Field Test Results after Nine Years for CCA and ACQ Preservative-treated Wood Fixed in Different Climates
2003 - IRG/WP 03-30303
During assessment of the ground contact stakes in the Norwegian test field, we have frequently found that the first visual rot attack is in the zone of the stakes, where the stakes have been in contact with each other during the fixation. These parts are usually light green, caused by the lack of light during fixation, compared to the rest of the stake surface, which has a darker colour. To inves...
F G Evans


Influence of bark damage on bluestain development in pine logs
1997 - IRG/WP 97-10197
Mechanized harvesting of conifers can lead to extensive bark damage, with the resulting wounds providing suitable entry points for bluestain fungi that are not associated with bark beetle vectors. However, the amount of bluestain colonisation can vary greatly between the different types of wound. To evaluate the effect of wound type seven different types of wounds were artificially created on fres...
A Uzunovic, J F Webber, D J Dickinson


Programme section 3, Wood protecting chemicals
1996 - IRG/WP 96-30119
IRG Secretariat


Evaluation and approval of wood preservatives in the Nordic countries
1988 - IRG/WP 2311
This paper reviews the system for evaluating and approving the efficacy of wood preservatives for industrial use currently in force in the Nordic countries Denmark, Finland, Iceland, Norway and Sweden....
B Henningsson, J Jermer


Protecting wooden structures
1980 - IRG/WP 392
Chromium-containing chemicals that effectively retard weathering of wood improve performance of subsequently applied finishes. Current work is focusing on the performance of wood-derived products (plywood, hardboard, fiberboard, particle board) after surface treatment with inorganic chemicals. The overall objective of the continuing research is to investigate new environmentally safe procedures to...
W C Feist


The present classification of wood degradation factors
1993 - IRG/WP 93-10031
Contemporary classification of biotic and abiotic wood degradation factors is presented in two aspects: etiological and simptomatical one....
J Wazny


Measurement of VOC emissions from curative treated wood: A new emission test chamber
2001 - IRG/WP 01-50166-13
A poor indoor air quality (IAQ) is now recognized as a potential factor affecting occupants health. There are three basic strategies to improve IAQ: source control, improvement of the ventilation and use of air cleaners. Usually, the most efficient way to improve IAQ is to eliminate the different pollutant sources or to reduce their emissions. In order to precisely measure emissions from building ...
F Maupetit, O Ramalho, C Yrieix


The microbiological treatment of chlorophenolic preservative in spent utility poles
1993 - IRG/WP 93-50001-24
The number of pentachlorophenol (PCP) treated poles being removed from service is increasing, but disposal options for this material are limited. Biological Degradation of the preservatives in spent poles, before disposal or reuse, offers a promising technique. The reduction of PCP in treated timber, after inoculation with PCP-degrading bacterial species, Rhodococcus chlorophenolicus and Flavobact...
A McBain, F Cui, J N R Ruddick


OECD's latest activities on wood preservatives
2001 - IRG/WP 01-50166-05
PPT-Presentation...
M Paneli


Plastic-coated marine piling in Los Angeles Harbour
1984 - IRG/WP 4105
G Horeczko


Work program of CEN/TC 38 (April 1993). Durability of wood and wood-based products
1993 - IRG/WP 93-20012
R Hüe


The use, approval and waste management of industrial wood preservatives. A preliminary report
1994 - IRG/WP 94-50033
The structure on the wood preservation through the world is heterogenous. Environmental legislation, approval policy and application practices differ in each geographical region and in individual countries. This preliminary report gives a rough estimation of the production of treated timber, the use of wood preservatives and a bief summary of environmental status of wood impregnation in selected c...
A J Nurmi


Testing wood in ground contact: An artificial soil
1977 - IRG/WP 280
This document is an interim report on the development of the artificial soil medium. It includes some information on the relationship between soil, wood and water which is of relevance in testing....
E F Baines, D J Dickinson, J F Levy


Bioconversion of wood wastes into gourmet and medicinal mushrooms
1999 - IRG/WP 99-50129
Increased wood wastes, including thinned material from stagnated and overstocked small-diameter forests, are a menace to forest health, to the sustainability of ecosystems, and to community economic viability. The objective of this study is to recycle wood wastes into value-added products, such as gourmet and medicinal mushrooms, by using the white-rot basidiomycetes, Pleurotus ostreatus, P. popul...
S C Croan


