On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Wood decay in Danish buildings
1985 - IRG/WP 1261
At Technological Institute identification of fungi and advisory activity concerning repair of damages has taken place since 1935. Statistical analyses based on material from 1982 and 1983 are compared to earlier investigations worked out by L. Harmsen. The material shows that building traditions influence the diversity and frequency of fungal species. Many fungal damages in the last decade have sh...
A P Koch


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Methods of assessing decay in poles in service with the Pilodyn wood tester
1978 - IRG/WP 2107 A
H Friis-Hansen


Report on biological control of decay in poles
1977 - IRG/WP 149
The following its a brief report on a preliminary experiment carried out for the United Kingdoms Midland Electricity Board during 1974-1975 to establish, under laboratory conditions, the potential controlling value of some non-decay fungi against Lentinus lepideus. Lentinus lepideus has been confirmed to be the commonest Basidiomycete causing decay in poles in the Boards area....
T A Oxley


Characterization of glycopeptide from white-, brown- and soft rot fungi
2002 - IRG/WP 02-10424
Extracellular low-molecular-weight substances that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radicals have been isolated from wood degrading cultures of white-rot, brown-rot, and soft-rot fungi. They contained protein, neutral carbohydrate, and Fe(II). These substances were glycosylated (glycated) peptides and suggested to form Amadori product (ketoamine). The...
H Tanaka, S Itakura, A Enoki


Soil chemistry and wood decay
1978 - IRG/WP 2109
Soil is a most complex biological, chemical and physical material; its study is effectively a separate branch of science but almost entirely in relation to ist ability to grow plants - this paper is intendet just to note some known facets that might have relevance to the decay of wood and the performance of wood preservatives....
E A Hilditch


Studies on the preservation of structrual plywood - Part 1: Decay resistance of structural plywood
1974 - IRG/WP 238
The weight loss and the decreases in the compression strength and in the modulus of elasticity were measured to determine the decay resistance of structural plywood (lauan). Test pieces (50x25xA mm³) were exposed to the wood destroying fungi (Coriolus versicolor and Coriolellus palustris) for 2-3 or 2-4 months. After exposure, the measurement of the compression strength was carried out on the pie...
K Minami, Y Kenjo, S Sugiyama


Protection of Ochroma pyramidale from fungal decay with N,N-napthaloylhyroxylamine
1998 - IRG/WP 98-30182
Fungal decay of wood in service results in billions of dollars (U.S.) in losses annually. Recent environmental restrictions, both U.S. and international, are limiting and eliminating the use of broad-spectrum, heavy metal biocides for wood preservation. Restrictions result primarily from problems with disposal. New wood preservatives need to be developed and tested which specifically target key el...
F Green III, T L Highley


Effect of asphyxiation on wood decay fungi treated with argon and nitrogen gas
2002 - IRG/WP 02-10452
The effects of low-oxygen conditions, achieved with either argon or nitrogen gas, on the viability of wood decay fungi Coniophora puteana, Antrodia vaillantii and Trametes versicolor, cultivated on PDA medium and infected wood samples, were examined. The fungal cultures were exposed to low oxygen concentration (below 10 ppm) for one to five weeks in hermetically sealed vessels. Anoxic treatment di...
C Tavzes, F Pohleven, M Janisek, R J Koestler


The secondary treatment of creosoted electricity poles with fused boron rods
1988 - IRG/WP 3485
After preliminary trials selected poles were treated at the groundline with fused boron rods. Early samplings showed that movement was slow in the dry heartwood but after six years the distributions obtained indicate that the system has merit for the treatment of the heartwood of poles in service....
D J Dickinson, P I Morris, B Calver


Effect of soft-rot decay on the static bending strength of wood
1991 - IRG/WP 2361
In this study, a modified static bending test has been developed as a method for measuring soft-rot decay in soil bed studies. A good correlation was found between the strength loss of the southern pine test specimens and extent of decay. This data suggests that it may be possible to develop a dynamic test based on stress relaxation that is more sensitive than static bending....
D D Nicholas, J A Wilson, R C Vasishth


Use of fluorescent-coupled lectins as probes for studying fungal degradation of wood
1986 - IRG/WP 1288
The ability of the fluorescent-coupled lectins wheat germ agglutin (WGA) and Concanavalin A (Con A) to react with selected Basidiomycetes, Ascomycetes, and Fungi Imperfecti was evaluated using pure cultures of 35 fungi grown on malt extract agar. WGA, which binds specifically to the n-acetylglucosamine residues found in fungal chitin, reacted with nearly all hyaline fungal structures but did not r...
J J Morrell, R L Krahmer, L C Lin


Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer


A field test with anti-sapstain chemicals on sawn pine timber in Finland
1986 - IRG/WP 3368
Fourteen formulations, each in two concentrations, were tested for effectiveness against sapstain, mould and decay on Scots pine (Pinus sylvestris L.) in a field test in South-Finland. The trial was commenced in June 1985 and finished in October 1985. During the test the boards were infected mainly by mould fungi. In kiln dried boards the protective effects of nine and in green boards of four trea...
L Paajanen


Climate indices at work: Above ground decay L-joint tests (EN 330 and AWPA E9) at two sites 12000 km apart and with Scheffer climate indices of 60-65 and 300-330
1996 - IRG/WP 96-20095
Matched sets of Scots pine sapwood (Pinus sylvestris) L-joints were exposed above ground at two field sites for approximately five years. One site, at Garston, Watford, UK has a climate index between 60 and 65 while the other, close to Hilo, HI, USA has an index between 300 and 330. The joints were treated with a range of organic solvent treatments applied either by three minute dip immersion or b...
A F Preston, K J Archer, D M Roberts, J K Carey, A F Bravery


Investigation of the fixation in wood of chromated zinc chloride and copperised chromated zinc chloride preservatives
1976 - IRG/WP 372
A biological method of evaluating the extent to which CZC and CCZC preparations are retained in wood in terms of the potential protection which they afford against destruction by Merulius lacrymans (dry rot) is given. CCZC is recommended for protection of wood under moderate leaching conditions, while the use of CZC under such conditions is not recommended....
V N Sozonova, D A Belenkov


Decay, decayed wood and the Shigometer
1980 - IRG/WP 281
A L Shigo


Identification card for Coriolopsis polyzona (Pers.) Ryv
1977 - IRG/WP 161
A Ofosu-Asiedu


The Pilodyn instrument as a non-destructive tester of the shock resistance of wood
1978 - IRG/WP 2107
A new non-destructive shock resistance tester, the PILODYN, has been developed. The instrument measures the fracture surface area created by a constant amount of energy. It operates by shooting a blunt pin into wood by an exact amount of energy. The penetration depth is read on a scale. A wide field of application is open to a non-destructive shock resistance tester such as: 1) assessment of the r...
P Hoffmeyer


Spatial arrangement of lignin peroxidase in pine decayed by Phanerochaete chrysosporium and Fomitopsis pinicola
1988 - IRG/WP 1343
By applying immunoelectronmicroscopic methods, lignin peroxidase of the white rot fungus Phanerochaete chrysosporium has been localized in the cytoplasm of hyphae, close to the plasmalemma and on the plasmalemma. Infiltration of wood specimen with culture filtrates, concentrated 300-fold, gave clear information on the penetration of the enzyme into the wood cell wall. Penetration was restricted to...
E Srebotnik, K Messner


Detection of trace organics by ion mobility spectrometry
1990 - IRG/WP 3635
Ion Mobility Spectrometry (IMS) is a time of flight analytical technique that is suited to detect chemicals in the low parts per billion range. Some of the advantages of IMS are: operation at atmospheric pressure, fast response time (0.1-10 sec), and the ability to characterize individual chemical species in complex matrices without any prior sample preparation. In this paper, the utility of IMS i...
A H Lawrence


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


Inspection of tropical hardwood window frames in Nigeria for decay presence
1987 - IRG/WP 2294
A method of in situ inspection of hardwood window frames for expression of decay is discussed in this paper. The results show that about 6% of the frames inspected or 23% of the volume of wood in all the frames sampled in buildings erected between 1920 and 1984, exhibited evidence of advanced decay. Protection by the length of the eaves, species of the framing timber used, length of exposure to se...
M A Odeyinde, M A Amakiri, E B Lucas, J O Eyenike, S Akanni


Ground contact performance of wood treated by the MSU process
1990 - IRG/WP 3609
Environmental concerns have prompted a renewed interest in accelerated fixation schemes for CCA-treated wood. Results from stake tests of southern pine (Pinus sp.) treated using a conventional Bethell cycle are compared with matched stakes treated using the MSU Process. The effects of adding boric acid to the preservative formulation are also discussed. Differences among test plots are discussed....