IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3311 documents. Displaying 25 entries per page.


Effects of heat treatment on water repellence and anti-swelling efficiency of beech wood
2002 - IRG/WP 02-40223
The heating of solid wood to higher temperatures is the simplest and the cheapest means for stabilizing its dimensions. For the investigation of the effect of thermal treatment on water repellency effectiveness and anti-swelling efficiency of beech wood (Fagus orientalis Lipsky), air-seasoned samples of beech wood were heated in presence of air at temperatures of 130 C, 150 C, 180 C and 200 C for ...
S Yildiz


Acceleration of the fixation of chromated wood preservatives by UV-radiation
1989 - IRG/WP 3544
Preliminary laboratory tests demonstrated that the fixation of chromated water-borne wood preservatives may be accelerated by UV-radiation. The degree of fixation depends on the intensity of radiation and the prevailing temperature. Three hours radiation at 20°C in a device for artificial weathering diminished the leaching of chromium to 43% and of copper to 23% compared to not-radiated samples. ...
H M Illner, H Willeitner, K Brandt


A Preliminary Report on the Properties of Engineered Wood Composite Panels Treated with Copper Naphthenate
2005 - IRG/WP 05-40294
This paper reports on our preliminary investigation of the properties of randomly oriented strandboard which had waterborne or powdered copper naphthenate (CuN) incorporated into the board during manufacture. When compared to zinc borate-treated controls (ZnB), the mechanical properties of strandboard (MOR, MOE, work-to-maximum load, internal bond strength) were not adversely affected by treatmen...
J W Kirkpatrick, H M Barnes


Soil-bed studies. Part 2: The efficacy of wood preservative
1983 - IRG/WP 2205
Various methods of decay assessment were investigated. Three stages or phases of decay were identified which could be used to describe the efficacy of a preservative system or virulence of a soil-bed testing medium. These included the lag, decay, and senescent phase. Premature senescence could arise if wood samples became waterlogged. It was concluded that time to failure was unsuitable as a metho...
P Vinden, J F Levy, D J Dickinson


Anatomical Characteristics to the Distribution of Water-borne Copper Wood Preservatives in Wood
2004 - IRG/WP 04-40277
The objective of this study was to understand the micro-distribution of a copper-based preservative in wood in connection with anatomical morphology and to consider the fixation of copper in wood. Bulk specimens and semi-ultra thin sections (0.5µm) obtained from Japanese cedar were treated with a CuAz preservative solution. After fixation, SEM-EDXA was used to investigate the micro-distribution...
H Matsunaga, J Matsumura, K Oda


Moisture condition in treated wood exposed outdoors. A progress report
1989 - IRG/WP 3533
Wood treated with water-borne preservatives, mainly CCA (copper/chromium/arsenic), CCB (copper/chrome/boron) or CC (copper/chrome) is often said among users in Sweden to absorb more water than untreated wood. In laboratory tests this statement has not been confirmed but no field tests have been carried out in Sweden to study this phenomenon. In 1986 a project was started to compare water absorptio...
M-L Edlund, C E Sundman


Durability of surface preserved wood particle boards submitted to atmospherical influence
1995 - IRG/WP 95-40039
The worldwide problem of the continuously growing deficit of high quality natural wood material has caused the attempts of many research workers to find effective composites such as wood particle boards (WPBs) for replacing the massive wood for constructive purposes, depending on where the boards are exploited - in the open or under a shed, they are submitted to various climatic factors such as he...
L Valcheva


Determination of fixation properties by bioassays - A proposal for the assessment of safety indexes in wood protection
1990 - IRG/WP 3566
In the determination of environmental effects of chemicals tests with fishes, daphnia and algae have proved to be practicable. With respect to wood protection such bioassays are suitable to control effects of treated timber against aquatic organisms. By using the fish-acute-toxicity-test the development of a laboratory test method is described for the checking of the fixation rate of a copper-chro...
H-W Wegen


