Bundle tests - Simple alternatives to standard above ground field test methods
2016 - IRG/WP 16-20581
Within this study we applied different new above ground test set ups to untreated Norway spruce (Picea abies Karst.) and Scots pine sapwood (Pinus sylvestris L.) which are frequently used as reference or control species in wood durability field tests. The overall aim of this study was to find a simple alternative method to the few standardized above ground field test methods, such as the L-joint a...
C Brischke, L Meyer-Veltrup


Durability of a willow/plastic composite mat
2016 - IRG/WP 16-20592
Developing uses for wood wastes could enhance utilization of low value renewable materials while creating opportunities for rural development. Small diameter willow stems have little use in China, but they could be combined with high density polyethylene to create wood plastic composite mats for decorative applications. These mats could be used in exterior, above ground exposures, but would still ...
Li Yan, Haiyan Duan, Beizhan Quan, J Cappellazzi, J J Morrell


Evaluation of field test data
2016 - IRG/WP 16-20594
The resistance against fungal decay and insect attack of wood can be highly variable, between boards and even within boards. The variability in durability is not always an issue, but for high demanding applications information about its reliability is required. This comprises the variability of outdoor performance. Durability testing in laboratory and outdoor exposures can provide a good basis to ...
F Bongers, C Brischke, J Van den Bulcke, W Gard, I De Windt, H Militz


Assessment of the biological durability of wood treated with organosilicon compounds
2016 - IRG/WP 16-30685
The European wood construction market is in need of environmentally friendly wood-based products whose service life meets the expectations of end users. Non-biocidal silicon-based water repellents, which can be applied to different materials, help minimize their vulnerability/susceptibility to liquid water. Consequently, they have the potential of increasing wood’s resistance against decay fungi...
M Kutnik, M Montibus, S Derocker, S Salivati, J-P Lecomte


Screening of fastener resistance in contact with untreated wood using different test designs
2016 - IRG/WP 16-30686
The performance of fasteners in wooden constructions is an important aspect especially regarding corrosion resistance. In an early stage corrosion of fasteners in untreated timber becomes often visible as a discoloration on the surface of the timber resulting in bad appearance of the product followed by complaints. In order to develop an accelerated test for the assessment of fastener performance ...
E Melcher, S Wolf, U Cera


Laboratory and Field evaluation on Resistance of Thiacloprid-treated Pine Species to Termites in Mexico
2016 - IRG/WP 16-30687
The usage of Neonicotinoids for wood preservatives is common practice in several countries. Especially the active ingredient Imidacloprid is well established for this application due to its high efficacy against termites. (2Z)-3-(6-chloro-3-pyridylmethyl)-1,3-thiazolidin-2-ylidene-cyanamide, also known as Thiacloprid showed a good efficacy against Reticulitermes santonensis De Feytaud in efficacy ...
P Meckler, T Jaetsch, I Rodriguez


Decay resistance of wood treated with bio-friendly preservative systems
2016 - IRG/WP 16-30698
Due to more restrictive toxicological requirements and increased ecological awareness of consumers, wood preservatives containing biocides are no longer desired on the market. Therefore, research on new environmentally friendly formulations is of great importance. One of the possible solutions is to develop new preservatives based on natural substances, which are harmless to humans, animals and th...
B Mazela, G Cofta, W Perdoch, L Ross Gobakken, P Kwaśniewska-Sip


Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti


Durability of Thermally Modified Engineered Wood Products
2016 - IRG/WP 16-40745
In this study, rated plywood, oriented strand board (OSB), laminated strand lumber (LSL), and laminated veneer lumber (LVL) were thermally modified as a post-treatment at 140 °C, 150 °C, 160 °C, 170 °C, and 180 °C using a closed, pressurized treatment method. Eastern larch OSB manufactured from heartwood and sapwood was also thermally modified as a post-treatment at 160 °C and 180°C. All ...
H M Barnes, M D Aro, A Rowlen


