IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 232 documents. Displaying 25 entries per page.


The performance in the sea of seven experimental piles after sixteen years at Port Douglas, North Queensland
1989 - IRG/WP 4151
After 16 years at Port Douglas, two double-treated Pinus radiata piles were in excellent condition, a CCA-treated Pinus elliottii pile was in good condition other than for a confined streak of teredinid attack, while two CCA-treated and two untreated turpentine piles were moderately to severely attacked by Sphaeroma in the tidal zone. The marine borers collected were Sphaeroma terebrans, Martesia ...
L J Cookson, J E Barnacle, C N McEvoy


Differentiation of Scots pine heartwood and sapwood by near infrared spectroscopy
2003 - IRG/WP 03-10459
In Scandinavia Scots pine heartwood has, in recent years, gained popularity as material for external structures exposed to moderate risk of decay. As non-durable sapwood surrounds the heartwood in pine trunks it is of crucial importance to separate this wood from the heartwood during log processing into heartwood products. Heartwood and sapwood can be differentiated by visual evaluation of colour ...
P O Flæte, E Ystrøm Haartveit


Effect of Pseudomonas cepacia on the activity of a mixture of wood staining fungi on ponderosa pine sapwood
1995 - IRG/WP 95-10107
There are major incentives for limiting the degree of fungal discoloration which occurs during wood processing. Most lumber producers apply prophylactic fungicides which limit microbial growth, but increasing restrictions on the use of these chemicals have encouraged the search for alternative stain prevention strategies. Among the possible strategies for stain prevention is biological control. Wh...
J J Morrell, R K Velicheti


Log fumigation prevents enzyme-mediated sapwood discolorations in hardwoods
1993 - IRG/WP 93-10003
Non-microbial sapwood discolorations in hardwood lumber can cause economic loss by degrade of quality. Based on the hypothesis that the enzyme-mediated sapstain may develop in part from byproducts of parenchyma cells in wood, reshly felled logs of red oak (Quercus spp.) and sugar hackberry (Celtis laevigata) were fumigated under a plastic tarp with methyl bromide. Log sections were checked after f...
E L Schmidt, T L Amburgey


Study of modulus of rupture, circumference taper, sapwood thickness and CCA treatment of Norwegian origin Pinus sylvestris poles
1994 - IRG/WP 94-20054
Nondestructive strength testing with Pilodyn (6J) of Norwegian Pinus sylvestris poles revealed effective modulus of rupture (MOR) of 54.39 N/mm² at wet conditions after CCA-C treatment and circumference measurement revealed circumference taper of 0.021 m/n. Sapwood thickness or penetration of CCA-C study revealed that 77% poles were with sapwood thickness equivalent to 39.6% of radius of poles an...
A K Lahiry, S Begum, G N M Ilias, M A B Fakir, R U Hafiz


Prevention of non-microbial sapwood discolorations in hardwood lumber: chemical and mechanical treatments
1997 - IRG/WP 97-30137
Sapwood discolorations in hardwood lumber that are non-microbial in origin result from the formation of pigmented starch-like granules in ray parenchyma cells. These discolorations can be prevented by treating unseasoned lumber with an antioxidant (sodium bisulfite). Exposing unseasoned lumber to microwaves or treating logs with fumigants also will prevent these discolorations. Subjecting unseason...
T L Amburgey, S Kitchens


A study of fungal biodeterioration in unseasoned, packaged hem-fir lumber
1978 - IRG/WP 2116
This study was undertaken to determine the extent of biodeterioration that could occur within British Columbia (BC) prior to the export of packaged Canadian Lumber Standard Hem-Fir (Tsuga heterophylla, Abies amabilis and small amounts of Abies grandis). By examining the anti-stain treatments received by the lumber and identifying and characterizing the organisms responsible for the biodeterioratio...
P W Perrin, A J Cserjesi


Nondestructive assessment of biodegradation in southern pine sapwood exposed to attack by natural populations of decay fungi and subterranean termites
1994 - IRG/WP 94-20042
Field methods for evaluating decay resistance of experimentally treated materials lack a means for quantitative measurement of residual strength. Quantitative relationships between speed of impact-induced waves travelling parallel to the grain and residual compressive strength have been demonstrated in softwood attacked by brown rot-decay fungi, but the effects of termites have not been documented...
R C De Groot, R J Ross, W Nelson


