Effects of exposure time on detection of the behavior of white-rot fungi on Oriental beech wood properties
2017 - IRG/WP 17-10902
The comparison of fungal degradation of Orientalis beechwood by two white-rot fungi was evaluated in this study. Biological, mechanical, and chemical assessments of beech wood were carried out at 30 day interval for 120 days. The results demonstrated that both fungi have greater effects on beech wood during each exposure time. However, Trametes versicolor degraded beech wood more effectively than ...
E Bari, D D Nicholas, K M Ohno


UV-curable coatings developed for aesthetic and biological protection of wood outdoors
2017 - IRG/WP 17-40821
To avoid wood greying, dimensional variations, and degradation by biological agents wood is protected with preservation products and coatings when used outdoors. For some wood species used for cladding, a treatment with a preservation product is required, and is frequently additionally protected with a coating. In this study, Mäder Group developed a new UV-curable coating for outdoors application...
C Reynaud, A S Schuller, M Kutnik, L Podgorski


Impact of temperature and relative humidity on spatio-temporal fungal growth dynamics of Basidiomycetes
2018 - IRG/WP 18-10905
Basidiomycetes can cause considerable damage to wood and other bio-based building materials. Knowing at which environmental conditions these decay fungi generally thrive, and how the environmental conditions affect fungal growth characteristics, is therefore of particular interest. In this paper, we use image analysis to assess the impact of the environmental conditions on the growth dynamics of C...
L De Ligne, G Vidal-Diez de Ulzurrun, J Van den Bulcke, J M Baetens, B De Baets, J Van Acker


Interactions between wood polyphenols and detoxification enzymes of the white rot Trametes versicolor
2018 - IRG/WP 18-10906
Wood decay fungi have complex detoxification systems that enable them to cope with secondary metabolites produced by plants. Although the number of genes encoding for glutathione transferases (GSTs) is especially expanded in lignolytic fungi, little is known about their physiological target molecules. In this study, by combining thermal shift assay and affinity crystallography we highlighted inter...
M Schwartz, T Perrot, E Aubert, S Dumarçay, F Favier, P Gérardin, M Morel-Rouhier, G Mulliert, F Saiag, C Didierjean, E Gelhaye


Understanding of the effect of ancestral and natural saltwater treatment on durability, fibers densification and chemical modification of palm wood
2018 - IRG/WP 18-10921
The palm-tree sector plays a very important role on both the socioeconomic and ecological levels, in Tunisia. There are three million trees in Tunisian palm plantations, ensuring a potential significant wood production, mainly in the craft and furniture industries. In the past, Date Palm wood (Phoenix dactylifera L.,) was also used as structural material. Its low natural durability and its low m...
M T Elaieb, A Namsi, M Tella, M-F Thévenon, K Chandelier


Use of x-ray microdensitometry for assessing the resistance to the fungus C puteana of a hybrid larches population
2018 - IRG/WP 18-10923
The aim of this research was to utilize the X-ray microdensitometry to determine the natural durability and its variability of a hybrid larch population. The method was applied on slices obtained by increment cores collected on standing trees before cutting them down. The methodology was discussed also in order to propose as a new screening method especially suited for trees populations. X-ray mic...
S Palanti, F Alderighi, F Stefani, J P Charpentier, L E Pâques


The impact of coatings on the service life of wood decking
2018 - IRG/WP 18-20635
The durability of wood decks depends on the nature of the environment in which they are exposed to, the dimensions and configuration of the components, the resistance of the wood to degrading factors in that environment, and the maintenance performed on the deck. The present work seeks to better understand the performance of selected wood decking systems when maintained and unmaintained. This expe...
R Stirling, D Wong


Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz


Towards durability classification of preservative treated wood – first attempts using different European standards
2018 - RG/WP 18-20638
EN 350 (2016) gives guidance on methods for determining and classifying the durability of wood and wood-based material against biological wood destroying agents. “Wood-based materials are those derived from trees and include amongst others: untreated wood, heat treated wood, chemically modified wood, glue laminated wood, wood-based panels, wood polymer composites and wood treated with wood prese...
S Bollmus, A Gellerich, C Brischke, H Militz


