The association of bacteria with the increased permeability of water-stored spruce wood
1973 - IRG/WP 325
A microbiological investigation was undertaken to check our earlier work on patterns of bacterial counts and pH changes in water-stored wood. A survey of industrial activity was conducted upstream from the storage site with a view to explaining the existing bacterial flora. Further experiments were carried out with spruce bolts in enclosed tanks, using lake water with its natural bacterial flora a...
J A Dunleavy, J P Moroney, S E Rossell


Thickened boron treatment
1990 - IRG/WP 3632
Commercial trials with thickened boron preservatives "Diffusol™" indicate a number of advantages when compared to traditional methods of dip-boron preservative treatment. These include: (i) more even uptake and distribution of preservative on and within the timber; (ii) faster diffusion times; (iii) the treatment of gauged timber (though improved retention); (iv) saving in energy costs (heating ...
P Vinden, J A Drysdale, M Spence


The development of a new boron-based wood preservative
1995 - IRG/WP 95-30085
The paper describes a new boron based wood preservative for the treatment of green timber. The product offers many benefits over conventional boron diffusion treatment including: 1. high viscosity, high concentration formulation; 2. permits dip treatment of a wide range of sawn board and pole sizes at ambient temperatures; 3. permits full cross section diffusion of borates without block stacking a...
P Turner, D Conradie


Wood injurers found at wood processing plants in SR Sloveni
1981 - IRG/WP 1140
This report describes the stating of damages on wood and taking stock of wood injurers found in the warehouses of wood processing plants in SR Slovenia. The results of this research show that in the process of manufacture vast quantities of spruce-wood, pine-wood, beech wood, oak-wood, and poplar-wood are exposed to numerous injurers, both fungi and insects. The reasons for such a state lie in con...
R Benko


An analysis of the effects of some factors on the natural durability of pine (Pinus sylvestris L.) and spruce (Picea abies Karst.)
1986 - IRG/WP 1279
The effects of some factors on the natural resistance of pine and spruce sapwood against fungal decay and against attack of house-longhorn beetle larvae have been studied in laboratory tests and the results are evaluated by analysis of variance and regression analysis. Following conclusions were reached: Wood from summer-felled trees did not have a lower inherent natural durability against fungal ...
J B Boutelje, T Nilsson, S Rasmussen


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Application of oscillating pressure to improve treatability of refractory species
1987 - IRG/WP 3449
Under practical conditions a minimum moisture content of 80% demande by the German quality standard RAL-RG 411 can not be guaranteed throughout the year. Storage of logs with bark prolonges the drying process; a storage without bark must be avoided. A sufficient penetration according the standard can be achieved at least with a moisture content of 60%, optimal conditions may prevail between 100% a...
R-D Peek


Anti-sapstain chemicals for diffusion treatment of rubber wood
1986 - IRG/WP 3367
Performance of Sinesto B and Akzo EN 494, two formulated products of alkyl ammonium compounds, was tested as fungicidal additive in the boron solution to control mould and stain during diffusion storage of rubber wood. Sinesto B at 2.0% (a.i.) concentration has given good control over mould and its protection against sapstain was only satisfactory. Akzo EN 494 at 0.7% (a.i.) concentration has give...
R Gnanaharan


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Borate diffusion from fused borate rods in douglas-fir transmission poles
1994 - IRG/WP 94-30042
Pressure-treated utility poles have given many years of excellent service, but their lifetime is often shortened by internal decay of the untreated heartwood center, particularly in refractory species, such as Douglas-fir. This paper reports the distribution of boron from fused borate rods installed in CCA-treated Douglas-fir transmission poles. The boric acid equivalent was roughly monitored by t...
T L Highley, W Finney, F Green III


Redistribution of boric acid in radiata pine during drying after preservative treatment
1993 - IRG/WP 93-40010
Samples of 100 x 50 mm² radiata pine were processed with a variety of options to produce dry, boron-treated wood. Concentrations of boric acid in the central one-ninth and in the whole of the wood cross-sections were determined by chemical analysis and compared. Diffusion treated material was dried by air, conventional kiln (70/60°C), or high temperature kiln (120/70°C). Four different predryin...
A J Bergervoet, D R Page, J A Drysdale


Methods of testing anti-stain chemicals for protecting sawn timber during storage and transport
1976 - IRG/WP 273
No international standard method for testing anti-stain chemicals for protecting fresh sawn timber exists. The methods used can be divided into three types: a) Rapid screening tests for finding chemicals effective against blue-stain and mould fungi. The chemicals are tested in agar medium, in pieces of filter paper or on small pieces of wood using pure cultures. b) Laboratory tests for evaluating ...
T Vihavainen


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 4: Conversion reactions during storage
1974 - IRG/WP 332
Precipitates simulating those produced in wood by preservative fixation reactions were prepared by the reduction of Boliden K 33 and Celcure AP solutions with hydrogen peroxide and hydrazine. The pH changes on aging at 20 and 50°C were studied and related to the chemistry of fixation previously described. Hydrolysis of copper arsenates may render arsenic acid temporarily water soluble pending pre...
S-E Dahlgren


Mould growth and permeability in relation to wet-storage
1989 - IRG/WP 1414
The positive influences of wet-storage of roundwood to avoid attack by blue stain fungi and insects and to avoid cracking of wood during storage are well documented. Comparatively little information is, however, available on the effects on microbial susceptibility of the material after the storage period. The permeability of the wet-stored and the non-wet-stored material was determined. Wood block...
J Bjurman, E L Holappa


