Some aspects of laboratory and field testing methods of antitermite wood preservatives
1973 - IRG/WP 235
Various methods for laboratory testing of antitermite activity of wood preservatives are described. The results of simultaneous tests of three water-borne preservatives, according to the various methods are discussed, and comparison is made with results of field tests on the same three preservatives, showing a fairly good accordance between laboratory results and field results....
M Fougerousse


Short-term field test method with accelerated infection of Basidiomycetes in wood
1981 - IRG/WP 2155
In the ŠIPAD - IRC Wood Protection Laboratory an attempt has been made to develop a simple short-term method for field testing out-of-ground contact wood using accelerated infections with Basidiomycetes. This method makes it possible to obtain a preliminary assessment of a preservative's quality and to estimate the possibility of achieving promising results in more expensive long-term te...
N Vidovic


Vertical distribution of fouling and wood-boring organisms in the Trondheimsfjord (Western Norway)
1981 - IRG/WP 467
Results of a detailed study on the vertical distribution of fouling and wood-boring organisms of Trondheimsfjord at an interval of 3 m from intertidal level to a depth of 30 m, has been presented, based on data collected from two series of panels, exposed from 15 March 1977 to 15 July 1977 (Series I) and from 22 July 1977 to 13 March 1978 (Series II). The intensity of fouling generally decreased w...
L N Santhakumaran


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


Assessing the risks from the use of wood preservatives
2001 - IRG/WP 01-50166-07
PPT-Presentation...
C B Welch


The Tenth Report of the International Research Group on Wood Preservation 1979-1980
1980 - IRG/WP 5110
R Cockcroft


Studies on the infestation behaviour of the powder-post beetle Lyctus brunneus (Steph.) and its physical control in the wood yards of the Caspian forests of Iran
1985 - IRG/WP 1271
Lyctus brunneus (Steph.) is a pest which has not been previously thoroughly studied in Iran. It severely attacks Iranian hardwoods, especially those used in wooden houses and that have not been treated. Research work was necessary to determine the natural resistance of the most important timber species in Iran against this insect....
P Niloufari


Tebuconazole, a new wood-preserving fungicide
1990 - IRG/WP 3634
TEBUCONAZOLE, an anti-fungal triazole compound, has been tested to assess the effectivness as wood preserving fungicide. Tests were made with the active ingredient and also in formulations against basidiomycetes, blue-staining fungi and mould. Results of the DESOWAG laboratories and also from official institutes will be presented. In addition to this there were made different toxicological and eco...
B Wüstenhöfer, H-W Wegen, W Metzner


Decay resistance of wood removed from poles treated with Trichoderma
1989 - IRG/WP 1386
Wood blocks removed from a distribution pole previously treated with a biological control product (Binab FYT pellets) were exposed in soil block tests to selected basidiomycetes. The blocks were removed from regions of poles where Trichoderma colonization had been confirmed by extensive sampling and computer mapping of microbial inhabitants. The results indicate that material from pole interiors c...
A Bruce, B King, T L Highley


Comparative investigations on the influence of wood seasoning, wood properties and temperature on the toxic values of wood preservatives against Hylotrupes egg larvae
1970 - IRG/WP 28
Comparative tests carried out at three institutes indicated the influence of kiln temperature, position of wood specimens in the cross sectional area and test temperature on the toxic values determined in accordance with DIN 52165 with egg larvae of the house longhorn beetle (Hylotrupes bajulus L.). The preservatives applied were boric acid in distilled water and g-benzene-hexachloride dissolved i...
G Becker, T Hof, O Wälchli


Preservative treatment of Eucalyptus saligna fence posts by the double-diffusion method
1982 - IRG/WP 3196
Eucalyptus saligna fence posts treated by the double-diffusion method with two chemical combinations showed average lives of 11.2 years (copper sulphate and potassium dichromate at 10.5 kg/m³ retention)and of 14.3 years (copper sulphate and sodium mono-H arsenate at 7.1 kg/m³ retention), as determined in five test sites in the State of Sao Paulo, Brazil. The exponential model was the best fit wh...
E S Lepage, A R De Freitas


Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem


The Sixth Annual Report of the International Research Group on Wood Preservation 1974-1975
1975 - IRG/WP 541
IRG Secretariat


Wood Preservation in France. A statement of quality control early 1986
1986 - IRG/WP 3389
A statement of quality control in France early 1986 - Summary of new - Standards criteria for preservatives and treated wood - Aptitude of treated wood for use per class of biological hazard...
M Romeis, G Ozanne


