IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3045 documents. Displaying 25 entries per page.


Buffered Amine Oxide Treatment Systems for Ammonical Copper Wood Preservatives
2014 - IRG/WP 14-40685
Wood is the most versatile, practical and sustainable building material in the world. In modern countries, wood is a well-managed renewable resource that has a small carbon footprint. Wood does suffer from a lack of durability against invasive organisms such as insects and fungi. Steel, aluminum and composites have emerged as viable alternative building materials. These sectors market the defi...
R W Clawson Jr


Laboratory Study of Relative Leachability of Chromated Copper Arsenate Preservative from Treated Woods among Soil Types of Sarawak
2014 - IRG/WP 14-50307
Wood and soils are important natural resources from the environment and serves mankind well respectively as structural materials and natural platform erecting such materials. With shortfalls of naturally durable timber species for protected in-ground uses under Malaysian environments, Chromated Copper Arsenate (CCA) treated woods are widely used instead, incurring serious potential threats of pres...
A H H Wong, P K F Chong


Ammoniacal zinc borate as solid wood preservative
2014 - IRG/WP 14-30659
Zinc borate, well-known for its fungicidal, insecticidal and flame resistant properties, is widely used in manufacture of lignocellulose particle board. This form of borate is the least water soluble form available providing advantages as well as disadvantages for use as a wood preservative. This form does not leach from wood under conditions of high humidity, but it is also very difficult to appl...
C Ibáñez, C Mantero, A Ibarra, M Rabinovich


Douglas-fir PSL Treated with Oilborne Copper Naphthenate – Treatment Experience & Efficacy
2014 - IRG/WP 14-40687
Treating characteristics, field stake efficacy and the results from treatment trials for oilborne copper naphthenate (CuNap) and Douglas-fir parallel strand lumber (PSL) are summarized in this paper. Treatment with a P9 Type-C based solution in laboratory tests showed full cross section penetration of large cross sections could be achieved. Commercial treatment trials using a P9 Type-A solution ...
G P Merrick


Influence of the moon phase on durability against wood decay fungi of Larix kaempferi and Pseudotsuga menziesii wood species
2015 - IRG/WP 15-10836
The analysis of the natural durability of wood is essential when establishing the level of protection required, depending on the designated end use of timber. On the other hand, there is a popular belief based on the influence of the moon phase in felling timber, recommending the waning moon as the optimum for felling trees. In fact, some companies now offer among their products, sawn timber felle...
M T Troya, M Conde, M J Barriola, F Llinares, V Dorronsoro


Interpretation of moisture monitoring data - Relevance of moisture content thresholds for fungal decay
2015 - IRG/WP 15-10839
It is widely accepted that besides temperature wood moisture content (MC) is the key factor when it comes to durability of wooden structures exposed to weathering. Many approaches to predict the service life of wooden structures have therefore been based on using wood MC as one major input-variable to develop dose-response relationships between material climate and decay response. However, to impr...
L Meyer, C Brischke


Investigations on the durability of several Congo basin wood species
2015 - IRG/WP 15-10840
The sawdust of ten wood species was studied to assess their natural resistance to decay. The extractives and lignin contents were primarily determined (between 2.7-16.0% and 26.8-35.9% respectively) to give an overview of the chemical distribution. Then, a phytochemical screening (colorimetric methods) characterized the different chemical functional groups in all extracts studied. Antioxidant act...
S Mounguengui, J-B Tchinda Saha, M Kor Ndikontar, S Dumarçay, C Attéké, D Perrin, E Gelhaye,


Chemical composition of extractives of different wood compartments of Pinus merkusii and their potential implication in wood durability
2015 - IRG/WP 15-10841
Amounts and nature of extractives differ strongly according to the compartment of wood and to the nature of the wood species. Previous studies reported that knotwood of several European Pinus sp. contains extractives contents much higher than stemwood consisting mainly of lignans which may find valuable applications in cosmetic, nutraceutic or pharmaceutic sectors. Different explanations have been...
A Wijayanto, S Dumarçay, R Kartika Sari, W Syafii, P Gérardin, C Gérardin-Charbonnier


