IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 2168 documents. Displaying 25 entries per page.


Some data on the activity of alternative fungicides for wood preservation
1985 - IRG/WP 3333
Data from laboratory tests against basidiomycete fungi are presented for 9 alternative fungicides in organic solvent formulations and also in water for one product. Results are compared with data for reference preservatives, tributyltin oxide, copper and zinc naphthenates and pentachlorophenol. Of special interest is the apparently better than additive effect of mixing tributyltin naphthenate and ...
A F Bravery, J K Carey


Properties of plywood and Oriented Strand Board manufactured with an organic insecticide incorporated in the adhesive formulation
2000 - IRG/WP 00-40174
The efficacy of Fipronil as an insecticide has been established by laboratory and field experiments and commercial use against a broad range of insect pests for various crops. It can be used by either foliar or soil application. Development is underway for the non-agricultural uses of fipronil. Research is ongoing for the control of ants, cockroaches, fleas, ticks, houseflies, mosquitoes, termites...
D P Kamdem, J H Hope, A Jermannaud


Comparative performance of several ammoniacal copper preservative systems
1997 - IRG/WP 97-30151
The efficacy of several ammoniacal copper-based wood preservative systems was evaluated in this study. The selection of potential co-biocides was based on the results of an agar plate test. Following this, the most promising systems were evaluated in a standard field stake test. Good correlation was found between the agar plate and field stake test results. Of the preservative systems tested, copp...
D D Nicholas, T Schultz


Decay and mold resistance of borate modified oriented strandboard
2003 - IRG/WP 03-40260
Decay and mold resistance of zinc borate (ZB) and calcium borate (CB) modified oriented strandboard (OSB) from southern mixed hardwoods and yellow pine was investigated in this study. Tests were done with brown rot, Gloeophyllum trabeum, and white-rot, Trametes versicolar, fungi for 8 and 12 weeks, respectively. Wood species and fungus type had significant influence on the decay resistance. Decay...
Q Wu, S Lee, J P Jones


The use of modulus of rupture and modulus of elasticity in natural durability testing
1997 - IRG/WP 97-20117
Losses in weight, losses in bending strength and changes in elastic behaviour were assessed in a fungus cellar test with beech wood stakes (Fagus sylvatica). Results were gained after 8, 12, 16 and 20 weeks resp . The outcomes show, that the non-durable species beech is very rapidly attacked by fungi and loses up to 60% of its initial bending strength even within the first 8 weeks. Earlier researc...
L Machek, H Militz, W Gard


In vitro sporulation of selected wood decay fungi
1978 - IRG/WP 190
Basidiospores produced axenically without laborious attention in the laboratory are useful in studies of wood decay initiation. Such spores presumably approach those collected from natural sporophores in size and germinability (Morton, 1964). Production of spores in vitro by inversion of cultures grown on 2% malt extract agar in deep glass dishes (100x80 mm²) has been the preferred method (Morton...
E L Schmidt, D W French


A new technique for testing decay resistance of framing lumber
2002 - IRG/WP 02-20247
Model house frame units (two studs, top and bottom plates and a central “dwang”) were constructed using short (500-600 mm) lengths of framing timber. Constructed frames were impregnated with water using a mild pressure schedule to raise the initial moisture content to 35-40 % mc. The back face of each unit was then covered with black polyethylene. Two locations at the stud/dwang and stud/botto...
M E Hedley, D Page, B E Patterson


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


The influence of the natural extractives of opepe (Nauclea diderrichii) and African padauk (Pterocarpus soyauxii) timbers on their durability
1996 - IRG/WP 96-30098
Many timbers contain chemical extractives that undoubtedly play a key role in the timber's natural durability. Opepe (Nauclea diderrichii) and padauk (Pterocarpus sp.) are both very durable timbers (class 1), yet they are described as being moderately permeable. This suggests the presence of biocidal chemicals within these timbers, rather than simple blocking agents. Initial trials on the...
E D Suttie, R J Orsler