Above-ground testing methods – review of Rotorua, New Zealand test site results after ten years
2018 - RG/WP 18-20642
A series of seven different types of above ground durability tests were initially conducted over four years to determine which type of tests would give the fastest, most consistent results. Five types of test; ground proximity, two types of decking, flat panels and double layer, were reassessed after ten years. Exposure conditions varied between tests with ground proximity producing close to groun...
D Page, T Singh


Resistance of modified wood to termite attack assessed in laboratory and field testing: A review of internal research
2018 - IRG/WP 18-40824
Within the past decades, new wood modification technologies have been investigated in order to improve certain wood characteristics and enable the use of timber products for outdoor applications. Some of these non-biocidal technologies have been developed and commercialized recently. Thus, various material properties were studied intensively and shown to be improved. To a great extent, previous re...
L Emmerich, P Gascón-Garrido, H Militz


Multiscale modification on water resistance and dimensional stability of Populus cathayana by alkali lignin combined with heat treatment
2018 - IRG/WP 18-40826
The aim of this study was to enhance the water resistance and dimensional stability of fast growing wood by alkali lignin combined with heat treatment. Poplar (Populus cathayana) samples were first impregnated with alkali lignin solution and then subjected to heat treatment at 140, 160, and 180°C respectively for 2h. Properties of leachability, moisture adsorption and water absorption, contact an...
H Zhou, J Li, E Ma


Influence of different triazoles as co-biocides in wood preservatives on efficacy and the environmental impact
2018 - IRG/WP 18-50333
In this study we investigated the efficacy and impact on the environment of different co-biocide triazoles in wood preservatives. Four different formulations (all containing 9.5% Copper) contained individual and combinations of cyproconazole, tebuconazole, propiconazole as co-biocides. Four formulations were tested according to EN 113 and EN 84 (ageing) to determine the brv for each formulation. T...
M Klamer, T Jensen, S Bang-Achton, E Morsing


Long service life or cascading? The environmental impact of maintenance of wood-based materials for building envelope and their recycling options
2018 - IRG/WP 18-50336
A major restraint in choosing bio-based materials (i.e. wood-based) for external use, is the lack of confidence that architects, designers and customers have toward these materials. In particular, the limit state of bio-based materials, which defines the frequency of maintenance operations, might be reached earlier for wood than for other materials (i.e. concrete). On the other hand, resource and ...
M Petrillo, J Sandak, P Grossi, A Kutnar, A


Decay and water resistance of Siberian and European larch wood
2019 - IRG/WP 19-10941
The occurrence of larch wood is rather frequent in civil engineering. Namely, in building façades, terraces and balcony fences. In Slovenia and other central European countries, the use of the Siberian larch is especially popular. In this research, the durability against decay fungi in laboratory conditions and water exclusion ability of plantation-grown and naturally grown Siberian larch (Larix ...
B Lesar, D Krzisnik, M Humar


Natural durability of four Tunisian Eucalyptus wood species and their respective compositions in extractives
2019 - IRG/WP 19-10942
In the 50’s, Tunisia government introduced more than 11 Eucalyptus wood species. Eucalyptus species were planted in Tunisia in different arboreta throughout the country for close observation and adaptation to climate and soil. These fast-growing wood species were mainly used as fire wood, for the production of mine wood and to fight against the erosion. These tree species were adapted themselve...
S Ben Ayed, M T Elaieb, S Dumarçay, B De Freitas Homen De Faria, M-F Thévenon, P Gerardin, K Candelier


Determining the natural durability on xylarium samples: mini-block test, wood powder and chemical profiling
2019 - IRG/WP 19-10944
Xylaria, or wood collections, can be considered sleeping beauties in terms of wood technological and biological output. In this study we focus on determining the natural durability of xylarium specimens from the Federal Xylarium in the Royal Museum for Central Africa. The Federal Xylarium contains over 80,000 specimens, covering more than 13,000 species, mainly from Central Africa. These specimens...
V Deklerck, L De Ligne, J Van den Bulcke, E Espinoza, H Beeckman, J Van Acker


