Preservative treatment and field test monitoring of spruce pole stock: Pressure and diffusible chemical treatments
1990 - IRG/WP 3605
One hundred and forty four spruce (test species) and southern yellow pine (reference species) poles were variously treated by center boring, incising, or kerfing, followed by pressure treatment with CCA and/or diffusible preservatives. The diffusible preservatives included NaF/creosote, borax and ammonium bifluoride. The poles were set at a test site and evaluated for preservative distribution and...
B Goodell, A J Pendlebury


Early detection of brown-rot decay in southern yellow pine using immunodiagnostic procedures
1990 - IRG/WP 2356
Immunodiagnostic procedures have been used to detect incipient decay of southern yellow pine by six common brown-rot fungi. Rabbit polyclonal antibodies were raised to liquid culture fractions of the six fungi. The antibodies, after preadsorption to sawdust, were tested in particle agglutination assays, immuno-dot blot, and ELISA for their·ability to detect the decay organisms when they were grow...
C A Clausen, F Green III, T L Highley


Comparing the resistance of a number of lesser known species of tropical hardwoods to the marine borer Limnoria using a short term laboratory assay
2003 - IRG/WP 03-10500
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, durability was assessed by measuring the production of faecal pellets by ...
L M S Borges, S M Cragg, J R Williams


Relationship of wood durability and extractives
2003 - IRG/WP 03-10493
The durability of the following five wood species, Zelkova carpinifolia, Ulmus glabra, Pterocarya fraxinifolia, Carpinius betulus and Acer laetum, were studied. Wood blocks were exposed to Coriolus versicolor under laboratory conditions according to DIN 52176 standard. After 16 weeks incubation the heart wood of Z carpinifolia showed 2,19 % weight loss, U glabra 41,69 %, C betulus 45,64 %, A laetu...
S M Kazemi


Detection of a brown-rot fungus using serological assays
1986 - IRG/WP 1305
Polyclonal antisera produced to Poria placenta (Fr.) Cooke were used in two tests to qualitatively assay for the fungus. Fungal hyphae were fixed to slides and fluorescent antibody (FA) techniques used to visualize the hyphae under the microscope. Fluorescence of non-Poria fungi, when present, could be reduced but not eliminated by cross-absorbing the sera with these fungi. The antisera was also u...
B Goodell, J Jellison


A laboratory technique to measure the performance of preservative treated hardwoods in ground contact
1982 - IRG/WP 2172
A laboratory technique to measure the performance of preservative treated timber in ground contact is described. It uses partially sealed blocks of timber which are treated, leached and sawn into small stakelets for soil exposure in a fungal cellar. Performance is monitored by the loss of static bending strength with time, and a simple apparatus for measuring the deflection of a stakelet under a l...
E F Baines


A comparison of effectiveness of three waterborne preservatives against decay fungi in underground mines- An appraisal
2005 - IRG/WP 05-30366
To understand the effectiveness of waterborne preservatives and to explore the behaviour of roof supporting poles after pressure treatment, an experiment was conducted and thorough investigation was carried out during the last decade in the underground mines. Prior to commencement of the experiment, a survey was conducted at different depths in underground mines and collected decayed wood samples ...
P Narayanappa


Remedial ground-line treatment of CCA poles in service. A final report after 60 months' testing
1989 - IRG/WP 3534
Remedial treatment of CCA treated utility poles of Pinus sylvestris with incipient decay was carried out in 1983 and the results of chemical and microbiological analyses 6 months after treatment were reported in Document No: IRG/WP/3388 while microbiological studies 12 and 28 months after treatment as well as chemical analyses of poles treated with boron rods or boric acid paste 28 months after tr...
B Henningsson, H Friis-Hansen, A Käärik, M-L Edlund


