Termite Response to Oil-Heat-Treated Norway spruce, Scots Pine and Eucalyptus Wood
2006 - IRG/WP 06-20325
The work here presented focused on the behaviour of subterranean termites (Reticulitermes grassei Clément) towards Oil-Heat-Treated (OHT) Norway spruce (Picea abies L.), Scots pine (Pinus sylvestris L.) and eucalyptus (Eucalyptus globulus Labill) wood, with a particular interest in the development of simple methods adequate to study the resistence of these materials to termite attack. Small test ...
L Nunes, T Nobre, C Welzbacher, A O Rapp


Enhancing the Performance of Transparent Coatings by UV Protective Pre-treatments
2006 - IRG/WP 06-30399
Most industry observers anticipate a change from copper-based preservatives to metal-free combinations of organics for residential treated wood products in North America within the next one to five years. While the chromium copper provide considerable protection against UV, metal-free formulations will need UV protection in the form of additives or coatings. While transparent coatings can be made ...
P I Morris, S McFarling


Is Field Test Data from 20 x 20mm Stakes Reliable? Effects of Decay Hazard, Decay Type and Preservative Depletion Hazard
2006 - IRG/WP 06-20327
Effects of decay hazard, decay type and preservative depletion hazard on the performance of variously preservative treated 20 x 20 x 500 mm Radiata pine and Fagus sylvatica test stakes across 13 field test sites in New Zealand and Queensland Australia were determined. Radiata pine treated with an ammoniacal copper quaternary preservative (ACQ) (1.56% m/m a.i.) and copper chrome arsenate (CCA) (...
R Wakeling


Effect of wood decay on the proportional limit of thin wood samples stressed in the bending mode
2006 - IRG/WP 06-20334
When using bending stiffness as a measure of wood decay it is advantageous to repeatedly test individual samples after they are exposed to decay fungi for varying periods of time. In order to obtain reliable results, variation in modulus of elasticity (MOE) values of the test samples that are repeatable bent to a given deflection must be considered. In this study it was shown that sound 3mm thick ...
G Li, D Nicholas, T Schultz


Re-sealing cut ends of envelope-treated softwood framing timber to protect against damage by the Australian subterranean termite Coptotermes acinaciformis: A revisitation
2006 - IRG/WP 06-20335
The claim that Australian Coptotermes acinaciformis (Froggatt) do not appear to initiate damage on timber from the end grain, thereby negating the need for treating exposed cut ends of softwood framing material (35 ? 90 mm) which has a repellent Tanalith? T envelope, was further investigated. Specimens of commercial Pinus radiata D.Don framing timber (untreated) and Pinus elliottii Englem. (untrea...
B C Peters, M Lenz, J W Creffield


The Use of Modulus of Elasticity and Modulus of Rupture to Assess Wood Decay in Laboratory Soil-Bed Test
2006 - IRG/WP 06-20338
The efficacy of wood preservatives were determined in a soil-bed test. Samples of alder wood sapwood (Alnus glutinosa subsp. barbata) (5x10x100 mm) were treated with Solutions of CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Modulus of Elasticity, modulus of rupture, mass loss and decay rate according to AWPA E7 wer...
A Temiz, Ü C Yildiz


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


Testing durability of treated wood according to EN 252. Interpretation of data from Nordic test fields
2006 - IRG/WP 06-20341
To evaluate the effectiveness of new wood preservatives intended for treated wood in ground use there is a European standard, EN 252. The test shall run for five years before any formal interpretation of the results can be made. Due to environmental concerns, the use of wood preservatives based on copper, chromium and arsenic (CCA) has been restricted in recent years. As a consequence of restrict...
M L Edlund, F G Evans, K Henriksen, T Nilsson


Performance of boron-treated radiata pine in above ground field tests in New Zealand
2006 - IRG/WP 06-30406
Boron treatment was approved for exterior, above ground use in New Zealand in 1958, provide treated commodities were painted with a three-coat paint system. Above ground tests of rail units and L-joints were established at the NZ Forest Research Institute (now Scion) between 1967 and 1980 to monitor performance of boron treatment in relation to that of untreated and CCA-treated timber. Results sh...
M Hedley, D Page


