IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 477 documents. Displaying 25 entries per page.


Chemical protection of historic timber structures: Results and future needs
2010 - IRG/WP 10-40487
The paper concentrates on the analysis of the effectiveness of chemical protection for timber structures in the Russian State Museums “Kizhi” (Karelia) and “Vitoslavlitsy” (Novgorod). The condition of historic timber was tested at the monuments treated with PCP, borax, potassium carbonate, boric acid, Pinotex chemicals in the 1970-80. Long-term analysis revealed that in many cases the...
M Kisternaya, V Kozlov


Study on the thickness swelling of mould-resistant chemical treated bamboo strand woven outdoor flooring
2010 - IRG/WP 10-40489
To prevent bamboo strand woven flooring from mould, several preservatives were chosen to treat bamboo strand before dipping into adhesives and pressing. The thickness swelling and mould resistant effect of the finished board were studied. Results showed that different preservatives had different influences on the thickness swelling of BSWF, and in order to reduce the thickness swelling of the fini...
Fangli Sun, Binfu Bao, Shenyuan Fu, Anliang Chen


Direct estimation of the durability of high-pressure steam modified wood by ESR-spectroscopy
2010 - IRG/WP 10-40508
Heat generated persistent free radicals have been detected by electron spin resonance measurement of thermally modified wood, prepared by high pressure superheated steam treatment. The specific density of these radicals have been correlated with the durability against basidiomycetes, as measured by the European standard EN113 test. In the lower range of specific radical densities, the found correl...
W Willems, A Tausch, H Militz


Chapter 10 - Preservation of muli bamboo
2007 - IRG/WP 07-10635-10
Environmentally and economically very important mulibamboo (Melocanna baccifera) grown in Bangladesh was fond to be easily pressure treatable with CCA-C at green and air dry conditions. The green and air-dried bamboo treated at same treating conditions and concentration showed 110 per cent (2.10-times) higher retention in air-dried bamboo than green one. Adequate lower retention equivalent t...
A K Lahiry


Theoretic discussion on the way and driving forces of moisture migration in wood during vacuum drying
2011 - IRG/WP 10-40538
Most of parameters in conventional drying cannot explain a lot of phenomena appeared in vacuum condition, so it is necessary to further explore the moisture migration way and driving forces in wood under vacuum condition. For the water movement channel in wood is very narrow, the characteristic of heat and mass transfer in wood is similar to that in microscale. This article applies theory of liqui...
Zhengbin He, Xueli Yao, Liqiong Chen, Songlin Yi


Multilayer hot-press drying and chemical modifying of poplar wood with urea-formaldehyde prepolymer
2011 - IRG/WP 10-40539
The objective of this study was to determine the technology of chemical modifying and multilayer hot-press drying on poplar wood. The chemicals were impregnated into cell lumen space by pulse-dipping machine to improve the dimension stability and mechanical property of timber. The timbers were compressed and dried by the multilayer hot-press drying to increase the density of timber. Results indica...
Guofeng Wu, Yifei Jiang, Sheng Yao, Junwen


Comparative investigations between thermal and microwave assisted digestion as a novel tool for the chemical analysis of inorganic wood preservative components
2011 - IRG/WP 11-20461
The correct chemical impregnation of wood requires an internal as well as external quality control of the treated wood. The active is located in a solid matrix, therefore it is often difficult to analyse such material since most analytical procedures are based on liquid systems. Because of this quite a number of methods – like extraction or thermal digestion - were developed in order to transfer...
H Ahl, J Fromm, E Melcher


Slice - Cut and Analyze Laser Microdissection (LMD): A method to produce sample material from modified wood for chemical quality analysis
2011 - IRG/WP 11-20478
Wood modification with its various systems is an established way to enhance a wood products’ service life in outdoor applications. Per definition, selected material properties are enhanced by means of modification without producing toxic substances or residues during service life and combustion afterwards. The systems of impregnation modification include a physical and often chemical alteration ...
K Zimmer, E Larnøy, A Treu, M Fongen


