IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 211 documents. Displaying 25 entries per page.


Controlled envelope treatments of Pinus sapwood, achieved by modifications to impregnation process and carrier solvents
2003 - IRG/WP 03-40258
Specimens of slash pine or radiata pine were treated to a target retention of 0.02% m/m permethrin with conventional light organic solvent fluids or with oil-modified fluids (Tanalith® T). Best achievable envelopes from LOSP fluids were poorly controlled, penetrating not only the target outer 0-5 mm zone (mean 0.019%, RSD 28%), but also breaking through into the 5-10 mm zone (mean 0.013%, RSD 37%...
M J Kennedy, P R S Cobham


The nature of osmiophilic particles and their distribution during different stages of brown and white rot decay
1983 - IRG/WP 1213
The distribution of osmiophilic particles during the course of brown and white rot decay was investigated by applying transmission electron microscopic (TEM) methods. It was found that it correlates with the brown and white rot pattern.The osmiophilic particles are produced by the fungus and are supposed to be wood rotting enzymes....
K Messner, H Stachelberger


Practical experiments with Boracol 10 Rh used as a fungicide in the repair process after attack by the dry rot fungus (Serpula lacrymans)
1987 - IRG/WP 3458
The test is carried out in an old house in Nyhavn, Copenhagen. The roof and the walls close to were heavily attacked by dry rot fungus (Serpula lacrymans) because damage to the zinc covering the frontspice were letting in water to the wood and wall construction. An attack by the dry rot fungus is more complicated to repair compared with other wood destroying fungi because beside the damage on wood...
J Bech-Andersen


Hyphal tunnelling of belian (Eusideroxylon zwageri) wood cell walls
1996 - IRG/WP 96-10152
Belian (Eusideroxylon zwageri) is highly regarded among the naturally durable Malaysian hardwoods. Visual inspections at the groundline of belian transmission poles from Sarawak, Malaysia, showed only surface decay of wood after 20 years in service. The cause of decay in belian was investigated by light and transmission electron microscopy. Light microscopy of transverse sections of surface tissue...
A P Singh, A H H Wong


Diffusion and interaction of components of water-borne preservatives in the wood cell wall
1988 - IRG/WP 3474
This study investigates the rates of diffusion and ultimate distributions of copper and arsenate components of wood preservatives in wood cell walls following vacuum treatment. Adsorption studies of copper on red pine (Pinus resinosa) and trembling aspen (Populus tremuloides) wood confirm the importance of cation exchange reactions on the ultimate distribution of copper in the wood substance and i...
P A Cooper


Protection of rubberwood timber. Part 1: Impregnation with boron preservatives
1989 - IRG/WP 3551
Rubberwood (Hevea brasiliensis) were treated with a 3% proprietary mixture of borax/boric acid using three different treatment schedules i.e. full-cell, full-cell to refusal and full-cell with 12 cycles of vacuum/pressure. Freshly cut samples had mean preservative retentions of 187 kg/m³, 214 kg/m³ and 178 kg/m³ respectively. Pre-air dried samples for one week had retentions of 252 kg/m³, 308 ...
L T Hong, C C K Liew


Step-wise pressure process for reducing surface roughness in Japanese cedar timber
2003 - IRG/WP 03-40256
Sixteen dried sawn-timber (10.5 x 10.5 x 360 cm) were cut into half. The half of them was treated by step-wise pressure process with 2.5 MPa maximum, and the other half was treated by conventional pressure process with 2.5 MPa maximum. Average DDAC preservative absorption was 461 kg/m3 in the former and 525 kg/m3 in the later. Surface roughness was expressed as the profile element height of collap...
K Yamamoto, M Nozoki


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content
2004 - IRG/WP 04-20304
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different wood claddings and the ability to maintain the appearance of the surfaces, when the wood is used in service class 3. A façade construction is exposed t...
B Lindegaard, N Morsing


