Effect of steam on fixation of Cu-amine preservative treated wood
2008 - IRG/WP 08-50251
The rates of copper fixation in copper amine preservative treated wood were investigated with different fixation conditions (20° with drying and 50° without drying) and post-steaming. We also measured the degree of leaching for other biocide components (azoles, quatz, and Cu-HDO). Treatments conditioned at 20° with drying required 50 days or more to fix in woods. While copper was stabilized i...
Sung-Mo Kang, In-Yong Hwang, Suk-Kuwon Kim


Leachability of Arsenic, Chromium and Copper from Weathered Treated Wood
2008 - IRG/WP 08-50255
The objective of this study was to quantify the loss of arsenic, chromium and copper from weathered treated wood under normal field conditions as most residential structures currently in service in the U.S. have been constructed at least 3 years ago. For comparison, leaching from different retention levels of weathered CCA treated wood (low, medium and high) is compared to leaching from new ACQ tr...
A R Hasan, Ligang Hu, H M Solo-Gabriele, Yong Cai, L A Fieber


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Laboratory Studies on Copper Availability in Wood Treated with Soluble Amine Copper and Micronized Copper Systems
2008 - IRG/WP 08-30489
A laboratory method has been employed to investigate the level of soluble copper in wood treated with various copper-based preservative systems, such as micronized copper (particulate copper) and amine copper solutions. This report describes the methodology and preliminary results on determination of the soluble copper in the treating solutions and the treated wood by these systems, as well as th...
L Jin, P Walcheski, A Preston


Alkaline copper treated wood for use in residential decking
2008 - IRG/WP 08-30490
Alkaline copper quaternary ammonium compound (ACQ) treated decking was exposed in a field experiment and the mobile copper assessed based on that collected in the leachate. The amount of copper which leached was modeled after 4 years. The results showed that boards which leached most chemical initially provided the greatest loss over four years. The reduction in the mobility of copper with time wa...
J N R Ruddick


Corrosion of fastener and connector in contact with alkaline copper treated wood – it is a problem
2008 - IRG/WP 08-40437
For many decades, chromated copper arsenate (CCA) was the most common wood preservative used in North America for residential and industrial applications. Since December 31, 2003, the use of CCA for residential application was voluntarily terminated. One of the most widely accepted alternative wood preservatives in Western Canada is Alkaline Copper Quaternary Compound (ACQ). This paper will compar...
J N R Ruddick


Comparison of laboratory and natural exposure leaching of copper from wood treated with three wood preservatives
2008 - IRG/WP 08-50258
Standard and non-standard laboratory and field leaching tests were used to compare copper leaching from wood treated to above ground and ground contact specified retentions for three wood preservative systems, CCA-C, ACQ-D and a micronized copper formulation with quat DDAC as co-biocide. Copper leaching was highest for the ACQ formulation. Percent leaching was lowest for the micronized copper sy...
P A Cooper, Y T Ung


Durability and fungal colonisation patterns in wood samples after six years in soil contact evaluated with qPCR, microscopy, TGA, chitin- and ergosterol assays
2009 - IRG/WP 09-20402
There is a need to establish new objective and sensitive methods for early detection and quantification of decay fungi in wood materials. Molecular methods have proven to be a useful tool within wood protection issues, however, this field is still poorly explored and so far relatively few have used these methods within the field of wood deterioration. Among the techniques used in the indirect quan...
A Pilgård, G Alfredsen, I Børja, C Björdal


Copper to quat ratio in alkaline copper quat (ACQ) wood preservative - Effects on fixation and leaching of preservative components in red pine
2009 - IRG/WP 09-30496
This study investigates the effect of the relative proportion of copper oxide (CuO) to didecy dimethyl ammonium carbonate (DDACb) in an alkaline copper quat (ACQ) formulation on the rate of copper fixation or stabilization and the resistance of treated wood to leaching of copper and quat (DDACb). Red pine samples were treated with ACQ, having CuO to DDACb ratios of 2:1 (the normal ratio for ACQ-D...
S Pankras, P A Cooper, T Ung, L Awoyemi


Re-Distribution of Copper in the Cell Walls of Wood Treated with Micronized Copper Quat
2009 - IRG/WP 09-30506
Wood treated with copper-based preservatives to be used in ground contact may fail to inhibit soft rot fungi if penetration of copper into the cell wall is insufficient. Preservatives containing soluble copper are known to penetrate the cell wall; however, it is not known whether preservatives containing particulate copper will also migrate into the cell wall in sufficient quantities to control so...
R Stirling, J Drummond


Mold-resistance Effect of Bamboo Wood Treated with CCC-organic Complexes
2009 - IRG/WP 09-30514
Mold resistant effect of CCA, ACQ, CuAz, CCC and the compound of CCC and propiconazole were researched on bamboo wood of Phyllostachys pubescens were reported in this paper. Results showed that all of the test fungicides could protect bamboo wood better from Penicillam citrinum than from Trichoderma viride and Aspergillus niger. The complex of CCC and propiconazole had the best resisting effect on...
Sun Fangli, Yang Le, Chen Anliang, Bao Binfu, Li Qiao


Rapid Microwave-Assisted Acid Extraction of Metals from Chromated Copper Arsenate (CCA)-Treated Southern Pine Wood
2009 - IRG/WP 09-50262
The effects of acid concentration, reaction time, and temperature in a microwave reactor on recovery of CCA-treated wood were evaluated. Extraction of copper, chromium, and arsenic metals from chromated copper arsenate (CCA)-treated southern pine wood samples with three different acids (i.e., acetic acid, oxalic acid, and phosphoric acid) was investigated using in microwave reactor. Oxalic acid wa...
Bin Yu, Chung Y Hse, T F Shupe