Effects of UV Radiation on Melanization and Growth of Fungi Isolated from Weathered Wood Surfaces
2015 - IRG/WP 15-10842
This research tests the hypothesis that fungi isolated from weathered wood will respond to elevated levels of UV radiation by increasing their melanin production. To test this hypothesis, we measured the melanin production and mycelial color of Aureobasidium pullulans and Cladosporium cladosporioides, before and after the fungi were grown under artificial UV, visible light and complete darkness. T...
V A Hernández, P D Evans


Short-term protection of palm wood against moulds and decay fungi by environment-friendly organic acids
2015 - IRG/WP 15-10843
Felled palm trunks are susceptible to fungi as long as their moisture content is above fibre saturation. During this period, it has to be protected against moulds and decay fungi. The study tested environmental-friendly organic acids for their protecting efficiency. Small samples of Date palm (Phoenix dactylifera) and Oil palm (Elaeis guineensis) wood were treated with weak organic acids and subse...
M Bahmani, O Schmidt


Glutathione transferases and wood extracts
2015 - IRG/WP 15-10845
Wood rotting fungi have developed an efficient detoxification system allowing them to be well adapted to their way of life, these fungi generating and encountering potential toxic compounds during wood degradation. Belonging to this detoxification network, glutathione transferases are particularly extended in these fungi and their presence could reflect the chemical environments encountered by the...
A Deroy, F Saiag, Z Kebbi-Benkeder, N Touahri, M Morel-Rouhier, F Colin, S Dumarcay, P Gérardin,


Natural durability of Chilean commercial wood exposed to the action of marine borers
2015 - IRG/WP 15-10849
Results of field experiences of natural durability of ten commercial wood, exposed to the action of Bankia martensi (Stempell) in the South coast of Chile are presented. Tested species were seven types of native wood and three types of exotic ones. Test specimens of standard dimension of 0.02 x 0.045 x 0.23 m with three replications by species were used. The degree of attack was determined accord...
R Carmona C, C Osorio, A Almuna


An update on durability of New Zealand grown timber
2015 - IRG/WP 15-10851
Classification and predication of in-service performances of naturally durable timber is much more difficult than preservative treated timber due to the variability of wood properties within and between trees of the same species and the variable nature of the hazard to which the timber will be exposed. A combination of field test and in-service testing has been used to classify the suitability of ...
D Page, T Singh


Penetration of phenol formaldehyde (PF) resin into beech wood studied by light microscopy
2015 - IRG/WP 15-20558
In this study, we examined the distribution and penetration depth of phenol-formaldehyde (PF) resin into wood specimens by light microscopy (LM). Two PF resins from different producers, of concentrations 9, 18 and 27 wt % in water, were vacuum impregnated into European beech wood (Fagus sylvatica) blocks of 15x25x50 mm³. The presence of chemical agent in the wood was carried out by way of their i...
V Biziks, S Bicke, H Militz


Influence of artificial and natural weathering on water exclusion efficacy of wood
2015 - IRG/WP 15-20559
Water exclusion efficacy (WEE) is one of the most important properties of wood that contributes to the overall performance of naturally durable wood species in outdoor above ground applications. WEE is in strong correlation with moisture dynamics of wood, its hydrophobicity and can indicates susceptibility against wood decay fungi. Despite of the importance of this parameter, WEE is not completely...
M Žlahtič, M Humar


Applicability of wood durability testing methods to bio-based building materials
2015 - IRG/WP 15-20561
It is well known that organic materials may be susceptible to attack from a range of fungal organisms and any bio-based material used in locations where there is the possibility of microbiological activity must be expected to be able to withstand or prevent such attack. There are a wide range of test methods and standards in place to test susceptibility although most of these test individual compo...
S F Curling, B K Stefanowski, E Mansour, G A Ormondroyd


Durability of treated wood Corymbia torelliana and Eucalyptus grandis x Eucalyptus urophylla against subterranean termite
2015 - IRG/WP 15-20563
This work aimed to analyze the durability of woods against termite Nasutitermes corniger Motsch. Fence posts from this study were collected in Pinheiros, north of Espírito Santo state, Brazil. Used the Corymbia torelliana and Eucalyptus grandis x Eucalyptus urophylla species with 11 and 9 years, respectively and plant spacing of 3.00 x 2.00 m. Were used 72 samples from discs removed the 0.50 m of...
D Junior Verly Lopes, J Benigno Paes, P N de Medeiros Neto, G dos Santos Bobadilha


