Effect of sterilization method on germination of spores of wood decay fungi observed by contact agar block method
1978 - IRG/WP 2117
Previous studies of germination of spores of wood decay fungi on wood have generally concluded that method of wood sterilization has little significant effect on germination response. This study expands the numbers of test fungi as well as number of sterilization methods employed to determine the influence of sterilization method on spore germination response of decay fungi. Germination was assess...
E L Schmidt, D W French


A laboratory soil-block decay evaluation of plywoods edge-treated with preservatives
1982 - IRG/WP 2174
Preservative-treated plywood used under conditions or severe decay hazard frequently has its original, or cut edges, protected by the application of a field-cut preservative. This study uses a laboratory test method to compare the efficacy of four commercial preservative treatments against two commonly occurring brown-rot fungi. The results are not meant to indicate the service life of such treate...
R S Smith, A Byrne


Final draft of a monographic card for Pole Fungus A, L Harmsen, Rigidoporus vitreus (Fr.) Donk according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 178
L Harmsen


The influence of building design on wood decay
2000 - IRG/WP 00-10339
The cheapest and most effective way to prevent wood decay is to KEEP THE WOOD DRY! You and I know that, but we often forget and attempt a preservative solution to a problem better solved with good design and construction. It's also the answer to a frequently missed exam question in my Architecture class. Just as caulking is a poor substitute for proper design, so preservative treatment sh...
W W Wilcox


A short note on the subject of pretreatment decay in wood
1984 - IRG/WP 1245
The paper reviews five national standards for wood utility poles and some literature that concerns the problems of pretreatment decay. Finally it is proposed to form a new sub-group to study that problem....
J A Taylor


Monographic information on Serpula (Merulius) lacrymans (Schum. ex Fr.) S. F. Gray, according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 170
J Segmüller, O Wälchli


Non-enzymatic Gloeophyllum trabeum decay mechanisms: Further study
2001 - IRG/WP 01-10395
Information will be presented on the mechanisms involved in, and potential application of, non-enzymatic wood decay by brown rot decay fungi. Specifically, the hypothesized role of low molecular weight phenolate derivatives will be discussed in relation to non-enzymatic degradation of wood. The mechanism of binding of iron by cellulose, and binding and reduction of iron by fungal derivatives and m...
B Goodell, J Jellison


Combined effects of the treatment of wood with formaldehyde
1978 - IRG/WP 3117
Treatment of fibrous materials with reagents in a vapor phase is neither new nor unique. Numerous examples exist in literature of vapor phase experiments on cellulose fibers and fabrics, and on wood. For many years the textile research and industry have used vapor phase processes for the treatment of textiles. The chemical modification of cellulose is based on different types of reactions e.g. est...
M Stevens, J Schalck


The potential of 2-deoxy-D-glucose as an active ingredient in wood preservation
1999 - IRG/WP 99-30205
2-deoxy-D-glucose (2-DOG) is a potential active ingredient against wood decaying fungi. When dissolved in water, it can be used in pressure treatment of wood. Thereby the wood is protected from attack by wood decaying fungi. A concentration of 1.5% (mean retention 9.7 kg/cubic meter sap-wood) is adequate for brown rot fungi, and 3% (mean retention 19.5 kg/cubic meter sapwood) will also provide protection against white rot fungi. 2-DOG is easily soluble in water, and is therefore easily leached from the wood upon completion of the preservation process. Different types of fixa-tion methods have been tried and evaluated. It is possible to produce 2-DOG by the hydrolysis of chitin, a constituent of the exterior skeleton of shellfish and insects. There is a potential for exploita-tion of this waste product provided by the crab and shrimp industry. The yield of 1 kg of fresh shrimp is 75 g of 2-DOG.
O V Frederiksen, A P Koch


Evaluation of the decay caused by Chaetomium globosum Kunze, in the course of time
1987 - IRG/WP 2288
The main research done on soft rot has been directed to determining, by microscopic study, the different stages of penetration into the wood of the fungi that cause it. On the basis of the information furnished by this research, in this work we have tried to quantify its effect, by evaluating the weight loss caused by Chaetomium globosum Kunce in wood of Pinus sylvestris L. and Fagus sylvatica L. ...
M T De Troya, A M Navarrete


Soil-bed studies
1982 - IRG/WP 2181
This paper discusses factors affecting the design and use of a soil-bed....
P Vinden, J G Savory, D J Dickinson, J F Levy


