IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3322 documents. Displaying 25 entries per page.


Sapwood staining fungi
1974 - IRG/WP 125
The compilation is based on the available literature and on research results from the Royal College of Forestry, Stockholm but I am aware that there are great gaps in it and so it must be looked upon as a basis for collecting more information about these fungi. The review in the presented form needs an explanation. Preparing this review, the presented schedule was set up to facilitate summarisatio...
A Käärik


Estimation of effective diffusion path lengths in wood by swelling studies
1989 - IRG/WP 3524
The effective average distance that a solute must diffuse to penetrate the cell wall matrix following pressure treatment is estimated from the rate of swelling of wood, vacuum treated with water. It is assumed that the diffusion paths are similar for water and a solute such as a wood preservative component. Since bound water diffusion coefficients for water in wood have been estimated by others, t...
P A Cooper, R Churma


The yeast Pichia sp. As a short-term biological control agent to fungal spoilage of sawn softwood timber
2000 - IRG/WP 00-10362
Previous work has found isolates of the yeast Pichia to be a successful biological control agent toward moulding of fruits. An isolate was tested for the ability to protect sapwood of Pinus sylvestris timber against visual degrade by surface growth of moulds and staining fungi. Successful protection of autoclaved wood sprayed with a mixture of common wood moulding fungi was achieved when the yeast...
C Payne, H J Staines, A Bruce


Changes to New Zealand Timber Treatment Specifications
2004 - IRG/WP 04-20288
Changes have been made to the New Zealand timber treatment specifications in response to frequent incidences of decay in framing timber and doubts about the long-term performance of tributyltin formulations when used in exposed situations. Changes have been made to Hazard Class H1 to allow a level of treatment to provide short to medium decay resistance to framing which would protect it, should l...
M E Hedley


Testing method for the treatability of wood
1994 - IRG/WP 94-40031
In order to test and classify the treatability of wood species in pressure treatment processes with water-based solutions, a laboratory method was developed which allows the testing of small samples and limited sections of a stem, e.g. sapwood. The penetration of different liquids was determined separately concerning the three anatomical directions of wood. The common parameters for pressure impre...
A O Rapp, R-D Peek


Waste management of wood products in life cycle assessment
2000 - IRG/WP 00-50154
Within the framework of the European project LIFE SYS WOOD (contractnr. FAIR CT95-7026) TNO has performed a study on the waste management of wood demolition waste for inclusion in Life Cycle Assessment. In LIFE SYS WOOD one of the main aims was to develop a consistent LCA methodology for wood products. LCA case studies have been performed by partners on wood as raw material, glulam contructions, O...
P Esser, P Eggels, A Voss


Evaluation of New Zealand staining fungi for degradation of radiata pine
1999 - IRG/WP 99-10310
This investigation sought to determine the potential of selected NZ staining fungi to induce weight loss and changes in toughness (impact bending strength) and composition in unseasoned radiata pine sapwood. Furthermore, assays were performed to eveluate enzyme production by staining fungi. Sets of side-matched specimens were inoculated with Ophiostoma floccosum, Sphaeropsis sapinea and O. plurian...
A Schirp, R L Farrell, B Kreber


Laboratory evaluation of fipronil (a phenyl pyrazole) as a candidate termiticide in the protection of wood against the subterranean termite, Coptotermes acinaciformis (Froggatt) Rhinotermitidae
1997 - IRG/WP 97-10225
In this laboratory evaluation, radiata pine wood blocks (50 x 25 x 15 mm3) were impregnated with fipronil (a phenyl pyrazole) at various concentrations (0, 5, 10, 20, 40, 80, 100 and 200 ppm). Half the treated blocks underwent a leaching schedule for 5 days, while the remainder were unleached after treatment. Five replicates per treatment regime were presented to the test termite, Coptotermes acin...
B M Ahmed, J R J French, P Kwint, G Webb


Durability of wood in the area of wood-inhabiting termites in Slovenia
1981 - IRG/WP 1139
This report describes a research dealing with resistance and durability of five different species of wood. The experiment was made in natural conditions in the Slovene area of wood-inhabiting termites. The results of our experimental field, which correspond to the results of the former laboratory experiments, show a very weak resistance of spruce-wood, fir-wood, and beech-wood. They also show thei...
L Kervina


Development of an Australasian protocol for assessment of wood preservatives
1994 - IRG/WP 94-20043
The Australasian Wood Preservation Committee (AWPC) is currently developing a suite of assessment procedures (protocols) for the biocidal efficacy of wood preservatives for approval in Australasia (Australia, New Zealand, Papua New Guinea, Fiji). Protocols are being prepared for the six hazard levels recognised in the relevant standards of member countries and represent the minimum procedures requ...
W D Gardner, H Greaves, M E Hedley, K J McCarthy, J Norton


Wooden windows, avoidance of damage via constructional measures
1990 - IRG/WP 3591
Increasing awareness of the environment reinforces the trend to use wood as a building material for windows in modern building constructions. Wood is a natural building and construction material. Under certain circumstances such as persistent humidity exceeding 30%, wood is rapidly degraded by decay fungi into CO2 and inorganic salts. The cost caused by damage (e.g. replacement of windows) represe...
R Gründlinger, K Messner


