Soil-bed decay resistance evaluation of strandboards treated with preservative at different points of the manufacture process after 18 months exposure
2002 - IRG/WP 02-40230
Strandboards were treated with a copper-boron water-based preservative at different points of manufacture process namely, green strand diffusion, vacuum, spray application in the resin blender and post manufacture heat and cold quench. Preservative was applied to achieve five different retentions (0, 1.5, 3, 6, 12 kg m-3). The modulus of rupture and modulus of elasticity were assessed before expo...
G J Goroyias, M D C Hale


Laboratory evaluation of copper naphthenate pressure treatments against the Formosan subterranean termite
1993 - IRG/WP 93-10005
Southern pine wafers and Douglas-fir cubes pressure treated with copper naphthenate in AWPA P9 Type A oil or in toluene were evaluated for resistance to attack by the Formosan subterranean termite, Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae). Wood samples were pressure treated to target copper retentions of 0.040, 0.075, 0.095, or 0.150 pcf, conditioned to simulate field exposure, a...
J K Grace, R T Yamamoto, P E Laks


The difficult choice of the preservation industry when changing to more environmentally acceptable products
2000 - IRG/WP 00-50156
Until recent years the preservation industry in Norway had no problems with the environmental authorities. However, during the last three years the pressure has increased, and the authorities' solution to restrict hazardous chemicals is to introduce green (environmental) taxes for the products containing these chemicals, and also for the pressure-treated wood. The preservation industry ac...
F G Evans


Comparison of variable, constant and fluctuating pressure methods
2001 - IRG/WP 01-40212
The objective of this work was to evaluate potential improvements in pressure treatment arising from the use of a control valve. A constant pressure of 1035 kPa was compared to the conventional variable pressure method where the pressure is allowed to drop to 860 kPa as the solution is absorbed by the wood. A fluctuating pressure method (FPM) where the pressure cycles between 1000 and 1070 kPa was...
S M McFarling, P I Morris


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Standardization of preservative treated timber species for conductor, insulator and transformer packing of REB
1996 - IRG/WP 96-40071
In order to resolve the post landing failure problem of wooden packing for conductor, insulator, transformer of REB, the names of the suitable timber species from different parts of the world, irrespective of countries of origin have been standardized along with their strength and treatability grades. The CCA treatability of some Pakistani timber species have been presented for example which was t...
A K Lahiry


Persistance of active ingredients in treated wood
1993 - IRG/WP 93-50001-20
Disposing of chemically protected waste wood implies the distinction between surface and pressure treatment. Considering that barked round-wood merely contains, after 7 months open storage, less than 30 g per ton of bark or 25 mg per ton of sapwood, depending on the type of insecticide, the bark or sapwood shavings may be incinerated normally, according to less severe legal prescriptions than for ...
E Graf, P Manser, S Rezzonico, B Zgraggen


Strategies for enhancing usage of treated wood in Indian context
2005 - IRG/WP 05-40305
India constitutes 2% of the world’s forest area but it has to support over 15% of the human and nearly 14% of the cattle population and therefore forests in India are under immense biotic pressure. The main concern today is the rate at which avoidable factors or man made threats accelerate the process of forest degradation and to evolve measures to check the same. Man made threats include expl...
P K Aggarwal, S C Gairola


Wood kiln drying. Simple process of material treament or soft method of preservation? (Le séchage arificiel du bois. Simple opération de traitement du metériau ou méthode douce de préservation?)
1993 - IRG/WP 93-50001-14
Among the processes enabling to extend wood durability, kiln drying can be considered as a treatment and soft preservation method. Dry woods are naturally durable provided they are not subject to important retaking of the moisture. Drying thanks to the application of temperatures from 50 to120°C enable to execute a thermic treatment which kills grubs and mushrooms to ensure a sterilization that c...
F More-Chevalier


Adequate preservative treatment of kiln dried Eucalyptus camaldulensis and Acacia mangium for tropical and subtropical wood poles
1996 - IRG/WP 96-40075
The Eucalyptus camaldulensis and Acacia mangium round timbers kiln-dried at EMC and full cell pressure treated with CCA-C ensured requisite penetration and adequate dry retention (30 kg/m³ or 4% w/w). The sufficient inherent strength, seasoning property, treatability of sapwood and heartwood equivalent to 44% of radius, natural durability of heartwood, and field investigation on service performan...
A K Lahiry


Tebuconazole - A new triazole fungicide for wood preservation
1990 - IRG/WP 3629
The main cause of economic damage to timber and millwork worldwide are Basidiomycetes (brown and white rot). After testing a wide range of triazole derivatives for their effectiveness against decay fungi, Tebuconazole, a triazole compound, was selected. The physico-chemical, toxicological and ecotoxicological data of this substance are described. Tebuconazole is unleachable, light-stable, heat-sta...
R Gründlinger, O Exner


Some aspects of testing water repellents
1998 - IRG/WP 98-40113
Several test methods are used to determine the efficiency of water repellent treatments on wood. The most common are: contact angle measurement, swelling rate of samples immersed under water and, the increase in mass of wood samples with time or after a fixed period of time either fully immersed under, or partially immersed in or floating on water. In this paper, some fundamental aspects of the l...
D Lukowsky, M Farnow, T Rypstra


