IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1171 documents. Displaying 25 entries per page.


A deflection test for monitoring decay in miniature beams
1986 - IRG/WP 2269
A laboratory apparatus for assessing decay in small stakes is described. It involves the measurement of deflection in a static bending apparatus using a displacement transducer linked to a microcomputer. Measurements are non-destructive, rapid, accurate and automatic and decay can be assessed repeatedly over long time periods....
S M Gray


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


Effects of the anaerobic wood decay bacterium Clostridium xylanolyticum on unbleached Pinus and Eucalyptus pulp
1991 - IRG/WP 1506
Clostridium xylanolyticum has been shown to produce extracellular enzymes capable of degrading wood. The present work was conducted to quantify growth on various lignocellulosic substrates and degradation of pulped wood fibre. In the latter tests Clostridium xylanolyticum was incubated at 35°C under anaerobic conditions in a medium containing 0.2% (w/v) peptone and 4% (w/v) unbleached Pinus and E...
G D Shelver, U Matai, W Van Wyk, A A W Baecker


Decay resistance of resin treated wood
1999 - IRG/WP 99-30206
Selected natural resin systems were evaluated for their potential as wood protecting agents according to standard test procedures. As indicated by the European standard EN 599 both a Basidiomycete test according to EN 113 and a ENV 807 soil bed test were carried out. Six resin treatments were tested using 3 concentration or treatment levels. Using the biocidal activity criteria as usually applied ...
J Van Acker, A J Nurmi, S M Gray, H Militz, C Hill, H Kokko, A O Rapp


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Translation of CEN Letter to Mr R Cockcroft dated 24 November 1980
1980 - IRG/WP 2147
G Castan


The performance of glue laminated railway ties after 40 years of service in the main line track
1989 - IRG/WP 2325
Two series of horizontally glue laminated ties made of a softwood body and topped with a hardwood lamination were creosoted and installed in 1947 in a tangent and a curved main line track. The tests are now 40 years old and the excellent condition of the ties of these two series suggest that a service life of 50-60 years can be expected....
J P Hösli, E E Doyle, C P Bird, T Lee


A baiting technique to monitor the development and control of decay in transmission poles
1981 - IRG/WP 2149
P I Morris, D J Dickinson


Micromorphology of the decay caused by Chondrostereum purpureum (Pers.:Fr.) Pouzar and Flammulina velutipes (Curt.:Fr.) Singer
1988 - IRG/WP 1358
Two basidiomycetes, Chondrostereum purpureum and Flammulina velutipes, form typical soft rot cavities in hardwoods and softwoods. Cavity formation is prececed by T-branching or bending of hyphae penetrating the wood cell walls. The two fungi also cause erosion of the wood cell walls....
T Nilsson, G F Daniel


Wood decay in Danish buildings
1985 - IRG/WP 1261
At Technological Institute identification of fungi and advisory activity concerning repair of damages has taken place since 1935. Statistical analyses based on material from 1982 and 1983 are compared to earlier investigations worked out by L. Harmsen. The material shows that building traditions influence the diversity and frequency of fungal species. Many fungal damages in the last decade have sh...
A P Koch


Termiticidal chemicals derived from tropical tree resins
1991 - IRG/WP 1477
To test the hypothesis that defensive chemicals protect tropical primary forest trees against biological attack, a bioassay and fractionation program was conducted in Indonesia. Fresh dipterocarp resins were fed in no-choice tests to Neotermes dalbergiae termites on 4.5 cm filter papers, or tested for inhibition of fungal growth. Fractionation of biologically active resins via flash column chromat...
A Messer, K McCormick, D Richardson, Sunjaya, H Hagedorn, J Meinwald


Treatment of messmate (Eucalyptus obliqua L'Hérit) by double-diffusion: Preliminary report
1983 - IRG/WP 3234
Modified double-diffusion is suggested as a method of impregnation for mixed tropical hardwoods for certain types of ground contact use in less developed countries. Compared with vacuum/pressure impregnation, capital costs are low and little skill is needed for the operations involved. Treatment of messmate (Eucalyptus obliqua L'Herit) rounds involving pre-heating in water prior to their ...
F F K Ampong, C-W Chin