Performance of wood decking after 5 years of exposure: verification of the combined effect of wetting ability and durability
2019 - IRG/WP 19-20647
Wood is one of the most important construction materials and its use in building applications has further expanded in recent decades. In order to enable even more extensive and reliable use of wood, factors affecting wood’s service life need to be understood. More recently, a new concept to characterize the durability of wood-based materials and to predict the service lives of wood was proposed,...
M Humar, D Krzisnik, B Lesar, C Brischke


Durability classification of preservative treated and modified wood
2019 - IRG/WP 19-20659
EN 350 (2016) allows formally to determine durability classes (DC) for wood products and wood-based materials, which was previously only possible for untreated wood in the form of natural durability. In a first study, the University of Goettingen carried out the durability classification of chemically modified (modified with 1,3-dimethylol-4,5-dihydroxyethyleneurea, DMDHEU) and preservative-treate...
S Bollmus, L Bachle, C Brischke, H Militz


Use of resin obtained from Italian guayule crops for wood preservation purposes: some preliminary results
2019 - IRG/WP 19-30736
The potential of guayule (Partenium argentatum Gray) as a source of anti-termite, anti-fungal and insect repellent products to be used in wood preservation, has been largely explored in the past. The fact that such products are obtained as byproducts in the process of natural rubber extraction from this plant, thus increasing the profit of the process, together with the ability of this crop to gr...
S Palanti, E Conti, M Russo, F Stefani, C Querci


Identification of Antifungal Compounds in Konjac Flying Powder and Assessment against Wood Decay Fungi
2019 - IRG/WP 19-30737
The antifungal activity of konjac (Amorphophallus rivieri) flying powder (a by-product produced during mechanical processing of konjac flour) ethanol extract was evaluated against wood decay fungi in culture. Compounds associated with antifungal activity in the extracts were isolated and purified by silica gel column chromatography. The antifungal active fractions were identified by ultra-high-per...
Z Bi, F Yang, Y Lei, J J Morrell, L Yan


Relative efficacy of various oxine copper formulations against brown-rot fungi
2019 - IRG/WP 19-30741
This paper investigates the relative resistance of three different oxine copper formulations (oil-borne, water-borne, water-borne with pH-adjustment) as a preservative treatment for wood against brown-rot fungi. Impregnated southern pine sapwood cubes were exposed to R. placenta and G. trabeum cultures in a soil-block test. After eight weeks, the weight losses of the cubes were examined in relatio...
M Petruch, J Lloyd, A Taylor


Economic and Alternative Preservative Research with an Overview of its Impact on the Dynamics of Wood Tie Markets and Railroads
2019 - IRG/WP 19-30751
This presentation will discuss the Railway Tie Association’s (RTA) efforts in economic research for the North American wood tie industry, along with decades-long research into improving wood preservation processes and its resulting economic impact for railroads. Ongoing research is continuing to expand the knowledge-base by comparing existing standard creosote (C) and borate-creosote (B-C) dual...
J C Gauntt


Using X-ray scattering to elucidate the mechanisms behind the moisture and fungal decay resistance of epoxybutene modified wood
2019 - IRG/WP 19-40854
Chemical modification of the hydroxyl groups of wood can improve the properties of wood by providing moisture and biological resistance, as well as dimensional stability. Southern pine solid wood was chemically modified to various weight percentage gains (WPG) with epoxybutene (EpB, 8%-38% WPG). After modification, specimens were extracted with a toluene: ethanol (2:1) solution for 2 hours or wate...
R E Ibach, N Plaza


The impact of additional interior layers to the moisture dry-out and mould growth risk of CLT walls
2019 - IRG/WP 19-40876
The objective of this study was intended to determine the maximum allowable initial moisture content for CLT walls having both exterior and interior thermal insulation. A laboratory test was conducted, for which four test walls with two different insulation solutions and two different initial moisture contents were built. Based on the test results a simulation model was configured and simulations ...
V Kukk, J Kers, T Kalamees