IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1021 documents. Displaying 25 entries per page.


The resistance of timbers to impregnation with wood preservatives
1979 - IRG/WP 3137
It is anatomical structure which determines liquid flow rate within different timber species. This cannot be deduced from properties such as density or rate of growth, and can only be found by experiment. A standard test has been in use at the Princes Risborough Laboratory for many years, employing a pressure-impregnation treatment, and a large number of timbers have been studied. The test consist...
Anonymous


A comparison of analytical and visual techniques used for assessment of weathering properties of chromium and copper azole treated timber
1994 - IRG/WP 94-20023
The weathering properties of preservative treated timber were studied by measuring surface lignin loss and by microscopic examination after weathering, and results were related to qualitative assessments of visual appearance after weathering. Measurement of relative rates of delignification of untreated and preservative treated timber obtained by FTIR analysis, and weight loss determined on thin v...
J A Cornfield, M D C Hale, G Fettis


Life cycle approached environmental information to promote treated timber
2005 - IRG/WP 05-50224-13
This paper exemplifies the possibilities to compare products and product systems with help of life cycle assessment (LCA) as a tool for environmental assessment. IVL Swedish Environmental Research Institute has developed a concept for evaluation of environmental impacts based on normalisation, based on so called environmental quality objectives (EQO). This concept makes it possible to compare a pr...
M Erlandsson


Performance of Copper-Chrome-Arsenic (CCA) and Copper-Chrome-Boric (CCB) treated panels of Bombax ceiba and Paraserianthus falcataria against bio-deterioration at Krishnapatnam harbour, east coast of India
2003 - IRG/WP 03-30310
Results of investigations on the durability of light weight timber species (Specific gravity below 0.4) i.e., Bombax ceiba and Paraserianthus falcataria in treated and untreated condition conducted at Krishnapatnam harbour (Lat 13o28’ to 13o59’ N; Long: 80o10’ to 80o16’E) along the east coast of India are reported in the paper. Exposure trails were conducted with panels (Size: 30 x 3.8 x...
B Tarakanadha, N R Raveendra Prasad, K S Rao


Recycling of CCA treated wood in the US
1998 - IRG/WP 98-50101-08
The production of CCA treated wood has increased dramatically in recent years. Previous estimates of the volume of treated wood to be removed were based on the assumed service life of the material, generally 20 to 25 years. This study based on a survey of contractors installing treated decks, determined that the actual service life of these decks is much shorter than their assumed functional servi...
J McQueen, J Stevens, D P Kamdem


Durability of some alternatives to preservative treated wood
2004 - IRG/WP 04-30353
The environmental discussion in Sweden has lead to an increasing use of naturally durable domestic wood species and wood treated according to alternative methods for use above ground. A number of these alternatives have been tested according to field- and laboratory tests and compared to wood treated with preservatives for above ground use. Seven untreated wood species, four alternative wood treat...
M-L Edlund


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic applications. Part 1: Laboratory scale investigation
1995 - IRG/WP 95-50046
In order to investigate the applicability of current prestandard leaching test methods, a series of experiments has been performed on CCA impregnated wood dealing with the influence of pH, temperature and agitation of the surrounding water. The leaching method used in this first part of the investigation is the European prestandard drafted by CEN/TC38/WG11, a short term dynamic leaching test under...
G M F Van Eetvelde, R J Orsler, G E Holland, M Stevens


Termite resistance of treated wood in an above-ground field test
1986 - IRG/WP 1300
This paper provides an update on the results from an above ground field test evaluating the effectiveness of wood preservatives against subterranean termites. Results for the one and two year inspections of treated southern pine sapwood exposed in Hawaii to Coptotermes formosanus are presented. Chromated copper arsenate is providing excellent protection as is the pyrethroid deltamethrin. Borate an...
A F Preston, P A McKaig, P J Walcheski