Fungal Stain Development in Canadian Hardwood Logs
2004 - IRG/WP 04-10505
In most sawmills around the world, trees are harvested into logs and stored in the forest or in a log yard for a period of time before being sawn into lumber. These logs may be attacked by various pigmented fungi, which results in staining of the wood. Since hardwood species are used to a great extent in furniture manufacturing and in the making of other valuable wood products, the reduction of wo...
Dian-Qing Yang, M-C Bisson


Effect of soil parameters on biocide depletion: laboratory and field studies of water- and emulsion-borne preservatives
2000 - IRG/WP 00-30234
Two field test sites with different soils were selected. Soil analysis showed that the soil at the two sites had considerable texture, base saturation, acidity, and cation exchange capacity differences. Five sets of field stakes were treated as follows: three with water-borne CCA to about 0.4 pcf (6.4 kgm-3) retention, one with 0.75% DDAC, and one with 0.75% DDAC:0.25% chlorothalonil. The last two...
T Schultz, D D Nicholas, D E Pettry, M G Kim


Effectiveness of copper/chromium salts as wood preservatives against Limnoria tripunctata Menzies in laboratory tests
1977 - IRG/WP 431
During the last joint meeting of IRG and COIPM a co-operative programme of tests with copper/chromium salts as wood preservatives against marine borers was discussed and agreed. In this connection the results of a laboratory test in the BAM with Limnoria tripunctata Menzies will be of interest. But as the respective paper is written in German (H. Kühne; G. Becker: Laboratoriumsversuche über die ...
H Kühne


Influence of pre-swelling conditioning on swellometer results for CCA and water repellent additive treated wood
1997 - IRG/WP 97-20125
The pre-test moisture content and conditioning history of wafers cut from wood treated with CCA and an emulsion water repellent additive can dramatically influence swelling curves generated using a standard swellometer apparatus. The rate of water uptake and swelling increased significantly as wafers were dried to lower moisture contents prior to immersion swelling. The pre-swelling conditioning h...
A R Zahora


Evaluation of the corrosivity of the treated wood - Laboratory vs field test methodologies
2000 - IRG/WP 00-20211
The corrosivity of treated wood to fasteners has been evaluated using laboratory test procedures, including AWPA Standard E12-94. The standard method was modified in order to allow detailed study of commercial metal fasteners in terms of sample types, installation configuration and exposure conditions. Parallel field tests were also performed. The experimental results generated from these tests su...
L Jin, A F Preston


Evaluating possibilities of leaching of deltamethrin and TCMTB (insecticides and fungicide for protecting wood) by rain water or by soaking in water
1988 - IRG/WP 3464
Deltamethrin and TCMTB have been subjected to several field leaching tests on freshly fallen trees and in the laboratory, using standard EN 84. All the trials gave the same results and confirm that Deltamethrin and TCMTB are not washed out after they have been allowed to penetrate the trunk surface properly. According to the EN 84 standard, less than 1% Deltamethrin and less than 1.7% TCMTB were r...
J S Duguet, V Dartigues


Improvement of some technological and biological properties of poplar wood by impregnation with aqueous macromolecular compounds
1992 - IRG/WP 92-3721
Poplars (Populus spp) belong to the most important tree species in afforestation programs of the Netherlands. Due to their rapid growth, the wood quality is usually low. Therefore, studies were performed to elucidate whether some technological properties and the resistance against fungal attack could be improved by impregnation with water-soluble resins. The results showed that swelling and shrink...
R D Peek, H Militz, J J Kettenis


Properties of hot oil treated wood and the possible chemical reactions between wood and soybean oil during heat treatment
2005 - IRG/WP 05-40304
Thermal treatment with hot oil as the heating media based on the original idea from oil-heat treatment in Germany was investigated. The treatment was mainly carried out at 200ºC and 220ºC for 2 hours and 4 hours, and the wood species were mainly spruce and fir. This paper focuses on the difference between soybean oil and palm oil and the possible chemical reactions between wood and soybean oil. ...
Jieying Wang, P A Cooper