Fungal degradation of wood treated with metal-based preservatives. Part 2: Redox states of chromium
1996 - IRG/WP 96-10164
Concerns have arisen about the leaching of heavy metals from wood treated with metal-based preservatives, such as chromated copper arsenate (CCA). Of particular concern is the toxic redox state of chromium and arsenic in aging and decayed CCA-treated wood. Generally, hexavalent chromium is more toxic than trivalent chromium and trivalent arsenic is more toxic than pentavalent arsenic. The desired ...
B Illman, S Bajt, T L Highley


The effective control of moulds on freshly impregnated wood
2004 - IRG/WP 04-30352
Beside natural timber it is known, that moulds can also groth at the surface of impregnated wood. This material shows “defects” like resistant dark spots or color changes and causes complaints. During the last years, the problem by moulds seems to increase. Laboratory studies were carried out to show the effect of impregnations against moulds. Wood samples (Pinus sylvestris L.) were impregn...
G Cofta, K Lutomski, P Jüngel


A review of environmental emissions from building and construction materials in comparison with preserved wood
2005 - IRG/WP 05-50224-11
A review of the public domain literature concerning emissions to the environment from materials which are used in the construction of buildings (e.g. Concrete, Asphalt, Galvanised Steel), in comparison with preserved wood, and a review of the approaches taken by the construction sector in assessing the risk from environmental emissions, in comparison with the approaches taken by the wood preservat...
E F Baines


Disposal of treated wood - Canada
1990 - IRG/WP 3563
It is estimated that treated wood removed from service each year in Canada contains about 16,000 tonnes of creosote, 1000 tonnes of pentachlorophenol and 245 tonnes of CCA or ACA. The amount of CCA treated wood for disposal is expected to increase more than ten-fold by the year 2020. At present, most treated wood is disposed of in landfills, burned (creosote only) or recycled as other products. Ot...
P A Cooper


A field test with Benzotar, an industrial residue, as a wood preservative
1985 - IRG/WP 3349
Benzotar, a residue of production of benzoic acid, was tested in field as a wood preservative. Results, after 6.5 years of exposure, showed that this product presents properties that improve the performance of wood in ground contact. This paper describes these results and presents a discussion an some aspects of its potential utilization in Brazil....
S Milano, L R Silva


The Pilodyn instrument as a non-destructive tester of the shock resistance of wood
1978 - IRG/WP 2107
A new non-destructive shock resistance tester, the PILODYN, has been developed. The instrument measures the fracture surface area created by a constant amount of energy. It operates by shooting a blunt pin into wood by an exact amount of energy. The penetration depth is read on a scale. A wide field of application is open to a non-destructive shock resistance tester such as: 1) assessment of the r...
P Hoffmeyer


Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


Environmental risk assessment of preservative treated wood
1998 - IRG/WP 98-50101-19
This paper reviews the status of the environmental risk assessment of preservative treated wood and confirms the distinction between the risks presented by wood preservatives and preservative treated wood. The paper proposes a tiered approach to risk assessment and discusses the rationale. Flowcharts are presented which summarise the tiered approach to risk assessment, show the tests required, and...
E F Baines, S J Davis


Detection of trace organics by ion mobility spectrometry
1990 - IRG/WP 3635
Ion Mobility Spectrometry (IMS) is a time of flight analytical technique that is suited to detect chemicals in the low parts per billion range. Some of the advantages of IMS are: operation at atmospheric pressure, fast response time (0.1-10 sec), and the ability to characterize individual chemical species in complex matrices without any prior sample preparation. In this paper, the utility of IMS i...
A H Lawrence


Checking of sodium pentachlorophenate fixation in wood
1990 - IRG/WP 3620
In order to estimate the volatilization of sodium pentachlorophenate from treated wood, wood samples treated with pentachlorophenate were analysed after various durations of an EN 73 weathering The results giving no clear evidence of volatilization, treated wood samples were put in a test chamber with precise climatic conditions, the air used in the experiment being analysed. The pentachlorophenat...
M Lamour, H Sageot


Methods of assessing decay in poles in service with the Pilodyn wood tester
1978 - IRG/WP 2107 A