Fluoride and chromium concentrations in soil adjacent to remedially treated distribution poles
1996 - IRG/WP 96-50066
Soils adjacent to Rentex treated 'on-line' distribution poles were analysed for total fluoride and chromium content for comparison with background values of these elements. Soil samples 6 cm and 25 cm downslope of selected poles were recovered at 1 week, 1 month, 6 and 12 months after treatment. Background soil samples were taken 50 m from the poles at sampling times. Fourteen po...
D C R Sinclair, G M Smith, A Bruce, H J Staines, P Durrant


Examination of preservative-treated Pinus sylvestris using electron paramagnetic resonance
1992 - IRG/WP 92-3710
EPR is currently being used to help elucidate the nature and extent of the chemical reactions occurring between wood and copper based timber preservatives. In the work reported here treated Scots pine samples were examined at room temperature and in the frozen state. Plots of the electronic parameters A|| vs. g|| were found to be a useful index of the electronic properties of the various formulati...
A S Hughes, R J Murphy, J F Gibson, A J Cornfield


Life Cycle Assessment of borate treated wood
2005 - IRG/WP 05-50224-12
Life Cycle Assessment (LCA) is being used increasingly around the world by decision-makers to help incorporate the environmental component of sustainability into their activities. U.S. Borax regularly assesses how its products contribute to sustainable development. Using data gleaned from LCA of its products, the company recently completed its first ISO 14040 compliant cradle-to-grave LCA of lum...
M J Manning


The microbial ecology of treated birch stakes in a soil-bed
1983 - IRG/WP 1209
The microbial ecology of small birch stakes exposed in soil beds in two Fungus Cellars was investigated. Patterns of fungal colonisation and decay initiation are described in untreated birch and copper fluosilicate-treated stakes. Results are based on fungal isolation onto selective media and direct light microscopical observations of decay features. In untreated stakes there was a rapid build-up ...
C P Clubbe


Present status of using treated wood and private house owner’s expectations in Bangladesh
2004 - IRG/WP 04-30329
In a developing country like Bangladesh more than 80 % of the total population lives in rural areas where building materials are mainly comprised of wood, bamboo, thatch grass, golpata, etc. All these materials, being cellulosic, are easily infected by deteriorating agencies like fungi, termites, beetles etc., as climatic condition of the country is ideal for their thrive. This is a great wastage ...
M A Islam, A K M A Bosunia, S C Ghosh, M O Hannan, A K Lahiry


Quantification of creosote migration down wooden poles and the prevention of its depletion during flood irrigation
1994 - IRG/WP 94-50032
Polyethylene field liners heat-shrunk onto soil-contact surfaces prevented decay of creosote-treated Eucalyptus grandis vineyard poles under flood-irrigation. The present work quantified losses of creosote from these poles after six and 24 months' service. After six months' service the mean creosote retention of unlined poles above the ground line was 12.62% (m/m dry wood), with ...
M Behr, A A W Baecker


Depletion of preservatives from treated wood: Results from laboratory, fungus cellar and field test
1993 - IRG/WP 93-50001-07
This paper compares results of preservative component losses using a range of test procedures with several different water-borne preservatives. The data shows that laboratory leaching tests are in some cases comparable to, but in other cases significantly underestimate preservative component losses when compared with field or fungus cellar depletion tests. The results also suggest that preservativ...
L Jin, A F Preston


Leaching of Copper from ACQ treated wood exposed above ground
2004 - IRG/WP 04-50219
The leaching of chemicals of ACQ Type C treated wood exposed above ground for 16 months was studied. Commercially treated Hem-fir boards (Tsuga heterophylla Raf. and Amabilis fir Forb) of 37.5 mm by 87.5 mm were used. The amounts of chemical leached monthly by the rainfall were determined and the leachate was collected and analyzed. Also, the environmental factors influencing the leaching were ...
P A Chung, J N R Ruddick