Factors affecting sodium hypochlorite extraction of CCA preservative components from out of service treated wood for recycling
2009 - IRG/WP 09-50263
Significant amounts of chromated copper arsenate (CCA) treated wood products such as utility poles and residential constructions remain in service. There is an increasing public concern about environmental contamination from CCA treated wood when it is removed from service for reuse or recycling, placed in landfills or burned in commercial incinerators. In this paper, we investigate the effects of...
E D Gezer, P A Cooper


Microscopy evaluation of microbial decay patterns in wood stakes after 6 years in soil contact
2010 - IRG/WP 10-10715
Most studies on wood modification have so far been concerned with service life predictions rather than investigating the decay protection mechanism. Very little is known about the mode of action of these new treatments and about the strategies used by wood degraders in order to utilize the wood material despite a treatment. Access to such knowledge would allow further modification and improvement ...
A Pilgård, C G Björdal


Toward an assessment of copper bioavailability in treated wood
2010 - IRG/WP 10-20445
Many modern wood preservative systems rely on copper (Cu). Some oxalate-producing fungi detoxify Cu by immobilizing it in crystals, and this may decrease its physiological availability (bioavailability). Cu bioavailability may also decrease during wood treatment. Cu retention in wood, however, is typically measured as a weight-to-volume concentration without an estimate of its bioavailability and ...
J S Schilling, J J Inda


Mould growth on wood-based materials – a comparative study
2010 - IRG/WP 10-20455
Ten different wood-based materials - preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce - were tested for mould growth according to SP method 2899 during 42 days at 90% RH and 22°C. Even though the results must be interpreted carefully, they indicate significant differences in mould resistance between the materials tes...
P Johansson, J Jermer


The use of thermal desorption and pyrolysis combined with a semiconductor VOC detector for the on-site detection of preservative-treated wood
2010 - IRG/WP 10-20456
The purpose of this study was twofold; to identify possible marker molecules released from preservative-treated wood upon heat treatment and then develop a prototype detector for this marker. Two methods for heating the samples were used: Pyrolysis combined with Gas-Chromatography with IR-detection and Thermal Desorption combined with Gas-Chromatography with mass detection. A first prototype detec...
I Svensson, A Gonzalez, L Irusta, Mª J Fernandez-Berridi, O Munné


Mobility of Copper from MCQ in Shell-Treated Wood Exposed Above Ground
2010 - IRG/WP 10-30534
Most Canadian treated decking in service has been given just a thin shell of preservative treatment but it has still performed very well. This is because copper migrated into checks and prevented germination of basidiospores on the freshly exposed untreated wood. Unlike soluble copper systems, MCQ has its copper primarily in the form of small basic copper carbonate particles. For MCQ to be effecti...
R Stirling, P I Morris


Metal Migration from Douglas-fir Poles Treated with Ammoniacal Copper Zinc Arsenate According to Best Management Practices
2010 - IRG/WP 10-50272
The potential for migration of metal components from ammoniacal copper zinc arsenate treated (ACZA) poles was examined using pole sections treated using Best Management Practices. Copper and zinc levels were highest in runoff collected following the first rainfall events, then declined. Copper and zinc levels in runoff averaged 20 ppm and 5 pm respectively. The metal levels were then used to pr...
J J Morrell, C S Love, C Freitag


Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht


Gene expression analysis of a copper-tolerant brown rot fungus on MCQ-treated wood
2011 - IRG/WP 11-10748
Most brown rot fungi are copper-tolerant, which makes them difficult to control with copper-based wood preservatives like MCQ. To better understand what biological processes are regulated, we used our model species, Antrodia radiculosa, to examine expression of genes on MCQ-treated wood. Our hypothesis was genes that decreased copper bioavailability would be up-regulated early, when wood showed ...
J D Tang, A Perkins, S V Diehl


Comparative investigations between thermal and microwave assisted digestion as a novel tool for the chemical analysis of inorganic wood preservative components
2011 - IRG/WP 11-20461
The correct chemical impregnation of wood requires an internal as well as external quality control of the treated wood. The active is located in a solid matrix, therefore it is often difficult to analyse such material since most analytical procedures are based on liquid systems. Because of this quite a number of methods – like extraction or thermal digestion - were developed in order to transfer...
H Ahl, J Fromm, E Melcher


The potential for using CuO nanoparticles as a wood preservative
2011 - IRG/WP 11-30569
The potential for using nano-copper particles for wood protection was investigated using mini-agar slant and wood block tests with Gloeophyllum trabeum or Trametes versicolor. Nano-copper was more effective against G. trabeum than T. versicolor, although neither of these fungi would be considered copper tolerant. Nano-copper solutions were stable over a 17 week storage period, but precipitated w...
I S Weitz, K Knani, M Maoz, C Freitag, J J Morrell


Further Studies on the Distribution of Copper in Treated Wood Using an XRF Microscope Technique
2011 - IRG/WP 11-40549
There are two distinct forms of copper in aqueous copper based wood preservative systems that are currently used in the United States for treatment of southern pine lumber. These are systems using either soluble copper (typically amine based) or the more recent particulate or “micronized” copper as the primary biocide. Studies reported last year showed that there were distinct differences in...
A Zahora


Copper Migration from Micronized Copper Preservatives Treated Wood in soil contact:
2011 - IRG/WP 11-50280
Emerging formulations of preservatives made with micronized basic copper carbonates with azoles and/or quat to control copper tolerant fungi have been used to replace formulations containing soluble copper to reduce the leaching of copper and the corrosion of metal in contact with wood. This study proposes to use laboratory soil leaching test AWPA standard (E20-08) to estimate the amount of copper...
Lei Wang, D P Kamdem