Gaseous boron treatments of wood and wood products
1992 - IRG/WP 92-3691
Treatment of wood and wood products by gaseous organoborates has now been under study for about 5 years. This technique has potential for boron treatment of a wide range of substrates from solid wood through to wood composite materials such as particleboard or wet and dry formed fibreboards. The vapour treatment technique is proving to be very flexible in that it can be adapted to integrate into a...
A J Bergervoet, R Burton, K Nasheri, D R Page, P Vinden


Development process of a new anti-sapstain formulation and its present status with the relevant problems
2001 - IRG/WP 01-30257
An anti-sapstain formulation, which contains 2-(thiocyanomethylthio)benzothiazol (TCMTB) and methylene-bis-thiocyanate (MBT) as active ingredients, was developed by a technical agreement with Buckman Laboratories (Memphis, TN, USA) as an alternative to chlorinated phenols for the Japanese market. The formulation was commercialized as BAM 12 years ago. As anti-sapstain treatment is commonly conduct...
K Nobashi, Y Nomura, K Tsunoda


Evidence for actinomycete degradation of wood cell walls
1990 - IRG/WP 1444
Several unique patterns of degradation occurring in wood cell walls have been observed in wooden stakes inserted in unsterile soil in the laboratory. Some of the patterns have also been observed in coniferous wood taken from forest floors. All the observed attack types occur within wood cell walls, mainly within the S2 layer. Attack is characterised by channels of varying diameter or small fusifor...
T Nilsson, G F Daniel, S L Bardage


On the nature of the tertiary wall in wood cells. Summary of lecture given at 9th Annual Meeting, Noordwijk-aan-Zee, Holland
1977 - IRG/WP 169
During recent discussions on the possible causes of failure of treated hardwood species by soft rot fungi, the uneven micro distribution of toxic components was found to be of importance; this might be attributed to a restricted diffusion of the preservative from the cell lumina into the cell wall.·In this context, the nature of the tertiary wall as the inner lining of wood cells merits special a...
W Liese


Ingestion of wood-degrading micro-organisms
1991 - IRG/WP 4169
An ultrastructural study was carried out on the digestive tract contents of Limnoria lignorum, frass, gallery walls and surface structures of the animals. The purpose of the study was to determine whether wood-degrading bacteria, fungi and other microbes and/or wood degraded by these microbes were present in gut regions and therefore could provide indirectly a nutritional source for Limnoria. Both...
G F Daniel, S M Cragg, T Nilsson


Industrial fixation of chromium based wood preservatives
1990 - IRG/WP 3630
Fixation is an abstract and non-defined process. Nevertheless it is a specified requirement in most impregnation standards. The impregnation industry is facing increased pressure to deliver fixed products and to increase the safety of the handling of impregnated products. Industrial fixation of impregnated wood can be obtained by using different methods. The purpose of the process is to transform ...
T Christensen


The multi-phase pressure (MPP) process. One-stage CCA treatment and accelerated fixation process - The process as a new concept in preservative treatment
1997 - IRG/WP 97-40078
The background to current commercial CCA treatment schedules used in New Zealand and fixation processing is reviewed. The limitations of these conventional practices with respect to treated product quality and CCA solution handling issues are defined. A novel, patented treatment schedule has been developed using a combination of hydraulic and pneumatic pressure phases and hot (~ 75°C) CCA solutio...
K Nasheri, A J Pendlebury, J A Drysdale, H Pearson, M E Hedley


Immunolocalization of extracellular metabolites from Poria placenta
1988 - IRG/WP 1361
Polyclonal antisera produced to Poria placenta extracellular metabolites was used in immuno-fluoresence microscopy and immuno-gold TEM studies. In the fluorescence work, labelling of Poria placenta hyphae in wet fixed wood material was observed but not in infected wood which was oven dried prior to sectioning and immunolabelling. TEM studies provided better resolution, with gold labelling detected...
B Goodell, G F Daniel, J Jellison, T Nilsson


Effect of treatment process on performance of copper-chrome-arsenate. Part 1: Fungus cellar tests
1995 - IRG/WP 95-40045
Pinus radiata sapwood stakes 20 x 20 x 400 mm³ were treated with CCA Type C using a range of concentrations and three treatment processes; Bethell, Lowry and Rueping. Preservative retention was determined by chemical analysis of treated material. Following fixation, fungus cellar stakelets, 5 x 10 x 180 mm³ were cut from treated material and after leaching were exposed in unsterile soil beds in ...
M E Hedley, J Anderson, J B Foster, B E Patterson