The impact of catalyst on the properties of furfurylated beech wood
2016 - IRG/WP 16-40748
European beech (Fagus sylvatica L.) is a major tree species of European forest that is underexploited because of its low dimensional stability and durability. Similarly to what has been developed with radiata pine, furfurylation might be the answer to optimize the utilization of local beech wood. Beech wood furfurylation process was studied using five different catalysts: maleic anhydride, maleic ...
P S Sejati, A Imbert, C Gérardin, S Dumarçay, E Fredon, E Masson, D Nandika, T Priadi, P Gérardin


Encapsulation of poles to prevent moisture uptake – a laboratory test
2016 - IRG/WP 16-40753
Premature failure of utility poles due to decay in soil contact is the main reason for early removal of utility poles, a measure that implies extra costs for utilities. Remedial treatments and barriers are common methods to prolong the service life of utility poles. The first part of this paper gives an overview of mode of action and commercial application of barrier systems as described in the li...
K-C Mahnert, U Hundhausen


Development of a new method for wood hydrophobizing and fixation of copper compounds by chemical hardening of vegetable based modified oils
2016 - IRG/WP 16-40754
Wood products with ground and direct water contact, but without sufficient biological durability, have to be protected against biological degradation by fungi and other microorganisms. Due to European legislation (Biocidal Products Regulation 528/2012), the selection of possible chemical agents, which are still allowed to be used, is diminishing rapidly. The use of previously widely applied, very ...
C Swaboda, M Fischer, K Jacobs


The Environmental Impact of Timber Products Compared to other Building Materials - A Survey of Published Environmental Product Declarations
2016 - IRG/WP 16-50314
One of the positive aspects of using wood in construction is the environmental benefits that this can potentially bring. However, manufacturers of all construction products and materials make claims about the ‘environmental friendliness’ of their products, making it exceedingly difficult for the end user to make informed choices about the advisability of using one product over another. This st...
C Hill, J Dibdiakova


Effects of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger
2017 - IRG/WP 17-10878
Effect of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger was studied. Specimens from A4 papers were also prepared for comparison purposes. Paper specimens were dipped in aqueous nanowollastonite (NW) with 10, 20, 30, and 40% concentrations and compared with control specimens. In order the nanofibers be fixed on paper specimens, 5% of polyvinyl acetat...
H R Taghiyari, A Kalantari, A Ershad-Langroudi, A Kalantari


Comparative studies on the durability of English oak (Quercus robur L.) under in-service, field and laboratory conditions
2017 - IRG/WP 17-10881
The durability of many wood species varies due to differences in extractive content, anatomical features, growth conditions, and not at least in dependence of the respective exposure conditions either under test or in real life applications. And so does the durability of English oak (Quercus robur L.), which has recently been considered in the revised European standard EN 350 (2016) and is now cla...
C Brischke, L Meyer-Veltrup, A Soetbeer, M Höpken, E Melcher, J Trautner


Assessing the natural durability for different tropical timber species using the mini-block test
2017 - IRG/WP 17-10886
The Xylarium in the Royal Museum for Central Africa (RMCA, Tervuren, Belgium) contains over 60,000 wood-samples, comprising over 12,000 species. These samples are of great historical and scientific value yet have a random format, which complicates standard testing. The wood-durability against Coniophora puteana and Trametes versicolor was tested for 36 species. Due to the random sample sizes the s...
V Deklerck, I De Windt, N Defoirdt, J Van den Bulcke, H Beeckman, E Espinoza, J Van Acker


Laboratory test to determine the effect on durability of combining biobased building materials with timber in construction
2017 - IRG/WP 17-20604
The use of Structural Insulated panels is a construction approach that is seeing more abundant use and is becoming a widely available method. Preformed units are usually a composite structure which often include a range of bio-based materials such as timber, wool or straw. Traditional laboratory based wood decay tests do not take into account this combination of biobased materials and it may be po...
S F Curling, G A Ormondroyd


Efficacy of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsamdua) water extractives on the durability of five Ghanaian less used timber species of varying perviousness and retentiveness
2017 - IRG/WP 17-30705
Conventional wood preservatives are not only toxic to target bio-deterioration organisms but also to humans, other organisms and the environment. In an effort to find preservatives that are less toxic or non-toxic to man, other organisms and the environment, efficacy of branch bark and heartwood water extracts (0.65 g/ml) of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsa...
A Asamoah, K Frimpong-Mensah, C Antwi-Boasiako


