts, and other marine craft where wood is jointed by means of various metal connectors. Up to date information demonstrates that in wood surrounding copper connectors, when in proximit...
J Raczkowski


Weathering trials on natural wood finishes in New Zealand
1986 - IRG/WP 3383
The weathering properties of various transparent and semi-transparent exterior finishes for New Zealand-grown radiata pine are currently being examined. After 12 to 16 months' weathering, unpigmented water repellents have failed to provide satisfactory protection from weathering under field test conditions. With the exception of two formulations, penetrating oil-based stains are already s...
D V Plackett, C M Chittenden


Remediation of wood treatment sites in Finland
1999 - IRG/WP 99-50139
Finnish legislation in connection with soil contamination are firstly waste management legislation and secondly public health legislation and water legislation. There is no separate legislation concerning soil protection or remediation. The Ministry of the Environment has published a proposal for official contaminant guideline values to be used both as criteria for contamination and clean-up targe...
S Salonen


A report of the Technical Recommendations documents for the Canadian Wood Protection and Preservation Facilities and an environmental study of storm water runoff from anti-sapstain treatment plants
1988 - IRG/WP 3478
With the completion of the Final draft of the Technical Recommendations (TR) documents for the Wood Preservation and Wood Protection Industry, there are naturally questions on what is expected from these documents and how Environment Canada and Provincial regulatory agencies may interact with the wood preservation industry. In general, it is expected that the Canadian Wood Preservation and Protect...
G Das, V N P Mathur


Preservative treatment of green timber by soaking in ammoniacal copper borate
1984 - IRG/WP 3292
Freshly sawn boards of radiata pine sapwood were preservative treated by soaking in ammoniacal copper borate. Optimum schedules were obtained by partially seasoning the boards for one week prior to treatment. This aided the absorption of preservative and reduced the required soaking time to approximately 2 hours. Complete boron penetration was obtained after one week of block storage under cover a...
P Vinden, A J McQuire


Previous Page | Next Page