Wood preservative development: Have we learnt anything, and where will it take us?
1994 - IRG/WP 94-30054
This paper addresses the disparate approaches to the development and approval of wood preservatives used in a number of regions, and the implications of the test requirements, or lack thereof, on the likely performance of the subsequent treated wood in service. The test methodologies and performance criteria used in various regions will have long term consequences for the future of the wood preser...
A F Preston


Second international symposium on wood preservation "The challenge safety-environment" 8-9 February 1993, Cannes-Mandelieu, France
1993 - IRG/WP 93-50001
Contains the following 34 Documents (IRG/WP 93-50001/1 - IRG/WP 93-50001/34) and 4 abstracts: A methodology for the life-cycle assessment of treated timber products (IRG/WP 93-50001/1) Initial results and observations of a model system to assess the efficacy and environmetal impact of preservative treated wood (IRG/WP 93-50001/2) Borates as wood preservatives - an environmental, health and safe...
Anonymous


Comparative environmental impact analysis of telecommunication utility poles: Treated wood and fibreglass
1999 - IRG/WP 99-50136
This study is aimed at providing the information necessary to assess the main environmental implications of different materials utilised in construction of utility poles. The study was performed on fibreglass and CCA treated poles timber. The work has been carried out by identifying and quantifying energy and materials used and wasted released during the entire life of the pole. The interactions w...
A Cugliandolo, M Onofrio, A Quaglino


Evaluating the potential of modified wood for use in marine environments using a short-term laboratory bioassay
2004 - IRG/WP 04-10525
Chemically modified wood may be an alternative to preservative treated timber for marine structures. In this study a screening laboratory test using the wood-boring isopod crustacean Limnoria quadripunctata was used to assess the durability of chemically modified Pinus sylvestris, Pinus radiata and Picea sp. Most of the treatments used a combination of one of two of types of the resin dimethyloldi...
L M S Borges, S M Cragg, M van der Zee


Information from the COIPM Wood Group
1986 - IRG/WP 4130
The Chairman outlined the progress of the co-operative work "testing the resistance to marine borers of heat shrinkable polyolefin sheathings and of wood treated by vacuum/pressure with polymers (polystyrene)". The first part of the work has been started: the samples of wood wrapped with shrinkable polyolefin sheathings have been prepared and sent to the stations participating. The second part of ...
A Gambetta


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


An evaluation on durability of untreated mining timber support
1997 - IRG/WP 97-20121
Wedge blocks in dimension of 5 x 7 to 8 x 155 cm3 were cut from indigeneous scots pine pitprops. Each of wedge block pairs were numbered and half of them were placed as the test blocks between the steel arches and the strata in a hard coal pit. Controls in laboratory and test wedge blocks in the mine were then sawn into 20 by 20 by 300 mm standard test sticks. Impact bending, static bending and MO...
A Bobat


Soft rot decay of Eucalyptus maculata Hook. in different soils from Queensland, Australia
1980 - IRG/WP 1113
In the present work, different Queensland soils were chosen and their gross effects on the decay of treated and untreated Eucalyptus maculata examined. The soils were also amended with various levels of phosphate to study the response of the wood decay mycota to an increasing supply of this nutrient. Phosphate amendment was chosen because of the wide-scale use of superphosphate on Queensland soils...
L E Leightley, I W Russell


Chromium on the surface of CCA-treated wood
1978 - IRG/WP 386
Chromium in solutions of CCA preservatives is predominantly in the hexavalent state (Cr VI). It is well known that Cr VI is associated with dermatitis and skin ulceration in workers handling chromium containing products and processes. When reduced to the trivalent state, however, chromium is considerably safer. An essential part, therefore, of safety procedures in any chromium - using industry is ...
C R Coggins, P Hiscocks


Comparisons of differences in electrical conductivity and corrosivity between CCA-oxide and CCA-salt treated wood
1981 - IRG/WP 3178
CCA preservatives have served well in many applications throughout the world. In developed areas it is the preservative in demand for clean dry paintable surfaces with long durability. In developing areas it is widely used for economic and logistical reasons. With the current emphasis on energy resources, the CCA preservatives are gaining greater acceptance as a substitute for hydrocarbon-related ...
J A Taylor


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


The volatilization of arsenic on burning copper-chrome-arsenic (CCA) treated wood
1978 - IRG/WP 3111
Small scale burning experiments are described involving copper-chrome-arsenic treated wood. Approximately 20 per cent of the arsenic was volatilised when the wood was burned in air but 60 per cent when burned in an oxygen-enriched atmosphere, this increase is attributed to an increase in combustion temperature. Although a small increase in arsenic evolution was found with an increased concentratio...
A-J Dobbs, C Grant


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


Balance of arsenic and recycling
2002 - IRG/WP 02-50189
Instead of importing considerable quantities of arsenic to Europe, it would be sensible to utilize the arsenic recovered in the recycling process in the manufacture of CCA-wood, in the metallurgical industry as well as in other ways. When copper is also processed into a form easy to utilize, it may be possible to utilize chrome as well. When these developments are implemented, it can be said th...
L Lindroos


Previous Page | Next Page