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


A deflection test for monitoring decay in miniature beams
1986 - IRG/WP 2269
A laboratory apparatus for assessing decay in small stakes is described. It involves the measurement of deflection in a static bending apparatus using a displacement transducer linked to a microcomputer. Measurements are non-destructive, rapid, accurate and automatic and decay can be assessed repeatedly over long time periods....
S M Gray


Translation of CEN Letter to Mr R Cockcroft dated 24 November 1980
1980 - IRG/WP 2147
G Castan


The performance of glue laminated railway ties after 40 years of service in the main line track
1989 - IRG/WP 2325
Two series of horizontally glue laminated ties made of a softwood body and topped with a hardwood lamination were creosoted and installed in 1947 in a tangent and a curved main line track. The tests are now 40 years old and the excellent condition of the ties of these two series suggest that a service life of 50-60 years can be expected....
J P Hösli, E E Doyle, C P Bird, T Lee


The use of C CP/MAS NMR in the chemical identification of decayed and undecayed, tropical timber species
1984 - IRG/WP 1224
13C CP/MAS NMR was found to be an extremely powerful tool for elucidating the chemical composition of Eucalyptus maculata, Pinus elliottii and Alstonia scholaris. The differences in lignin composition were different for each timber and discussed in relation to decay caused by soft-rot and white rot fungi. In particular the presence of syringyl and guaiacyl lignin types are discussed.
L E Leightley


Étude in vitro de la colonisation et de la dégradation structural du bois de hêtre par Coriolus versicolor (L.) Quélet
1976 - IRG/WP 158
L'attaque du bois de Hêtre par Coriolus versicolor (L.) Quélet, agent de pourriture fibreuse blanche est étudiée après des périodes d'exposition à ce champignon variant de 15 jours à trois mois. L'observation des premiers stades, c'est à dire de la colonisation du bois par les filaments de champignon est faite en microscopie optique, puis au fur et à m...
D Dirol


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


Effects of the anaerobic wood decay bacterium Clostridium xylanolyticum on unbleached Pinus and Eucalyptus pulp
1991 - IRG/WP 1506
Clostridium xylanolyticum has been shown to produce extracellular enzymes capable of degrading wood. The present work was conducted to quantify growth on various lignocellulosic substrates and degradation of pulped wood fibre. In the latter tests Clostridium xylanolyticum was incubated at 35°C under anaerobic conditions in a medium containing 0.2% (w/v) peptone and 4% (w/v) unbleached Pinus and E...
G D Shelver, U Matai, W Van Wyk, A A W Baecker


A baiting technique to monitor the development and control of decay in transmission poles
1981 - IRG/WP 2149
P I Morris, D J Dickinson


Micromorphology of the decay caused by Chondrostereum purpureum (Pers.:Fr.) Pouzar and Flammulina velutipes (Curt.:Fr.) Singer
1988 - IRG/WP 1358
Two basidiomycetes, Chondrostereum purpureum and Flammulina velutipes, form typical soft rot cavities in hardwoods and softwoods. Cavity formation is prececed by T-branching or bending of hyphae penetrating the wood cell walls. The two fungi also cause erosion of the wood cell walls....
T Nilsson, G F Daniel


Natural durability studies in an accelerated field simulator - A novel approach
1983 - IRG/WP 2197
A study of the natural durability of untreated timbers to both decay and termite attack is described. The work illustrates the versatility of the Accelerated Field Simulator as a novel approach to biodeterioration research....
G C Johnson, J D Thornton, J W Creffield, C D Howick


Monographic information on Serpula (Poria) incrassata according to the "Model Questionnaire for preparation of monographic cards for wood-destroying fungi"
1980 - IRG/WP 160
J G Palmer, W E Eslyn


Soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, in ground contact in Australia
1986 - IRG/WP 1280
The performance against soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, was examined after 20 months in ground contact at Pennant Hills, Australia. The results indicate that between these species soft rot decay is excluded by different levels of CCA salt suggesting that the threshold level for exclusion of soft rot in these hardwoods is a function of anatomical structure/ultrastru...
R S Johnstone


Decay resistance of resin treated wood
1999 - IRG/WP 99-30206
Selected natural resin systems were evaluated for their potential as wood protecting agents according to standard test procedures. As indicated by the European standard EN 599 both a Basidiomycete test according to EN 113 and a ENV 807 soil bed test were carried out. Six resin treatments were tested using 3 concentration or treatment levels. Using the biocidal activity criteria as usually applied ...
J Van Acker, A J Nurmi, S M Gray, H Militz, C Hill, H Kokko, A O Rapp