The more important wood-destroying insects found in buildings in Poland
1974 - IRG/WP 128
In the different regions (voievodships) of the country Anobium punctatum and Anobium pertinax were to be found in the range of 47.7 to 63.5%. These insects were the main pests in urban buildings. In the second place came Hylotrupes bajulus occurring in the range of 25.9 to 45.1%. The other insects were to be found within the limits of 0.1 to 10.0%; only in a single instance did the amount reach 24...
J Dominik, J Wazny, M Czajnik


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


How to determine what is a realistic emission from treated wood - basic reflections
1998 - IRG/WP 98-50105
Emissions from treated wood occur by evaporation and by leaching. Up to date by far more experience exists on leaching tests than on evaporation test. The methods applied will be of interest to give answers to the questions about the quantity of possible emissions. Standardisation on leaching started very early. One of the first attempts to quantify the effect of leaching on the remaining efficacy...
H Willeitner, R-D Peek


Work program of CEN/TC 38 (January 1994). Durability of wood and derived materials
1994 - IRG/WP 94-20019
R Hüe


The most important wood-destroying insects in various countries (Results of questionnaire)
1981 - IRG/WP 1136
M-M Serment


New conception for shortering the duration of fungitoxic test on wood preservatives. Part 1: State-of-art
1994 - IRG/WP 94-20044
The review of agar-block and soil-block methods published during 90 years focused of shortening the duration of fungitoxic test of wood preservatives is presented. Special attention was given to miniaturisation of wood specimens....
J Wazny, P Witomski


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


Wood extractive concentration and sem examination of pretreated southern yellow pine wood chips with blue-stain fungi for mushroom production
2001 - IRG/WP 01-10407
Mushroom-producing white-rotting basidiomycetes either do not colonize or else colonize very poorly on freshly prepared southern yellow pine wood chips. This study evaluates the resinous extractive content of southern yellow pine before and after treatment with colorless mutant blue-stain fungi. The blue-stain fungi penetrate into the sapwood of southern yellow pine and utilize nonstructural resin...
S C Croan, J Haight


The effects of heat treatment on anatomical changes of beech wood
2004 - IRG/WP 04-40284
The effects of heat treatment on anatomical changes of beech wood (Fagus orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2x2x3 cm and than conditioned at 25 °C and 65 % relative humidity for 3 weeks. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and ...
Ü C Yildiz, Z Gerçek, B Serdar, S Yildiz, E D Gezer, E Dizman, A Temiz


Bacterial wood degradation by a pure culture
1995 - IRG/WP 95-10093
A single-celled bacterium isolated from lake water yielded cell wall degradation in Scots pine sapwood samples. The bacterium attacked all cell wall layers in one month of laboratory culture. It was identified as Aureobacterium luteolum....
O Schmidt


List of Members of IRG and contributing workers proposed for membership in IRG/WP/ - I - Sub-group 5
1976 - IRG/WP 154
S Cymorek


Wood-destroying Rhinotermitidae (Isoptera) in the oriental region
1984 - IRG/WP 1236
Species of the family Rhinotermitidae are important wood-destroying termites. From the Oriental zoogeographical region, 85 species of the family are reported of which some are wide spread and cause extensive damage to wood, wooden articles and other cellulosic products. The distribution, biology, ecology and pest status of the important wood-destroying species, in the Oriental region, are given in...
O B Chhotani


Metal carboxylates for wood pest control
1996 - IRG/WP 96-30109
Metal carboxylates have been used as wood preservatives for more than fifty years. Predominantly salts of naphtenic acids have been commercially applied so far. They have water repellent as well as fungicidal and insecticidal properties. In the last years, metal carboxylates of saturated fatty acids were introduced. Fatty acids with 7-10 carbon atoms already have fungicidal activity by themselves....
F Pohleven, M Petric


Risk assessment and the approval of wood preservatives in the United Kingdom
1995 - IRG/WP 95-50040-23
An approval system operates in the United Kingdom (UK) for the regulation of wood preservatives. The regulatory authority uses a risk assessment approach to evaluate how far the potential for harm to people and the environment from wood preservatives is likely to be realised in practise, and hence the controls required for products to be, used safely. The evaluation for approval purposes also take...
R M Turner