Inadequacies in preservative retention and formulation as contributory causes of premature failure of CCA-treated vineyard posts
1984 - IRG/WP 3280
Analyses of severely decayed or failed vineyard posts and examination of stake test data on effectiveness of copper-chrome-arsenate (CCA) preservatives have suggested two contributory causes of premature failure of vineyard posts: 1. Preservative retentions in posts are such that after 15 years' exposure some decay is inevitable. 2. The high arsenic, low chrome formulations with which the...
M E Hedley


The field performance of CCA-C treated sawn refractory softwoods from North America
1997 - IRG/WP 97-40085
Approximately 15% of the total volume of wood treated in the United States consists of difficult to treat softwoods known as "refractory softwoods". The long term positive performance record of CCA treated sawn material is based upon the testing of yellow pine sapwood stakes with only limited field data available for sawn refractory softwoods. As a result, the existing North American wood preserva...
M J Richards, W S McNamara


Antifungal properties of metabolites produced by Trichoderma isolates from sawdust media of edible fungi against wood decay fungi
1994 - IRG/WP 94-10051
Trichoderma isolated from a sawdust medium of Pholiota nameko produced filtrates which had antifungal activities to four wood decay fungi tested on the agar plates. Filtrates produced from another isolate, from a sawdust medium of Lentinus edodes, had antifungal activities only to the white rot fungi, Coriolus versicolor and Pycnoporus coccineus. These results did not agree with those from earlier...
S Doi, M Mori


Resistance of various wood species against decay by Coniophora cerebella (Pers) Duby and Lenzites trabea (Pers) Bres
1976 - IRG/WP 142
Both fungi, Coniophora cerebella and Lenzites trabea, are important destroyers of timber. Coniophora often occurs inside buildings and Lenzites trabea has been observed on southern facades of buildings, on balconies and window frames. In most instances that we investigated coniferous timber had been decayed. But both species are known to attack also various hardwoods. For this reason tests similar...
O Wälchli


Biostatic film as a primary treatment against pole failure in soil
1995 - IRG/WP 95-40053
Field liners of low density polyethylene (LDPE) film applied as primary treatment of soil-contact surfaces of creosote-treated poles prevented their detoxification and premature failure by establishing hurdles against microbiological colonisation. These hurdles include low water activity, low oxygen tension and nutrient limitations. Moreover, under conditions of high soil moisture, field trials sh...
A A W Baecker, M Behr


Premature failure of treated timber in wharfs in Papua New Guinea, attributed to defects in design
1991 - IRG/WP 4158
The performance of timber in wharfs in Papua New Guinea has been monitored for a number of years. Premature failure of wharf structures was found in many cases to be due to defects in design rather than ineffective preservative treatment. Above-water timbers were found to be prone to severe checking followed by decay. Protection for the end grain of pile tops and the limiting of radial checking in...
S M Cragg


Application of a novel strength evaluation technique during screening of wood preservatives
1986 - IRG/WP 2262
The effectiveness of CCA and ACA in treated aspen mini stakes tested using a novel bag procedure, with unsterile soil fortified with Chaetomium globosum and Ceratocystis albida, is reported. Good agreement between toxic limits determined using the standard weight loss procedure, and those determined by the strength technique were found, with some indication that the strength loss method is more se...
J N R Ruddick


Distribution of copper/chrome/boron preservative in light red meranti (Shorea leprosula) before and after exposure test for 72 months
1995 - IRG/WP 95-20073
Copper/chrome/boron (CCB) preservative at 6% w/w was impregnated into light red meranti (Shorea leprosula) by full cell process. The quantitative analysis for copper, chrome and boron contents in treated wood samples was carried out by Inductive Couple Plasma (ICP). Electron Probe Microanalyser (EPMA) was used to monitor the distribution of copper, chrome and boron in the various treated wood tiss...
S Salamah, S Ani


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 6: Report of third inspection (24 months) in Australia
1980 - IRG/WP 456
This report presents the results of the third inspection of the IRG/COIPM International Marine Test specimens installed at the Goat Island Marine Biological Station of the Maritime Services Board of New South Wales, in Sydney Harbour. The inspection was completed on 5th December, 1979, after 24 months exposure. As on previous occasions, this inspection was carried out in conformity with the provis...
J Beesley


