Gaseous preservative treatment of wood
1990 - IRG/WP 3631
A recent development in processing wood with a gaseous preservative means that dry, treated wood can be produced in under 30 hours with the benefits of product diversification, faster stock turnover and the ability to respond to short term demand. About 400,000 m³ of wood are treated each year in New Zealand with boron salts to protect from borer infestation. Traditionally this treatment is effec...
R Burton, A J Bergervoet, K Nasheri, P Vinden, D R Page


Environmental characterisation of retification process by-products (liquid and gaseous wastes)
2005 - IRG/WP 05-50224-10
In order to reduce environmental risks during the service life of the treated wood and to find new alternative developments on the durability of wood, some research and technology development have been made on thermal treatment. The retification process is one of these processes. The retification process induces chemical modification of the lignin and cellulosic components and modifies the intrins...
G Labat, E Bucket, S Legay, C Yriex, P Marchal, E Raphalen, M Vernois, R Guyonnet, H Besset, E Fredon), G Vilarem, L Rigal, C Raynaud


Wood preservatives treatment of black spruce
1997 - IRG/WP 97-40092
A representative sample of black spruce logs from Central Newfoundland was harvested and processed to dressed 2"x4" lumber. Over 400 pieces of lumber were then incised and treated with ACQ preservative in a semi-industrial retort. 9 charges of 20 samples were used to determine treating parameters and 11 charges of 20 pieces were treated using the optimized process. This material was inspected by a...
A R Zahora, J P Hösli


Bacterial degradation of wood cell wall: A review of degradation patterns
1990 - IRG/WP 1460
Information from bacterial degradation studies of 60's and 70's was reviewed by Nilsson in 1982. The application of electron microscopy to this area in recent years has provided much useful information and has eliminated earlier scepticism among workers about the ability of bacteria to degrade lignified wood cell walls. Studies using transmission electron microscopy together with...
A P Singh, J A Butcher


Detoxification of salt impregnated wood by organic acids in a pulping process
1993 - IRG/WP 93-50012
The paper descibes a novel method to detoxify pine wood (Pinus silvestris L.) treated with CCB-, CCF- CC-, and Cu-HDO-type salt preservatives. In the process of biological detoxification organic acids produced by strains of Antrodia vaillantii and other brown rot fungi are used for the dissolution of the previously fixed inorganic compounds. These findings are the basis for applying an acid pulpin...
I Stephan, H H Nimz, R D Peek


Free radical process controlled by manganese peroxidase and lipid-related metabolites produced by Ceriporiopsis subvermispora
2001 - IRG/WP 01-10412
Ceriporiopsis subvermispora, a specific lignin-degrading fungus produced free unsaturated fatty acids (USFAs) including 9,12-octadecaienoic asid, together with saturated fatty acids (SFAs) at an incipient stage of cultivation on wood meal cultures. In prolonged cultivation period after two weeks, the amount of intact fatty acids decreased with increasing in organic hydroperoxide and TBARS producti...
T Watanabe, M Enoki, S Sato, Y Honda, M Kuwahara, N Shirai, K Messner


Utilisation of carbohydrates by stain fungi in agar culture
1998 - IRG/WP 98-10248
Stain fungi are often defined by their ability to utilise the starch and free sugars found in ray parenchyma cells, and their inability to utilise other wood constituents. However, several species of stain fungi produce bore holes in wood cell walls. This suggests that enzymatic activity capable of degrading structural polysaccharides and/or lignin is associated with the growth of the appressorium...
J Snow, P Vinden, S M Read


Degradation of woods by obligately anaerobic fungi
1990 - IRG/WP 1452
Little is known about the processes occurring during the degradation of wood by obligately anaerobic fungi. When woods from a range of hardwood species were incubated for 11 days with a strain of the Chytrid Neocallimastix frontalis many of the woods were measurably fermented; Fagus sylvatica (23%) was the most highly degraded. Microscopic examination of Populus tremuloides wood after incubation w...
K N Joblin, G E Naylor


