Effect of fungal attack on maximum load capacity of simulated wall assemblies
2007 - IRG/WP 07-20363
The effects of moisture intrusion and fungal attack on the maximum load capacity of nailed assemblies was investigated using one white and one brown rot fungus against 4 material combinations over a 20 week period. Wetting significantly reduced the maximum load capacity of all four material combinations, while wetting and autoclaving only affected the OSB sheathing/spruce stud. The white rot fung...
N Melencion, J J Morrell


Comparison of laboratory termite test methods
2007 - IRG/WP 07-20365
Seven standardized laboratory tests with termites were evaluated. The bioassays were made in accordance with EN 117, SAA32 E08, SAA32 E09, Ebw 02, the American Wood-Preservers’ Association (AWPA) Standard E1-97, the Japan Wood Preserving Association (JWPA) Standard 11 (1) and The Protocols for Assessment of Wood Preservatives. Two different wood preservatives each in three concentrations and add...
H-U Kruschinski, W Unger, A F Preston


Marine Borer Resistance of Modified Wood - Results from Seven Years in Field
2007 - IRG/WP 07-40375
Wood modified by several methods has been tested for seven years in a marine field with high marine borer activity. Several wood modification methods were included, e.g. thermal modification (with different processes), acetylation, maleoylation, succinylation, furfurylation, treatment with methylated melamine resin and modification with reactive linseed oil derivative. Furthermore, some combinatio...
M Westin, A O Rapp, T Nilsson


Influence of ethanolamine on lignin depolymerization and copper leaching from treated Norway spruce and beech wood
2007 - IRG/WP 07-30423
Copper-ethanolamine based wood preservatives are replacing several classical copper-chromium based solutions, due to foreseen ban of chromium. Fixation of copper-ethanolamine based wood preservatives is not as good as fixation of copper-chromium ones. The main object of this manuscript was to prove, that ethanolamine is the prime reason for insufficient fixation of copper-ethanolamine formulations...
M Humar, B Bucar, M Zupancic, D Žlindra, F Pohleven


Laboratory test of blue stain control by chemicals
2007 - IRG/WP 07-30430
8 chemicals and some mixtures against Botryodiplodia theobromae Pat., Fusarium verticillioides(Sacc.)Nirenberg, Trichoderma harzianum Rifai, Trichoderma viride Pers., and Penicillium purpurogenum Stoll were conducted in laboratory by inhibition zone in the paper. The results were shown that: CBZ and benomyl as well as copper oxine alone are much high efficacy for inhibiting most of the 5 fungi tha...
Zhijuan Wang, Zehui Jiang, Mingliang Jiang, Chungen Piao


Synthesis of boric acid ammonium oleate salt for wood preservation: Leachability and termite resistance test
2007 - IRG/WP 07-30435
A new chemical compound coupling boric acid and oleic acid through a joint of ammonium salt has been produced and its synthesis followed and validated by Fourier Transformed Infra Red (FTIR). This compound named ammonium borate oleate (BAO) combining biocidal properties of boron and water repellence of fatty acids has then been studied as a wood preservative. Synthesis of BAO involved different...
F Lyon, A Pizzi, Y Imamura, M F Thevenon, S N Kartal, J Gril


Fire, flame resistance and thermal properties of oil thermally-treated wood
2007 - IRG/WP 07-40361
Oil thermal treatment, first developed by German scientists, is a promising technology for improving the durability and dimensional stability of wood for outdoor above-ground residential uses such as siding and shingles. The present authors’ previous research showed that 220ºC is an optimal treatment temperature, with 2 hours’ treatment producing wood with significantly improved moisture and ...
Jieying Wang, P Cooper


Multivariate analysis of infrared spectra for the prediction of the mechanical performance and dimensional stability of thermally modified wood
2007 - IRG/WP 07-40367
The use of calibrated mid-infrared Fourier transform (FTIR) spectroscopy for predicting the main bending strength parameters of thermally modified wood is described for the first time. The analysis is based on the handling of OSC-filtered FTIR data from control and treated wood samples, using partial least squares (PLS) regression. Sets of Norway spruce, Scots pine and Beech wood samples were th...
M M González-Peña, M D C Hale


