IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3359 documents. Displaying 25 entries per page.


Bioprocessing preservative-treated waste wood
2000 - IRG/WP 00-50145
Disposal of preservative-treated waste wood is a growing problem worldwide. Bioprocessing the treated wood offers one approach to waste management under certain conditions. One goal is to use wood decay fungi to reduce the volume of waste with an easily managed system in a cost-effective manner. Wood decay fungi were obtained from culture collections in the Mycology Center and Biodeterioration res...
B Illman, V W Yang, L Ferge


Moisture uptake and volumetric swelling as probable factors also affecting leaching in CCA-treated wood. A preliminary study of treated Eucalyptus saligna sapwood
2003 - IRG/WP 03-30318 IRG/WP 03-30318
A number of factors affecting leaching of CCA from treated wood have been variously investigated and discussed. However, the possible effects of moisture movement in treated timbers on leaching have not received attention yet. The present study examines and compares moisture uptake and volumetric swelling in CCA-treated and untreated sapwood of Eucalyptus saligna, and tries to establish a correl...
R Venkatasamy


Initial results and observations of a model system to assess the efficacy and environmetal impact of preservative treated wood
1993 - IRG/WP 93-50001-02
The development of a closed model system for the laboratory assessment of the efficacy and environmental impact of a chromated fluoride remedial treatment for creosoted distribution poles has been described (IRG/WP/2395-92). The model consists of a precipitation apparatus above a treated pole section positioned in a soil profile from which leachate was collected via a series of simulated field dra...
D C R Sinclair, G M Smith, A Bruce, H J Staines


The effect of hemicellulose degradation on the mechanical properties of wood during brown rot decay
2001 - IRG/WP 01-20219
Incipient decay of wood by brown rot fungi causes measurable strength losses in wood before measurable weight loss occurs. Previous studies have shown that the high levels of strength loss that occur during incipient brown rot decay may be related to loss in hemicellulose. This paper investigates the effect of decay on hemicellulose composition and the relationship to the mechanical properties of ...
S F Curling, C A Clausen, J E Winandy


Chemical and biological studies of organotin treated and painted wood stakes after outdoor exposure
1987 - IRG/WP 3419
Organotin based wood preservatives containing tributyltin oxide (TBTO) or tributyltin naphthenate (TBTN) are used in Sweden mainly for double-vacuum treatments of window joinery of Pinus sylvestris. After impregnation the joinery is painted or stained in different colours. To evaluate this effect (different colours on the degree of degradation of TBTO and TBTN, effected by different temperatures i...
M-L Edlund, B Henningsson


Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel


The new National Directive on wood preservation in the Netherlands
1998 - IRG/WP 98-50101-03
In the Netherlands the major part of treated timber is sold under the KOMO-certificate. The National Directive for vacuum pressure treated timber on which certification is based, is currently being revised. The new National Directive will contain a code of good practice including maximum leaching figures. It incorporates quality requirements for treated timber, existing legislative requirements an...
W J Homan, J K B Kwisthout, J Dubelaar


Evaluation of the corrosivity of the treated wood - Laboratory vs field test methodologies
2000 - IRG/WP 00-20211
The corrosivity of treated wood to fasteners has been evaluated using laboratory test procedures, including AWPA Standard E12-94. The standard method was modified in order to allow detailed study of commercial metal fasteners in terms of sample types, installation configuration and exposure conditions. Parallel field tests were also performed. The experimental results generated from these tests su...
L Jin, A F Preston


Natural exposure weathering tests: Their role in the assessment of wood preservative efficacy
1993 - IRG/WP 93-20006
Previous work has demonstrated the potential and usefulness of natural ageing procedures in e evaluation of wood preservative efficacy. This results from the combination of physico-chemical influences and microbiological interactions with both substrate and wood preservative. In this paper, results are presented for a range of biocide types. Discussions are centred on the value of natural exposure...
G R Williams, J Brown


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


Correlation between changes in colour and chemical composition during photo-degradation of wood surfaces
2005 - IRG/WP 05-40301
Changes in colour of wood (yellowing) during photo degradation or weathering reflect chemical changes in wood. Therefore, the relationship between changes in chemical composition and CIELAB colour parameters is very important to characterize photodegradation of lignocellulosic surfaces. In this study, the changes in chemical composition and yellowing due to photo-degradation was studied by expos...
K K Pandey


Evaluating the natural durability of native and tropical wood species against Reticulitermes flavip
2004 - IRG/WP 04-10539
Environmental pressures to eliminate arsenate from wood preservatives has resulted in voluntary removal of CCA for residential applications in the United States. A new generation of copper organic preservatives has been formulated to replace CCA for decking and in-ground applications but there is no guarantee that these preservatives represent a permanent solution to all related problems. There...
R A Arango, F Green III, K Hintz, R B Miller


Wood-based composites exposed to fungal degradation: Laboratory results
2001 - IRG/WP 01-40215
Oriented strandboard (OSB) and laminated veneer lumber (LVL) are widely used as residential construction materials. The durability of OSB and LVL against biological degradation has not been studied comprehensively. The objective of this research was to investigate the durability of OSB and LVL when exposed to wood decay fungi. Fourteen brown-rot and eight white-rot wood decay fungi were screened f...
V W Yang, B Illman, L A Ferge, R J Ross


