IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 232 documents. Displaying 25 entries per page.


Preservative effect of cellulose insulation material against some mould fungi and brown rot fungus Coniophora puteana in pine sapwood
1991 - IRG/WP 1484
The influence of mineral wool and loose-fill cellulose wool on biodeterioration of pine sapwood was studied. The test fungi were mould fungi Aspergillus versicolor, Cladosporium sphaerospermum, Penicillium sp. and Aureobasidium pullullans and brown rot fungus Coniophora puteana. Cellulose wool inhibited the growth of mould fungi on the face of wood contacted with insulation material at RH of 97 an...
H Viitanen


An Australian test of wood preservatives. Part 1: Preservatives, principles and practices
1978 - IRG/WP 2123
Between November, 1963, and July, 1964, a graveyard test of some 6000 preservative-treated stakes was installed at 8 sites equally distributed between Papua New Guinea in the tropics, through Queensland and New South Wales to Victoria. More than 40 different preservatives and preservative mixtures, mostly at several different levels of retention, were used to impregnate sawn specimens of Pinus rad...
J Beesley


Resistance of various wood species against decay by Coniophora cerebella (Pers) Duby and Lenzites trabea (Pers) Bres
1976 - IRG/WP 142
Both fungi, Coniophora cerebella and Lenzites trabea, are important destroyers of timber. Coniophora often occurs inside buildings and Lenzites trabea has been observed on southern facades of buildings, on balconies and window frames. In most instances that we investigated coniferous timber had been decayed. But both species are known to attack also various hardwoods. For this reason tests similar...
O Wälchli


Natural progression of decay in unrestrained, Southern pine sapwood exposed above ground
1995 - IRG/WP 95-20060
In this study, the natural progression of decay is being monitored in 2.4-m (8-ft) lengths of dimension lumber. The 2.4-m lengths are supported without restraint in a horizontal plane approximately 0.75 m above ground in a partially shaded field plot in southern Mississippi. The lumber is 100% sapwood. Prior to installation in the field, each piece was planed to exactly 38 by 89 mm² (1.5 by 3.5 i...
R C De Groot, R J Ross, W Nelson


Comparative studies on the species effects of wood preservatives
1989 - IRG/WP 3521
For the examination of the resistance against fungal attack, wood blocks of 3 softwood species were treated with CCA (type 3), CFK, AAC and IF-1000 independently. The wood blocks were exposed to the fungal decay with Tyromyces palustris. The degradation of the wood blocks treated with these preservatives was quite widely different among wood species examined in this study. Hem-fir treated with CCA...
K Yamamoto, S Matsuoka


The effect of wood preservatives on the relation between the electric resistance and moisture content in scots pine (Pinus sylvestris L.) sapwood
1998 - IRG/WP 98-20142
The effect of two types wood preservatives (TBTO and CuHDO) on moisture content measurements with an electric resistance meter in pine sapwood is assessed. High and low concentration impregnated pine sapwood is climatized at different relative humidities. Once climatized the samples are weighed and the moisture content is measured with an electric resistance meter by fixed stainless steel, isolate...
B W Holleboom, W J Homan


The effect of primary blue-staining fungi on the strength properties of Scots pine sapwood
2004 - IRG/WP 04-10515
The fungi action may have influence on wood properties especially Basidiomycotina fungi causing wood decay. The investigation of influence of fungi causing mainly wood discoloration and disfigurement on wood properties is still in development process. There were determined the differences between the bending strength, the compression along the grains and impact strength of control and blue stained...
A Fojutowski


Control of sapwood-inhabiting fungi by fractionated extracellular metabolites from Coniophora puteana
1991 - IRG/WP 1494
The objective of this study was to test the fractionated metabolites released by Coniophora puteana for their antagonistic activity against the sapstain fungi Ceratocystis coerulescens and Aureobasidum pullulans, and the molds Asperigillus niger and Penicillium spp. The acetone-soluble fraction obtained from the culture filtrate prepared from Coniophora puteana grown on 6% malt extract agar inhibi...
S C Croan, T L Highley


In-ground field test of scots pine (Pinus sylvestris L.) sapwood and heartwood
2004 - IRG/WP 04-30336
Scots pine (Pinus sylvestris L.) sapwood and heartwood stakes treated with CCA-C and creosote were tested for one- year in a field plot in Bartın region in Turkey. Scots pine heartwood stakes had lower preservative retention than sapwood stakes. Bending strength of the stakes was decreased after impregnation and one-year field test. While the bending strength of untreated sapwood was 93....
H Sivrikaya, H Hafizoglu


Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


Models of the critical time of humidity and temperature conditions for the development of mould fungi in pine and spruce sapwood
1995 - IRG/WP 95-20066
Regression models of the time factor for the growth of mould fungi in pine and spruce sapwood are studied. The first group of models are based on the results of exposures of mould fungi in static humidity and temperature conditions indicating the time for the start of mould growth in wood. The second group of models are based on the exposures of mould fungi in fluctuating or alternating humidity a...
H Viitanen


Effect of bioextracts on colonisation of radiata pine sapwood by three sapstain fungi
2003 - IRG/WP 03-10485
The objective of this study was to investigate the effect of aqueous bioextracts prepared following two-week incubation of forest soil, garden compost and chicken manure respectively, on the ability of Ophiostoma flocossum, Leptographium procerum and Sphaeropsis sapinea to colonise unseasoned radiata pine sapwood. The research showed that all bioextracts tested retarded the rate of fungal colonis...
J van der Waals, C Chittenden, B Kreber