Fire Safety of Wood Floor Assembly: Model and Full-scale Test
2007 - IRG/WP 07-20375
The present paper describes the model for the prediction of fire safety of wood floor assemblies. The model includes heat transfer model for the calculation of the flow of heat in floor assembly and structural model for the analysis of the mechanical performance of wood joists. The floor assemblies considered in this paper are constructed with nominal 2x10 (38x241mm) wood joists lined by Type X ...
H Takeda


Comparative Laboratory Leaching Test Methods to Study Post-Treatment Storage Period Impacts on CCA Leachability and Fixation in Treated Kempas (Koompassia malaccensis) Heartwood
2007 - IRG/WP 07-20376
Three laboratory leaching test methods were compared to determine the effects of different post-treatment storage fixation periods on leachability/fixation of CCA components from treated kempas (Koompassia malaccensis) permeable heartwood. End-sealed test wood blocks of permeable were treated with CCA to target retention of 5.6 kg/m3, immediately stored to fix at ambient conditions for 0 and 48 ho...
A H H Wong, H C Lai


Evaluation and identification of extractives from Iranian walnut (Juglans regia L.) by GC/MS technique for protection of non-decay resistant species
2008 - IRG/WP 08-10670
The use of walnut extractives is interest as environment friendly wood preservatives in the wood preservation industry. In this study, organic solvents were used to remove extractives from Iranian walnut heartwood samples. The solvent was removed by rotoevaporation, and Identification of chemical compounds in the Walnut extractives was done by using GC/MS technique. The toxicity of various extract...
S K H Hashemi, D Parsapajouh, H Khademi Eslam


Relationship between coating properties and their performance on treated wooden decks
2008 - IRG/WP 08-30454
Preservative treated wood benefits from the application of a surface coating to protect it from weathering (UV and rain). Different preservative formulations may affect surface properties of treated wood differently; therefore compatibility of coatings with different preservative treated wood types should be considered. This paper examines coatings characteristics and their weathering performance ...
M Ahmadinejad, P A Cooper


Field Trial of Copper Treated Moso Bamboo in Southern China
2008 - IRG/WP 08-30455
The field trial of moso bamboo treated by 9 copper preservatives for 5 years in Guangzhou was conducted in the paper. The result shown that: two ammonia based copper azole formulations F17/F18 and 1 amine copper formulation with boron F10, as well as 2 ammonia based ACQ, at the copper retention of 3.2 kg/m3 or above, have good resistant for decay and fine resistant for termites after 5 year field ...
Mingliang Jiang


Validity of above ground testing according to ENV 12037
2008 - IRG/WP 08-20379
The standard ENV 12037 for testing of treated and untreated wood (lap-joint) exposed above ground was issued in 1996 by The European Committee for Standardization. A draft for the development of the standard was presented by CEN-TC 38/WG 25/DOC N 076 in 2002. For a test to become valid the median rating of decay for untreated control replicates (Scots pine sapwood) must be equal or greater than ...
Ö Bergman, U Råberg, N Terziev


Mechanical strength of wood from the Vasa shipwreck
2008 - IRG/WP 08-20381
Samples from three ancient ship wrecks (Vasa, Elefanten, and Gröne Jägaren) and recent oak samples as reference were examined with regard to mechanical strength using the high-energy multiple impact (HEMI) - test method, which delivers the resistance to impact milling (RIM) of a material. Adoption and optimisation of the test method for the particular sample size of the wooden drilling cores was...
A O Rapp, C Brischke, C R Welzbacher, T Nilsson, C Björdal


In-service performance of wood depends upon the critical in-situ conditions. Case studies.
2008 - IRG/WP 08-20382
Wood is a unique building material, but is by nature designed to deteriorate. A detailed understanding of the factors and interactions involved are important when working with service life prediction of wooden components in buildings. Wood may experience exponential fungal degradation caused by variation in the climatic factors within a small limited area and by minor imperfection in the wooden ...
L Ross Gobakken, J Mattsson, G Alfredsen


A preliminary note on the role of moisture absorption rate in durability assessment
2008 - IRG/WP 08-20383
The rate of moisture uptake was studied in 15 wood species using vermiculite at varying moisture levels as the exposure medium. As might be expected, moisture uptake varied widely among the species studied. While some of the more durable wood species were also resistant to moisture uptake, this was not always true. The results are discussed in relation to performance in under varying environmenta...
J J Morrell, L P Francis