Clean creosote - its development, and comparison with conventional high temperature creosote
1983 - IRG/WP 3235
Pigment emulsified creosote (PEC) is presently being tested and shows considerable stability in terms of water content, pigment level, pH, viscosity, rheological behaviour and microscopy. Timber samples from several eucalypt species have been treated with PEC and side matched samples treated with conventional high temperature creosote (HTC). The PEC treated specimens showed higher weight retention...
C W Chin, J B Watkins, H Greaves


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


Controlled envelope treatments of Pinus sapwood, achieved by modifications to impregnation process and carrier solvents
2003 - IRG/WP 03-40258
Specimens of slash pine or radiata pine were treated to a target retention of 0.02% m/m permethrin with conventional light organic solvent fluids or with oil-modified fluids (Tanalith® T). Best achievable envelopes from LOSP fluids were poorly controlled, penetrating not only the target outer 0-5 mm zone (mean 0.019%, RSD 28%), but also breaking through into the 5-10 mm zone (mean 0.013%, RSD 37%...
M J Kennedy, P R S Cobham


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Utilization of coconut timber from north Sulawesi, Indonesia. Part 2: Treatability
1994 - IRG/WP 94-40025
Under tropical conditions coconut wood is quickly degraded by mold and blue stain fungi. Low density wood in ground contact is commonly decomposed by wood destroying fungi within a period of only a few months, higher density wood from the outer stem regions within 24 to 30 months (MOSTEIRO, CASIN, SERIBAN 1976; McQUIRE 1975). Moreover, according to McQUIRE (1975) green wood of lower density is hig...
R-D Peek


Practical experiments with Boracol 10 Rh used as a fungicide in the repair process after attack by the dry rot fungus (Serpula lacrymans)
1987 - IRG/WP 3458
The test is carried out in an old house in Nyhavn, Copenhagen. The roof and the walls close to were heavily attacked by dry rot fungus (Serpula lacrymans) because damage to the zinc covering the frontspice were letting in water to the wood and wall construction. An attack by the dry rot fungus is more complicated to repair compared with other wood destroying fungi because beside the damage on wood...
J Bech-Andersen


Protection of rubberwood timber. Part 1: Impregnation with boron preservatives
1989 - IRG/WP 3551
Rubberwood (Hevea brasiliensis) were treated with a 3% proprietary mixture of borax/boric acid using three different treatment schedules i.e. full-cell, full-cell to refusal and full-cell with 12 cycles of vacuum/pressure. Freshly cut samples had mean preservative retentions of 187 kg/m³, 214 kg/m³ and 178 kg/m³ respectively. Pre-air dried samples for one week had retentions of 252 kg/m³, 308 ...
L T Hong, C C K Liew


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content
2004 - IRG/WP 04-20304
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different wood claddings and the ability to maintain the appearance of the surfaces, when the wood is used in service class 3. A façade construction is exposed t...
B Lindegaard, N Morsing


Gaseous boron treatments of wood and wood products
1992 - IRG/WP 92-3691
Treatment of wood and wood products by gaseous organoborates has now been under study for about 5 years. This technique has potential for boron treatment of a wide range of substrates from solid wood through to wood composite materials such as particleboard or wet and dry formed fibreboards. The vapour treatment technique is proving to be very flexible in that it can be adapted to integrate into a...
A J Bergervoet, R Burton, K Nasheri, D R Page, P Vinden


Ammoniacal wood preservatives for use in non-pressure treatment of spruce and aspen poplar. Part 2
1984 - IRG/WP 3274
A series of thermal diffusion treatments were carried out on unseasoned white spruce (Picea glauca (Moench) Voss) lumber and air dry aspen poplar (Populus tremuloides Michx.) timbers using an ammoniacal copper arsenate wood preservative. Under the specific conditions described, certain charges of lumber met the present Canadian Standards Association Wood Preservation Committee's requireme...
C D Ralph, J K Shields


Development process of a new anti-sapstain formulation and its present status with the relevant problems
2001 - IRG/WP 01-30257
An anti-sapstain formulation, which contains 2-(thiocyanomethylthio)benzothiazol (TCMTB) and methylene-bis-thiocyanate (MBT) as active ingredients, was developed by a technical agreement with Buckman Laboratories (Memphis, TN, USA) as an alternative to chlorinated phenols for the Japanese market. The formulation was commercialized as BAM 12 years ago. As anti-sapstain treatment is commonly conduct...
K Nobashi, Y Nomura, K Tsunoda


Estimation of the impregnation degree of pine wood by the distribution analysis of active ions concentration in the cross-section
1999 - IRG/WP 99-20174
Samples in the form of pine wood rollers of diversified moisture content of ca. 50, 28 and 12% were impregnated with a water solution of the mixture type CCB with the use of the full-cell process. Moisture content was determined in individual layers from the girth to the pith. In the same way the concentrations of copper and chromium ions with the use of the spectrophotometric method and recalcula...
K Lutomski, B Mazela


Studies on the determination of the durability of wooden poles and fence posts
1982 - IRG/WP 3195
This study was carried out by the Forestry Research Institute. 5 Turkish main tree species, Oak (Quercus), pine (Pinus sylvestris), beech (Fagus orientalis) and Fir (Abies bornmülleriana) wooden poles and fence posts, were treated with Tanalith-U and creosote applying pressure process. Tanalith-U was applied by full-cell process and creosote was applied by empty cell process. Treated and untreate...
R Ilhan, O Taskin, A P Erten