Performance of Preservative Treated Parallel Strand Lumber in Marine Exposures.
2006 - IRG/WP 06-30407
The performance ACZA treated Douglas-fir and CCA southern pine parallel strand lumber (PSL) was studied in marine exposures in Florida or Oregon. While materials treated to retentions below the recommended levels for marine exposure were attacked in Oregon, properly treated panels of either species performed well. Panels treated with these same chemicals and exposed in Florida experienced attack ...
J J Morrell, C S Love, P Merrick


Overview of European discussions on Standardisation and list of proposed standards for WPC performance qualification
2006 - IRG/WP 06-20345
The standardisation is a driving force to promote the development of Wood Polymer Composites (WPC) by giving confidence to users and consumers. In Europe, the high interest of WPC require at this time a diffusion of information concerning the performances of WPC products. The WPC performances must be assessed according relevant standards in order to qualify the intrinsic properties of WPC (mechani...
G Labat, M Vernois, T Gay


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


Standard Test Methods for Wood Preservatives by Laboratory Agar-Block Test
2006 - IRG/WP 06-20350
Wood is one of the most valuable and versatile resources for all sorts of constructional purposes. But timber in its various forms is subjected to several types of deterioration. This standard lays down the method for the laboratory determination of threshold value of wood preservatives against fungi. Most chemicals are initially tested for their ability to control decay fungi in agar-block tests....
P K Sarker, M A Rahman, M R Bulbul, T Das, G N M Ilias


Preliminary screening of a boron based wood preservative for biological efficacy (fungicidal) in treated timber
2006 - IRG/WP 06-30396
The resistance of Pinus radiata D.Don sapwood blocks, treated with a boron based preservative, to attack by five wood destroying fungi (Fomitopsis lilacino-gilva, Coniophora olivacea, Gloeophyllum abietinum (boron resistant), Serpula lacrymans and Perenniporia tephropora) was investigated. A phenyl pyrazole termiticide (fipronil) was also incorporated into the formulation to examine if its presen...
S R Przewloka, J A Hann, P Vinden


One year performance of graveyard stakes in the Northern Territory of Australia
2006 - IRG/WP 06-30398
This paper presents the one year progress performance of in ground graveyard stakes exposed to numerous termite species and decay fungi in tropical field conditions. The field study examines the efficacy of a new timber preservative formulation developed at the University of Melbourne, Australia. The biocides used in the formulation are fipronil (a phenyl pyrazole) and trimethyl borate. The pre...
B Ahmed, J Hann, S Przewloka, P Vinden, P Blackwell, P Plews


Above and Below-Ground Depletion of Copper, Chromium and Arsenic from Pinus radiata and Fagus sylvatica at Thirteen Test Sites in New Zealand and Australia
2006 - IRG/WP 06-30402
The objective was to determine the significance of site and wood species on preservative depletion for a copper chrome arsenate preservative (CCA) from 20 x 20 x 500 mm field test stakes after 5.5 and 4.5 years for pine and beech respectively. At least 5 sacrificial stakes were used to produce site means. Site and wood species had a major effect on copper, chromium and arsenic loss from CCA treate...
R Wakeling


Long term marine performance of ACZA treated Hem fir in Krishnapatnam harbour, east coast of India
2006 - IRG/WP 06-30409
The performance of Hem fir (Tsuga heterophylla) and Southern pine (Pinus sp.) treated with ammoniacal copper zinc arsenate (ACZA) and copper dimethyldithio carbamate (CDDC) at two retention levels of each preservative was assessed in tropical marine waters at Krishnapatnam harbour on the east coast of India. Panels treated with ACZA of lower loadings (23.1 Kg/m3) had failed in 38 months while the ...
B Tarakanadha, K S Rao, J J Morrell


