Effect of nutrient regimes, temperature, pH, and wood sterilization method on performance of selected bioprotectants against wood staining fungi
1992 - IRG/WP 92-1551
The effect of nutrient regimes, incubation temperature, media pH, and wood sterilization method on performance of four potential bioprotectants (Pseudomonas putida, Pseudomonas cepacia, Bacillus subtilis, and Trichoderma harzianum) against wood staining fungi were evaluated using small ponderosa pine samples over a four week period. Incubation at 32°C resulted in slight increases in the degree of...
J J Morrell, C M Secton


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Environmental fate of copper-based wood preservatives in different soil substrates - Part 1: Screening of the metal adsorption potential
1998 - IRG/WP 98-50101-21 a
In treatment plants, spillage of wood preservatives onto soil may be of environmental concern. This potential soil contamination served as an objective for a screening study. Three different mineral soils, a mineral substrate and two horticultural substrates are examined for their sorptive potential of copper through mixing with wood preservative solutions. Depending on the soil/substrate charact...
G M F Van Eetvelde, J M Mwangi, F Tack, R Hartmann, M Stevens


An attempt to grow dry rot fungus Serpula lacrymans on mortar substrate in non-sterile conditions
1989 - IRG/WP 1385
According to many experts, Serpula lacrymans is probably the most dangerous wood destroying fungus in houses. Investigations of KOCH, A.P. (2) showed that incidence of this fungus in percent was around 20% when the frequency of some other standard fungi was far below (Coriolus versicolor: 0.2% for example). The work presented here is a part of a program carried out at CTFT for assessing the resist...
L N Trong


A bioassay to determine preservative retention in hardwoods and southern pines
1982 - IRG/WP 2183
In this paper the author discusses and suggests a new method of evaluating preservative retention in treated woods by means of bioassays. Twelve North American species were tested with different retention levels of pentachlorophenol (PCP) and copper/chrome/arsenic (CCA) preservatives. The results observed in this work show that among other fungi, Aspergillus niger responds to both preservatives, w...
J C Moreschi


Fungal siderophores and their rôle in wood biodegradation
1990 - IRG/WP 1442
Iron and other metals such as manganese, play an important role in the metabolic functions of fungi that cause wood deterioration. These transition metals are also found in, or associated with, the extracellular fungal enzymes shown to be directly involved in the decay process. Recently our research group was able to show that siderophores (low molecular weight biological chelators) are produced b...
J Jellison, B Goodell, F Fekete, V Chandhoke


Preservation of wood-based panels against fungi and insects and and testing its efficiency
1976 - IRG/WP 270
Wood-based panel products which are made of susceptible wood species may be destroyed by fungi under wet conditions and by termites. The glues do not provide sufficient protection unless very high concentrations are applied. Particle boards and fibre boards are not susceptible to beetle infestation, although some species may attack plywood. Various types of preservatives provide sufficient protect...
G Becker, M Gersonde


Microbial decay in an extremely durable Malaysian hardwood Belian (Eusideroxylon zwageri) - an overview
1997 - IRG/WP 97-10216
The heartwood of Belian (Eusideroxylon zwageri) is highly regarded among the naturally durable Malaysian hardwoods, and is therefore a choice timber for soilcontact use in the humid tropics such as untreated telecommunication poles, fence posts and railway sleepers. The high microbial resistance of the wood is evidenced by the mere superficial degradation observed in some pole samples after 20 yea...
A H H Wong, A P Singh


Current status of AAC preservatives in New Zealand
1980 - IRG/WP 3141
Two types of alkylammonium compounds (AAC) have been approved as commercially acceptable wood preservatives by the NZ Timber Preservation Authority (TPA). They are alkyldimethylbenzyl ammonium chloride and alkyldimethylamine acetate, both of which must contain either (a) 70% alkyl chains of C12 + C14 and less than 10% of any other individual chain length, or (b) 85% alkyl chains of C12 + C14 with ...
J A Butcher


European standardization for wood preservation
1991 - IRG/WP 2365
Since the last IRG 21 conference in New-Zealand, there one meeting of the plenary committee and several meetings of working groups. The interprative documents prepared by CCE for expliciting the essential requirements of the CCE Directive on the construction products and specially: mechanical resistance and stability / hygiene, health and environment / safety in use are waited to valid the progra...
Anonymous


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Efficacy of fumigants in the eradication of decay fungi implanted in southern pine timbers
1986 - IRG/WP 3365
Southern pine timbers (15.2 cm x 15.2 cm x 4.26 m) were fumigated at midlength to evaluate the effectiveness of the fumigants chloropicrin, Vapam, Diazomet, Busan 40, Vanicide 51, Vanicide TH, sodium bisulfite, and ethanolamine in eradication of decay fungi. The fumigants were introduced into 2.54 cm holes which were closed immediately with rubber stoppers. Movement and persistence of lethal conce...
T L Highley, W E Eslyn