Acceptance levels of surface disfigurement - tolerance to defects of coated wood
2015 - IRG/WP 15-20564
Service life planning (PSL) has become an important issue in performance based building and substantial progress has been made in recent years. The role of predicting the aesthetical service life of wooden building components has been underestimated for quite long time but is recently attracting more and more notice. It is influenced by numerous factors such as discoloration, fading, flaking, crac...
C Brischke, P Kaudewitz


The potential of 2D NIR imaging for wood protection research
2015 - IRG/WP 15-20566
Investigating wood and wood-based materials using infrared spectroscopy has since long been explored. Recently, image-based systems have been developed that are used in food and pharmaceutical industries for rapid screening. Such hyperspectral cameras are able to collect spatial and spectral information simultaneously, resulting in a volume with a spectral profile for each pixel of the image. We p...
J Van den Bulcke, N Defoirdt, W Li, J Van Acker


Introduction of the COST FP 1303 Cooperative Performance Test
2015 - IRG/WP 15-20567
COST Action FP 1303 “Performance of bio-based building materials” successfully started in October 2013 and an ambitious program was set up for the four year programme. COST Actions provide an excellent opportunity for collaborative research, e.g. in the frame of Round Robin tests. The idea of this respective test was to distribute a fairly simple test set up to as many places in Europe as poss...
M Humar, C Brischke, L Meyer, B Lesar, N Thaler, D Jones, S Bardage, C Belloncle, J Van den Bulcke, J M Abascal, G Alfredsen, D Baisch, B Brunnhuber, G Cofta, E Grodås, E Frühwald Hansson, M Irle, H Kallakas, J Kers, M Klamer, P Larsson Brelid, A B Maider, K C Mahnert, E Melcher, R Möller, M Noël, L Nunes, G A Ormondroyd, S Palanti, N Pfabigan, A Pilgård, A O Rapp, P Schumacher, E Suttie, T Teppand, M Touza, J Van Acker


Interaction between Aspergillus niger fungus and other filamentous fungi on salt-agar medium and their growth on natural wood and wood treated with fungicide
2015 - IRG/WP 15-20569
Aspergillus niger (An) is very often used alone or in mixture with other filamentous fungi of the genus in testing biocides in disinfection procedures, safety, hygiene, medical fields as well as for testing resistance of wood and wood-based materials to moulds. Softwood species as well as hardwood are overgrown with An fungus very easily, causing drop of mainly the aesthetic value of wood product....
A Fojutowski, A Kropacz, A Koziróg


Wood protectors to control Bursaphelenchus xylophilus
2015 - IRG/WP 15-30661
Bursaphelenchus xylophilus, the pine wilt nematode (PWN), is a quarantine organism with a high potential to damage Conifer forests in Europe. The European Union is concerned in the protection of forest stands from the propagation and dispersion of this pathogen. In this line, the current control measures have been unsuccessful in preventing the dispersion of this organism, as it continues to be de...
M T Troya, C S Arcos, A Navas, L Robertson, M Conde, F Llinares


Building solid foundations to support market growth of preserved wood in the UK – treatment quality, product approval and the largest national field trial of preservative treated wood in 50 years
2015 - IRG/WP 15-30662
The Wood Protection Association (WPA) has just commissioned Britain’s largest ever durability trial of home grown timber, having contracted Building Research Establishment (BRE) to conduct a long term controlled field trial of sawn and pressure treated British Softwood posts at two sites with differing soil conditions. This large scale Field Trial is the last of an innovative and substantial thr...
E Suttie, G Ewbank


Factors Affecting Performance of Preserved Wood Decking Against Decay Fungi
2015 - IRG/WP 15-30663
Decking is the largest market for residential preserved wood in the United States. Preserved decking must be resistant to colonization by decay fungi initiating from spores, and occasionally from mycelia due to elevated soil levels or adjacent untreated wood. The most vulnerable parts of a preserved wood deck are untreated, or under-treated, wood that becomes exposed by field cuts and checking. Fi...
R Stirling, P I Morris


Effect of a wood stabilizer on checking of red oak log sections
2015 - IRG/WP 15-30664
Abstract: Reduced check development and dimensional stability can be important attributes in wood products used for decorative applications. The potential for using a silane-based stabilizer product to reduce checking was assessed on red oak stem and log sections. Pressure treatment produced the largest uptakes, although the levels suggested that the solution had failed to completely penetrate th...
C S Love, J J Morrell


Previous Page | Next Page