Anti-fungal activity of rutin and rutin-metal complexes as wood protectants
2017 - IRG/WP 17-30708
The anti-fungal activity of Rutin, a flavonoid, alone or complexed with copper or zinc was investigated in a petri dish test with Gloeophyllum trabeum and Trametes versicolor as the test fungi. Rutin and the Rutin-metal complexes showed significant inhibition against each fungus. Rutin-Cu and Rutin-Zn strongly inhibited the brown rot fungus, G. trabeum, while Rutin and Rutin-Zn inhibited T. versic...
Li Yan, J J Morrell, Jie Zhong, Xiuzhu Mao


Copolymers of tannin extracts as wood protection agents
2017 - IRG/WP 17-30709
Wouldn´t be a dream to preserve wood with the substances which the nature already synthesizes for protecting itself? The idea we would like to pursue is simple: Increase the concentration of these substances, the tannins, trying to fix them properly in wood. It appears easy but it is not. Sensibility against leaching, fungal decay and weathering were observed. In this paper new flavonoid co-polym...
G Tondi, L Sommerauer, A Oberle, A Petutschnigg, M-F Thevenon


Bio-friendly wood protection systems - resistance to mould and blue-stain fungi
2017 - IRG/WP 17-30713
With stricter restrictions on the use of biocides and increasing environmental awareness there is a pronounced need for effective bio-friendly protection systems in the wood preservative and wood coating industry. One of the possible pathways is to exploit and utilize natural substances with active biological effects. Silanes, caffeine, natural oils and potassium carbonate were chosen as compounds...
L Ross Gobakken, W Perdoch, B Mazela, P Kwaśniewska-Sip, G Cofta


Agar block durability test of plywood made of neem (Azadiracta indica) leaves treated veneer using two white rot fungi
2017 - IRG/WP 17-40782
This study has been undertaken to investigate the durability of plywood made from non-durable wood (simul, Bombax ceiba) veneer treated by neem (Azadiracta indica, A. Juss.) leaves. The veneers were treated with cold and hot water solution of neem leaves of different concentrations (10%, 5%, 2.5%) and treatment durations (1, 2, 3 days) for cold water and 20, 40 and 60 minutes for hot water. The pl...
K Akhter, M A Hashem, S Akhter


Impact of heat treatment on physico-mechanical properties of torrefied Antholceistha djalonensis wood
2017 - IRG/WP 17-40811
Thermal modification at relatively high temperatures is an effective method to improve the dimensional stability and mechanical properties of wood. This study was carried out to investigate the impact of heat treatment on the physic-mechanical properties of torrefied Anthocleistha djalonensis wood. Thirty nine defect-free specimens of dimensions 20 mm × 20 mm × 60 were prepared for the determina...
E A Iyiola, B Olufemi, J A Fuwape, J M Owoyemi


Durability of energy efficient wooden buildings: a building physical point of view
2017 - IRG/WP 17-40812
The drive for more energy efficient and sustainable buildings resulted in an increased popularity of wooden buildings, even in countries with a masonry tradition. Often guidelines and prescriptions then are copied from other countries. Different climatic boundary conditions and tradition of finishing, though, do require different moisture tolerance criteria. This is clearly the case for water vapo...
S Roels, J Langmans


Testing of the resistance of acetylated wood against marine borers at three Italian sites
2017 - IRG/WP 17-30719
The aim of this research is the determination of resistance of acetylated wood against marine biodeterioration in use class 5 (EN 335) in temperate sea waters. The resistance of acetylated Pinus radiata (radiate pine) in solid and MDF form is compared with that of the untreated radiata pine and other untreated wood of European species such as Fagus sylvatica (European beech) Castanea sativa (chest...
S Palanti, M Faimali, D Tagliapietra, M Andrenacci, M Anichini, M Sigovini


Previous Page | Next Page