Eco-tax - A new threat for wood preservation? The Belgian experience
1993 - IRG/WP 93-50001-32
At the end of January 1993, a bill was put for Belgian Parliament related to the introduction called "Eco-taxes" on a series of products, such as packaging for drinks (especially on PVC-bottles), non-returnable articles (shavers, small cameras), batteries, pesticides for non-agricultural use and paper....
G Van Steertegem, F De Jaeger


Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal


Establishment of a laboratory method to characterise the ecotoxicity of a polluted soil
1998 - IRG/WP 98-50101-23
This method consists in using the underground grub of the Oxythyrea funesta beetle as a bioindicator of the soils pollution. Due to the significant tolerance of the organism, a large type of substrate of different nature and grain size could have been studied. We have tested substances and preparations such as wood preservation products even under powder or liquid form but also some wastes of di...
P Martinet


Selective adsorption of antisapstain actives from two aqueous suspensions, and movement of actives into wood
1996 - IRG/WP 96-30103
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, NeXgenâ and Busanâ Sap Stain Preventative (Busan 1009), at three product concentration levels. Concentrations of active ingredients (NeXgen: CTL (chloro-thalonil) and MTC (methylene bisthiocyanate); Busan 1009: TCMTB (2(thiocyanomethylthio)-benzothiazole) and MTC) wer...
M J Kennedy, T L Woods


Blue stain in service on wood surface coatings. Part 2: The ability of Aureobasidium pullulans to penetrate wood surface coatings
1992 - IRG/WP 92-1557
The ability of Aureobasidium pullulans to penetrate seven different wood surface coatings was examined. Eight isolates of Aureobasidium pullulans were used. Following penetration, light microscopy was used to examine the effect of the fungus upon the coating, and growth at the wood-film interface. The fungus showed different growth capabilities with different types of surface coatings. Some isolat...
P R Sharpe, D J Dickinson


Studies of the distribution and degradation of tributyltin naphthenate in double-vacuum treated wood
1983 - IRG/WP 3230
The effects of forced solvent evaporation by kilning redwood (Pinus sylvestris) that has been double-vacuum treated with tributyltin naphthenate (TBTN) have been investigated. Contrary to previous studies reported, it has been shown that forced evaporation can have a considerable influence on the losses of the fungicide. It has been found that, whether the solvent is allowed to evaporate slowly or...
J Jermer, M-L Edlund, W Hintze, S V Ohlsson


Update on lab and field test results for polymeric alkylphenol polysulfide treated wood
2002 - IRG/WP 02-40240
The possibility of using Polymeric Alkylphenol Polysulfide (PXTS) as a wood preservative has been undergoing evaluation in our laboratories for the past four years. Various formulations prepared from this compound have been tested and found to be effective against wood decay fungi and insects in field stakes after 42 months exposure. In accelerated soil bed tests, PXTS has been shown to be consi...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Corrosion of fasteners in heat-treated wood – progress report after two years’ exposure outdoors
2005 - IRG/WP 05-40296
The corrosion of common fastener materials now in use - mild steel, zinc-coated steel, aluminium and Sanbond Z-coated steel – has been evaluated after two years’ exposure outdoors in untreated and heat-treated spruce (Picea abies) respectively. Spruce from South-western Sweden was used. The heat-treatment was carried out in Finland according to the ThermoWood process at a maximum temperature ...
J Jermer, B-L Andersson


Fluorine compounds for wood preservation
1971 - IRG/WP 304
Fluoride compounds have gained a considerable importance in wood preservation, especially in Germany and some other countries of Europe. They are used as single compounde or in mixtures of different compounds. In the International Research Group on Wood Preservation which continues the activities of a former OECD-Group, it was moved to prepare a survey on fluorides in wood preservation together wi...
G Becker


Factors affecting leaching of preservatives in practice
1978 - IRG/WP 3113
At the 7th Meeting of the IRG in Poland in May 1975, the findings of collaborative laboratory leaching techniques were discussed, and the dangers inherent in using such results to predict the behaviour of preservative-treated components in service were emphasised. In order to improve our understanding of the factors governing leaching of preservatives in practice, and to identify areas where furth...
R Cockcroft, R A Laidlaw


Light organic solvent preservative treatment of glue-laminated radiata pine
1986 - IRG/WP 3380
The high permeability of radiata pine (Pinus radiata D. Don) is associated with ray-tissue and in particular the cross-field pits linking ray-tissue to tracheids. This pathway is absent in the tangential grain direction, leading to poor preservative penetration when treatment is restricted to the radial face - for example, timber fabricated into glue-laminated beams....
P Vinden