Further discussion of biological durability assessments of acetylated wood from several European institutes
2006 - IRG/WP 06-40340
In the last decade, interest in the development of wood modification systems has increased in Europe. Alongside several industrial initiatives for heat treatments, there have also been scaling up and pilot plant projects for chemical wood modification. Between 2000-03, the European Commission funded the "Thematic Network on Wood Modification". This paper features a re-evaluation of work undertaken...
D Jones, W Homan, F Bongers


Effect of fumigation with Sulfuryl Difluoride on wood inhabiting fungi, a laboratory test
2006 - IRG/WP 06-30410
Special methods are necessary for the control of wood destroying organisms in the preservation of monuments and historic buildings because of the conservation of their originality and uniqueness. The control of wood destroying organisms can be realized with conventional liquid wood preservatives or alternative methods. One of these methods is the fumigation. One fumigant, which was in the past of...
A Pfeffer, W Unger, G Fröba, G Binker


Performance evaluation of Borax: Boric Acid treated Green bamboo through new VAC-FRI and conventional processes
2006 - IRG/WP 06-40327
Amongst giant arborescent grass bamboo is the only versatile member containing lignocellulosic materials like wood. Therefore it offers almost parallel uses where wood is traditionally an established material. The wood scarcity, environmental role of our natural forests, longer rotation cycle of plantation species, ban in felling, the ever growing utilization demands of wood to the tune of 3.2 mil...
S Tripathi, S N Nautiyal


Wood plastic composites from modified wood. Part 2 - Durability in laboratory decay tests
2006 - IRG/WP 06-40353
The decay resistance of wood plastic composites, WPCs, was tested according to modified versions of AWPA E10 (soil-block test) and ENV 807 (tests in three un-sterile soils, terrestrial microcosms, TMCs). The WPC materials were conically extruded profiles with 30% polypropylene content. The 70% wood content was untreated Scots pine sapwood, acetylated pine and heat treated Norway spruce, respective...
M Westin, P Larsson Brelid, M L Edlund, G Alfredsen


Laboratory Leaching Tests to Study the Effects of Post-Treatment Storage Periods on CCA Leachability and Fixation in Treated Permeable and Refractory Malaysian Hardwoods
2006 - IRG/WP 06-50240
The biological resistance and environmental safety of CCA-treated wood relies on the extent of post-treatment storage fixation of CCA in wood prior to being utilized. A study on the comparative leachability (fixation) of CCA-treated refractory and permeable heartwoods of 3 Malaysian hardwoods subjected to different post-treatment storage (fixation) periods of up to 4 weeks, at 2 laboratory leachin...
A H H Wong, H C Lai, N P T Lim


Current state of world standardization in the toxicometric methods for testing of wood preservatives
2007 - IRG/WP 07-20354
The paper presents an outline of the history of forming standardized toxicometric methods for testing of wood preservatives in the world during last 100 years. Numerous studies resulted in three main methods which are currently used for official and basis assessment of biocides: - agar-block method in Europe (EN 113); - soil-block method in the USA and Pacific countries (ASTM D 1413); - modifi...
J Wazny


A roadmap for performance-based specification of wooden components based on service life prediction
2007 - IRG/WP 07-20351
The need for an unified and harmonised system for performance classification and specification of wood and wood-based products in Europe emanates from requirements of users and the European Construction Products Directive, CPD. A road to a feasible specification system is outlined. Exposure-related performance prediction was worked out as a key task on the way to product specification. Therefore s...
C Brischke, A O Rapp


Accelerated Above-ground Testing of Wood Preservatives
2007 - IRG/WP 07-20358
The Canadian wood preservation industry is interested the introduction of new preservative formulations, some of which are intended only for above ground uses. Canada’s Pest Management Regulatory Agency requires data from field tests under Canadian conditions but these can take many years to generate results. Forintek has therefore developed an accelerated above ground test, under contract to a ...
P I Morris, S McFarling