Propolis for wood finishing
2008 - IRG/WP 08-30464
Possibilities of use of propolis for finishing of beech, maple and spruce wood were investigated. In the first part of the paper, an overview of propolis composition, properties and applications is given. 33.6 % mixture of propolis with 96 % ethanol was prepared and the ethanol solution of soluble propolis components (29.0 %) was applied to wooden substrates. Thin propolis films were formed on woo...
F Budija, M Humar, B Kricej, M Petric


The effect of gamma radiation on selected wood properties
2008 - IRG/WP 08-40394
As an easy, fast, and effective sterilisation method, gamma irradiation changes molecular structures not only in pest’s living cells, but also in wooden cell walls. Radiation-induced depolymerisation causes significant changes in some properties of wood crucial for restoration and for laboratory testing of wood-preservative effectiveness. The influence of gamma radiation concerning total amount ...
R Despot, M Hasan, A O Rapp, C Brischke, C R Welzbacher


Effect of CCA and Tanalith E on the performance of surface finishing
2008 - IRG/WP 08-40405
Effect of CCA and Tanalith E treatment on the performance of surface finishing properties was the objectives of this study. Sapwood of scots pine, (Pinus sylvestris L.) and oriental beech (Fagus orientalis Lipsk.) specimens (300 x 100 x 15 mm along the grain) were impregnated with aqueous solution of CCA 2% and Tanalith E 2%. Surface roughness, dry film thickness, adhesion strength, gloss measur...
T Ozdemir, A Temiz, I Aydin


Cantilever bending test of furfurylated poles
2008 - IRG/WP 08-40424
Ten, 8 m long poles of Scots pine (Pinus sylvestris) were treated with furfuryl alcohol to a WPG of approximately 40 %. A bending test was performed according to the principles in the draft European standard for wooden poles, prEN 14229 - Structural timber - Wood Poles for overhead lines. The bending strength and stiffness (MOE) for the poles tested were compared to an earlier study by the Swedish Wood Preservation Committee. In the latter study untreated, CCA-treated, ammoniacal Cu-PCP treated and creosoted poles were tested in bending. These types of poles were considered not to differ in strength and stiffness. The results of the furfurylated poles fit well with the results from the previous study. The bending strength and MOE values obtained are compared to the upper and lower 95-percentile values of the results from the previous study and all poles treated with furfuryl alcohol fit within this interval.Thus, this study indicates that a treatment with furfuryl alcohol does not result in a decrease of strength or stiffness. Further testing with a larger population of poles is necessary in order to get a statistically reliable result. In addition to further demonstration of the durability, the treatment process must be optimised to ensure full sapwood penetration and measures have to be taken to avoid the serious cracking observed in this trial before furfurylation can be considered for treatment of Pinus sylvestris poles.
R Ziethén, J Jermer, A Clang


Emission Rates of Active Substances from Preserved Wood in Use Class 3
2008 - IRG/WP 08-50256
The evaluation of an active substance or a biocidal product under the Biocidal Products Directive (BPD) requires that an environmental risk assessment is carried out. The risk assessment for wood preservatives includes scenarios for preserved wood (e.g. cladding on a house), in which the predicted environmental concentration (PEC) in soil is calculated, using an emission rate for the active subs...
E F Baines


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


To decay or not to decay: An accelerated field test of the validity of the Scheffer index
2008 - IRG/WP 08-20392
The Scheffer Index was introduced in 1971 to predict the relative decay hazard of untreated wood exposed above-ground. Precipitation and temperature parameters are used in the calculation. A higher Scheffer Index value implies a greater risk of decay. An accelerated 18-month study using seven field sites with Scheffer Indices ranging from 35 to 400 and two wood types (Populus tremuloides and Pi...
G M Larkin, P E Laks


Effectiveness of MOQ® OX 50 (CCB-Oxide) wood preservative – Part 2: Field tests
2008 - IRG/WP 08-30483
MOQ® OX 50 is a chromated copper borate preservative known around the world as CCB. In Brazil, this product is the only CCB-oxide type preservative with fungicide and insecticide properties registered at the Brazilian Institute for the Environment and Renewable Resources (IBAMA) that complies with the requirements of the Brazilian and European markets for preserved wood. For over five decades, s...