A Novel Type of Multiple Cavity Attack in Wood Cell Walls of Heat-treated Timber Exposed in Seawater – Preliminary Observations
2004 - IRG/WP 04-10523
Samples of untreated and heat-treated Norway spruce and Douglas fir were submerged in Langstone Harbour, Portsmouth for 4 years at a depth of ca. 0.3 metres. The heat-treated samples had been prepared using the Plato process. Samples were initially assessed for the severity of marine borer damage and were then examined microscopically for evidence of microbial decay. Longitudinal and transverse wo...
R A Eaton, C Björdal, T Nilsson


The risk assessment process. Point of view of a biocide manufacturer [Évaluation du risque. Point de vue d'un fabricant de biocide]
1990 - IRG/WP 3568
Risk assessment is an inherent part of our everyday lives. The risk assessment equation combines Hazards and Exposure. For the Wood Preservation Industry, the hazards may be characterised by the toxicity a the ecotoxicity of chemicals and the exposure by the identification of exposed people, of the exposure routes and exposure frequency. To quantify the exposure, good co-operation is required betw...
D Baur


Exclusion of anions from the wood cell wall
1991 - IRG/WP 3661
Anionic components of wood preservatives and fire retardants such, as arsenates and phosphates, equilibrate at much lower concentrations in the cell wall bound water than in the free solution in the cell lumens. A degree of anion exclusion is expected in wood, due to the Donnan membrane effect. Fixed anions in the wood cell wall, produced by pH-dependent dissociation of the weak acid groups in woo...
P A Cooper


A new process for in situ polymerization of vinyl monomers in wood to delay boron leaching
1998 - IRG/WP 98-40110
Efforts were accelerated on effective use of boron compounds in wood preservation owing to their environmentally safe characteristics and relatively low costs in addition to their well-known high bioactivity and fire resistant properties. Although having these unique favorable properties, they are readily leachable from treated wood at humid conditions. Therefore, they had limited market for exter...
M K Yalinkilic, W Dwianto, Y Imamura, M Takahashi


Penetration of oil-borne preservatives in American elm
1975 - IRG/WP 355
Pressure treatment of elm posts and cants by Rueping schedules resulted in erratic penetration. Instead of the expected gradual decrease in retention from surface inward in posts, inner zones frequently contained more preservative than the surface quarter inch. Heartwood was found penetrated when sapwood was not. There were numerous skips in treated zones. The prevalence and possible causes were i...
E A Behr


Chitin synthetase activity in cellular fractions of wood-decay fungi
1992 - IRG/WP 92-1524
This study was an attempt to explain the variability of in vivo sensitivity of wood decay fungi to the chitin synthetase (CS) inhibitor, polyoxin, by comparing CS distribution in cellular fractions. The five species studied were the brown-rot fungi Coniophora puteana, Gloeophyllum trabeum, Fibuloporia vaillantii, and the white-rot fungi Schizophyllum commune and Ganoderma applanatum. The CS activi...
B R Johnson, S C Croan, B Illman


Conforming to European standards on preservative treatment
1998 - IRG/WP 98-20150
New European standards require that specifications for the preservative treatment of timber are written in terms of the penetration and retention of preservative within the treated commodity that result from the treatment process. In order to check compliance with this type of specification, suitable methods of quantitative analysis must be available. This paper presents the results of a study by ...
E D Suttie, R J Orsler


The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick


Amenability of radial permeability of Sitka spruce (Picea sitchensis (Bong.) Carr.) as affected by aspects of cell ends in uniseriate ray parenchyma tissue
2003 - IRG/WP 03-40252
The principal objective of this article was to recognise and understand the amenability of ray parenchyma cell ends (end platform) in uniseriate ray tissue to influence the radial permeability of Sitka spruce (Picea sitchensis (Bong.) Carr.) by examination of most (Queen Charlotte Islands in Rhondda, South Wales) and the least (South Oregon in Dalby, North-East England) seed origins that grown in ...
I Usta, M D C Hale