The use of low cost X-ray fluorescence instruments in the determination of copper chromium and arsenic in preservative treated wood
1987 - IRG/WP 2278
Internal quality control in timber treatment plants can be pursued by analysis of preservative treatment solutions and treated timber. Treaters must proceed with costly and lengthy analyses through analytical laboratories. An alternative approach for the timber treater, is to use low cost analysers (L.C.A.'s) based upon x-ray fluorescence. Detailed comparisons have been made between stand...
J Norton, L E Leightley


Preservative leaching from copper-chrome-arsenic treated timber: Towards an international standard for environmental monitoring
1996 - IRG/WP 96-50076
A review of standards and legislative requirements around the world relating to environmental contamination from copper-chrome-arsenic wood preservative indicates a plethora of methodologies for expressing and determining contamination levels. The imposition of arbitrary quarantine periods for treated timber, or special fixation processes, appear to be applied without a rational analysis of what l...
S Walley, P R S Cobham, P Vinden


LCA examination of preservative treated timber products and alternatives; initial results
1995 - IRG/WP 95-50040-04
Co-operative development of an LCA methodology suitable for application to preservative treated products has been carried out, based on scoping assessments of two products, CCA treated fenceposts and creosote treated distribution poles. The general results of these scoping exercices are described, based on the CCA case study. These include the identification of critical stages in the life-cycle on...
W Hillier, R J Murphy, D J Dickinson, J N B Bell


Degradation of woods by obligately anaerobic fungi
1990 - IRG/WP 1452
Little is known about the processes occurring during the degradation of wood by obligately anaerobic fungi. When woods from a range of hardwood species were incubated for 11 days with a strain of the Chytrid Neocallimastix frontalis many of the woods were measurably fermented; Fagus sylvatica (23%) was the most highly degraded. Microscopic examination of Populus tremuloides wood after incubation w...
K N Joblin, G E Naylor


IRG/COIPM INTERNATIONAL MARINE TEST - To determine the effect of timber substrate on the efectiveness of different preservatives in sea-water: Coding scheme
1976 - IRG/WP 420
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying only the reference species treated with th...
Anonymous


Leaching Characteristics of Alder Wood Treated with Copper Based Wood Preservatives
2005 - IRG/WP 05-50225
In this study, it was designed for determining leaching characteristics of CCA and alternatives wood preservatives. Alder wood blocks were treated with CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Leaching studies were conducted according to AWPA E11-97. Copper analyses of leachate were determined Atomic absorption...
A Temiz, Ü C Yildiz, E D Gezer, S Yildiz, E Dizman


Quantification of creosote and fluoride in remedially-treated poles
1997 - IRG/WP 97-40097
Three creosoted transmission poles were put into service in 1961 and they were subsequently remedially-treated with a proprietary fluoride remedial paste formulation in 1981. The poles were removed from service in 1996 and their ground-contact regions were analysed for creosote and fluoride contents. It was found that the poles were undecayed. Creosote retentions decreased down the profiles of the...
B P Hill


A Novel Type of Multiple Cavity Attack in Wood Cell Walls of Heat-treated Timber Exposed in Seawater – Preliminary Observations
2004 - IRG/WP 04-10523
Samples of untreated and heat-treated Norway spruce and Douglas fir were submerged in Langstone Harbour, Portsmouth for 4 years at a depth of ca. 0.3 metres. The heat-treated samples had been prepared using the Plato process. Samples were initially assessed for the severity of marine borer damage and were then examined microscopically for evidence of microbial decay. Longitudinal and transverse wo...
R A Eaton, C Björdal, T Nilsson


Performance of borate-treated lumber in a protected, above-ground field test in Japan
2004 - IRG/WP 04-30344
This document is supplemental to the previous IRG document (Tsunoda et al., 2002). An experiment to simulate the sill plate (dodai) of the Japanese houses was conducted at the termite field test site of the Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. ...
K Tsunoda, A Byrne, P I Morris, J K Grace


Previous Page | Next Page