An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Glulaminated poles - Progress report after 7 years' testing
1987 - IRG/WP 3444
In 1979 a number of glulaminated poles with various preservative treatments were placed in a greenhouse at Uppsala, at the Simlångsdalen test field in southern Sweden and under a power line just south of the Arctic circle in order to study their resistance against biological degradation. The tests have shown that the comparatively best performance will be obtained if each lamination is treated wi...
J Jermer, Ö Bergman


Soft rot decay of Belian (Eusideroxylon zwageri) wood
1995 - IRG/WP 95-10119
The heartwood of Belian (Eusideroxylon zwageri), an East Malaysian timber species, is naturally durable due to its certain unique anatomical features and high content of extractives. The timber can tolerate years of exposure to hazardous conditions in ground contact and other situations without any significant loss in its strength. A few Belian transmission poles sampled from one locality in Saraw...
A H H Wong, A P Singh


Thermal modification of non-durable wood species 1. The PLATO technology: thermal modification of wood
1998 - IRG/WP 98-40123
The PLATO technology is an innovative upgrading technology with low environmental impact, which can be applied to fast grown and non-durable wood species. This technology is based on a thermal modification of solid wood without the addition of chemicals (e.g. preservatives), consisting of a hydrothermal treatment, followed by drying and curing. The PLATO technology results in a substantial improve...
M J Boonstra, B F Tjeerdsma, H A C Groeneveld


Evaluating the performance of preservative/water repellent emulsion systems
1997 - IRG/WP 97-20127
Water repellent emulsions are being combined with wood preservatives to improve the weathering properties of treated wood in service. Unfortunately, few standard procedures are available to objectively compare the performance of these systems and as a result quality issues are almost completely neglected. The value of swellometer tests, water immersion tests and accelerated weathering regimes in t...
K J Archer, F Cui


Improvements of stability and durability of beechwood (Fagus sylvatica) by means of treatment with acetic anhydride
1991 - IRG/WP 3645
In the present investigations, beechwood (Fagus sylvatica) was treated with non-catalysed acetic anhydrid at 120°C and some physical- and biological parameters of the treated wood were compared with those of non-treated wood. The radial and tangential shrinkage and swelling, respectively, and the absorption capacity of the acetylated wood against moisture is considerably lower. The durability aga...
H Militz


Determination of total fluoride and boron in preservative-treated wood fluoride by ion selective electrode without steam distillation, and boron colorimetrically using azornethine-h
1998 - IRG/WP 98-20135
An analytical method was developed to determine total fluoride and boron in wood treated with aqueous or solid diffusing fluoride or borate-fluoride formulations. Ground wood was mixed with 30% sodium hydroxide solution and oven-dried for 2 hours before furnacing at 600° C for 1 hour. The cool fused product was dissolved in hot water, transferred to a plastic beaker and neutralised. Fluoride was ...
P A Collins, M J Kennedy


Soft rot - Soil burial - Tests. Influence of the water content of the soil on wood decay
1972 - IRG/WP 212
The decay of wood samples buried in the soil is influenced by various factors. Decisive are the water content, the content of organic substances, pH-value content of mineral nutritive substances etc. of the soil. For the tests, carried out by the EMPA until now, it was always started with a water content of 35%, refered to the dry weight of the EMPA-soil = 75% of its water capacity. In order to in...
O Wälchli


Environmentally benign biological wood preservatives by Streptomyces rimosus, SC-36
1997 - IRG/WP 97-10196
Microbiocides obtained from mutant culture Streptomyces rimosus SC-36 were evaluated for their abilities to inhibit the growth of brown-rot, soft-rot, white-rot, and sapstain fungi on wood. The test fungi were the brown-rot fungi Antrodia carbonica, Gloeophyllum trabeum, Neolentinus lepideus, and Postia placenta; soft-rot fungi Chaetomium globosum, Paecilomyces variotti, Phialocephala dimorphospor...
S C Croan


The effect of water-repellent additives on the leaching of CCA from simulated southern Yellow pine decks
2000 - IRG/WP 00-50158
End-matched SYP boards were pressure-treated with CCA or CCA in combination with commercial water repellent additives. After fixation and drying, the boards were placed in plastic boxes and exposed outside in Harrisburg, NC. Plastic supports were used to keep the boards above the water collected. Over a period of five months, rain run-off water from 14 natural rainfalls were collected and analyzed...
F Cui, P J Walcheski


Decay resistance of Siberian larch wood against brown rot fungi - Part 2. The effect of genetic variation
1998 - IRG/WP 98-10287
Wood natural decay resistance is mainly restricted in the heartwood part of tree and based on wood microstructure and chemical composition. However, the variation of decay resistant in different wood species is vide and the effect of genotype on decay resistance of Siberian larch wood grown in Finland is not known. The aim of this work was to find out the variation on decay resistance of Siberian ...
H Viitanen, L Paajanen, T Nikkanen, P Velling


Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


Field testing of alkylammonium wood preservatives
1983 - IRG/WP 3248
The field test performance of five alkylammonium wood preservatives is described. The relative effectiveness of three unmodified formulations was determined by calculation of a Performance Index. Of the three, didecyldimethylammonium chloride was found to be superior to octyldecyldimethylammonium chloride, and both were more effective than alkyltrimethylammonium chloride. However, none were consid...
J N R Ruddick