Evaporation and redistribution of creosote in pine poles during storage
1996 - IRG/WP 96-50064
During the work with European standards for pressure treated wood, it has been questioned if the lapse of time between impregnation and chemical analysis of the retention is critical, especially for creosote. "The Norwegian Control Scheme for Preservative Treated Wood" has not discovered any retention problems analysing CCA preservatives in wood. If the lapse of time between impregnation with creo...
F G Evans, B Nossen


Diffusion treatment of gauged radiata pine timber using "Boracol 20"
1987 - IRG/WP 3437
Green gauged 100 x 50 mm radiata pine timber was preservative treated by brush application of "Boracol 20" followed by diffusion storage. Preservative retention analyses indicated that retention requirements in the core could be achieved within a six week diffusion period, thus representing a time saving of 25% over conventional boron treatment of rough-sawn radiata pine. Similar treatment of kiln...
D R Page, P Vinden, S Retter


Boracol 40 - A potential remedial and preservative treatment for lyctids
1983 - IRG/WP 1192
The paper reports on a preliminary assessment of the efficacy of a diffusion formulation, Boracol 40, when applied as a brush treatment: to the surface of Eucalyptus obliqua against the powder-post borer Lyctus brunneus. After a five month bioassay, Boracol 40 has severely retarded the progress of active infestations of Lyctus brunneus and has been 100 per cent effective as a preventative treatmen...
J W Creffield, H Greaves, C D Howick


The Development of a novel method to preserve reeds using an environmentally friendly timber preservative and a unique engineering design.
2006 - IRG/WP 06-40335
Reeds are used in the construction of bush lodges in Northern Kwa- Zulu Natal, South Africa. Fungal, insect and ultra-violet damage to these reeds is posing a severe problem. Within a space of two years, the reeds are attacked and have to be subsequently replaced; a time consuming and costly exercise. A novel method has been used to successfully preserve these reeds with an environmentally friendl...
K Govender, K G Moodley


Laboratory Leaching Tests to Study the Effects of Post-Treatment Storage Periods on CCA Leachability and Fixation in Treated Permeable and Refractory Malaysian Hardwoods
2006 - IRG/WP 06-50240
The biological resistance and environmental safety of CCA-treated wood relies on the extent of post-treatment storage fixation of CCA in wood prior to being utilized. A study on the comparative leachability (fixation) of CCA-treated refractory and permeable heartwoods of 3 Malaysian hardwoods subjected to different post-treatment storage (fixation) periods of up to 4 weeks, at 2 laboratory leachin...
A H H Wong, H C Lai, N P T Lim


The effect of wood moisture content and rod dosage on movement of boron through Douglas-fir heartwood
2007 - IRG/WP 07-30431
The potential for moisture sorption by boron rods following application to wood to affect subsequent boron diffusion was investigated in small Douglas-fir blocks conditioned to 30, 60 or 90% moisture content (MC). MCs tended to decline over the 180 day test period, but there was no evidence that the rods acted to draw moisture away from the wood. As expected, boron movement tended to increase with...
Y Cabrera, J J Morrell


Bamboo Protection Research: Contributions from India
2007 - IRG/WP 07-40355
Bamboo preservation has become more important in India because of Government’s directions to develop bamboo resources and adopt their rational utilization to conserve natural forests. This paper traces the development of various processes for treatment of bamboo and their effectiveness. Results obtained by various workers since 1947 when systematic work on bamboo protection was first published. ...
S Kumar


Refinement of emission values for preserved wood in the ‘Storage Scenario’, for use in the environmental risk assessment of Wood Preservatives under the Biocidal Products Directive
2007 - IRG/WP 07-50244
The evaluation of an active substance or a biocidal product under the Biocidal Products Directive (BPD) requires that an environmental risk assessment is carried out. The risk assessment for wood preservatives includes a scenario for the treated wood in storage after treatment, in which the predicted environmental concentration (PEC) in soil, surface water and groundwater is calculated, using emis...
E F Baines


Comparative Laboratory Leaching Test Methods to Study Post-Treatment Storage Period Impacts on CCA Leachability and Fixation in Treated Kempas (Koompassia malaccensis) Heartwood
2007 - IRG/WP 07-20376
Three laboratory leaching test methods were compared to determine the effects of different post-treatment storage fixation periods on leachability/fixation of CCA components from treated kempas (Koompassia malaccensis) permeable heartwood. End-sealed test wood blocks of permeable were treated with CCA to target retention of 5.6 kg/m3, immediately stored to fix at ambient conditions for 0 and 48 ho...
A H H Wong, H C Lai


Developments in Borate Treatment of Canadian Species for Decay and Termite Resistance
2007 - IRG/WP 07-30443
The increased interest in boron treatment of wood over the past 20 years is mainly due to its environmental acceptability, potentially deep penetration in wood, and its efficacy against decay and termites. Based on Forintek’s research in the past two decades, the boron penetration and retention requirements for decay and termite protection in various national and international standards for Cana...
Jieying Wang, P Morris, S McFarling, T Byrne


Run-off quality from sprinkled debarked logs and logs with bark from Picea abies and Pinus contorta
2007 - IRG/WP 07-50248
Storage of roundwood is necessary for efficient industrial production at sawmills and pulpmills. The need for wood storage becomes even more critical when large storm fellings create huge volumes of wood that is at risk for deterioration. In Scandinavia, the technique of sprinkling of water on roundwood is used to protect stored wood from fungal and insect infestation and drying during the summer....
M Jonsson