Natural resistance of timbers to marine borer attack. A laboratory test with Limnoria tripunctata
1977 - IRG/WP 430
Attack of the timber specimens was much less severe in the laboratory than in some marine localities. This is not surprising. One reason is certainly that wood-boring molluscs (Teredinidae and Pholodidae) which were missing in the laboratory are the most important wood-destroying organisms in the open sea. Another reason is that it is not possible to offer the gribbles optimal environmental condit...
H Kühne


Laboratory evaluation of potential antisapstain treatments for Pinus radiata
1983 - IRG/WP 3237
Twelve formulations were tested in the laboratory using a 'mini' board test for effectiveness on Pinus radiata (D. Don) against sapstain, mould and decay fungi. Three formulations, sodium pentachlorophenoxide (NaPCP) plus borax, Haipen 50 WP, and Mitrol 375, are used commercially in New Zealand. Busan 1009 (0.5% product), IWD Product A (0.2% ai), IWD Product B (0.3% ai), Fennotox...
J A Drysdale


A field method for determining the above-ground resistance of wood and wood products to attack by subterranean termite
1994 - IRG/WP 94-20035
A method for determining the above-ground resistance of wood and wood products to subterranean termites in the field is described. Termites are aggregated in 20-litre steel drums, each containing a highly susceptible timber substrate. At the centre of each drum, specimens of the test material under evaluation are sandwiched, using circular sections of wire mesh, between two layers of the substrate...
J W Creffield


Evaluation of bacteria for biological control of wood decay
1990 - IRG/WP 1426
Laboratory soil-block and agar-block tests were carried out to evaluate the efficacy of bacteria as biological control agents against 5 brown-rot and 3 white-rot fungi. Pretreatment of Southern pine and sweetgum with a bacterial solution prevented decay in agar-block tests. However, the bacteria were generally ineffective in preventing decay in Southern pine, Douglas-fir, sweetgum and yellow popla...
R Benko, T L Highley


Evaluation of wood durability by laboratory test - A new equation to predict wood durability
2001 - IRG/WP 01-20230
To estimate the wood durability in a short term, periodical weight determination was carried out in a laboratory test. This test provided the results comparable to those of the field test and the fungus cellar test, but it required much more jobs in comparison to the usual accelerated laboratory test. To save the time and jobbing for this method, a new equation was devised from simple two assumpti...
I Momohara, K Yamamoto


Protection of southern pine using N,N-Napthaloylhydroxylamine: Field tests, soft-rot cellars and aquatic bioassay leach testing
1999 - IRG/WP 99-30204
Recent environmental restrictions are limiting the use of broad-spectrum biocides for wood preservation. There is an urgent need for new, sharply targeted, environmentally benign wood preservatives. N'N-Napthaloylhydroxylamine (NHA), a water-soluble calcium-precipitating agent, has been shown to inhibit decay by brown-rot and white-rot fungi in soil-block tests and prevent damage by Easte...
D M Crawford, F Green III


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 14: Report of fifth inspection (48 months) in Australia
1982 - IRG/WP 484
This report presents the results of the fifth inspection of the IRG/ COIPM Internatlonal Marine Test specimens installed in Sydney Harbour in December, 1977. This inspection took place on 9th December, 1981, just 48 months after the specimens were installed. Earlier reports have contained full details of the treatment and installation of the specimens as well as results of all previous inspections...
J Beesley


Quantification of wood decay effects by HPLC analysis
1992 - IRG/WP 92-1576
The present work quantified the effects of the white rot basidiomycetes Coriolus versicolor and Phanaerochaete chrysosporium, and also those of the brown rot fungi Coniophora puteana and Lentinus lepideus, on Pinus patula and Eucalyptus grandis. Wood colonisation was quantified by Kjeldahl nitrogen determinations converted to biomass assays, and degradation was quantified by weight losses produced...
V Singh, M Tarin, G D Shelver, A A W Baecker