Dimension of lysimeters and the evaluation of the migration of wood preservative components in soil
1996 - IRG/WP 96-50065
In the past, investigations concerning the migration behaviour of wood preservatives were made to a minor extent and no uniform methods of test exist. The migration behaviour of CFB was determined using 5 lysimeters of different dimension. The results of the migration and distribution of the anions in the soil showed considerable differences between both ions. Approximately the whole quantity of c...
E Melcher, R-D Peek


Performance of CCA wood preservative and CCA treated wooden materials (pole, anchor log, cross-arm etc) with special reference to Bangladesh (Series 1)
2005 - IRG/WP 05-40318
Wood is an important renewable natural resources produced by plants which is without question oldest and versatile construction material. It is composed of cellulose, hemicelluloses and lignin. Cellulose and hemicelluloses accounts for about two-thirds of the dry weight of the wood which perform the major structural role. Lignin is the remaining one-third of the wood which holds the cellulose and ...
G N M Ilias


The fungal degradation of quaternary ammonium compounds in wood
1998 - IRG/WP 98-10263
This work focuses on the biodegradation of didecyldimethylammonium chloride (DDAC) by the mould fungus Gliocladium roseum within a woody matrix. Three sawdust types, distinguished by their treatment and amount of DDAC retained, were inoculated with the fungus and their DDAC loss was measured over 11 weeks. The rates of degradation varied depending on the sawdust; however, a significant loss of DDA...
J W Dubois, J N R Ruddick


Biological detoxification processes - A check list for assessments
1998 - IRG/WP 98-50120
The number of scientific publications on the biological purification of preservative treated wood implies that the biological treatment of wood wastes becomes more and more important. But an information about a successful industrial application is almost missing in all cases. Therefore the applicability of the proposed purification processes is often uncertain. The feasability of such a biological...
H Leithoff, R-D Peek


The degradation of wood surfaces by water
1984 - IRG/WP 3289
Thin radial/longitudinal sections (~100 µ) of Scots Pine (Pinus sylvestris) and lime (Tilia vulgaris), were exposed to deionised water over the temperature range 25-65°C. Losses in wet tensile strength and toughness occurred rapidly at temperatures from about 50°C upwards. After about 2 months' exposure pine lost some 10-30% of its tensile strength and 20-60% of its toughness. For lime...
W B Banks, P D Evans


Soft rot decay of Belian (Eusideroxylon zwageri) wood
1995 - IRG/WP 95-10119
The heartwood of Belian (Eusideroxylon zwageri), an East Malaysian timber species, is naturally durable due to its certain unique anatomical features and high content of extractives. The timber can tolerate years of exposure to hazardous conditions in ground contact and other situations without any significant loss in its strength. A few Belian transmission poles sampled from one locality in Saraw...
A H H Wong, A P Singh


Determination of total fluoride and boron in preservative-treated wood fluoride by ion selective electrode without steam distillation, and boron colorimetrically using azornethine-h
1998 - IRG/WP 98-20135
An analytical method was developed to determine total fluoride and boron in wood treated with aqueous or solid diffusing fluoride or borate-fluoride formulations. Ground wood was mixed with 30% sodium hydroxide solution and oven-dried for 2 hours before furnacing at 600° C for 1 hour. The cool fused product was dissolved in hot water, transferred to a plastic beaker and neutralised. Fluoride was ...
P A Collins, M J Kennedy


Will political initiatives stop the use of preservative-treated wood in Sweden?
1990 - IRG/WP 3578
The Swedish government has initiated several investigations on how to reduce the use of different chemicals. Among these chemicals are creosote, arsenic, chromium and organotin. A special investigation was carried out concerning wood preservatives resulting in different proposals on how to reduce the use of preservatives and preservative treated wood. The most important proposals were an "environm...
J Jermer, M-L Edlund


In situ timber treatments by spraying. Distribution of preservative in wood
1991 - IRG/WP 3678
This study was carried out in order to make the Pest Control Operators able to achieve correct treatments and enhance their efficacy. It was carried out in two steps: 1) in laboratory, to learn the influence of various parameters like spraying pressure, use of repeated applications, distance from nozzle to wood; 2) in situ on roof timber of five buildings. In this case, the applications of the pre...
C Defoin, G Dupont, M Lamour, H Sageot, M-M Serment


Technical viability of deltamethrin as a pre-treatment wood preservative
1993 - IRG/WP 93-30012
This paper presents the results of tests conducted on freshly-cut logs and lumber during the seasoning period to verify the effectiveness of Deltamethrin on insect control. The tests were carried out in Quedas do Iguaçú, Paraná (southern region of Brazil) and Breves, Pará (northern region of Brazil) during the-dry and rainy seasons, and used different species of wood and insecticide/fungicide ...
A M F Oliveira, S Milano, J L A Bahia, F Teleginski


Distinguishing isolates of Aureobasidium on the basis of their ability to utilise lignin breakdown products as a sole carbon source
1996 - IRG/WP 96-10151
Wild isolates of Aureobasidium were obtained by dilution plating from a ca 20 year old painted pine window frame. Four isolates were obtained from the paint/wood interface region and four isolated from regions deep in the wood. The isolates were then used to inoculate liquid cultures containing ferulic acid, a lignin breakdown product, present as the sole carbon source. Ability of the isolates to ...
M W Schoeman, D J Dickinson


Previous Page | Next Page