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Natural durability studies in an accelerated field simulator - A novel approach
1983 - IRG/WP 2197
A study of the natural durability of untreated timbers to both decay and termite attack is described. The work illustrates the versatility of the Accelerated Field Simulator as a novel approach to biodeterioration research....
G C Johnson, J D Thornton, J W Creffield, C D Howick


Monographic information on Serpula (Poria) incrassata according to the "Model Questionnaire for preparation of monographic cards for wood-destroying fungi"
1980 - IRG/WP 160
J G Palmer, W E Eslyn


About the relations between the natural durability of some tropical species and their extractives content
1983 - IRG/WP 1208
G R Y Déon


Soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, in ground contact in Australia
1986 - IRG/WP 1280
The performance against soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, was examined after 20 months in ground contact at Pennant Hills, Australia. The results indicate that between these species soft rot decay is excluded by different levels of CCA salt suggesting that the threshold level for exclusion of soft rot in these hardwoods is a function of anatomical structure/ultrastru...
R S Johnstone


Sex pheromone of the male house longhorn beetle Hylotrupes bajulus (L.) (Coleoptera: Cerambycidae)
1995 - IRG/WP 95-10100
Since 1990 studies have been conducted with respect to the chemical communication of the house longhorn beetle Hylotrupes bajulus (L.) (Coleoptera: Cerambycidae). The structure of glands located in the prothorax of the beetles was examined with light and scanning electron microscopy. The analyses of different extracts from beetles resulted in the finding and identification (GC-, GC/MS-, and HR-GC/...
U Noldt, R Fettköther, F Schröder, H Meyer, K Dettner, W Francke, W A König


Studies on the preservation of structrual plywood - Part 1: Decay resistance of structural plywood
1974 - IRG/WP 238
The weight loss and the decreases in the compression strength and in the modulus of elasticity were measured to determine the decay resistance of structural plywood (lauan). Test pieces (50x25xA mm³) were exposed to the wood destroying fungi (Coriolus versicolor and Coriolellus palustris) for 2-3 or 2-4 months. After exposure, the measurement of the compression strength was carried out on the pie...
K Minami, Y Kenjo, S Sugiyama


Protection of Ochroma pyramidale from fungal decay with N,N-napthaloylhyroxylamine
1998 - IRG/WP 98-30182
Fungal decay of wood in service results in billions of dollars (U.S.) in losses annually. Recent environmental restrictions, both U.S. and international, are limiting and eliminating the use of broad-spectrum, heavy metal biocides for wood preservation. Restrictions result primarily from problems with disposal. New wood preservatives need to be developed and tested which specifically target key el...
F Green III, T L Highley


Methods of assessing decay in poles in service with the Pilodyn wood tester
1978 - IRG/WP 2107 A
H Friis-Hansen


Report on biological control of decay in poles
1977 - IRG/WP 149
The following its a brief report on a preliminary experiment carried out for the United Kingdoms Midland Electricity Board during 1974-1975 to establish, under laboratory conditions, the potential controlling value of some non-decay fungi against Lentinus lepideus. Lentinus lepideus has been confirmed to be the commonest Basidiomycete causing decay in poles in the Boards area....
T A Oxley


Questionnaire on the distribution of the house borer Hylotrupes bajulus
1982 - IRG/WP 1170
H Becker


Characterization of glycopeptide from white-, brown- and soft rot fungi
2002 - IRG/WP 02-10424
Extracellular low-molecular-weight substances that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radicals have been isolated from wood degrading cultures of white-rot, brown-rot, and soft-rot fungi. They contained protein, neutral carbohydrate, and Fe(II). These substances were glycosylated (glycated) peptides and suggested to form Amadori product (ketoamine). The...
H Tanaka, S Itakura, A Enoki


Effect of asphyxiation on wood decay fungi treated with argon and nitrogen gas
2002 - IRG/WP 02-10452
The effects of low-oxygen conditions, achieved with either argon or nitrogen gas, on the viability of wood decay fungi Coniophora puteana, Antrodia vaillantii and Trametes versicolor, cultivated on PDA medium and infected wood samples, were examined. The fungal cultures were exposed to low oxygen concentration (below 10 ppm) for one to five weeks in hermetically sealed vessels. Anoxic treatment di...
C Tavzes, F Pohleven, M Janisek, R J Koestler


Previous Page | Next Page