Evaluating possibilities of leaching of deltamethrin and TCMTB (insecticides and fungicide for protecting wood) by rain water or by soaking in water
1988 - IRG/WP 3464
Deltamethrin and TCMTB have been subjected to several field leaching tests on freshly fallen trees and in the laboratory, using standard EN 84. All the trials gave the same results and confirm that Deltamethrin and TCMTB are not washed out after they have been allowed to penetrate the trunk surface properly. According to the EN 84 standard, less than 1% Deltamethrin and less than 1.7% TCMTB were r...
J S Duguet, V Dartigues


Treatment of lumber with preservative/water repellent emulsions - The significance of shear stability on penetration
1997 - IRG/WP 97-20124
Currently, the treatment of lumber with a water repellent emulsion and a wood preservative formulation in combination is the most cost effective way to prevent decay and to maintain the appearance of uncoated lumber in service. Water repellents influence the movement of moisture into and out of wood and, by so doing, can decrease checking and splitting significantly. Adequate penetration of the em...
F Cui, K J Archer


Controlling the sapstain fungus Ceratocystis coerulescens by metabolites obtained from Bjerkandera adusta and Talaromyces flavus
1993 - IRG/WP 93-10024
Sapstain causes severe damage to wood and wood products, posing a major economic problem for the wood industry. The purpose of this study was to determine if metabolites from Bjerkandera adusta and Talaromyces flavus would (1) decolorize stain in wood caused by Ceratocystis coerulescens and (2) prevent sapstain by Ceratocystis coerulescens. We studied the interaction of the sapstain fungus Ceratoc...
S C Croan, T L Highley


Test of N-tritylmorpholine in combination with synthetic pyrethroids against marine borers in tropical Australia and Panama
1991 - IRG/WP 4168
Test blocks ol Pinus sylvestris sapwood were pressure impregnated with white spirit solutions of N-tritylmorpholine, either alone or in combination with permethrin, deltamethrin or cypermethrin. They were exposed in the intertidal zone at Mourilyan Harbour, North Queensland, Australia and subtidally at either end of the Panama Canal. After 5 months' exposure at Naos Island at the Pacific ...
S M Cragg, J D Bultman


Field test results for the elimination of subterranean termite (Coptotermes formosanus) colonies by a bait system containing the IGR hexaflumuron
1997 - IRG/WP 97-10222
Field studies were conducted at Chichijima (Ogasawara Islands, Tokyo) to determine the effectiveness of a termite bait system (commercial name: Sentricon* system) containing hexaflumuron (Insect Growth Regulator: IGR) in the elimination of subterranean termite (Coptotermes formosanus) colonies. The level of subterranean termite activity on Ogasawara Islands is high resulting in extensive damage to...
K Suzuki, Y Morita, K Yamauchi


Effects of surfactants and ultrasonic energy on the treatment of wood with chromated copper arsenate
1977 - IRG/WP 3108
Sugar pine stakes 1'' x 1" x 16" were treated by a hot-water bath followed by soaking in cold CCA solution for 10 to 30 minutes. A similar number of stakes were treated by a cold-cold bath. Half of the stakes were subjected to ultrasonic energy during the CCA bath. The mean absorption for stakes given the hot-cold bath was 18.52 pcf (297 kg/m³) and 4.64 pcf (74 kg/m³) for those...
C S Walters


Decrease in the mechanical resistance of blue stained and "orange stained" Pinus radiata wood
1999 - IRG/WP 99-10313
It is recognised that sapwood attacked by Ceratocystis pilifera increases its permeability to pressure preservative treatments. Since hiphae not only utilise pits, but also the cell wall for crossing from one cell to another, the mechanical resistance of the stained wood might be affected. The orange colour very commonly present in Pinus radiata logs heartwood under water sprinklers, has not recei...
M C Rose, L Reyes, J Alvarez, A Andaur, C Beltran, D Rivera


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers
1991 - IRG/WP 2381
Standardized heartwood blocks of kempas (Koompassia malaccensis), keruing (Dipterocarpus sp.) and tualang (Koompassia excelsa) were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicola grisea, Petriella setifera and Trichurus spiralis in a containerized vermiculite-burial decay system according to draft CEN/TC 38 WG 4....
A H H Wong, R-D Peek