Influence of wood swelling agents on penetration and copper leaching of copper-ethanolamine based wood preservatives
2011 - IRG/WP 11-30556
Copper ethanolamine based preservatives are currently the most important solutions for impregnation of wood in ground contact in Europe. One of the issues related to those and similar water based solutions is insufficient penetration to refractory wood species like Norway spruce. In order to elucidate this issue, commercial copper ethanolamine based solution was supplemented with five different wo...
M Humar, N Thaler, B Lesar


Phytosanitary standards and the potential for acceptance of chemical treatments as a phytosanitary measure
2011 - IRG/WP 11-30558
Regulations governing international trade in forest products must balance the economic and social benefits of trade with the potential risks of transporting invasive species. The International Plant Protection Convention (IPPC) is an international agreement intended to manage this process. It develops international phytosanitary standards (ISPMs) that are recognised by the World Trade Organisation...
A Uzunovic, R Stirling, J J Morrell, P I Morris, C F Schauwecker


The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon


Effects of nano-silver on brittleness of heat-treated solid woods
2011 - IRG/WP 11-40572
The present study is aimed at the effect of heat-treatment of normal as well as nano-silver-impregnated Populus nigra, Populus deltoides, and Fagus orientalis on brittleness. Specimens were impregnated with 200 ppm water-based solution of nano-silver particles under 3 bars in a pressure vessel using empty-cell process. For heat treatment, both nano-silver-impregnated and normal specimens were kept...
H Reza Taghiyari, B Moradi Malek, A Karimi


Connecting fungal genomic variations to wood chemical composition: A way to understand the adaptation of wood decaying fungi
2012 - IRG/WP 12-10776
The development of new sequencing methods allows now exploring the detoxication systems of wood-decaying fungi. These systems, called xenome, are mainly composed of oxidative enzymes (phase I) and of conjugation enzymes (phase II). These enzymes belong to superfamilies, which are extended in the plant cell-wall interacting fungi. From different approaches coupling in particular comparative genomic...
E Gelhaye, Y Mathieu, E Meux, A Thuillier, M Mélanie


Micromorphological and chemical characteristics of waterlogged archaeological bamboos excavated from the Yellow Sea
2012 - IRG/WP 12-10785
Bamboos have widely used as documentation material in Far Eastern countries such China, Korea and Japan. In particular, bamboo slips as documentation material were extensively used even after the wide spread of paper in those countries. A large number of bamboo slips have been excavated from the shipwreck since 2009 in Korea. Understanding the cause of deterioration of ancient bamboos is crucial f...
Mi Young Cha, Yoon Soo Kim


Use of Variable Pressure Scanning Electron Microscopy for in situ Observation of Degradation of Wood Surfaces during Artificial Weathering
2012 - IRG/WP 12-20489
Variable pressure scanning electron microscopy (VPSEM) is capable of observing electrically non-conductive materials like wood without the need to render the surface conductive by applying a coating of gold, platinum or carbon. Hence, there is the possibility that VPSEM could be used to non-destructively follow the structural changes occurring at wood surfaces during weathering, because specimens ...
F Hatae, Y Kataoka, M Kiguchi, H Matsunaga, J Matsumura


Supercritical impregnation of wood with siloxane
2012 - IRG/WP 12-30595
This paper describes the effect of supercritical impregnation with siloxane on the water repellency of Scots pine (Pinus sylvestris) sapwood samples. Samples were impregnated with a low amount of siloxane dissolved in supercritical carbon dioxide using isopropanol as a co-solvent. Siloxane retention (i.e. weight percent gain (WPG)) of the treated samples was 1.3 % (w/w) as found by mass balance. T...
A Kjellow, F Imsgard, J Fernandes, O Henriksen, E Klaassen, R Wagner, J Delis


