On-site test for indicative determination of leaching of components of preservatives from treated timber
1993 - IRG/WP 93-50001-12
In the late eighties the environmental concern about treated timber increased and it is still a hot issue in the Netherlands. From the environmental point of view three phases in the timbers life cycle can be distinguished: - the production phase - the service life - the waste phase. In the Netherlands at this moment much emphasis is laid on the production phase. In 1992 this has led to a new legi...
W J Homan, H Militz


Biochemical relationships between biodegradation of cellulose and formation of oxalic acid in brown-rot wood decay
1991 - IRG/WP 1472
Non-enzymic hydrolysis of cellulose with low concentrations of oxalic acid was examined. The incubation of pine wood pulp with 1% oxalic acid (pH 1.3) at 35°C for 4 weeks reduced the original viscosity to 60%. Reducing sugars were liberated from various cellulosic samples by the oxalic acid treatment. However, crystallinities of cellulose in those samples did not change before and after the treat...
M Shimada, Y Akamatsu, A Ohta, M Takahashi


Accelerated decay tests on DNBP-treated Pinus patula and Eucalyptus grandis
1987 - IRG/WP 3441
Blocks (10 x 10 x 5 mm³) of Pinus patula and Eucalyptus grandis were impregnated to 0, 1.5, 3.0 and 4.5 kg/m³ 2-sec-butyl, 4, 6 dinitrophenol (DNBP). They were monitored microscopically and for weight losses over 16 weeks against monocultures of Coriolus versicolor and Coniophora puteana. Treated ministakes (10 x 10 x 100 mm³) and blocks in soil contact were similarly monitored to determine wei...
L D Abraham, A A W Baecker


Biocidal screening method of wood extractives by a direct use of cellulose TLC plate
2001 - IRG/WP 01-20226
Most of the methods to evaluate the biological durability of woods have focused on decay fungi and termite as deteriorating organisms and it is well known that one of the most important factors affecting the biological characteristics of wood is extractives. Bioassays for evaluating the biological activities of wood extractives have been mainly conducted with treated filter papers for termites or ...
R Yusiasih, T Yoshimura, T Umezawa, Y Imamura


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


A marine borer test with water-borne preservatives
1980 - IRG/WP 452
The use of preservative treated timber in sea-water where marine borers are active is of great economic importance, since untreated wood immediately will be damaged. Vacuum/pressure treated timber has been tested in several marine exposure trials on the Swedish west coast since the 1930s (Hager 1941, Hultman 1949, Sandstrom 1951, Nylinder-Norman et al. 1974). Since new interesting materials or pre...
B Henningsson, E Norman


Analysis of D-glucose metabolism of wood decay fungi using 13C-NMR and 13C-labeled substrates
2003 - IRG/WP 03-10475
D-Glucose metabolism is thought to be important during wood decay by fungi, not only for anabolic and catabolic purposes of central metabolism, but also as a potential source of peroxide required by extracellular peroxidases. There has been some confusion in the literature as to whether this peroxide-generating activity is of the glucose 1-oxidase or pyranose 2-oxidase (glucose 2-oxidase) type wi...
T H de Koker, M D Mozuch, P J Kersten


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Preservation of robinia wood (Robinia pseudoacacia L.) stakes by vintners
1982 - IRG/WP 3194
This work discusses decay resistance of robinia wood to fungi Trametes versicolor (L.ex Fr.) Pil. and Coniophora puteana (Schum. ex Fr.) Karst., and also the possibility of influencing its resistance by means of chemical protection. The results showed that natural resistance of robinia wood to these two different agents of wood decay is not the same. It is much less resistant to the fungus Conioph...
R Benko


The natural durability story
1997 - IRG/WP 97-20119
Wood species with superior natural durability were in use since the beginning of timber utilisation. Their importance decreased with increasing industrial timber impregnation. In recent time, however, they gained worldwide new interest due to environmental problems involved with treated timber. In Europe a special Standard (EN 350) has been published and a multinational research project on testing...
H Willeitner, R-D Peek


A technique for assessing the preventive efficacy against decay fungi of preservative treatments applied to wood
1988 - IRG/WP 2309
A method is described in which test blocks with envelope preservative treatments can be challenged by selected test fungi previously established on an untreated feeder block. The progress of the test fungus through the treated zone is monitored using novel baits or sensors inserted in holes drilled into blocks to within predetermined distances of the face being challenged. Preliminary results show...
J K Carey, A F Bravery


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 1: Laboratory screening tests using a filter paper technique
1977 - IRG/WP 290
Thirty-one miscellaneous formulations have been screened using a filter paper assay technique, for their efficacy in controlling the growth of Chaetomium globosum, Cephalosporium acremonium, and a mixed inoculum of finely ground soft-rotted wood obtained from preservative treated transmission poles. The formulations consisted of various organic compounds and inorganic preparations made from differ...
H Greaves


Remedial ground-line treatment of CCA poles in service. Results of chemical and microbiological analyses 6 months after treatment
1986 - IRG/WP 3388
CCA-treated poles in service with incipient internal soft rot were remedially treated by inserting borate rods, brushing with a boron/glycol solution and injecting boric acid paste, copper/creosote paste or a commercial product (DFCK paste). The spread of active chemicals in the treated zone as well as the change in microflora have been studied with time. After six months chemicals had spread to m...
B Henningsson, H Friis-Hansen, A Käärik, M-L Edlund