The degradation of wood surfaces by water
1984 - IRG/WP 3289
Thin radial/longitudinal sections (~100 µ) of Scots Pine (Pinus sylvestris) and lime (Tilia vulgaris), were exposed to deionised water over the temperature range 25-65°C. Losses in wet tensile strength and toughness occurred rapidly at temperatures from about 50°C upwards. After about 2 months' exposure pine lost some 10-30% of its tensile strength and 20-60% of its toughness. For lime...
W B Banks, P D Evans


Soft rot - Soil burial - Tests. Influence of the water content of the soil on wood decay
1972 - IRG/WP 212
The decay of wood samples buried in the soil is influenced by various factors. Decisive are the water content, the content of organic substances, pH-value content of mineral nutritive substances etc. of the soil. For the tests, carried out by the EMPA until now, it was always started with a water content of 35%, refered to the dry weight of the EMPA-soil = 75% of its water capacity. In order to in...
O Wälchli


Preliminary results of the treatment of wood with chlorosilanes
1981 - IRG/WP 3172
It is clear from the initial data reported here that the treatment of pine sapwood with chlorosilanes under the reaction conditions employed did not significantly reduce the decay by both white rot and brown rot fungi. Only the dichlorosilane compounds showed to possess some protective action against fungal attack. Before drawing conclusions on the application of organosilicon compounds as potenti...
M Stevens


Selective chromate elimination from the storage-drainage-water of a wood impregnation plant
1980 - IRG/WP 3153
With the Enviro-Chrom-Ex process it is possible to eliminate ecologically and economically hexavalent chromium (chromate) from water selectively. The process which is based on the principle of selective ion exchange works with different chromate concentrations and under the presence of other ions, irrespective of the water hardness. The values of water-offtake reach 0.1 mg CrVI at maximum, causing...
O Wälchli, R Ott, R Hugener, E Graf, B Lieberherr


Vertical distribution of fouling and wood-boring organisms in the Trondheimsfjord (Western Norway)
1981 - IRG/WP 476
Results of a detailed study on the vertical distribution of fouling and wood-boring organisme of Trondheimefjord at an interval of 3 m from intertidal level to a depth of 30 m, has been presented, based on data collected from two series of panels, exposed from 15-3-1977 to 15-7-1977 (Series I) and from 22-7-1977 to 13-3-1978 (Series II). The intensity of fouling generally decreased with increasing...
L N Santhakumaran


Marine trials with ammoniacal wood preservatives
1980 - IRG/WP 423
Ammoniacal wood preservatives have been known for many years and are considered among the best water-borne systems for protecting wood in ground contact. In recent years attention has been increasingly focussed on these preservatives because of their ability to penetrate difficult-to-treat species better than most other fixed water-borne preservatives. This is particularly important for example, i...
M A Hulme, D P Ostaff


Risk assessment of energetic valorization of treated wood - wooden recycling
1996 - IRG/WP 96-50072
The most useful method for the valorization of wood wastes and wooden wastes is energetic valorization. In France the percentage of wood treated by antisaptain products is around 30%. Currently with the growing regulation, there is a need for cleaner methods and technology to allow sustainable valorization. The preservatives concerned are common organochlorine compounds (NaPCP) less used nowadays ...
G Deroubaix, P Marchal, G Labat


Analysis of water repellents in wood treated with water borne formulations using FTIR
2000 - IRG/WP 00-40176
The use of aqueous water repellent emulsion formulations has increased significantly in the wood treatment industry. These products are primarily used to enhance the weathering characteristics of wood products treated with water borne preservatives systems used in exterior above ground applications. They are also used in pole treatments to improve climbing characteristics and in low VOC millwork t...
P J Walcheski, L Jin


Effects of two wood preservatives and one water repellant on the settlement of fouling communities in a tropical marine environment
2002 - IRG/WP 02-30293
Observations made on recruitment of fouling organisms on treated panels exposed at an Indian harbour, Krishnapatnam on the east coast (Lat: 13028’ to 13059’ N; Long: 80010’ to 80016’ E) during November, 1997 to October, 1999 are reported and compared with fouling communities on control panels. Wooden panels of Erythrina variegata, Paraserianthus falcataria, Tetrameles nudiflora an...
B Tarakanadha, K S Rao


Previous Page | Next Page