Accelerated diffusion treatment of sawn Sitka spruce grown in the UK
1986 - IRG/WP 3395
The treatment of 'green' sapwood and heartwood of Sitka spruce by diffusion methods was investigated. Steam/dip treatment processes gave increased solution uptakes and depths of penetration of copper in comparison with a simple dip treatment. Further investigation is required to reduce diffusion gradients with copper based formulations and to improve the penetration of '...
R J Murphy, D J Dickinson


Microwave digestion of preserved wood for the determination of Cu, Cr, As, B and P in quality control
1991 - IRG/WP 2364
A microwave digestion method for the determination of copper, chromium, arsenic, boron and phosphorus in preserved woods is described. Samples were digested with nitric acid in pressure-relief type teflon PFA vessels by microwave heating in a commercial laboratory microwave oven. Fast, efficient and complete digestion was achieved within 29 min for 12 samples. The digestion time compared favourabl...
N Bernth, L B Sheard


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


International collaborative laboratory comparison of two wood preservatives against subterranean termites: Second update
1995 - IRG/WP 95-10117
As was agreed by members at the termite workshop at the 24th annual meeting of IRG in Orlando, USA, in May 1993 to initiate an international subterranean termite laboratory bioassay to compare the various preferred termite protocols used by IRG termitologists was initiated. The author was nominated to co-ordinate this comparative laboratory evaluation of two wood preservatives (CCA and Cu-naphthen...
J R J French


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Nasutitermes exitiosus and wood-rotting fungi in Eucalyptus regnans, E. acmenioides, E. wandoo, and E. marginata: force-feeding, laboratory study
1985 - IRG/WP 1231
Under a force-feeding regime, the termitid Nasutitermes exitiosus was fed on four eucalypt timbers infested with several fungal species to investigate the influence of such fungus-infested timbers on mass of wood lost, termite biomass, fat content and water content. The results showed that wood mass losses were markedly affected by species of fungi and timber. The interaction of fungi and timbers ...
D B A Ruyooka


Colonisation and detection of New Zealand sapstain fungi
2000 - IRG/WP 00-10329
Sapstain is the bluish black discolouration in logs and timber caused in New Zealand by Sphaeropsis sapinea (Diploida pinea) and more than twenty different species of the Ophiostomataceae Family. Laboratory and field trials were conducted by inoculating radiata pine to establish staining colour and extent of colonisation with various New Zealand sapstaining fungal species. Colonisation patterns, c...
J M Thwaites, R L Farrell


Improved preservative penetration of spruce after pre-treatment with selected fungi. II. Creosote treatment, analysis and strength testing
1998 - IRG/WP 98-40106
This paper describes the creosote treatment and analysis of logs pre-treated with selected fungal agents as a method of increasing the porosity of the wood prior to preservative treatment. The paper also reports the subsequent strength testing of the timber to evaluate the effects of the fungal pre-treatment on the structural integrity of the wood. European spruce logs were pre-treated with eithe...
E J Tucker, A Bruce, H J Staines, B Rosner, K Messner


Suitability of cotton strip testing as a screening method for the development of wood preservative formulations
2003 - IRG/WP 03-20270
This paper outlines a simple and rapid test method for screening the efficacy of wood preservative formulations against microbiological attack using cotton strips. The method was evaluated against soft rot and was found to provide reliable information on the protection of lignocellulosic material against microbiological attack. The assessment is based on visual interpretation of decay and on a sim...
H Leithoff, I Stephan, H Härtner


Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial


Organic nitrogen in wood: Growth substrates for a sapstain fungus
1993 - IRG/WP 93-10019
The nitrogen content of mature wood from lodgepole pine was 0.046% as determined by micro-Kjeldahl. Low molecular weight proteins between 14 and 21 kDa were identified in mature wood, branch wood and sap pressed from wood chips. Amino acids were quantified in acid-hydrolyzed wood samples and accounted for between 19 and 35% of the nitrogen in wood. The sapstaining ascomycete Ophiostoma piceae stra...
L D Abraham, C Breuil


Laboratory Evaluation and Field Trial of Chlorothalonil and Copper-based Preservatives and Leaching Performance of Copper in Copper Treated Wood
2002 - IRG/WP 02-30279
Soil block test and field trial of some Chinese plantation wood species pine and poplar treated with chlorothalonil formulations and copper-based preservatives such as ACQ-B and copper citrate (CC) were conducted. The results of soil block test indicated that chlorothalonil formulations and ACQ-B as well as CC are very effective for controlling the 2 fungi species Corious versicolor and Poria plac...
Mingliang Jiang, Ping Wang, Chungen Piao, Zhaobang Li, Quan Lu, Lei Liu


Previous Page | Next Page