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


The effect of water storage on the cell-structure of Sitka spruce (Picea sitchensis) with reference to its permeability and preservation
1970 - IRG/WP III 3A
Commercial treatment trials with full sized transmission poles have shown that water storage considerably improves the permeability of Sitka and Norway spruce. These results were confirmed by laboratory measurements which showed that in the sapwood of ponded Sitka spruce there is a vast improvement in permeability in all three grain directions. Heartwood permeability does not seem to be affected t...
J A Dunleavy, A J McQuire


Screening of the efficacy of tall oils against wood decaying fungi
2004 - IRG/WP 04-30354
Tall oil is a by-product in pulping of resinous wood by the sulphate process. Tall oil contains a complex mixture of wood extractives. Some of these extractives act as natural protection against wood decaying fungi while other serve as nutrition for the fungi. This report describes a screening of the efficacy of four refined tall oils with different chemical composition on wood decaying fungi. ...
G Alfredsen, P O Flæte, A Temiz, M Eikenes, H Militz


Field evaluation of the above-ground susceptibility of Pinus heartwood and untreated or treated sapwood to two species of Australian subterranean termites
1996 - IRG/WP 96-10147
Plantation-grown Pinus elliottii, Pinus caribaea and Pinus radiata specimens containing heartwood and untreated or preservative-treated sapwood were exposed above ground to the subterranean termites Coptotermes acinaciformis or Mastotermes darwiniensis near Sydney (NSW), Brisbane and Townsville (Qld), and Darwin (NT), using a variety of exposure techniques. Heartwood of Pinus elliottii and Pinus c...
M J Kennedy, J W Creffield, R H Eldridge, B C Peters


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


Determination of boron levels in solution and in treated wood
1994 - IRG/WP 94-20041
Four methods of measuring boron levels in solutions were investigated. The methods compared included the azomethine-H method which is commonly used in soils and plant tissues, the methods outlined in the Australian Standard AS 1605 (1974) and in Wilson (1958), and the atomic absorption spectrophotometry method. Defect-free radiata pine (Pinus radiata D. Don) sapwood and wood flakes were treated to...
F J Romero, P Vinden, P Kho


The effect of rate of pressure application on preservative uptake along and across the grain of fir (Abies bornmulleriana Mattf.) at different ramp and constant pressure times
2004 - IRG/WP 04-20292
This study was particularly design to determine the preservative uptake at different ramp (rate of increase in pressure) and constant pressure times on longitudinal, tangential and radial penetrations of fir (Abies bornmulleriana Mattf.) which grown indigeneously in Turkey. The samples of 2 cm cubes of kiln-dried wood (nominated to 12% moisture content) were treated at different ramp times varied ...
I Usta


Färbeverfahren zur Unterscheidung von Holzzonen mit unterschiedlichem Absorptionsvermögen, insbesondere bei Fichtenholz (Picea abies Karst.). [Staining method for distinguishing zones of wood with different absorption behaviour, particularly in spruce (Picea abies Karst.)]
1980 - IRG/WP 3163
A simple regressive staining method for crosscut wood surfaces is described. Phloroglucinol-hydrochloric acid serves as stain; flowing water and a solution of sodium carbonate are used for development and fixation of a picture showing the differences of absorption. Hydrophobic zones and, contrary to this, zones with a high water content can also be shown. Comparing green spruce wood before and dur...
S Cymorek


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


Controlled envelope treatments of Pinus sapwood, achieved by modifications to impregnation process and carrier solvents
2003 - IRG/WP 03-40258
Specimens of slash pine or radiata pine were treated to a target retention of 0.02% m/m permethrin with conventional light organic solvent fluids or with oil-modified fluids (Tanalith® T). Best achievable envelopes from LOSP fluids were poorly controlled, penetrating not only the target outer 0-5 mm zone (mean 0.019%, RSD 28%), but also breaking through into the 5-10 mm zone (mean 0.013%, RSD 37%...
M J Kennedy, P R S Cobham


Effect of thickened boron in preventing conidial germination of sapwood-inhabiting fungi
1994 - IRG/WP 94-30059
We evaluated the efficacy of thickened boron preservative "Diffusolä" in preventing conidia germination of sapwood-inhabiting fungi using plate bioassay, Southern Yellow Pine and sweetgum block tests, and green pine log sections. The test fungi were sapstain fungi Ceratocystis coerulescens, Ceratocystis minor, and Aureobasidum pullulans and mold fungi, Aspergillus niger, Penicillium spp, and Tric...
S C Croan


Evaluation of the natural durability and ultrasonic method for decay detection of some european hardwood and softwood species
2004 - IRG/WP 04-10537
This paper presents the first part of an investigation on the natural durability of mixed plywood made of durable and non durable plies from the following selected timbers : Cedrus atlantica, Cupressus sempervirens, Castanea sativa, Populus sp. I 214 and Fagus sylvatica. In order to carry out this study, the natural durability of the massive wood used to manufacture the plywood panels was asses...
F Faraji, M-F Thévenon, B Thibaut


Previous Page | Next Page