A combined method for drying and preserving wood in a single step process
2000 - IRG/WP 00-40183
Based on a convective dryer, this process allows to dry and treat wood blocks with diffusible preservatives in the same time. A boric acid solution (heated to fix the wet temperature of the system) is pumped and introduced in the flow system through a venturi, where the air coming back from the drying cell also arrives. The role of the venturi is to create a dispersion of boric acid solution micro...
O Colin, C Dupuis, E Mougel, A Zoulalian, M-F Thévenon


Development of a novel treatment process and its applications
1998 - IRG/WP 98-40111
An efficient treatment process called "Isostatic Compression Recovery (ICR) Process" for impregnating liquids into wood has been developed. The process comprises steps of isostatic compression of wood in the liquid at temperatures above its softening temperature and subsequent recovery of its original volume under liquid pressure. A large amount of surrounding liquid is absorbed into the wood in t...
T Arakawa, M Funato, A Hoshino, T Muraki


Time-of-Flight Secondary Ion Mass Spectrometry Analysis of Polyethylene Glycol Penetration into Wood Cell Walls
2006 - IRG/WP 06-20328
Penetration of high molecular weight polyethylene glycol (PEG) into wood cell walls was investigated in red pine. PEG of different molecular weights (1000, 8000 and 20000) was labelled by bromination and treated samples were analyzed on Time-of-Flight Secondary Ion Mass Spectrometry (TOF-SIMS) in dynamic mode. Both negative and positive spectra of the samples were collected in high spatial (bunche...
D Jeremic, P Cooper, P Brodersen


Overview of European discussions on Standardisation and list of proposed standards for WPC performance qualification
2006 - IRG/WP 06-20345
The standardisation is a driving force to promote the development of Wood Polymer Composites (WPC) by giving confidence to users and consumers. In Europe, the high interest of WPC require at this time a diffusion of information concerning the performances of WPC products. The WPC performances must be assessed according relevant standards in order to qualify the intrinsic properties of WPC (mechani...
G Labat, M Vernois, T Gay


CCB Preservative treatment of split muli (Melocanna baccifera ) bamboo by soaking process
2006 - IRG/WP 06-40336
This study was carried out in order to investigate the retention of chemicals inside the split muli ( Melocanna baccifera ) bamboo after preservative treatment by soaking process. Treatment with 10% aqueous solution of CCB (copper-chrome-boron) was applied in split bamboo of two sizes (1/4 part and 1/8 part) at three different moisture contents and five time periods (24, 48, 72, 96, 120 hours). It...
K Akhter, M H Chowdhury


Further discussion of biological durability assessments of acetylated wood from several European institutes
2006 - IRG/WP 06-40340
In the last decade, interest in the development of wood modification systems has increased in Europe. Alongside several industrial initiatives for heat treatments, there have also been scaling up and pilot plant projects for chemical wood modification. Between 2000-03, the European Commission funded the "Thematic Network on Wood Modification". This paper features a re-evaluation of work undertaken...
D Jones, W Homan, F Bongers


Wood furfurylation process development. Part 1: Oscillating Pressure Method
2007 - IRG/WP 07-40376
Furfurylated wood (wood modified by furfuryl alcohol) has over the last years gained marked shares from both tropical wood and conventional preservative treated wood and this has, in turn, generated several research projects concerning process development. The impregnation of spruce is well known from literature to be a difficult task. Furthermore, the sapwood of Scandinavian-grown Scots pine is a...
E Larnøy, M Westin, B Källander, S Lande


Wood furfurylation process development. Part 2: Lowry impregnation trials
2007 - IRG/WP 07-40377
The objective was to evaluate whether Lowry-impregnation of Scots pine with FA100-mix, instead of the FA40-mix, would lead to similar or slightly higher WPGs and to investigate any potential changes in penetration pattern. The results indicate that the penetration was better, also penetrating the outer zone of the heartwood. Furthermore, it was possible to reduce the WPG-levels for pine down to 50...
M Westin, E Larnøy, S Lande