IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3291 documents. Displaying 25 entries per page.


Exposure trial at tropical marine sites of pyrethroid/creosote mixtures as wood preservatives: Preliminary results
1989 - IRG/WP 4155
Pinus sylvestris sapwood blocks measuring 25 x 25 x 200 mm³, impregnated using a Lowry or Rüping pressure treatment cycle with solutions of permethrin, cypermethrin or deltamethrin in BS144 creosote, have been exposed at marine sites in Australia, Papua New Guinea, the U.K. and Singapore. The effectiveness of these solutions in preventing marine borer attack is being compared with the efficacy o...
S M Cragg


Soil blocks versus field test for evaluating and standardizing wood preservatives: A commercial view
1994 - IRG/WP 94-20024
On the basis of technical considerations, experience, costs and applicability, the author concludes that the soil block test and other laboratory tests have little meaning in a wood preservative standardization process and almost no merit in the commercialization of a wood preservative system. Field tests at sites known to be aggressive to preservative treated wood are strongly recommended....
W S McNamara


Über Wespen als Holzverderber - Schäden, Ursachen, Bekämpfung
1978 - IRG/WP 189
Observations and a number of actual cases over recent years show that wasps have been associated more frequently with damage to wood. The nature of such damage and the agents involved are as follows: 1. Decay following infestation by Woodwasps (Siricidae). 2. Punctate marks caused by superficial gnawing and also boring into wood by larvae of the Dock sawfly (Tenthredinidae). 3. Damage due to super...
S Cymorek


Resistance of the wood of Eucalyptus saligna and Paulownia tomentosa against some wood rotting fungi
1997 - IRG/WP 97-10238
Paulownia tomentosa and Eucalyptus saligna are not autochthonous species in Slovenia and we determined the resistance of their wood against our most common wood rotting fungi. The resistance against Coniophora puteana, Gloeophyllum trabeum and Trametes versicolor was determined according to EN 113 and compared to the resistance of beech (Fagus sylvatica) wood. It was stated, that both paulownia an...
F Pohleven, M Petric


Conforming to european standards for preservative-treated timber: Specifying with confidence
2000 - IRG/WP 00-20194
A four-year collaborative study between four industrial partners and BRE has assessed timber treated by current UK industrial practices in the light of current European Standards. Data were collected for CCA and creosote treated timber components, and compared with the requirements laid out in EN351-1 and -2. A number of difficulties were encountered that have been described in previous IRG papers...
E D Suttie, R J Orsler


Spore germination of Gloeophyllum trabeum on wood is related to the mass of the wood sample
1978 - IRG/WP 2118
E L Schmidt, D W French


Supplement to Document No: IRG/WP/56. Health and safety aspects of the use of wood preservatives
1975 - IRG/WP 356
H Willeitner


Wood preservation in France. "Bois plus" chain of quality. Description of the scheme early 1989
1989 - IRG/WP 3519
1989 - description of the French "CTB-BOIS PLUS" homologation scheme
G Ozanne


The Eighth Annual Report of the International Research Group on Wood Preservation 1976-1977
1978 - IRG/WP 569
IRG Secretariat


The Rubber Ruler: Continuous measurement of dimension changes in wood panels
1994 - IRG/WP 94-20033
A new application for a linear transducer called Rubber Ruler was developed. Rubber Ruler provides a simple and reliable method for continuous monitoring of dimension changes in wood panels. This paper presents the methodology. Results of priliminary experiments designed to simulate the movement in wood panels are also discussed....
Siew K Ho, P Vinden, P Kho


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1982 - IRG/WP 3207
J Beesley


An attempt to evaluate wood resistance against fungal decay in non-sterile conditions by measuring the variation of resistance to bending test
1988 - IRG/WP 2308
The main object of this work was to determine the variation of strength on large test specimens of wood (800 x 45 x 45 mm³) when exposed to accelerated fungal attacks close to natural conditions, out of test vessels. The modulus of elasticity (MOE) and the modulus of rupture (MOR) have been assessed. Thereby, the natural resistance of the wood species to fungal decay, the efficiency of preservati...
L N Trong


Local preservation with difluoride pills: Life-time of preservative
1998 - IRG/WP 98-40127
A brief history of the situation in the Netherlands with respect to the preservation of joinery is given. Already in the eighties in the Netherlands many spruce window frames were treated with difluoride pills. One of the possible disadvantages of this kind of diffusing preservatives is the high leaching rate found in laboratory situations. The leaching rate in practice is influenced by many facto...
W J Homan, C Blom, B W Holleboom


