IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1171 documents. Displaying 25 entries per page.


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests
1980 - IRG/WP 2135
With the exception of acid-copper-chromate, zinc-chrome-arsenate, and sodium pentachlorophenoxide, the relative performance of preservatives in the fungus cellar was similar to that in the field....
M E Hedley


A new approach to the maintenance of wooden railway sleepers. (Second report)
1988 - IRG/WP 3492
The microenvironment and micro-ecology of wooden railway sleepers was investigated to assess their condition to determine the necessary treatment, repair and replacement criteria. In this report the efficacy of the secondary preservative treatment with solid boron rods is discussed and the development of an in-situ, nondestructive test method based on the creation and assessment of structural dyna...
W Beauford, P I Morris, A M Brown, D J Dickinson


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


The resistance of fifteen Indonesian tropical wood species to the powder post beetle Heterobostrychus aequalis
1990 - IRG/WP 1429
A preliminary laboratory test on the resistance of 15 tropical wood species to Heterobostrychus aequalis has been carried out using small samples of 7.5 x 5 x 1.5 cm³. The results reveal that Pinus merkusii and Agathis borneensis are very susceptible to Heterobostrychus aequalis. Other 13 species vary between susceptible to resistance There is no signifisant relation between starch content and th...
Jasni, Nana Supriana


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


Prevention of brown-rot decay by chelators
1992 - IRG/WP 92-1540
In this work the brown-rot decay was shown to be prevented by chelating the endogenous metals existing in wood by using organic or inorganic chelators or iron-binding siderophores. The fungal growth and decaying ability were significantly decreased by the chelating treatments of the solid wood-based culture medium and pine wood pieces, respectively. The transition metals existing in native wood ar...
L Viikari, A-C Ritschkoff


Description of the damage produced by xilophagus Curculionides in Spain
1989 - IRG/WP 1408
Cossoninae are a reduced subfamily of Curculionidae. These xilophagus insects produce significant damage in Spain, mainly affecting old buildings. Their activity is a real problem for the preservation of the country's historical-artistic heritage. The three Cossoninae species most widespread in Spain are described for the first time as well as the conditions under which they develop. The ...
E L Rodríguez Trobajo


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Report on the status of collaborative experiments within the Sub-group on Basidiomycete tests
1983 - IRG/WP 2194
This report summarises the results of co-operative work carried out within the Sub-Group on Basidiomycete tests up to December 1982. The principle findings are recorded in the Conclusions Section. Work intended between IRG-13 in Turkey and IRG-14 in Australia is cited under Future Programme. An Annex provides a response sheet for existing and new participants to notify their contributions....
A F Bravery


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


Accelerated wood decay in a soil bed test under greenhouse conditions compared with a stake test under field condition
1991 - IRG/WP 2384
The rate of decay of oak, beech, Douglas fir, pine and spruce stakes in an outside test field were compared with the decay rate of the same species in a greenhouse soil-bed test. Strength loss after four and six months respectively was measured by determining the compression strength parallel to the grain. The results show that all species, strength loss in the greenhouse was 2 to 4 times higher t...
J E Polman, S G Michon, H Militz


Wood preservation in the Australian beekeeping industry
1988 - IRG/WP 3473
This paper reports the results of a survey of Australian commercial beekeepers working 200 or more hives in June/July 1985. Nine hundred and forty seven apiarists were asked to participate and to provide information on their wood preservation methods, painting procedures and maintenance of bee boxes. Three hundred and eighty-four apiarists returned completed questionnaires (41%). The main wood pre...
P J Robinson, J R J French


Effect of sterilization method on germination of spores of wood decay fungi observed by contact agar block method
1978 - IRG/WP 2117
Previous studies of germination of spores of wood decay fungi on wood have generally concluded that method of wood sterilization has little significant effect on germination response. This study expands the numbers of test fungi as well as number of sterilization methods employed to determine the influence of sterilization method on spore germination response of decay fungi. Germination was assess...
E L Schmidt, D W French


A laboratory soil-block decay evaluation of plywoods edge-treated with preservatives
1982 - IRG/WP 2174
Preservative-treated plywood used under conditions or severe decay hazard frequently has its original, or cut edges, protected by the application of a field-cut preservative. This study uses a laboratory test method to compare the efficacy of four commercial preservative treatments against two commonly occurring brown-rot fungi. The results are not meant to indicate the service life of such treate...
R S Smith, A Byrne


Final draft of a monographic card for Pole Fungus A, L Harmsen, Rigidoporus vitreus (Fr.) Donk according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 178
L Harmsen


The influence of building design on wood decay
2000 - IRG/WP 00-10339
The cheapest and most effective way to prevent wood decay is to KEEP THE WOOD DRY! You and I know that, but we often forget and attempt a preservative solution to a problem better solved with good design and construction. It's also the answer to a frequently missed exam question in my Architecture class. Just as caulking is a poor substitute for proper design, so preservative treatment sh...
W W Wilcox


A short note on the subject of pretreatment decay in wood
1984 - IRG/WP 1245
The paper reviews five national standards for wood utility poles and some literature that concerns the problems of pretreatment decay. Finally it is proposed to form a new sub-group to study that problem....
J A Taylor


Monographic information on Serpula (Merulius) lacrymans (Schum. ex Fr.) S. F. Gray, according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 170
J Segmüller, O Wälchli


Non-enzymatic Gloeophyllum trabeum decay mechanisms: Further study
2001 - IRG/WP 01-10395
Information will be presented on the mechanisms involved in, and potential application of, non-enzymatic wood decay by brown rot decay fungi. Specifically, the hypothesized role of low molecular weight phenolate derivatives will be discussed in relation to non-enzymatic degradation of wood. The mechanism of binding of iron by cellulose, and binding and reduction of iron by fungal derivatives and m...
B Goodell, J Jellison


Combined effects of the treatment of wood with formaldehyde
1978 - IRG/WP 3117
Treatment of fibrous materials with reagents in a vapor phase is neither new nor unique. Numerous examples exist in literature of vapor phase experiments on cellulose fibers and fabrics, and on wood. For many years the textile research and industry have used vapor phase processes for the treatment of textiles. The chemical modification of cellulose is based on different types of reactions e.g. est...
M Stevens, J Schalck


Evaluation of the decay caused by Chaetomium globosum Kunze, in the course of time
1987 - IRG/WP 2288
The main research done on soft rot has been directed to determining, by microscopic study, the different stages of penetration into the wood of the fungi that cause it. On the basis of the information furnished by this research, in this work we have tried to quantify its effect, by evaluating the weight loss caused by Chaetomium globosum Kunce in wood of Pinus sylvestris L. and Fagus sylvatica L. ...
M T De Troya, A M Navarrete


Étude in vitro de la colonisation et de la dégradation structural du bois de hêtre par Coriolus versicolor (L.) Quélet
1976 - IRG/WP 158
L'attaque du bois de Hêtre par Coriolus versicolor (L.) Quélet, agent de pourriture fibreuse blanche est étudiée après des périodes d'exposition à ce champignon variant de 15 jours à trois mois. L'observation des premiers stades, c'est à dire de la colonisation du bois par les filaments de champignon est faite en microscopie optique, puis au fur et à m...
D Dirol


Soil-bed studies
1982 - IRG/WP 2181
This paper discusses factors affecting the design and use of a soil-bed....
P Vinden, J G Savory, D J Dickinson, J F Levy


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


Previous Page | Next Page