IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3041 documents. Displaying 25 entries per page.


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Preservative absorption response of planks of Anogeissus acuminata for plank-built catamarans
2002 - IRG/WP 02-40245
Due to shortage of timber coupled with other compelling factors, traditional fishermen along the east coast of India, especially of Andhra Pradesh, of late, are departing from conventional log type wooden catamarans. Instead, they are fabricating catamarans out of timber planks of hard woods and utilizing thermocol for buoyancy. Mostly, locally available timber of a Combretaceae species, Anogeis...
V Kuppusamy, M V Rao, M Balaji, K Rao


How to determine what is a realistic emission from treated wood - basic reflections
1998 - IRG/WP 98-50105
Emissions from treated wood occur by evaporation and by leaching. Up to date by far more experience exists on leaching tests than on evaporation test. The methods applied will be of interest to give answers to the questions about the quantity of possible emissions. Standardisation on leaching started very early. One of the first attempts to quantify the effect of leaching on the remaining efficacy...
H Willeitner, R-D Peek


Restriction for use and waste management for pressure treated wood - The current situation in Norway
2001 - IRG/WP 01-50175
The Norwegian Environmental Authorities have this winter sent out a draft on restrictions in production and use of heavy metals in preservative treated timber. If it is passed, it will lead to drastic changes in the use of preservatives in Norway from this autumn. The environmental authorities and the preservative industry are both at present discussing waste management for CCA and creosote treate...
F G Evans


Spot-tests for TnBTO and AAC preservatives
1984 - IRG/WP 3279
Nineteen indicator systems were examined as potential alternative spot-tests for preservative penetration in TnBTO- (bis-tributyltin oxide) or AAC- (alkyl ammonium compound) treated wood. Results indicated phenylfluorone as an acceptable alternative to pyrocatechol violet for assessment of TnBTO, and cobaltous thiocyanate or a bromocresol green/quinine sulphate mixture as alternatives to bromophen...
D V Plackett


Waterborne silicones as wood preservatives
1995 - IRG/WP 95-30062
For more than thirty years silicones are used as water repellents for masonry. Their excellent properties make them also attractive for non-mineral substrates like wood. Although it was always thought that silicones are not able to perform on wood, a new type of aqueous silicone materials proofed the opposite: Excellent water repellency and astonishing durability were achieved. This paper describe...
R Hager


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


Wood extractive concentration and sem examination of pretreated southern yellow pine wood chips with blue-stain fungi for mushroom production
2001 - IRG/WP 01-10407
Mushroom-producing white-rotting basidiomycetes either do not colonize or else colonize very poorly on freshly prepared southern yellow pine wood chips. This study evaluates the resinous extractive content of southern yellow pine before and after treatment with colorless mutant blue-stain fungi. The blue-stain fungi penetrate into the sapwood of southern yellow pine and utilize nonstructural resin...
S C Croan, J Haight


The permanence of permethrin in wood preservation
1984 - IRG/WP 3288
The permanence of the synthetic pyrethroid permethrin in treated wood has been assessed for double vacuum and immersion treated Scots pine sapwood and whitewood using a 0.5% m/m solution of the insecticide in a hydrocarbon solvent. It is concluded that for all but the outermost 0.5 mm of the treated battens the distribution of the permethrin is relatively permanent. The outermost 0.5 mm appears vu...
R J Orsler, M W S Stone


The effects of heat treatment on anatomical changes of beech wood
2004 - IRG/WP 04-40284
The effects of heat treatment on anatomical changes of beech wood (Fagus orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2x2x3 cm and than conditioned at 25 °C and 65 % relative humidity for 3 weeks. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and ...
Ü C Yildiz, Z Gerçek, B Serdar, S Yildiz, E D Gezer, E Dizman, A Temiz


Restrictions or environmental taxes as regulatory means - How will they influence the use of pressure treated wood?
1998 - IRG/WP 98-50101-28
In all the Nordic countries except Norway, we have environmental restrictions on the use of pressure treated wood. In Norway we expect environmental taxes on a large number of various products in 1998/99 - probably also pressure treated wood with one or more of the heavy metals copper, chromium and arsenic. The paper will discuss how this can influence the use of pressure treated wood and cause a...
F G Evans


Minutes of WG I, Sub-group 5 Insects in dry wood
1983 - IRG/WP 1220
IRG Secretariat


Soil chemistry and wood decay
1978 - IRG/WP 2109
Soil is a most complex biological, chemical and physical material; its study is effectively a separate branch of science but almost entirely in relation to ist ability to grow plants - this paper is intendet just to note some known facets that might have relevance to the decay of wood and the performance of wood preservatives....
E A Hilditch