Preliminary observations on tributyltin treated Scots pine sapwood using 119Sn (Mössbauer and NMR) spectroscopic techniques
1984 - IRG/WP 3312
119mSn Mössbauer data are presented for bis(tributyltin) oxide, tributyltin ethanesulphonate, bis(tributyltin) carbonate and tris(tributyltin) phosphate, both in the pure form and in Scots pine sapwood. The structures proposed for these compounds, in the solid state, are supported by 119Sn nuclear magnetic resonance spectroscopy.
R Hill


The development of blue stain in service in sapwood of European softwood species
1997 - IRG/WP 97-10236
The utilisation of softwood species for window joinery applications is gaining importance in countries frequently using tropical hardwood species up to now. Since wood preservation is not always part of the total concept of window frames manufactured from sapwood containing wood elements it is essential to know the impact of durability on the performance. Moisture content control is a major tool i...
J Van Acker, R Klaassen, H Militz, M Stevens


A trial of "sour" felling to prevent bluestain by depletion of sapwood nutrients
2001 - IRG/WP 01-10404
Discoloration of conifer wood caused by bluestain causes large economic losses in Canada. Most deep stain develops in the log stage during storage or transport. In a search for control strategies that will not disrupt woodlands productivity we tested "sour" felling, termed "hagarashi" in Japan. The practice involves delaying the delimbing of freshly harvested trees. The tree continues to transpire...
A Byrne, A Uzunovic, D Minchin, C Breuil


Specifying preservative-treated resistant timber: Conforming to European Standards
2001 - IRG/WP 01-20235
The most common construction timbers used in the UK are of low natural durability and, generally, resistant to preservative treatment. These include species of spruce, hemlock and fir. However, their characteristically limited and non-uniform uptake of preservatives may still confer sufficient protection to give satisfactory durability performance in terms of biological resistance. This paper desc...
E D Suttie, A F Bravery, T B Dearling


"Refractory" is a relative term. Incised alpine fir is treatable
1991 - IRG/WP 3670
While certain wood species carry a reputation for being 'treatable' this normally refers to the sapwood. For most Canadian species, heartwood penetration is the major determinant of whether treatment meets Canadian, USA and Japanese standards and in this respect alpine fir turns out to be a treatable species. Alpine fir is the fir component of the Western Canadian spruce-pine-fir...
P I Morris


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton


Differential retention and leaching of CCA (C) in sapwood and heartwood of Kenyan-grown blue gum (Eucalyptus saligna) and black wattle (Acacia mearnsii)
2005 - IRG/WP 05-30371
Retention and leaching of CCA(C) in small samples of sapwood and heartwood of Kenyan-grown blue gum (Eucalyptus saligna) and black wattle (Acacia mearnsii) were tested under laboratory conditions. Clear samples (100mm x 30mm x 40mm) were removed from the sapwood and heartwood of sampled defect-free and sound plantation trees of the two species. These were separately air-dried to 15% MC, end-seal...
R Venkatasamy


Biological control of sapwood-inhabiting fungi by living bacterial cells of Streptomyces rimosus as a bioprotectant
1992 - IRG/WP 92-1564
The objective of this study is to evaluate the efficacy of antifungal activity of living bacterial cells for the protection of wood against sapwood-inhabiting fungi. The following sapwood-inhabiting fungi were selected: sapstain --Ceratocystis coerulescens, Ceratocystis minor, Ceratocystis pilifera, and Aureobasidum pullulans; mold fungi --Aspergillus niger, Penicillium spp, and Trichoderma spp. L...
S C Croan, T L Highley


Penetration and absorption of water-borne preservatives in conifers from the Western United States: A preliminary report
1988 - IRG/WP 3475
The treatment of most softwoods from the western United States with waterborne chemicals poses a major challenge. Although many of these species are commercially treated with waterbornes, there is considerable debate about their treatability. At present, there is little or no information on the treatability of western wood species with waterborne chemicals. The lack of accurate treatability inform...
S Kumar, J J Morrell


