Movement and persistence of chloropicrin, Vapam, Dazomet and methylisothiocyanate in red and white oak timbers
1992 - IRG/WP 92-3728
This study describes the movement and persistence of four fumigants in sawn red and white oak timbers exposed out of ground contact for 2 years. Chloropicrin moved the furthest from the point of application, and was the most persistent. Vapam was next best, followed by Dazomet. Methylisothiocyanate (MIT), applied as pellets, was not effective, probably because MIT was lost from pellets prior to tr...
T L Highley


The effect of creosote and Basilit on the boards of 4 wood species against destructive fungi in Northern Iran
1989 - IRG/WP 3555
The results of the experiments conducted on the boards of maple, hornbeam, alder and beech, show that under the humid and moderate climate condition of Northern Iran, after 30 months, the witness samples were about 10% destructed by fungi, especially by Schyzophyllum commune and Coriolus versicolor. The impregnated samples by Creosote Basilite using Rueping and Bethell methods, were quite intact. ...
D Parsapajouh


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Development of an Australasian protocol for assessment of wood preservatives
1994 - IRG/WP 94-20043
The Australasian Wood Preservation Committee (AWPC) is currently developing a suite of assessment procedures (protocols) for the biocidal efficacy of wood preservatives for approval in Australasia (Australia, New Zealand, Papua New Guinea, Fiji). Protocols are being prepared for the six hazard levels recognised in the relevant standards of member countries and represent the minimum procedures requ...
W D Gardner, H Greaves, M E Hedley, K J McCarthy, J Norton


An engineering model for the decay of timber in ground contact
2003 - IRG/WP 03-20260
To predict the residual strength of an engineered structure, it is first necessary to predict the effect of decay. A model was developed in which the effective area of structural decay in large section timbers was defined as that area that could be picked out with a pen-knife. Some limited studies indicated that for practical purposes the remaining wood could be assumed to have its full residual s...
R H Leicester, C-H Wang, M N Nguyen, J D Thornton, G Johnson, D Gardner, G C Foliente, C MacKenzie


Laboratory determination of the natural decay resistance of some lesser-utilized timbers from Tanzania against wood decay fungi
2004 - IRG/WP 04-10517
Four lesser known/utilized timber species (sap and heartwoods) from Tanzania, namely Albizia lebbeck, Zanthoxylum gilletii, Faurea saligna and Parinari curatellifolia were exposed to the brown rot fungi (Gloeophyllum trabeum and Coniophora puteana) and the white rot fungus (Coriolus versicolor) to determine their natural decay resistance according to the EN 113 standard procedure. The timbers were...
P R Gillah, R C Ishengoma, E Julias, S A Amartey, D H Kitojo


The performance of water repellants on radiata pine exposed to the weather
1989 - IRG/WP 3553
The effectiveness and resistance to weathering of four water repellent treatments, a commercial timber stain, and an oil-based clear finish, was assessed using 20x20x6 mm³ samples of untreated, copper-chrome-arsenic (CCA)-treated, and tributyltin oxide (TBTO)-treated radiata pine exposed to the weather over a four month period. The water repellency of each preservative/water repellent combination...
D V Plackett, F M Cameron


Fluoride woodpill
1987 - IRG/WP 3431
Decay problems of spruce joinery in the Netherlands in the 1960's and 1970's led to the introduction of preservative treatment. Because of the known penetration difficulties with Spruce, the results of the treatments were not always successful. The fact that the decay was found only in the joints led to development of the philosophy of "local preservation" of the joints in remedi...
J W P T Van der Drift, K J M Bonsen


Decay types observed in small stakes of pine and Alstonia scholaris inserted in different types of unsterile soil
1990 - IRG/WP 1443
The attack of various wood-degrading microorganisms occurring in mini-stakes of pine and Alstonia scholaris buried in various types of unsterile soil was studied. Attacks by white rot, brown rot, soft rot, erosion bacteria, tunnelling bacteria and actinomycetes were found. Soft rot occurred in all soils, whereas attack by white rot and especially brown rot and erosion bacteria was rare. The type o...
T Nilsson, G F Daniel


Soft rot decay of Eucalyptus maculata Hook. in different soils from Queensland, Australia
1980 - IRG/WP 1113
In the present work, different Queensland soils were chosen and their gross effects on the decay of treated and untreated Eucalyptus maculata examined. The soils were also amended with various levels of phosphate to study the response of the wood decay mycota to an increasing supply of this nutrient. Phosphate amendment was chosen because of the wide-scale use of superphosphate on Queensland soils...
L E Leightley, I W Russell


Effects of boron treatments on partially decayed oak and pitch pine heartwood
1996 - IRG/WP 96-30106
This paper reports results of borate based preservative treatment and leaching experiments on partially decayed oak and pitch pine heartwood. Previous experiments have shown little damage is caused to sound timber of these types when treated with Polybor and Boracol 20 preservatives. This experiment was carried out to assess the suitability of selected borate based preservatives for use in histori...
S McCutcheon, G M Smith, J W Palfreyman, P Durrant