Statistical evaluation of 'micro-bending' samples for classification of wood attacking fungi
1992 - IRG/WP 92-1544
Micro-specimens from both hardwood and softwood were exposed to selected species of field isolated fungi. The strength reduction and weight loss caused by these fungi were determined. A statistical procedure was then developed to classify the fungi into brown-, white-rot, or non-decay fungal categories based on these data. The procedure reveals the extent of hazard a fungus poses to wood members. ...
B Goodell, Jing Liu, A Homola, J Jellison, J Shottafer


Durability of five wood species against Coriolus versicolor
1992 - IRG/WP 92-1578
The durability of following five wood species Zelkova carpinifolia, Ulmus glabra, Carpinus betulus, Acer trauvetteri and Pterocarya fraxinifolia were studied against Coriolus versicolor under laboratory conditions according to DIN 52176 standards. Zelkova caprinifolia shows a reduction in weight of 2.19%, Ulmus glabra 41.69%, Carpinus betulus 45.64%, Acer trauvetteri 53.05%, and Pterocarya fraxini...
S M Kazemi


Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown


Alternatives to CCA for ground contact protection of timber: a perspective from UK on performance and service life expectations
2002 - IRG/WP 02-30289
The proposed amendment to the European Union's Marketing and Use Directive (1976/769/EEC) in respect of arsenic in CCA wood preservatives seeks to restrict the use of CCA across the European Union. CCA is an extremely important wood preservative in the UK from the manufacturing of the product to the extent of use of CCA-treated timber. Based on our experience and judgement on the use of ...
E D Suttie, A F Bravery, T B Dearling


An Australian test of wood preservatives. Part 1: Preservatives, principles and practices
1978 - IRG/WP 2123
Between November, 1963, and July, 1964, a graveyard test of some 6000 preservative-treated stakes was installed at 8 sites equally distributed between Papua New Guinea in the tropics, through Queensland and New South Wales to Victoria. More than 40 different preservatives and preservative mixtures, mostly at several different levels of retention, were used to impregnate sawn specimens of Pinus rad...
J Beesley


SEM investigation of the production of extracellular mucilaginous material (ECM) by some wood inhabiting and wood decay fungi when grown on inert surfaces
1997 - IRG/WP 97-10194
A range of wood inhabiting and wood decay fungi have been studied for their production of extracellular mucilage when grown on inert surfaces, for comparison with their growth on wood. The species tested were: Coniophora puteana, Coriolus versicolor, Chaetomium globosum, Trichoderma harzianum, Ceratocystis coerulescens, Ophiostoma piceae, Mucor sp. and Penicillium sp. They were grown on plastic me...
A R Abu, R J Murphy, D J Dickinson


The practice of using concrete on wood piling for marine use in Thailand
1982 - IRG/WP 492
The practice of using concrete on wooden poles has been carried on in Thailand for a long time in pile-houses and pier constructions which have been situated in, or partly in the sea. In such instances, the hewed round and/or square-sawn heartwood poles of naturally durable timber species have been coated with concrete of about 5 to 10 cm or more in thickness, and to about 100 cm above the highest...
B Anuwongse


Oxalic acid quantification, oxaloacetase assay and ESI localization of P, C, and Fe from the brown rot fungus Postia placenta
1994 - IRG/WP 94-10063
The mechanism by which brown-rot fungi initiate depolymerization of holocellulose in wood remains unknown. Recently, oxalic acid (OA) has received considerable attention in cellulose breakdown by brown-rot fungi. The OA could serve as a proton donor for hydrolytic or an electron donor for oxidative (Fenton's reaction-H2O2/Fe2+) cleavages of cellulose. The acid may originate via oxaloaceta...
C R Jordan, W V Dashek, T L Highley


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 21: Report of eighth inspection (7 years) in Australia
1985 - IRG/WP 4119
This report tabulates the seven year (86 month) inspection results, obtained on 28 Fabruary l985, of the IRG/COIPM International Marine Test at Goat Island, Australia. This test was installed in December 1977. The results are given in Tables 1-6. Table 7 lists the number of marine borers identified from blocks (2 cm and 6 cm long respectively) cut from the ends of specimens removed at the previous...
L J Cookson, J E Barnacle


Chlorothalonil: A new ground contact wood preservative
1992 - IRG/WP 92-3712
Extensive investigations have been conducted in recent years on the performance of chlorothalonil (tetrachloroisophthalonitrile) as a ground contact wood preservative. Efficacy information is presented on a soil block test with 11 Basidiomycetes, a fungus cellar evaluation, above-ground field testing against termites in Australia and Hawaii, and ground-contact field stakes installed in Florida (9 ...
P E Laks, T L Woods


Limiting Conditions for Decay in Wood Systems
2002 - IRG/WP 02-10421
Hygrothermal models can predict temperature and moisture conditions in wall components subjected to real weather data, but specific data and a fundamental understanding of how temperature and wood moisture content dictate the progression of decay under these conditions is required for modellers to predict consequences of decay on building performance. It is well understood that wood will decay abo...
P I Morris, J E Winandy


Proposed model for the penetration and decay of wood by the hyphal sheath of the brown-rot fungus Postia placenta
1989 - IRG/WP 1391
Scanning electron microscopy (SEM) of Pinus sp. decayed by the brown-rot fungus Postia placenta confirmed the existence of extracellular membranous structures previously described by transmission electron microscopy (TEM). These structures appear to be an integral part of the hyphal sheath and assume a variety of forms including lamellar sheets, fibrils, and vesicles. These structures were observe...
F Green III, M J Larsen, L L Murmanis, T L Highley


Previous Page | Next Page