Natural Durability of Tropical Species – Variations and Prospects
2005 - IRG/WP 05-10568
The tropical timber resources of the world play an unequivocal role in economic development of both the tropical timber producing and importing regions. This paper describes natural durability as an important and preferred wood quality of tropical species of the world with emphasis on Malaysian hardwoods, the link between various aspects of tropical hardwood durability, hardwood utilization and bi...
A H H Wong, Yoon Soo Kim, A P Singh, Wang Choon Ling


Accelerated decay tests to investigate postulated effects of tannins on CCA efficacy in wood
1988 - IRG/WP 3497
Five groups of blocks (10 x 10 x 5 mm³) viz., Pinus patula, Pinus patula impregnated to 4% (w/w) tannin; Eucalyptus grandis, Eucalyptus grandis with natural tannins extracted; and extracted Eucalyptus grandis with tannins returned as above; were prepared. Blocks from each group were then treated to 0, 5, 10 and 15 kg/m³ CCA and challenged in four 15-week decay tests, viz., soil burial, and expos...
U L Scherer, A A W Baecker


Effect of angle of exposure on degradation of radiata pine during weathering trials
1988 - IRG/WP 2301
The importance of angle of exposure on the degree of weathering of materials has not been adequately resolved. In conventional tests, specimens are exposed at an angle of 45° facing the equator, but more recently experiments on polymeric materials have suggested that an angle of 0° may be preferable since this angle maximises levels of received ultra-violet radiation. In this paper the degradati...
P D Evans


Fungicidal activity of some new water borne copper octanoate based formulations
1999 - IRG/WP 99-30198
Four new water borne formulations for preservation of wood were prepared: the composition of Cu(II) octanoate, 2-aminoethanol (ethanolamine) and water; the composition of complex of Cu(II) octanoate with nicotinamide, 2-aminoethanol and water; the one of Cu(II) octanoate, organic boron complex, 2-aminoethanol, dimethyl sulfoxide and water and finally, the mixture of Cu(II) octanoate, diazene, 2-am...
M Petric, M Pavlic, F Pohleven, P Segedin, B Kozlevcar, S Polanc, B Stefane, R Lenarsic


Biological detoxification processes - A check list for assessments
1998 - IRG/WP 98-50120
The number of scientific publications on the biological purification of preservative treated wood implies that the biological treatment of wood wastes becomes more and more important. But an information about a successful industrial application is almost missing in all cases. Therefore the applicability of the proposed purification processes is often uncertain. The feasability of such a biological...
H Leithoff, R-D Peek


Longterm monitoring of termite activity on multiple feeding sites: a laboratory method intended for the determination of attractant/repellent properties of wood preservatives and baits
2001 - IRG/WP 01-20225
A method is introduced allowing the continuous monitoring of the activity of a small laboratory termite- colony at 8 different feeding sites simultaneously. The test assembly consists of a small central polycarbonate-tube containing a colonie of Reticulitermes santonensis (de Feytaud) beeing connected with 8 external feeding sites by small glass-capillaries. The termites passing through the glass ...
M Pallaske, E Graf, H Takiuchi


The degradation of wood surfaces by water
1984 - IRG/WP 3289
Thin radial/longitudinal sections (~100 µ) of Scots Pine (Pinus sylvestris) and lime (Tilia vulgaris), were exposed to deionised water over the temperature range 25-65°C. Losses in wet tensile strength and toughness occurred rapidly at temperatures from about 50°C upwards. After about 2 months' exposure pine lost some 10-30% of its tensile strength and 20-60% of its toughness. For lime...
W B Banks, P D Evans


Application of roller-pressing method to the novel liquid impregnation treatment of green timber
2001 - IRG/WP 01-40198
A transverse compression technique enabled us to impregnate liquid into green timber through replacement of the free water in the timber with a treatment liquid without any critical physical damage to the timber by the roller-pressing method. The roller-pressing is supposed to remove free water the cell cavities and to concurrently introduce the treatment solution into green timber in the treatmen...
M Inoue, K Adachi, K Tsunoda, Y Imamura, S Kawai


Previous Page | Next Page