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


The Effects of Industrial-Scale Heat Treatment and Impregnation with Boron Compounds on Water Uptake and Tangential Swelling of Some Wood Species
2012 - IRG/WP 12-40599
This study evaluated the effects of boron impregnation and heat treatment on water uptake and tangential swelling of spruce (Picea orientalis), pine (Pinus nigra), beech (Fagus orientalis) and poplar (Populus deltoides) wood species. The samples (10 x 5 x 40 - tangential x radial x longitudinal cm) were impregnated with 4 % boric acid and 4 % borax according to the ASTM D-1413 standard method. Aft...
A Can, S Yildiz, Ü C Yildiz


Chemical Analysis of Hydrothermally Treated Beech Wood in Buffered Mediums
2012 - IRG/WP 12-40604
Hydrothermal treatment of beech wood in buffered mediums was carried out to study the effect of different mediums of heat treatment on crystallinity index of treated specimens due to degradation of carbohydrates. Different mediums (water, buffer5, 7 and 8) and temperatures (160 and 180 °C) were used. ATR spectra focusing on indexes of carbohydrates degradation obtained and analyzed. Results showe...
A Talaei, A Karimi


Scale-up of a chemical process for copper-based preservative-treated wood wastes recycling
2012 - IRG/WP 12-50286
In recent years, the development of appropriate wood waste disposal options has been encouraged by severe regulations and expensive fees associated with wastes landfilling or burning. An efficient and economically attractive leaching process was developed at laboratory scale (200 mL) for CCA-, ACQ- and CA-treated wood wastes recycling. This leaching process consisted of three leaching steps of 2 h...
L Coudert, L Gastonguay, J F Blais, G Mercier, P Cooper, P Morris, A Janin, N Reynier


Seed oil and defatted cake proximate composition of non timber product Annona squamosa (Annonaceae) grown in Benin
2012 - IRG/WP 12-30607
Annona squamosa L. is a small tree which grows wild in many places in the tropical regions, locally called “xwingle” in Benin. Its produces edible fruits, typically globular or heart-shaped which are highly appreciated and the seeds are not used. In the course of work about identifying new oil sources from a large number of oil bearing seeds grown in Benin, we report here on the chemical compo...
T S Djenontin, J Dangou, P Lozano, D Pioch, D C K Sohounhloue


Cell wall properties of softwood deteriorated by fungi: combined chemical analyses, FT-IR spectroscopy, nanoindentation and micromechanical modelling
2013 - IRG/WP 13-20527
Mechanical properties of wood are determined by its inherent hierarchical microstructure, starting at the nanometer scale, where the elementary components cellulose, hemicelluloses, and lignin build up the wood cell wall material. Fungi cause degradation and decomposition of these components and, thus, alter the mechanical properties of wood. The aim of this study is to gain new insight into these...
L Wagner, T K Bader, K de Borst, T Ters, K Fackler


The effects of impregnation with secondary metabolite extracted from Ipe on durability of Japanese cedar and beech wood
2013 - IRG/WP 13-30618
Ipe wood is known for its high durability; it has been widely used in exterior structures that are exposed to the weather. In this paper, to increase the durability of less durable wood, Japanese cedar and beech specimens were impregnated with a secondary metabolite from Ipe. In a previous study, secondary metabolites extracted by a Soxhlet extraction method showed antifungal properties. Therefore...
T Iida, R Konuma, K Kawarada


Hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment
2013 - IRG/WP 13-40623
The hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment was investigated by testing the water uptake, equilibrium moisture content (EMC) at various relative humidity levels, and contact angle of the poplar wood surface. The results showed that: (1) At the first moment, the heat treatment at temperatures lower than 160 ℃ did not reduce the water uptake be...
Weiyue Xu Yuan Zhu, Jinzhen Cao


Effect of the nature of the inert atmosphere used during thermal treatment on chemical composition, decay durability and mechanical properties of wood
2013 - IRG/WP 13-40625
Wood heat treatment is an attractive alternative to improve decay resistance of low natural durability wood species. Nowadays, several types of thermal treatments of wood exist. These treatments differ mainly by the nature of the inert atmosphere used to avoid wood combustion which may correspond to: nitrogen, vacuum, steam or oil. Decay resistances as well as mechanical properties are strongly co...
K Candelier, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Previous Page | Next Page