Examination of the Pilodyn as a non-destructive test method for detecting decay in CCA treated eucalypt poles
1982 - IRG/WP 2177
Below groundline condition of 274 CCA treated eucalypt poles comprising 13 different species was examined using 6 and 12 Joule Pilodyn units with 2 and 2.5 mm diameter pins. The data obtained was used to calculate regressions of density on pin penetration. A decrease in density was accompanied by an increase in pin penetration. The best correlation was found using the 6 Joule, 60 x 2.5 mm² diamet...
L E Leightley


Role of cell wall structure in soft rot decay of bamboo
1995 - IRG/WP 95-10133
Models of soft rot hyphal penetration of bamboo cell walls are proposed. Soft rot hyphae show an interesting capability of penetrating the bamboo cell wall in different forms; typical longitudinal penetrating hyphae and tangentially orientated penetrating hyphae. The second form of penetration was found to be different from that normally associated with wood cell walls. The differences can be attr...
O Sulaiman, R J Murphy


Initial microbial colonisation of CCA-treated, creosote-treated and untreated Pinus sylvestris L. blocks in seawater
1996 - IRG/WP 96-10171
CCA-treated, creosote-treated and untreated Pinus sylvestris sample blocks were immersed in a seawater through-flow system for periods of between 1 and 265 hours. Samples were fixed immediately on removal and examined both qualitatively and quantitatively using the scanning electron microscope. This study of primary microbial colonisation showed differences between treatments in the diversity of m...
K Sturgess, A J Pitman


Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki


Modelling the control of decay in freshly felled pine poles
1997 - IRG/WP 97-10206
In a recent study investigating control of decay in freshly felled pine utility poles, it became apparent that the efficacy of different treatment methods was strongly related to the size of the material being treated. A topical application of 5% w/v disodium octaborate tetrahydrate (DOT), brush applied to the cut surfaces of logs with otherwise intact bark was just as effective at excluding white...
M W Schoeman, W Van der Werf, J F Webber, D J Dickinson


Investigation of microwave as a means of eradicating dry rot attack in buildings
1992 - IRG/WP 92-1545
A microwave-apparatus developed for treatment of building-structures infested by dry rot was tested in the laboratory. The test-conditions simulated treatment of either infested timber or infested brickwork. Sawdust samples, both wet and dry, infested by viable mycelium of Serpula lacrymans were packed in glass-tubes. The tubes were then placed in the middle of either 20 cm thick wooden beams or 3...
C Kjerulf-Jensen, A P Koch


The performance of CCA treatment in bamboo against decay fungi
1993 - IRG/WP 93-30027
Samples of culm wall material from young (< 6 month age) and mature (> 3 years age) culms of the bamboo, Phyllostachys virideglaucescens were treated to equivalent% w/w retentions of a CCA preservative. After fixation and leaching the treated samples were exposed to decay by Chaetomium globosum FPRL S70K, Coriolus versicolor FPRL 28A and Coniophora puteana FPRL 11E. Thin section samples of u...
O Sulaiman, R J Murphy


Effectiveness of Busan 30 treated birch blocks in a soil medium
1987 - IRG/WP 3409
TCMTB based formulation has been anticipated for use in dip-diffusion treatment in Papua New Guinea to replace BFCA Wood preservative. One such formulation is the Penacide (TCMTB + MBT Boron) which is currently being tested against fungi and insects. Accelerated laboratory test in soil exposure was employed to test a related formulation (Busan 30) to determine its effectiveness against soil inhabi...
H C Konabe


Movement and persistence of Dazomet and pellected methylisothiocyanate in wrapped Douglas fir and southern pine timbers
1991 - IRG/WP 1496
The movement and persistence of Dazomet (tetrahydro-3,5-dimethyl-2 H-1,3,5 thiadiazine-6-thione) and pelleted methylisothiocyanate (MIT) was evaluated in wrapped Douglas-fir and Southern Pine timbers. MIT pellets did not impart a fungistatic effect to any of the timbers. Failure of MIT was probably due to loss of MIT from pellets prior to application. Fungistatic effect of Dazomet was consistently...
T L Highley


Studies on the fungicidal effectiveness of a petrol derived product as a creosote alternative
1986 - IRG/WP 3384
This work, appears first because of the necessity to find out a profitable use for a residual product of the petrol pyrolisis, and second, because the lack of high natural durability wood used until now-a-days to build posts and sleepers in creosote lacking countries. Our main objective was pointed to the characterization of this new product and to find out the effectiveness against the wood-destr...
A M Navarrete, M T De Troya.


Development on Damage Functions of Wood Decay for Building Envelope Design
2005 - IRG/WP 05-10556
For the hygrothermal analyses of building envelope systems for insulation design, we tried a natural decay test of wetted wood specimens without any inoculation of fungi. Three principal experimental types: under steady-state conditions (Experiment A), at a cyclic water dripping under Non-steady conditions (Experiment B) and at a cyclic water dipping under-steady conditions (Experiment C), were ca...
H Suzuki, Y Kitadani, K Suzuki, A Iwamae, H Nagai


A Soil Bed Test of the Effect of CCA Penetration on the Performance of Hem-fir Plywood
2004 - IRG/WP 04-30332
An accelerated decay test was set up to compare the performance of CCA-treated Western hemlock/amabilis fir plywood treated to meet the preserved wood foundation (PWF) retention standard with various patterns of preservative penetration. Short lengths of treated plywood and comparable untreated material were installed in a soil bed. After eleven years of exposure, the CCA treatments were all sou...
P I Morris, J K Ingram


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson