IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 233 documents. Displaying 25 entries per page.


A collaborative test to determine the efficacy of polyurethane coatings on wood samples in the marine environment. 3rd Interim Report
1993 - IRG/WP 93-10046
The results of al long-term marine trial to assess the protective effect of polyurethane coatings on wood samples exposed at different sites around the world are reported. The condition of samples exposed in the sea for up to 88 months was generally sound, although instances of marine borer infestation were reported at two sites. At one site, mechanical damage of a non-biological nature is believe...
R A Eaton


Research on wood protection at the Princes Risborough Laboratory 1975 & 1976
1977 - IRG/WP 3109
This paper is the latest of a 2-yearly series presenting a summarised account of the Laboratory's work in wood preservatives and related fields. The topics dealt with include: environmental studies on the usage of copper-chrome-arsenic and organic solvent preservatives; development of National and International Standards; recent developments in the preservation of external doors and windo...
J M Baker, R A Laidlaw, E R Miller, J G Savory


The evaluation of the effectiveness of wood preservatives by means of IUFRO's method for field tests with wooden stakes
1985 - IRG/WP 3348
Pinus elliottii and Eucalyptus saligna stakes treated with CCA-A, CCA-C, CCB, Cashew Nut Shell Oil and Benzotar solutions were exposed in seven test sites in Sao Paulo State, Brazil. After five years of exposure, between oil-borne preservatives Benzotar show better performance than CNSL (cashew nut shell liquid), and within waterborne preservatives the performance of CCB is not so good as that of ...
G A C Lopez, A M F Oliveira, E S Lepage


Ponding of radiata pine (Pinus radiata) - 2. The effect of ponding on coating penetration into wood
1998 - IRG/WP 98-10249
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks, dried and subsequently coated with a primer and examined by light microscopy after staining sections with Sudan IV to enhance the contrast of the primer material. A correlation between the extent of ponding and the extent of coating penetration into wood was observed. The coating penetration var...
A P Singh, S S Gallagher, U Schmitt, B S Dawson, Yoon Soo Kim


Evaluation of copperised Cashew nut shell liquid and Neem oil as wood preservatives
2005 - IRG/WP 05-30368
An effort has been made to develop eco-friendly wood preservatives using naturally available plant by-products with less toxicity. Copper was incorporated into Cashew nut shell liquid (CNSL) and Neem seed oil. Rubber wood samples were treated with these solutions employing dipping and pressure techniques in 3 different levels. These samples have been evaluated to find out the effectiveness as wood...
D Venmalar, H C Nagaveni


Influence of hydrophobic agents on the leachability of boron
1995 - IRG/WP 95-30064
Besides its low mammalian toxicity and a broad range of activity towards both fungi and insects, boron shows a high diffusibility, encouraging it to treat wood species of low permeability. However, its difussibility is at the same time responsible for a high risk of leaching, known since long. Nevertheless quantitative data about this process are only rarely available. Therefore, the leaching of b...
A Peylo, H Willeitner


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Fungicidal properties of wood tar being a side product of pyrolysis of previously treated wood with preservatives
2004 - IRG/WP 04-30340
The objective of the paper was to estimate the limit of the fungicidal value of wood tar being a product of pyrolysis of wood previously treated with creosote oil or salt preservative of the CCB type. The effectiveness of wood tar in wood protection against fungi causing brown rot and soft rot was compared to the effectiveness of creosote oil (type WEI-B). Wood was impregnated with alcohol solutio...
B Mazela, M Kielczewski, W Grzeskowiak


Fixation of CCA preservatives in cocos-, oil- and rattan-palm
1986 - IRG/WP 3371
In previous tests with jubaea-palm almost no fixation of a CCA-preservative Type B could be achieved, consequently, further leaching tests were carried out with samples of 1 cocos-, 1 oil- and 2 rattan-palms from Malaysia. A good fixation of chromium and copper took place in cocos-palm after 4 weeks storage at 28°C. Nevertheless the fixation was slower than in pine-wood and demanded an elevated t...
H Willeitner, K Brandt


Colonisation of painted wood by Aureobasidium pullulans - Analysis of features and consequences for failure in service
1996 - IRG/WP 96-10144
Wooden blocks of spruce were painted with different paint formulations. Water- and solvent-borne model and commercial paints were used. The painted wooden blocks were inoculated with a spore suspension of Aureobasidium pullulans (de Bary) Berkg. and placed in an environment of high humidity for 14 months. Different colonisation and growth patterns were observed on the different paint surfaces. The...
S L Bardage


In ground performance of wood treated with a substituted isothiazolone
1990 - IRG/WP 3612
Isothiazolones (I.T.A.'s) are a class of biocides that have potential for use as wood preservatives. The substituted ITA, RH-287, (4,5,dichloro-2-n-octyl-isothiazolone-3-one) is being evaluated as a broad spectrum wood preservative. The evaluation program includes in ground stake tests which were established at two test sites in Mississippi, USA The tests used southern yellow pine treated...
L E Leightley, D D Nicholas


Working plan: Second international collaborative field trial
1995 - IRG/WP 95-20056
This paper describes the scope, objectives, and approaches to be used in the second international collaborative field trial approved by the Scientific Programme Committee for partial funding in 1994. The trial is designed to develop a broad data base on causal mechanisms, interactions, and factor affecting the performance of treated wood in ground contact. The trial encompasses 12 different field ...
H M Barnes, T L Amburgey


Effect of Oil Content on The Performance of Wood Treated with Pentachlorophenol
2003 - IRG/WP 03-30324
This paper details a five-year study on southern pine treated with pentachlorophenol in oil at various oil contents. Results from field stake tests at two Gulf Coast test sites are presented. Both biological efficacy and preservative depletion data are discussed. Results suggest that increasing oil content leads to better performance of wood treated with pentachlorophenol. Test results indicat...
H M Barnes, T L Amburgey, M G Sanders


Anti-fungal properties of pyrolytic oils derived from softwood bark
2000 - IRG/WP 00-30218
Thermal decomposition of balsam fir and white spruce mixed bark residues at 450°C and under vacuum (< 20 kPa abs.) results in high yields of pyroligneous liquors rich in phenolic content. This vacuum pyrolysis process has been scaled-up to a pyrolysis plant with a feed capacity of 3.5 t/h of softwood bark, which is the largest plant of this type in the world. The pyrolytic aqueous condensates ...
D Mourant, Dian-Qing Yang, Xiao Lu, C Roy


Chemical treatment of chips for outdoor storage. Evaluation of sodium N-methyldithiocarbamate + sodium 2,4-dinitrophenol treatment
1980 - IRG/WP 2134
Fresh slash pine chips were treated by spraying them with a dilute aqueous solution of sodium N-methyldithiocarbamate and sodium 2,4-dinitrophenol. The were then formed into an experimental chip file 10 feet high, and the pile was maintained for seven months. The treatment effectively slowed heat release and retarded losses in wood substances, tall oil, pulp yield, and pulp strenght. Under certain...
E L Springer, M Benjamin, W C Feist, L L Zoch, G J Hajny


Moisture distribution in coated wooden panels. Studies of moisture dynamics by computerized axial tomography
1992 - IRG/WP 92-2413
Certain modern coatings have been held responsible for the rot damages in wood sidings, which have, during the past few years, appeared at an increasing extent in Scandinavia and which have occurred rather soon after the application of the coating. In this study, the moisture excluding effect of different coating systems intended for sidings have been studied with the help of an X-ray technique, c...
J Ekstedt, L O Lindgren, S Grundberg


Three-year field trials of polymeric formulations which provide a new basis for the invention and design of non-toxic wide-spectrum wood preservatives
1994 - IRG/WP 94-40029
Three types of non-toxic polymeric formulations invented using a new approach to wood preservation were challenged with termites and fungi in three-year ground-contact field trials in the sub-tropical climate of Natal. These formulations were copper soaps of carboxylic acid groups of unsaturated fatty acids of waxes and edible vegetable oils; of resin acids of rosin, and, of synthetic unsaturated ...
A A W Baecker, A Pizzi


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Observations on the destruction of fishing craft in India by marine wood-borers with special reference to the West Coast
1981 - IRG/WP 472
The paper highlights the economic importance of the destruction of fishing craft in India by marine wood-destroying agencies. The annual loss involved is to the extent of over 94 million rupees. Thirty-nine spectes and one variety of woodborer have so far been recorded from India, of which Bankia campanellata, Bankia carinata, Bankia rochi, Dicyathifer manni, Lyrodus pedicellatus, Teredo clappi, T...
L N Santhakumaran, J C Jain


Studies on the fungicidal effectiveness of a petroleum derived product as a creosote alternative
1986 - IRG/WP 3384 E
This work, appears first because of the necessity to find out a profitable use for a residual product of the petrol pyrolisis, and second, because the lack of high natural durability wood used until now-a-days to build posts and sleepers in creosote lacking countries. Our main objective was pointed to the characterization of this new product and to find out the effectiveness against the wood-destr...
A M Navarrete, M T De Troya


Wood protecting chemicals for the 21st century
1993 - IRG/WP 93-30018
After assessing the past research with protection chemicals, this paper proposes future avenues for research and development in wood protection. Three scenarios are put forward for consideration. First, more is not better and future systems will emphasize combination formulations which enhance properties while providing biological efficacy. Second, current systems, especially those based on copper...
H M Barnes


Algal growth resistance of paints for coating of wood; a laboratory study
1997 - IRG/WP 97-10213
Twelve paints were tested for resistance against algae. In addition, one algicidal compound commercially used for remedial treatments of algal growth on paints was tested for its effectiveness for prevention of algal growth. An agar diffusion bioassay was employed in which paint films on filter paper discs were placed on mineral salt medium and sprayed with an algal suspension containing a mixture...
J Bjurman


The effect of oil-borne preservative treatments on the shear strength of FRP/wood composite adhesive bonds
2003 - IRG/WP 03-40265
Reinforcement of structural wood components with Fiber Reinforced Polymer (FRP) will enhance the beam’s strength, but actual data on long-term durability is sparse, not well documented or not readily accessible. In this study, bond properties of FRP-wood composite materials were investigated following treatment with creosote or copper naphthenate preservatives. The properties investigated inclu...
B Herzog, B Goodell, R Lopez-Anido


Application of paint primers after light organic solvent preservative treatment
1986 - IRG/WP 3381
The application of three alternative paint primers is investigated, including a slow-drying oil-based primer, a fast-drying oil-based primer, and a fast-drying water-based primer. The treatment schedules employed, in particular the evacuation period after treatment, have a marked effect on subsequent paintability. Priming can potentially be carried out immediately after treatment with approved Tim...
P Vinden


Potential use of an emulsified tar oil fraction as a wood preservative: Preliminary technological and environmental assessment
1994 - IRG/WP 94-50028
In order to meet the recent environmental concern specifications of creosote are altered, the B[a]P content is limited and restrictions on the emission of volatile organic compounds (VOC) and higher polyaromatic hydrocarbons (PAH) are expected in some countries. Research has been conducted on an emulsion of a selected tar oil fraction. Using a waterborne formulation opens new perspectives for targ...
G M F Van Eetvelde, R Leegwater, M Stevens


Previous Page | Next Page