Low polymer levels containing bioactive monomer polymerized in situ provide resistance to Gloeophyllum trabeum
1995 - IRG/WP 95-30066
Wood preservation based on in situ polymerization of potentially bioactive monomers has been studied. Tributyltin oxide acrylate (TBTOA) and pentachlorophenol acrylate (PCPA) were synthesized. Wood samples were treated at 2, 5, 10, 15 and 20% by weight solutions with varying amounts of crosslinker (trimethylolpropane trimethacrylate, TMPTM) and polymerized in situ in wood samples (2.54 x 2.54 x 0....
R E Ibach, R M Rowell


The use of the Shigometer® and Pilodyn® as non-destructive test methods for detecting decay in CCA treated eucalypt poles
1981 - IRG/WP 2153
The groundline condition of sixty C.C.A. treated eucalypt poles comprising six different species was examined using the Pilodyn® and Shigometer®. Although sensitive to the presence of soft-rot decay, the Shigometer® would seem to offer little practical advantage in the eucalypt soft-rot decay situation, since a comparable visual examination could reveal the presence and extent of decay. Initial...
L E Leightley


Influence of sampling on the composition of test solutions
1985 - IRG/WP 2235
For four commercial products of CCB-salts the influence of the kind of sampling on the composition of test solutions has been tested. For each product several 5 g samples have been taken at random, after careful mixing the content of each bottle, and after grinding the whole content. With each sample a 5% test solution was made and analyzed on the content of chromium, copper and boron. Altogether ...
H Willeitner, K Brandt


Evaluation of the pulsed-current resistance meter (Shigometer®) for determination of the internal condition of utility poles
1979 - IRG/WP 2128
A number of Telecom poles, which had been removed from service to be replaced by a radio link, were inspected using an electrical resistance meter (Shigometer®). These poles were creosoted, non-durable Victorian species in service in New South Wales. Six of these poles, chosen to represent various internal conditions typical of the range of the population tested, are discussed here. Data, from tr...
J D Thornton, W G Seaman, M McKiterick


Modified Wood – Methods, testing and applications: Outcomes of the EU-Thematic Network
2003 - IRG/WP 03-40268
In the last decade, interest in the development of wood modification systems has increased in Europe. Alongside several industrial initiatives for heat treatments, there have also been scaling up and pilot plant projects for chemical wood modification. Between 2000 and 2003, the European Commission funded the "Thematic Network on Wood Modification". This paper will feature the modification process...
D Jones, W Homan, J Van Acker


Fixation of copper-chrome-arsenic treated timber: A comparison of leaching methodologies
1996 - IRG/WP 96-50075
Five packs of kiln dried radiata pine heartwood were treated with copper-chrome-arsenic preservative treated, utilising a modified Bethell treatment schedule. Two methods of determining the level of preservative fixation were compared. These included the diphenylcarbazide method and simulated rainfall testing. The fixation levels were generally higher for tests involving simulated rain leaching. F...
S Walley, P R S Cobham, P Vinden


Wood preservation using furanones derived from marine algae
2004 - IRG/WP 04-10506
Halogenated furanones that are analogues of natural compounds extracted from the red seaweed Delisea pulchra were examined in the laboratory for activity against termites and decay fungi. The furanones were found to have broad spectrum activity, some with solution strengths of 0.01% controlling Coptotermes acinaciformis in a filter paper trial, while 2% solutions impregnated into Pinus radiata blo...
L J Cookson, R de Nys, P Steinberg, N Chew


Leaching characteristics, decay and termite resistance of treated wood with boron compounds, N'-N-(1,8-Naphthalyl) hydroxylamine (NHA-Na), and hydroxynaphthalimide (NHA-H)
2003 - IRG/WP 03-30307
Despite many advantages of boron wood preservatives, boron itself does not adequately protect wood in ground contact and exterior applications because its natural diffusibility and susceptibility to leaching. As a result of previous studies to limit or decrease boron leaching, several fixation systems have been developed. In this study, we evaluated the effects of N'-N-(1, 8-Naphthalyl) h...
S N Kartal, Y Imamura


Selective chromate elimination from the storage-drainage-water of a wood impregnation plant
1980 - IRG/WP 3153
With the Enviro-Chrom-Ex process it is possible to eliminate ecologically and economically hexavalent chromium (chromate) from water selectively. The process which is based on the principle of selective ion exchange works with different chromate concentrations and under the presence of other ions, irrespective of the water hardness. The values of water-offtake reach 0.1 mg CrVI at maximum, causing...
O Wälchli, R Ott, R Hugener, E Graf, B Lieberherr


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany, where Oil-...
C R Welzbacher; A O Rapp


Durability of Bamboos in India against termites and fungi and chemical treatments for its enhancement
2005 - IRG/WP 05-10553
Bamboo is a very important forest resource that benefits the life of people in a myriad ways including meeting the need for structural uses like posts, pole fencing, scaffoldings, house building, etc. Although it is one of the strongest structural material available, often succumbs to fungal decay and biodeterioration by insects (termites and powder post beetles) during storage and usage. Studies...
O K Remadevi, R Muthukrishnan, H C Nagaveni, R Sundararaj, G Vijayalakshmi