Determination of the preventive efficacy against wood destroying basidiomycetes fungi, EN V 839 - CEN/TC 38 WG 9
1993 - IRG/WP 93-20015
The WG 9 of CEN TC/38 has presented to EC a mycological test to assess efficacy of preservatives applied by surface process. This method is now an experimental standard (EN V 839) which has to be approved by the different european delegations. The following paper is not the standard as it has been proposed but is a presentation of the principle of the method. The experimental standard specifies a ...
D Dirol


Gloeophyllum trabeum and Gloeophyllum abietinum, the most frequent brown rot fungi in fir wood joinery
1999 - IRG/WP 99-10319
In Croatia the primary raw material for joinery production is silver fir wood (Abies alba Mill). L-joints made of home-grown fir sapwood and prepared according to EN 330: 1993 were used to establish the infection and colonisation of micro-organisms, particularly wood decay fungi, to compare the performance of untreated and 1% TnBTO treated L-joints. The L-joints were coated with two types of coat,...
R Despot, M Glavas


European standardization for wood preservation
1989 - IRG/WP 2335
G Castan


Conservation of wooden cultural property
1994 - IRG/WP 94-30038
A survey of the conservation of wooden archtitectual monuments, art objects and archaeological finds is presented. Each of the three areas has typical conservation problems which reqire the use of selected wood preservatives and consolidation agents. Furthermore specific protection and consolidation methods are necessary. A precise damage diagnosis with non-destructive testing methods is the first...
A Unger, W Unger


Results of co-operative studies on determining toxic values against wood-destroying Basidiomycetes. Preliminary report to Sub-group members
1986 - IRG/WP 2271
A F Bravery, J K Carey


Japanese wood preserving industry
1990 - IRG/WP 3596
Although a great amount of wood is in use in Japan, a little attention has been paid to the significance and importance of wood preservation. The fact reflects that only less than 0.5% of the total wood consumption is treated with wood preservatives today in the country. Over the 20 years before 1970, the annual volume of preservative treated (pressure treatment) wood was relatively at a stable le...
K Tsunoda


Water-based wood preservatives for curative treatement of insect-infested spruce constructions
1998 - IRG/WP 98-30171
On laying down sanitation measures for wooden constructions infested by wood boring insects, we must take into account static risks for the construction - and, thus, for the security of the user - as well as risks for humans and environment due to the chemical preservative compounds of the treated wood. Analyses on many roof constructions made with spruce (Picea abies L.) have revealed that Hylot...
E Graf, P Manser, B Lanz


The resistance of painting materials and consolidants against wood-destroying insects
1997 - IRG/WP 97-10239
Natural and synthetic adhesives, varnishes, painting materials and consolidants were used in investigations of bioresistance against newly hatched larvae and beetles of Hylotrupes bajulus (L.). Animal glues, casein, drying oils and natural resins such as dammar resin and shellac, were not resistant to attack by these larvae. Similarly, semi- and all-synthetic polymers tested including hydroxypropy...
W Unger, H Fritsche, A Unger


Wood preservation in the USA
1982 - IRG/WP 3215
This report is a comprehensive survey of the status of the wood preservation field in the U.S.A. at the start of the 1980s. The importance of wood preservation is discussed and its industry described. Various statistics and analyses regarding the use of treated wood have been compiled. Both pressure and non-pressure applications have been covered, as well as remedial treatments and pest control op...
D D Nicholas, R Cockcroft


The susceptibility of 35 Amazon wood species to Cryptotermes brevis (Walker)
1982 - IRG/WP 1160
Laboratory tests were carried to evaluate the susceptibility of 35 Amazon hardwoods to Cryptotermes brevis (Walker). The results were analysed statistically and showed that five wood species were non resistant, nine were resistant and the other twenty-one in between those classes of resistance....
M D Canedo


The Ninth Annual Report of the International Research Group on Wood Preservation 1978-1979
1979 - IRG/WP 579
IRG Secretariat


Working Group I 'Biological Problems' Sub-group 'Insects in dry wood (other than termites)', Scope of work
1976 - IRG/WP 152
S Cymorek


Previous Page | Next Page