Partial characterization of inhibitors extracted from pine (Pinus sylvestris) sapwood active against germination of wood rotting fungi
1988 - IRG/WP 1351
Germination inhibitors in pine sapwood could be extracted and separated with the aid of solvent partitioning and chromatography on silicic acid. The inhibitory action was tested by three different bioassays. Active fractions have been characterized by TLC and HPLC. Inhibitory activity could be correlated with phenolic compounds. The minimum active concentration of inhibitors have been determined....
J Bjurman


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 3. Effect of process variables on sapwood treatment and CCA fixation.
1998 - IRG/WP 98-40114
The Multiple-Phase Pressure (MPP) Process achieves treatment and fixation as combined process using hot CCA, within a 2-3 hour time-frame. Timber is treated to saturation with hot CCA using an empty cell process. During the pneumatic pressure phase, hot solution is held in the wood in an otherwise liquid-free treatment vessel until fixation is >95% complete. This report details a factorial des...
H Pearson, K Nasheri, J A Drysdale, G Durbin, M E Hedley


The natural durability of wood in different use classes - PART II
2006 - IRG/WP 06-10598
The natural durability of important European wood species has been tested on 3970 speci¬mens in field trials. The wood was exposed at five test sites in Germany with different climates, at each site in European use class 4 and 3 (with and without soil contact). Within European use class 3 three different expositions were tested: vertical with sheltered end grain, vertical unsheltered and horizont...
A O Rapp, U Augusta, K Brandt


Moisture correction for ultrasonic MOE measurements above fibre saturation point in Scots pine sapwood
2006 - IRG/WP 06-20333
There is a high correlation between methods for dynamic modulus of elasticity (MOEdyn) and static modulus of elasticity (MOEstat). MOEdyn methods have been found sensitive to detect early stages of decay and may be seen as an option for non-destructive wood durability testing. As the MOEstat measurements do not change after reaching the fibre saturation point, the uncorrected MOEdyn data from ultr...
E Larnøy, G Alfredsen, H Militz


Long term marine performance of ACZA treated Hem fir in Krishnapatnam harbour, east coast of India
2006 - IRG/WP 06-30409
The performance of Hem fir (Tsuga heterophylla) and Southern pine (Pinus sp.) treated with ammoniacal copper zinc arsenate (ACZA) and copper dimethyldithio carbamate (CDDC) at two retention levels of each preservative was assessed in tropical marine waters at Krishnapatnam harbour on the east coast of India. Panels treated with ACZA of lower loadings (23.1 Kg/m3) had failed in 38 months while the ...
B Tarakanadha, K S Rao, J J Morrell


Lyctine susceptibility testing and dealing with rarely susceptible hardwood species
2007 - IRG/WP 07-10607
This study examined the lyctine susceptibility of 16 timber species or hybrids. Several of the timbers have been placed previously in a ‘rarely susceptible’ category, but for standards and compliance purposes, such in-between ratings are not acceptable. Timber specimens were spot tested for starch content, and exposed to three species of lyctine beetles in an insectary. New criteria were devel...
L J Cookson, J Carr, N Chew, J W Creffield


Protection of wood for above ground application through modification with a fatty acid modified N-methylol/paraffin formulation
2007 - IRG/WP 07-40378
Hydrophobic chemical modification can be regarded as an alternative approach to conventional wood preservation using biocides in order to protect wood in hazard class 3 according the European Standard EN 335-1. A formulation containing fatty acid modified N-methylol/paraffin and an aluminium salt catalyst was used to change the material properties of wood in order to protect wood from fungal dec...
Nguyen Hong Minh, H Militz, C Mai


Influence of Grain Direction on Penetration, Retention, and Leaching of CCA(C) in Sapwood and Heartwood of Kenyan-Grown Eucalyptus saligna and Acacia mearnsii
2007 - IRG/WP 07-40383
Penetration, retention, and leaching of CCA (C) in relation to grain orientation were tested in small (50mm x 50mm x 200mm) sapwood and heartwood samples of Eucalyptus saligna and Acacia mearnsii. In both sapwood and heartwood of the two species, the results showed a consistent pattern: Transverse > Radial > Tangential. Whereas penetration, retention, and leaching were significantly high i...
R Venkatasamy


Previous Page | Next Page