Comparison of the anti-fungal efficacy of Cobra with drill perforation on oscillating pressure treated spruce transmission poles -Laboratory test
1988 - IRG/WP 3469
A laboratory method for measuring the depth of penetration of the fungicidal concentrations effective against basidiomycetes (brown rot) was developed. The tests on CCB oscillating pressure treated spruce transmission poles have shown that the depth of salt penetration can be increased by about 10 mm by a drill perforation before the impregnation. An even better penetration is reached, however, if...
E Graf, B Zgraggen


Extracellular osmiophilic particles in connection with brown rot and white rot
1982 - IRG/WP 1157
The way of attack on Pine woodblocks of two brown-rot fungi (Fomitopsis pinicola, Coniophora puteana) differing in their cellulase activities, and one white-rot fungus (Trametes hirsuta) has been investigated by transmission electron microscopy. Even at early stages of decay, osmiophilic particles were found with all the fungi investigated. In the brown-rotted wood, the osmiophilic particles occur...
K Messner, H Stachelberger


Tilting and vacuum treatment - two methods to obtain a non-dripping freshly treated timber
1989 - IRG/WP 3535
Modern impregnation plants are designed to prevent spread of impregnation solutions from the plant through leakage, etc. It is also important that freshly treated timber does not spread solutions through dripping on the storage area. To prevent this, the impregnation procedure is terminated with a vacuum period. In many plants in Sweden this period is minimized or even excluded to gain time. Inste...
I Johansson, M-L Edlund


Cavitation bacteria
1984 - IRG/WP 1235
A form of bacterial wood degradation is described. The term "cavitation bacteria" has been coined in order to describe the discrete cavities that are formed within the wood cell walls. The bacteria observed within the cavities appeared to be polymorphic with rounded as well as filamentous forms recognised. TEM studies suggest that the bacteria produce diffusable wood-degrading enzymes. Cavitation ...
T Nilsson, A P Singh


Exterior wood stains
1979 - IRG/WP 3136
The use of semi-transparent exterior wood stains has grown remarkably since their development during the 1960s. This can be partly attributed to their offering a break with tradition at a time when it was being recognised that changes in the quality of timber and how it was used demanded different methods of exterior wood finishing. Information is already available on the characteristics and uses ...
E R Miller


Termite durability of sugi (Cryptomeria japonica) heartwood kiln-dried under high-temperature process in relation to wood extractives
2005 - IRG/WP 05-10547
Termite durability of sugi heartwood samples kiln-dried under a high-temperature process were evaluated by using Reticulitermes speratus (Kolbe) as a test termite sp. The n-hexane extractives of these samples were analysed by a GC technique. The less termite durability was shown on the wood samples dried under the high-temperature process, in comparison with that of the air-dried samples. No GC-p...
S Shibutani, E Obataya, K Hanata, S Doi


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 4. MPP compared with other processes for achieving acceptable treatment of radiata pine heartwood
1998 - IRG/WP 98-40115
Although radiata pine sapwood is very amenable to preservative treatment, it is often difficult to achieve the required standard for heartwood treatment. A preliminary investigation showed that to achieve the NZ Timber Preservation Council minimum penetration requirements for radiata pine heartwood using the Multiple-Phase Pressure (MPP) Process, a hydraulic pressure of at least 1250 kPa for 20 m...
K Nasheri, J A Drysdale, G Durbin, M E Hedley


The development of soft rot decay in bamboo fibres
1992 - IRG/WP 92-1572
The development of decay by soft rot fungus Chaetomium globosum was investigated in young and mature culms of bamboo Phyllostachys virideglaucescens. Soft rot decay was influenced both quantitatively and qualitatively by the differing levels of lignification in the material. Weight loss was significantly greater in the younger culm compared with the older, more heavily lignified culm. The distribu...
O Sulaiman, R J Murphy


Previous Page | Next Page