36 years of wood preservative tests in Tanzania
1992 - IRG/WP 92-3731
The performanee of major wood presevatives which are used widely commereially are given. These include creosote, CCA's and 5% Pentachlorophenol dissolved in heavy industrial diesel. Tests are conducted at three ecologically different using pine stakes. Results show that the striking performance of creosote and CCA's is noticeable at above 128 kg/m³ and 16 kg/m³ respectively....
K K Murira, P F Nangawe


A method of predicting the average life of field tests on preservative-treated stakes
1977 - IRG/WP 297
The paper presents an analysis of the results of completed field stake tests on untreated and preserved timber, and develops a method of predicting the average life of incomplete stake tests on wood preservatives from the failures that have occurred so far....
D F Purslow


Biological control of blue stain on wood with Pseudomonas cepacia 6253. Laboratory and field test
1989 - IRG/WP 1380
Pseudomonas cepacia strain 6253 was tested as a biological control agent on wood samples under laboratory conditions, as well as in the field. In the laboratory this bacterium controlled blue stain on Pinus radiata, but field test were not totally satisfactory. However, after 2 months of field test, the test samples were 1/3 to 1/2 less stained then the control samples....
R Benko


Evaluation of a solid remedial wood preservative containing boron and fluorine
1993 - IRG/WP 93-30022
The fungicidal and termiticidal effectiveness of a new rod form of diffusible remedial wood preservative, containing disodium octaborate tetrahydrate/sodium fluoride and marketed as Polesaver Rod, was evaluated in laboratory tests against three species of basidiomycete fungi (Coniophora olivacea, Pycnoporus coccineus, Perenniporia tephropora) and two species of subterranean termites (Coptotermes a...
K J McCarthy, J W Creffield, L J Cookson, H Greaves


Literature survey on the permanence and distribution of salt-type wood preservatives
1969 - IRG/WP III 1B
The objective of this survey is generally to review some of the more important published work dealing with the distribution and permanence of salt-type waterborne wood preservatives in treated timber. The survey is limited to the major chrome-containing formulations and the classification system proposed by Becker (1964) has been adopted throughout. CK - chromium, copper (copper, chrome); CKA - c...
Anonymous


Interaction mechanisms of F/Cr/As/B type preservative and wood
1981 - IRG/WP 3183
The paper reports results of investigations on the fixation of the components of a F/Cr/As/B preservative in wood and its lignin and cellulosic components....
N Ermush, I Andersone


Copper binding capacity of modified wood flour
1992 - IRG/WP 92-3709
Wood flour was modified by reaction with oxidising agents and CCA preservative. The copper chromium and arsenic were removed from the CCA treated wood flour by an acid leaching procedure. The modified wood flours were allowed to react with copper acetate solution and the level of copper fixation achieved was determined. The modified wood flours had greater affinity for copper ions present in solut...
N C Milowych, W B Banks, J A Cornfield


Biological degradation resistance of pine wood treated with dimethylol compounds
1989 - IRG/WP 3528
The study reports the increase of dimensional stability and biological degradation resistance of pine wood (Pinus sylvestris L) after impregnation with dimethyloldibydroxyethyleneurea. Decay resistance was determined according to BS 838:961. Nearly complete protection against Coniophora puteana, (Schum.ex Fr. Karst) weight loss of 2-3% was shown when modification, expressed as weight gain, exceede...
C L Videlov


Removal of heavy metals from treated wood using biological methods
2005 - IRG/WP 05-50226
Heavy metals were removed from wood treated with copper based preservatives using brown-rot fungus Fomitopsis palustris. The amount of effective elements removed by treatment methods was examined. The relationship between oxalic acid concentration and the amount of heavy metals removed from each treated wood was also investigated. The relationship between fungus weight and removal rate was also in...
Dong-won Son, Dong-heub Lee


HCB - a new preservative combination for wood pole maintenance
1996 - IRG/WP 96-30122
New combination of heavy creosoted boron (HCB) applied on hardwood and softwood logs at different moisture content revealed successful diffusion of boron in all sapwoods within 7 days and in all sapwoods plus hardwoods within 15 days. The new cost effective paste sterilizes wood through diffusion and suitable for pole maintenance at groundline and above groundline e.g. cut ends, drilled holes, woo...
A K Lahiry


Isolation and identification of the fungal flora in treated wood
1976 - IRG/WP 144
J F Levy