Metal carboxylates for wood pest control
1996 - IRG/WP 96-30109
Metal carboxylates have been used as wood preservatives for more than fifty years. Predominantly salts of naphtenic acids have been commercially applied so far. They have water repellent as well as fungicidal and insecticidal properties. In the last years, metal carboxylates of saturated fatty acids were introduced. Fatty acids with 7-10 carbon atoms already have fungicidal activity by themselves....
F Pohleven, M Petric


The preliminary evaluation of selected sulfonium salts for use in wood preservation
1984 - IRG/WP 3278
Five sulfonium compounds, including two sulfonium methosulfates, one sulfonium bromide and two amphoteric sulfonium propanesulfonates, were prepared in crude form and subjected to various biocidal screening tests. A rapid screening test in which treated Pinus radiata pulp pellets were exposed to one of three wood-decaying fungi growing on malt agar revealed that dodecyl dimethyl sulfonium methosul...
D V Plackett


The use of zirconium as an inert fixative for borates in preservation
2001 - IRG/WP 01-30256
Stand-alone borates have been used in internal protected situations as wood preservatives for about 60 years. They have not been deemed acceptable for external situations because of their leaching characteristics. Work carried out to reduce the leachability of borates has been reviewed briefly here, and a specific fixation agent based on zirconium has been tested in standard leaching and decay tes...
J D Lloyd, J L Fogel, A Vizel


Risk assessment and the approval of wood preservatives in the United Kingdom
1995 - IRG/WP 95-50040-23
An approval system operates in the United Kingdom (UK) for the regulation of wood preservatives. The regulatory authority uses a risk assessment approach to evaluate how far the potential for harm to people and the environment from wood preservatives is likely to be realised in practise, and hence the controls required for products to be, used safely. The evaluation for approval purposes also take...
R M Turner


Co-operative research at the Naval Research Laboratory on wood extractives and related compounds as antiborer agents
1977 - IRG/WP 429
J D Bultman, K K Parrish


Information from the Wood Group of COIPM
1982 - IRG/WP 494
A Gambetta


Contribution of wood components on the absorption of copper amine
2000 - IRG/WP 00-30216
The contribution of wood components on the absorption of copper amine was investigated. Holocellulose, lignin and xylan absorbed significant amount of copper. The amount of copper absorbed by cellulose was almost negligible. The removal of extractive also decreased the amount of copper absorption. This study clearly indicates the importance of lignin, hemicellulose in the absorption of copper amin...
D P Kamdem, Jun Zhang


Effect of soft-rot decay on the static bending strength of wood
1991 - IRG/WP 2361
In this study, a modified static bending test has been developed as a method for measuring soft-rot decay in soil bed studies. A good correlation was found between the strength loss of the southern pine test specimens and extent of decay. This data suggests that it may be possible to develop a dynamic test based on stress relaxation that is more sensitive than static bending....
D D Nicholas, J A Wilson, R C Vasishth


Wood preservation research at the Technical University in Zvolen - Slovakia
2004 - IRG/WP 04-10538
Presented paper gives basic information about wood protection in Slovakia and research in the field of wood preservation at the Technical University in Zvolen – the Faculty of Wood Sciences and Technology. The degradation processes in wood and wooden composites caused by fungi, environmental factors and fire, the identification of these processes, the protection of wood with fungicides and ot...
L Reinprecht


Termite barriers for new construction
2000 - IRG/WP 00-10341
Subterranean termite protection in Australia has traditionally relied upon the creation of a zone of poisoned soil under and around the structure to prevent termite attack from the ground. The transition away from persistent soil poisons which began with the withdrawal of cyclodienes in 1995 provided market opportunities for innovative barrier systems. The new barrier systems currently being used ...
D M Ewart


Evaluation of a solid remedial wood preservative containing boron and fluorine
1993 - IRG/WP 93-30022
The fungicidal and termiticidal effectiveness of a new rod form of diffusible remedial wood preservative, containing disodium octaborate tetrahydrate/sodium fluoride and marketed as Polesaver Rod, was evaluated in laboratory tests against three species of basidiomycete fungi (Coniophora olivacea, Pycnoporus coccineus, Perenniporia tephropora) and two species of subterranean termites (Coptotermes a...
K J McCarthy, J W Creffield, L J Cookson, H Greaves


Assessment of wood preservation facilities in Canada
1989 - IRG/WP 3557
This document sets out an assessment procedure for the current status of the wood preservation industry in Canada in relation to the Technical Recommendations (TR) documents for the Design and Operation of Wood Preservation Facilities published by the Government of Canada in April 1988. A questionnaire has been prepared in consultation with industry and the Canadian Institute of Treated Wood. An a...
G Das, V N P Mathur


Previous Page | Next Page